仿生苍耳球冠织构的Ni-Co-Zn超疏水合金涂层及其抗覆冰性能
收稿日期: 2023-02-18
修回日期: 2023-06-02
网络出版日期: 2023-12-18
基金资助
国家自然科学基金项目(51605203);江苏省自然科学基金项目(BK20211344)
Biologically Inspired Xanthium-Like Spherical Texture in Superhydrophobic Ni-Co-Zn Coatings and Their Anti-Icing Performances
Received date: 2023-02-18
Revised date: 2023-06-02
Online published: 2023-12-18
Supported by
National Natural Science Foundation of China(51605203);Natural Science Foundation of Jiangsu Province(BK20211344)
抗覆冰超疏水涂层被广泛应用于航天器羽翼和风电叶扇等领域。受传统工艺的复杂性及氟碳聚合物疏水涂料耐候性差及与基体结合力差等因素影响,严重制约了超疏水涂层的工业化应用。本工作提出在蜂窝多孔Ti上电沉积纳米晶Ni0.12Co0.88 - x Zn x (x = 0~0.36,%,质量分数)合金涂层,经200 ℃时效处理,无需进行二次含F低表面能涂层修饰即可得到超疏水表面。通过SEM、XRD和润湿性实验对其微观形貌及其超疏水性能进行表征。结果表明,在Zn2+浓度50 g/L (x = 0.24)和络合剂(柠檬酸钠(Na3Cit))添加量5 g/L等优化工艺下,涂层晶粒尺寸约为300 nm,且沿多孔Ti的孔道钉扎生长,显著提高了涂层与多孔Ti基体的界面结合能力。润湿性测试结果表明:多孔Ti基体和涂层均为亲水性,但经自然时效14 d后涂层表现出疏水特性,其水滴接触角最大为126.3°,滚动角最低为17.5°。研究了人工时效温度、时间与润湿性之间的关联性,结果表明,经200 ℃人工时效处理后,涂层的超疏水性最佳,水滴接触角高达153.2°且滚动角低于7.8°,这主要归因于该涂层所表现出的自组装行为属于热响应机制,人工时效加速了这一自组装演变进程,大量的ZnO枝晶在纳米晶Ni或Co球壳上择优生长,生成多触角ZnO枝晶的球冠织构,从而具备超疏水结构特征。在-10 ℃冷冻台上进行抗覆冰特性测试,结果表明,经200 ℃人工时效后的涂层试样,其表面水滴完全结冰所需时间最长,为1418 s,比多孔Ti基体的抑冰时间延长近20倍,表现出优异的抗覆冰性能。
关键词: 超疏水; Ni-Co-Zn涂层; 仿生苍耳织构; 抗覆冰特性
周小卫 , 郭云 , 荆雪艳 , 王宇鑫 . 仿生苍耳球冠织构的Ni-Co-Zn超疏水合金涂层及其抗覆冰性能[J]. 金属学报, 2025 , 61(5) : 783 -796 . DOI: 10.11900/0412.1961.2023.00066
Superhydrophobic surfaces are promising anti-icing solutions for industrial applications such as spacecraft wings and wind turbine fans. However, the complexity of traditional processes, poor durability, and low interfacial adhesion between the substrate and fluorocarbon polymer films restrict their widespread use. This study validates a one-step electroplating method for Ni0.12Co0.88 - x Znx (x = 0-0.36, %, mass fraction) coatings on honeycomb porous Ti surfaces, achieving super hydrophobicity without secondary modifications. SEM, XRD, and wettability tests are employed to characterize the surface features and hydrophobic properties. Optimized conditions (50 g/L Zn2+ (x = 0.24) and 5 g/L Na3Cit concentration) resulted in a compact microstructural texture and refined crystal size (300 nm), enhancing the interfacial bonding strength. The as-deposited coating exhibited hydrophobic features, with a maximum water contact angle (WCA) of 126.3° and a sliding angle (SA) of 17.5° after 14 d of natural aging. The textural evolution from Zn nanocrystals to ZnO dendrites with a multi-antenna structure was attributed to this phenomenon. Artificial aging at 100, 200, and 300 oC achieved a superhydrophobic surface in less than 7 d. The sample aged at 200 oC displayed a WCA exceeding 153.2° and an SA below 7.8° due to out-migration of the active ZnO phase and self-assembly evolution, forming xanthium-like spherical structures with nanocrystalline Ni or Co shells and multi-tentacle ZnO dendrites. Comparatively, anti-icing performances were assessed at -10 oC, showing a peach blossom ice shape on all coating samples. The sample aged at 200 oC exhibited an ice-resistant time of over 1418 s, 20 times longer than that of the porous Ti substrate, indicating excellent anti-icing performances. In summary, electroplating Ni-Co-Zn coatings onto porous Ti is a practical solution that meets the evolving requirements for superhydrophobic films in spacecraft shells for anti-icing and warship surfaces for anti-salt spray corrosion.
