搭接工艺对选区激光熔化镍基单晶高温合金DD491晶体取向与微观组织的影响
收稿日期: 2023-05-24
修回日期: 2023-09-18
网络出版日期: 2023-10-27
基金资助
国家自然科学基金项目(52275333);中国航空制造技术研究院稳定支持项目(KZ571801);武汉市知识创新专项项目(2022010801010302)
Effects of Overlapping Process on Grain Orientation and Microstructure of Nickel-Based Single-Crystal Superalloy DD491 Fabricated by Selective Laser Melting
Received date: 2023-05-24
Revised date: 2023-09-18
Online published: 2023-10-27
Supported by
National Natural Science Foundation of China(52275333);Stabilization Support Project of AVIC Manufacturing Technology Institute(KZ571801);Knowledge Innovation Special Project of Wuhan(2022010801010302)
镍基单晶高温合金是制造航空发动机单晶涡轮叶片的关键材料,选区激光熔化(SLM)制造单晶组织和复杂结构具有技术优势和可行性。在SLM中,熔道与熔道之间的搭接质量对单晶组织的完整性至关重要。本工作在4种激光功率和扫描速率的组合工艺下,探究了扫描间距(0.06、0.09、0.12和0.15 mm)对第四代镍基单晶高温合金DD491熔道微观形貌、冶金缺陷、晶体取向和微观组织的影响。结果表明,低功率、低速率和高功率、高速率的工艺参数能够为晶体定向生长提供稳定的几何形态和冶金条件,熔道底部晶体能够延续基底取向实现[001]定向生长。熔道内不同区域存在不同类型的晶体取向缺陷,包括顶部中间等轴晶、顶部[010]和[100]柱状杂晶、内部小角度取向偏差等。较小扫描间距的熔道重熔率较高,有利于减少熔道两侧的杂晶缺陷。
张振武 , 李继康 , 许文贺 , 沈沐宇 , 戚磊一 , 郑可盈 , 李伟 , 魏青松 . 搭接工艺对选区激光熔化镍基单晶高温合金DD491晶体取向与微观组织的影响[J]. 金属学报, 2024 , 60(11) : 1471 -1486 . DOI: 10.11900/0412.1961.2023.00230
Aero-engine turbine blades are operated under harsh conditions such as high temperature, pressure, and load. Therefore, weak grain boundaries at high temperatures should be eliminated from the turbine blades, whereas convection channels inside the blades should be added to dissipate heat. Achieving integrated manufacturing of specialized microstructure in complex components has been a long-term research priority in turbine blade manufacturing. Nickel-based single-crystal superalloys are key materials for manufacturing single-crystal turbine blades for aero-engines, and selective laser melting (SLM) is feasible and technically advantageous for manufacturing complex components with single-crystal microstructures. Owing to the extremely high temperature gradient and scanning speed during SLM, the melt pool is unstable, thereby interrupting directional crystal growth. The metallurgical environment of SLM is further complicated by the large number of overlapping tracks and stacking layers. The quality of the overlaps is critical for the integrity of the single-crystal structure during SLM. Herein, the effects of scanning hatch (h = 0.06, 0.09, 0.12, and 0.15 mm) on the melt track morphology, metallurgical defects, crystal orientation, and microstructure of DD491 fourth-generation nickel-based single-crystal superalloy were investigated. Directionally solidified and solution-aged DD6 single-crystal superalloy rods were used as the substrate, and DD491 powder was coated to a thickness of 40 μm. Electron backscatter diffraction was used to characterize the crystal orientation of the samples. Results show that low power/low speed (S1) and high power/high speed (S4) combinations of laser power and scanning speed provide geometrically and metallurgically stable conditions for directional crystal growth, and the grains at the bottom of the melt track can orient the substrate to achieve [001] directional growth. Different types of crystal orientation defects were observed in different regions, including equiaxed stray grains in the top middle region, [010] and [100] columnar stray grains in the top side regions, and small orientation deviation in the internal region. The scanning hatch affected the crystal orientation in the overlapping regions mainly through the remelted proportion of the old melt pool and the substrate microstructure of the new melt pool during solidification. The higher overlapping ratio with a smaller scanning hatch was beneficial for reducing stray grain defects on both sides of the melt tracks. The role of residual heat on solidification conditions was related to the heat gradient vector of laser input, and multitrack overlapping samples under the S1 process accommodated higher residual heat without causing orientation deviation in the overlapping regions. The multitrack overlapping samples under S1, h = 0.06 and0.09 mm, had maximum pole densities along the y-z plane as high as 47.66 and 46.85, respectively, exhibiting a typical [001] single-crystal structure.
