铸态及激光粉末床熔融AlCoCrFeNi2.1 共晶高熵合金的微观组织及力学性能
收稿日期: 2023-07-14
修回日期: 2023-09-07
网络出版日期: 2023-12-19
基金资助
国家自然科学基金项目(U21A2043);中国科学院青年创新促进会项目(2022191);Bintech-IMR研发计划项目(GYY-JSBU-2022-010)
Microstructure and Mechanical Properties of As-Cast and Laser Powder Bed Fused AlCoCrFeNi2.1 Eutectic High-Entropy Alloy
Received date: 2023-07-14
Revised date: 2023-09-07
Online published: 2023-12-19
Supported by
National Natural Science Foundation of China(U21A2043);Youth Innovation Promotion Association, CAS(2022191);Bintech-IMR Research and Development Program(GYY-JSBU-2022-010)
共晶高熵合金作为一种原位复合材料,因其具有典型的双相层片状组织和良好的流动性能,在组织以及性能调控方面具有巨大的潜力。本工作分别采用真空感应熔炼和激光粉末床熔融(LPBF)制备了AlCoCrFeNi2.1共晶高熵合金,分析了制备工艺对该合金微观组织的影响,并探究了2种样品在室温、500℃和700℃条件下的拉伸性能。结果表明,铸态和LPBF成形样品均呈现出由fcc相和bcc/B2相交替组成的共晶结构。LPBF过程中极高的加热和冷却速率有利于超细均匀共晶层片的形成,并且显著降低了元素偏析。在室温拉伸变形过程中,由于较强的相界强化和双相协同变形特性,使得LPBF成形样品的抗拉强度相较于铸态样品提升了约28%,并获得了10%的良好延伸率。在500℃拉伸条件下,铸态及LPBF成形样品的力学性能均有所下降,这可能归因于合金中剧烈的相变。随拉伸温度升至700℃,铸态样品的力学性能持续降低,而LPBF成形样品表现出更低的抗拉强度和优异的伸长率,其原因是其超细共晶层片在高温条件下易于沿相界发生相对滑动,此时合金的断裂机制以韧性断裂为主。
唐旭 , 张昊 , 薛鹏 , 吴利辉 , 刘峰超 , 朱正旺 , 倪丁瑞 , 肖伯律 , 马宗义 . 铸态及激光粉末床熔融AlCoCrFeNi2.1 共晶高熵合金的微观组织及力学性能[J]. 金属学报, 2024 , 60(11) : 1461 -1470 . DOI: 10.11900/0412.1961.2023.00301
Eutectic high-entropy alloys (EHEAs), as a typical kind of in situ composite, have become a potential alternative for conventional alloys because of their advantages in high-entropy alloys and eutectic alloys. Casting is the conventional preparation method of EHEAs, which is a well-established process with low production efficiency. Laser powder bed fusion (LPBF) is an economical and effective preparation technology that provides a novel way to directly form fine and complex EHEA components. In this study, considering the different application requirements and technical characteristics, AlCoCrFeNi2.1 EHEA was prepared by vacuum induction melting and LPBF, respectively. The effect of the preparation process on the microstructure of the alloy was investigated. In addition, tensile properties of the samples at 20, 500, and 700°C were investigated. Results showed that as-cast and LPBF-formed AlCoCrFeNi2.1 exhibited a eutectic structure composed of alternating fcc and bcc/B2 phases. The high heating and cooling rates during the LPBF process were conducive to the formation of ultrafine and uniform eutectic lamellae, which significantly reduced element segregation. During tensile deformation at room temperature, considering the strong phase boundary strengthening and dual-phase synergistic deformation, the ultimate tensile strength of the LPBF-formed sample was enhanced by about 28% compared with that of the as-cast sample, and a satisfactory elongation of 10% was obtained. At 500°C, the mechanical properties of the as-cast and LPBF-formed samples decreased probably because of the severe phase transformation in the alloy. When the testing temperature was increased to 700°C, the mechanical properties of the as-cast sample continued to decrease. The LPBF-formed samples showed a low tensile strength and superior elongation that should be attributed to the eutectic lamellae sliding along the phase boundaries at high temperatures. Meanwhile, the fracture mechanism of the LPBF-formed sample was dominated by ductile fracture. This work could provide a theoretical basis for the optimization of the microstructure and mechanical properties of EHEAs, thereby promoting their industrial application.