| 1 | Wang Y X, Guan L L, He Z, et al. Preparation and characterisation of AAO/Ni/Ni superhydrophobic coatings on aluminium alloys [J]. Surf. Eng., 2021, 37: 1246 |
| 2 | Lian F, Zang L P, Xiang Q K, et al. Tribological performance of super hydrophobic titanium alloy surface in artificial seawater [J]. Acta Metall. Sin., 2016, 52: 592 |
| 连 峰, 臧路苹, 项秋宽 等. 超疏水钛合金表面在人工海水中的摩擦性能 [J]. 金属学报, 2016, 52: 592 | |
| 3 | Kang Z X, Guo M J. Fabrication of superhydrophobic Ti surface by thermal oxidation and its anticorrosion property [J]. Acta Metall. Sin., 2013, 49: 629 |
| 康志新, 郭明杰. 热氧化法制备超疏水Ti表面及其耐腐蚀性 [J]. 金属学报, 2013, 49: 629 | |
| 4 | Shibuichi S, Onda T, Satoh N, et al. Super water-repellent surfaces resulting from fractal structure [J]. J. Phys. Chem., 1996, 100: 19512 |
| 5 | Zhou X, Yu S R, Zang J, et al. Colorful nanostructured TiO2 film with superhydrophobic-superhydrophilic switchable wettability and anti-fouling property [J]. J. Alloys Compd., 2019, 798: 257 |
| 6 | Jiang L, Wang R, Yang B, et al. Binary cooperative complementary nanoscale interfacial materials [J]. Pure Appl. Chem., 2000, 72: 73 |
| 7 | Xi W J, Qiao Z M, Zhu C L, et al. The preparation of lotus-like super-hydrophobic copper surfaces by electroplating [J]. Appl. Surf. Sci., 2009, 255: 4836 |
| 8 | Wang G W, Song D, Qiao Y X, et al. Developing super-hydrophobic and corrosion-resistant coating on magnesium-lithium alloy via one-step hydrothermal processing [J]. J. Magnes. Alloy., 2023, 11: 1422 |
| 9 | Shang W, Wu F, Jiang S Q, et al. Effect of hydrophobicity on the corrosion resistance of microarc oxidation/self-assembly/nickel composite coatings on magnesium alloys [J]. J. Mol. Liq., 2021, 330: 115606 |
| 10 | Hashjin R R, Ranjbar Z, Yari H, et al. Tuning up sol-gel process to achieve highly durable superhydrophobic coating [J]. Surf. Interfaces, 2022, 33: 102282 |
| 11 | Liu Q W, Liu G D, Li Z H, et al. Preparation and properties of superhydrophobic surface of magnesium alloy by nanosecond laser [J]. Laser Optoelectron. Prog., 2022, 59: 224 |
| 刘祁文, 刘国东, 李子航 等. 纳秒激光制备镁合金超疏水表面及其性能研究 [J]. 激光与光电子学进展, 2022, 59: 224 | |
| 12 | Liu Y H, Wang Z K. Superhydrophobic porous networks for enhanced droplet shedding [J]. Sci. Rep., 2016, 6: 33817 |
| 13 | She Z X, Li Q, Wang Z W, et al. Highly anticorrosion, self-cleaning superhydrophobic Ni-Co surface fabricated on AZ91D magnesium alloy [J]. Surf. Coat. Technol., 2014, 251: 7 |
| 14 | Peng Y J, Li P C, Li H, et al. Theoretical and experimental study of spontaneous adsorption-induced superhydrophobic Cu coating with hierarchical structures and its anti-scaling property [J]. Surf. Coat. Technol., 2022, 441: 128557 |