| 1 | Zhang J, Wang L, Wang D, et al. Recent progress in research and development of nickel-based single crystal superalloys [J]. Acta Metall. Sin., 2019, 55: 1077 |
| 张 健, 王 莉, 王 栋 等. 镍基单晶高温合金的研发进展 [J]. 金属学报, 2019, 55: 1077 | |
| 2 | Xia W S, Zhao X B, Yue L, et al. A review of composition evolution in Ni-based single crystal superalloys [J]. J. Mater. Sci. Technol., 2020, 44: 76 |
| 3 | Zhao X B, Gao S F, Yang C B, et al. Influence of crystal orientation on microstructure and mechanical properties and its control for nickel-base single crystal superalloys [J]. Mater. China, 2013, 32: 24 |
| 赵新宝, 高斯峰, 杨初斌 等. 镍基单晶高温合金晶体取向的选择及其控制 [J]. 中国材料进展, 2013, 32: 24 | |
| 4 | Liu L, Sun D J, Huang T W, et al. Directional solidification under high thermal gradient and its application in superalloys processing [J]. Acta Metall. Sin., 2018, 54: 615 |
| 刘 林, 孙德建, 黄太文 等. 高梯度定向凝固技术及其在高温合金制备中的应用 [J]. 金属学报, 2018, 54: 615 | |
| 5 | Li J G, Meng X B, Liu J D, et al. Common solidification defects and inhibition methods in single crystal superalloy turbine blades [J]. Spec. Cast. Nonferrous Alloys, 2021, 41: 1321 |
| 李金国, 孟祥斌, 刘纪德 等. 单晶高温合金涡轮叶片的常见凝固缺陷及控制方法 [J]. 特种铸造及有色合金, 2021, 41: 1321 | |
| 6 | Bondarenko Y A, Kablov E N. Directional crystallization of high-temperature alloys with elevated temperature gradient [J]. Met. Sci. Heat Treat., 2002, 44: 288 |
| 7 | Kong X C, Zhang Z Q, Zhu J Q, et al. Research progress on cooling structure of aeroengine air-cooled turbine blade [J]. J. Prop. Technol., 2022, 43(5): 1 |
| 孔祥灿, 张子卿, 朱俊强 等. 航空发动机气冷涡轮叶片冷却结构研究进展 [J]. 推进技术, 2022, 43(5): 1 | |
| 8 | Song B, Zhang J L, Zhang Y J, et al. Research progress of materials design for metal laser additive manufacturing [J]. Acta Metall. Sin., 2023, 59: 1 |
| 宋 波, 张金良, 章媛洁 等. 金属激光增材制造材料设计研究进展 [J]. 金属学报, 2023, 59: 1 | |
| 9 | DeBroy T, Mukherjee T, Wei H L, et al. Metallurgy, mechanistic models and machine learning in metal printing [J]. Nat. Rev. Mater., 2021, 6: 48 |
| 10 | Liu J, To A C. Quantitative texture prediction of epitaxial columnar grains in additive manufacturing using selective laser melting [J]. Addit. Manuf., 2017, 16: 58 |
| 11 | Kalidindi S R, Bronkhorst C A, Anand L. Crystallographic texture evolution in bulk deformation processing of FCC metals [J]. J. Mech. Phys. Solids, 1992, 40: 537 |
| 12 | Liu L T, Chen C Y, Li X, et al. Research progress in laser additive manufacturing technology of single crystal superalloy [J]. J. Netshape Forming Eng., 2019, 11(4): 73 |
| 刘龙涛, 陈超越, 李 霞 等. 激光增材制造单晶高温合金研究进展 [J]. 精密成形工程, 2019, 11(4): 73 | |
| 13 | G?umann M, Bezen?on C, Canalis P, et al. Single-crystal laser deposition of superalloys: Processing-microstructure maps [J]. Acta Mater., 2001, 49: 1051 |
| 14 | Lu N N. Single crystal growth controling of CMSX-10 superalloy via laser melting deposition [D]. Harbin: Harbin Institute of Technology, 2021 |
| 卢楠楠. CMSX-10高温合金激光熔化沉积单晶生长控制 [D]. 哈尔滨: 哈尔滨工业大学, 2021 | |