| 1 | Leong Z, Ramamurty U, Tan T L. Microstructural and compositional design principles for Mo-V-Nb-Ti-Zr multi-principal element alloys: A high-throughput first-principles study [J]. Acta Mater., 2021, 213: 116958 |
| 2 | Kies F, Wu X X, Hallstedt B, et al. Enhanced precipitation strengthening of multi-principal element alloys by κ- and B2-phases [J]. Mater. Des., 2021, 198: 109315 |
| 3 | Chen Y J, Chen D K, An X H, et al. Unraveling dual phase transformations in a CrCoNi medium-entropy alloy [J]. Acta Mater., 2021, 215: 117112 |
| 4 | Kautz E J, Schreiber D K, Devaraj A, et al. Mechanistic insights into selective oxidation and corrosion of multi-principal element alloys from high resolution and in situ microscopy [J]. Materialia, 2021, 18: 101148 |
| 5 | Ding J L, Xu H J, Li X, et al. The similarity of elements in multi-principle element alloys based on a new criterion for phase constitution [J]. Mater. Des., 2021, 207: 109849 |
| 6 | Vikram R J, Murty B S, Fabijanic D, et al. Insights into micro-mechanical response and texture of the additively manufactured eutectic high entropy alloy AlCoCrFeNi2.1 [J]. J. Alloys Compd., 2020, 827: 154034 |
| 7 | Das S, Robi P S. Processing and characterization of W23Mo23V17Cr8-Ta7Fe22 and WMoVCrTa refractory high entropy alloys [J]. Int. J. Refract. Met. Hard Mater., 2021, 100: 105656 |
| 8 | Dada M, Popoola P, Mathe N, et al. The comparative study of the microstructural and corrosion behaviour of laser-deposited high entropy alloys [J]. J. Alloys Compd., 2021, 866: 158777 |
| 9 | He J Y, Wang H, Huang H L, et al. A precipitation-hardened high-entropy alloy with outstanding tensile properties [J]. Acta Mater., 2016, 102: 187 |
| 10 | Rogal ?. Semi-solid processing of the CoCrCuFeNi high entropy alloy [J]. Mater. Des., 2017, 119: 406 |
| 11 | Tang Z, Senkov O N, Parish C M, et al. Tensile ductility of an AlCoCrFeNi multi-phase high-entropy alloy through hot isostatic pressing (HIP) and homogenization [J]. Mater. Sci. Eng., 2015, A647: 229 |
| 12 | Wang M L, Cui H Z, Zhao Y Q, et al. A simple strategy for fabrication of an FCC-based complex concentrated alloy coating with hierarchical nanoprecipitates and enhanced mechanical properties [J]. Mater. Des., 2019, 180: 107893 |
| 13 | Huang H L, Wu Y, He J Y, et al. Phase-transformation ductilization of brittle high-entropy alloys via metastability engineering [J]. Adv. Mater., 2017, 29: 1701678 |
| 14 | Li R D, Niu P D, Yuan T C, et al. Selective laser melting of an equiatomic CoCrFeMnNi high-entropy alloy: Processability, non-equilibrium microstructure and mechanical property [J]. J. Alloys Compd., 2018, 746: 125 |
| 15 | Wang Q, Ma Y, Jiang B B, et al. A cuboidal B2 nanoprecipitation-enhanced body-centered-cubic alloy Al0.7CoCrFe2Ni with prominent tensile properties [J]. Scr. Mater., 2016, 120: 85 |
| 16 | Lu Y P, Dong Y, Guo S, et al. A promising new class of high-temperature alloys: Eutectic high-entropy alloys [J]. Sci. Rep., 2014, 4: 6200 |
| 17 | Lu Y P, Dong Y, Jiang H, et al. Promising properties and future trend of eutectic high entropy alloys [J]. Scr. Mater., 2020, 187: 202 |
| 18 | Shi P J, Ren W L, Zheng T X, et al. Enhanced strength-ductility synergy in ultrafine-grained eutectic high-entropy alloys by inheriting microstructural lamellae [J]. Nat. Commun., 2019, 10: 489 |
| 19 | Nassar A, Mullis A, Cochrane R, et al. Rapid solidification of AlCoCrFeNi2.1 high-entropy alloy [J]. J. Alloys Compd., 2022, 900: 163350 |
| 20 | Wang J T, Long Z P, Jiang P F, et al. Microstructure, crystallographic orientation and mechanical property in AlCoCrFeNi2.1 eutectic high-entropy alloy under magnetic field-assisted directional solidification [J]. Metall. Mater. Trans., 2020, 51A: 3504 |