| 15 | Wang L, Teng C, Liu J, et al. Robust anti-icing performance of silicon wafer with hollow micro-/nano-structured ZnO [J]. J. Ind. Eng. Chem., 2018, 62: 46 |
| 16 | Xue C R, Dong L H, Liu T, et al. Preparation and anticorrosion performance of superhydrophobic TiO2 nanotube arrays on pure Ti [J]. Corros. Sci. Prot. Technol., 2012, 24: 37 |
| 薛超瑞, 董丽华, 刘 通 等. TiO2纳米阵列超疏水膜的制备及耐腐蚀性能 [J]. 腐蚀科学与防护技术, 2012, 24: 37 | |
| 17 | S?kmen M, Tatl?dil ?, Breen C, et al. A new nano-TiO2 immobilized biodegradable polymer with self-cleaning properties [J]. J. Hazard. Mater., 2011, 187: 199 |
| 18 | Zheng J X, Liu R, Liu D D, et al. Slippery liquid infused porous surfaces with anti-icing performance fabricated by direct laser interference lithography [J]. Prog. Org. Coat., 2023, 175: 107308 |
| 19 | Tian Y, Xu Y C, Zhu Z T, et al. Hierarchical micro/nano/porous structure PVDF/hydrophobic GO photothermal membrane with highly efficient anti-icing/de-icing performance [J]. Colloids Surf., 2022, 651A: 129586 |
| 20 | Guo P, Zheng Y M, Wen M X, et al. Icephobic/anti-icing properties of micro/nanostructured surfaces [J]. Adv. Mater., 2012, 24: 2642 |
| 21 | Bhat R S, Shet V B. Development and characterization of Zn-Ni, Zn-Co and Zn-Ni-Co coatings [J]. Surf. Eng., 2020, 36: 429 |
| 22 | Kapusta-Ko?odziej J, Syrek K, Pawlik A, et al. Effects of anodizing potential and temperature on the growth of anodic TiO2 and its photoelectrochemical properties [J]. Appl. Surf. Sci., 2017, 396: 1119 |
| 23 | Zhou X W, Lu Z, Jing X Y. Pinning growth of TiN films toward porous Ti matrix [J]. J. Mater. Sci, 2022, 57: 18949 |
| 24 | Zhou X W, Wu F J, Ouyang C. Electroless Ni-P alloys on nanoporous ATO surface of Ti substrate [J]. J. Mater. Sci, 2018, 53: 2812 |
| 25 | Abou-Krisha M M, Rageh H M, Matter E A. Electrochemical studies on the electrodeposited Zn-Ni-Co ternary alloy in different media [J]. Surf. Coat. Technol., 2008, 202: 3739 |
| 26 | Kazimierczak H, Ozga P, Socha R P. Investigation of electrochemical co-deposition of zinc and molybdenum from citrate solutions [J]. Electrochim. Acta, 2013, 104: 378 |
| 27 | Eliaz N, Venkatakrishna K, Hegde A C. Electroplating and characterization of Zn-Ni, Zn-Co and Zn-Ni-Co alloys [J]. Surf. Coat. Technol., 2010, 205: 1969 |
| 28 | Dikici T, Culha O, Toparli M. Study of the mechanical and structural properties of Zn-Ni-Co ternary alloy electroplating [J]. J. Coat. Technol. Res., 2010, 7: 787 |
| 29 | Abou-Krisha M M. Influence of Ni2+ concentration and deposition potential on the characterization of thin electrodeposited Zn-Ni-Co coatings [J]. Mater. Chem. Phys., 2011, 125: 621 |