| 21 | Gao X Z, Lu Y P, Zhang B, et al. Microstructural origins of high strength and high ductility in an AlCoCrFeNi2.1 eutectic high-entropy alloy [J]. Acta Mater., 2017, 141: 59 |
| 22 | Shi P J, Zhong Y B, Li Y, et al. Multistage work hardening assisted by multi-type twinning in ultrafine-grained heterostructural eutectic high-entropy alloys [J]. Mater. Today, 2020, 41: 62 |
| 23 | Xiong T, Zheng S J, Pang J Y, et al. High-strength and high-ductility AlCoCrFeNi2.1 eutectic high-entropy alloy achieved via precipitation strengthening in a heterogeneous structure [J]. Scr. Mater., 2020, 186: 336 |
| 24 | Wani I S, Bhattacharjee T, Sheikh S, et al. Tailoring nanostructures and mechanical properties of AlCoCrFeNi2.1 eutectic high entropy alloy using thermo-mechanical processing [J]. Mater. Sci. Eng., 2016, A675: 99 |
| 25 | Brif Y, Thomas M, Todd I. The use of high-entropy alloys in additive manufacturing [J]. Scr. Mater., 2015, 99: 93 |
| 26 | Tang X, Zhang S, Zhang C H, et al. Optimization of laser energy density and scanning strategy on the forming quality of 24CrNiMo low alloy steel manufactured by SLM [J]. Mater. Charact., 2020, 170: 110718 |
| 27 | Guo Y N, Su H J, Zhou H T, et al. Unique strength-ductility balance of AlCoCrFeNi2.1 eutectic high entropy alloy with ultra-fine duplex microstructure prepared by selective laser melting [J]. J. Mater. Sci. Technol., 2022, 111: 298 |
| 28 | He L, Wu S W, Dong A P, et al. Selective laser melting of dense and crack-free AlCoCrFeNi2.1 eutectic high entropy alloy: Synergizing strength and ductility [J]. J. Mater. Sci. Technol., 2022, 117: 133 |
| 29 | Ren J, Zhang Y, Zhao D X, et al. Strong yet ductile nanolamellar high-entropy alloys by additive manufacturing [J]. Nature, 2022, 608: 62 |
| 30 | Chen X S, Kong J, Li J L, et al. High-strength AlCoCrFeNi2.1 eutectic high entropy alloy with ultrafine lamella structure via additive manufacturing [J]. Mater. Sci. Eng., 2022, A854: 143816 |
| 31 | Miao J W, Wang M L, Zhang A J, et al. Tribological properties and wear mechanism of AlCr1.3TiNi2 eutectic high-entropy alloy at elevated temperature [J]. Acta Metall. Sin., 2023, 59: 267 |
| 苗军伟, 王明亮, 张爱军 等. AlCr1.3TiNi2共晶高熵合金的高温摩擦学性能及磨损机理 [J]. 金属学报, 2023, 59: 267 | |
| 32 | Tsai K Y, Tsai M H, Yeh J W. Sluggish diffusion in Co-Cr-Fe-Mn-Ni high-entropy alloys [J]. Acta Mater., 2013, 61: 4887 |
| 33 | Tang X, Zhang H, Zhu Z W, et al. Dual-phase synergistic deformation characteristics and strengthening mechanism of AlCoCrFeNi2.1 eutectic high entropy alloy fabricated by laser powder bed fusion [J]. J. Mater. Sci. Technol., 2023, 150: 75 |
| 34 | Mullins W W, Sekerka R F. Stability of a planar interface during solidification of a dilute binary alloy [J]. J. Appl. Phys., 1964, 35: 444 |
| 35 | Xiong M X, Liew J Y R. Mechanical properties of heat-treated high tensile structural steel at elevated temperatures [J]. Thin-Wall. Struct., 2016, 98: 169 |
| 36 | Qiang X H, Bijlaard F, Kolstein H. Dependence of mechanical properties of high strength steel S690 on elevated temperatures [J]. Constr. Build. Mater., 2012, 30: 73 |
| 37 | Jiang J, Bao W, Peng Z Y, et al. Experimental investigation on mechanical behaviours of TMCP high strength steel [J]. Constr. Build. Mater., 2019, 200: 664 |
| 38 | Shaheen M A, Presswood R, Afshan S. Application of machine learning to predict the mechanical properties of high strength steel at elevated temperatures based on the chemical composition [J]. Structures, 2023, 52: 17 |
| 39 | Yakel H L. Atom distribution in sigma phases. Ⅰ. Fe and Cr atom distribution in a binary sigma phase equilibrated at 1063, 1013 and 923K [J]. Acta Cryst., 1983, 39B: 20 |
| 40 | Chinese Society of Metals High Temperature Materials Branch. China Superalloys Handbook [M]. Beijing: Standards Press of China, 2012: 30 |
| 中国金属学会高温材料分会. 中国高温合金手册 [M]. 北京: 中国标准出版社, 2012: 30 |
/
| 〈 |
|
〉 |