| 30 | Jiang J W, Shen Y Z, Wang Z, et al. Anti/de-icing performance of the one-step electrodeposited superhydrophobic surfaces: Role of surface polarity regulated by hydrocarbon radical length [J]. Chem. Eng. J., 2022, 431: 133276 |
| 31 | Yan Y X, Wang J H, Gao J, et al. TiO2-based slippery liquid-infused porous surfaces with excellent ice-phobic performance [J]. Colloids Surf., 2022, 654A: 129994 |
| 32 | Shen Y Z, Wu Y, Tao J, et al. Spraying fabrication of durable and transparent coatings for anti-icing application: Dynamic water repellency, icing delay, and ice adhesion [J]. ACS Appl. Mater. Interfaces, 2019, 11: 3590 |
| 33 | Khorasani M T, Mirzadeh H, Kermani Z. Wettability of porous polydimethylsiloxane surface: Morphology study [J]. Appl. Surf. Sci., 2005, 242: 339 |
| 34 | Fu Q T, Wu X H, Kumar D, et al. Development of sol-gel icephobic coatings: Effect of surface roughness and surface energy [J]. ACS Appl. Mater. Interfaces, 2014, 6: 20685 |
| 35 | Wei F F, Xiang T F, Liu J, et al. Fabrication of superhydrophobic surface by combination of electrodeposition and hydrothermal synthesis and its self-cleaning and anti-icing properties [J]. Electroplat. Finish., 2022, 41: 502 |
| 魏菲菲, 项腾飞, 刘 剑 等. 电沉积-水热法构建超疏水表面及其自清洁和防结冰性能 [J]. 电镀与涂饰, 2022, 41: 502 | |
| 36 | Huang Y, Sarkar D K, Chen X G. Superhydrophobic nanostructured ZnO thin films on aluminum alloy substrates by electrophoretic deposition process [J]. Appl. Surf. Sci., 2015, 327: 327 |
| 37 | Zhou X W, Guo Y, Lu Z. 3D Xanthium-like of Ni-Co-Zn ternary alloys as superhydrophobic coatings toward porous Ti surface for its anti-icing performances [J]. Surf. Coat. Technol., 2023, 473: 130034 |
| 38 | Wang Z H, Li Y C, Zhang G J. Fabrication of superhydrophobic Zn-Ni coatings on LA43M magnesium alloy [J]. J. Mater. Eng. Perform., 2022, 31: 5333 |
| 39 | Huang L J, Huang H, Guo W, et al. 3D urchin-like of Zn-Ni-Co ternary oxide microspheres as high-performance electrodes for supercapacitors [J]. Electrochim. Acta, 2022, 434: 141317 |
| 40 | Wu C, Cai J J, Zhang Q B, et al. Hierarchical mesoporous zinc-nickel-cobalt ternary oxide nanowire arrays on nickel foam as high-performance electrodes for supercapacitors [J]. ACS Appl. Mater. Interfaces, 2015, 7: 26512 |
| 41 | Zhu D Y, Dai P Q, Luo X B, et al. Novel characterization of wetting properties and the calculation of liquid-solid interface tension (I) [J]. Sci. Technol. Eng., 2007, 7: 3057 |
| 朱定一, 戴品强, 罗晓斌 等. 润湿性表征体系及液固界面张力计算的新方法(Ⅰ) [J]. 科学技术与工程, 2007, 7: 3057 |
/
| 〈 |
|
〉 |