| 15 | Ci S W. Study on microstructure and mechanical properties of nickel-based single crystal supertalloy by laser additive manufacturing [D]. Hefei: University of Science and Technology of China, 2021 |
| 慈世伟. 激光增材制造镍基单晶高温合金显微组织和力学性能研究 [D]. 合肥: 中国科学技术大学, 2021 | |
| 16 | Liu X X, Cheng X, Wang H M, et al. Influence of processing conditions on formation of stray grains in DD5 single-crystal superalloys by laser melting multi-traced deposition [J]. Chin. J. Lasers, 2017, 44: 0602009 |
| 刘小欣, 程 序, 王华明 等. 不同工艺条件对激光熔化多道沉积DD5单晶高温合金杂晶的影响 [J]. 中国激光, 2017, 44: 0602009 | |
| 17 | Fernandez-Zelaia P, Kirka M M, Rossy A M, et al. Nickel-based superalloy single crystals fabricated via electron beam melting [J]. Acta Mater., 2021, 216: 117133 |
| 18 | K?rner C, Ramsperger M, Meid C, et al. Microstructure and mechanical properties of CMSX-4 single crystals prepared by additive manufacturing [J]. Metall. Mater. Trans., 2018, 49A: 3781 |
| 19 | Li Y, Yu Y F, Wang Z B, et al. Additive manufacturing of nickel-based superalloy single crystals with IN-738 alloy [J]. Acta Metall. Sin. (Engl. Lett.), 2022, 35: 369 |
| 20 | Matuszewski K, Rettig R, Matysiak H, et al. Effect of ruthenium on the precipitation of topologically close packed phases in Ni-based superalloys of 3rd and 4th generation [J]. Acta Mater., 2015, 95: 274 |
| 21 | Li J K, Zhang Z W, Yang Y Q, et al. Single-track morphology, crystal orientation and microstructure of DD91 nickel-based single crystal superalloy fabricated by selective laser melting [J]. Chin. J. Lasers, 2022, 49: 1402103 |
| 李继康, 张振武, 杨源祺 等. 激光选区熔化DD91镍基单晶高温合金的单道形貌, 晶体取向和微观组织 [J]. 中国激光, 2022, 49: 1402103 | |
| 22 | Guo C, Li G, Li S, et al. Additive manufacturing of Ni-based superalloys: Residual stress, mechanisms of crack formation and strategies for crack inhibition [J]. Nano Mater. Sci., 2023, 5: 53 |
| 23 | Li Y, Xu H J, Li K, et al. Effect of volumetric energy density on microstructure and properties of Hastelloy X alloy manufactured by selective laser melting [J]. Mater. Mech. Eng., 2020, 44(5): 38 |
| 李 勇, 许鹤君, 李 凯 等. 体能量密度对选区激光熔化成形Hastelloy X合金组织及性能的影响 [J]. 机械工程材料, 2020, 44(5): 38 | |
| 24 | Wei Q S, Xie Y, Teng Q, et al. Crack types, mechanisms, and suppression methods during high-energy beam additive manufacturing of nickel-based superalloys: A review [J]. Chin. J. Mech. Eng.: Addit. Manuf. Front., 2022, 1: 100055 |
| 25 | Jin T, Sun X F, Zhao N R, et al. Laser glazing rapidly solidified microstructure of DD8 single crystal Ni-based superalloy [J]. Acta Metall. Sin., 2009, 45: 711 |
| 金 涛, 孙晓峰, 赵乃仁 等. 单晶镍基高温合金DD8激光快速熔凝组织 [J]. 金属学报, 2009, 45: 711 | |
| 26 | Liang J J, Yang Y H, Zhou Y Z, et al. Microstructures of nickel-base single-crystal superalloy prepared by laser solid forming [J]. Rare Met. Mater. Eng., 2017, 46: 3753 |
| 梁静静, 杨彦红, 周亦胄 等. 激光立体成形镍基单晶高温合金显微组织研究 [J]. 稀有金属材料与工程, 2017, 46: 3753 | |
| 27 | Anderson T D, Dupont J N, Debroy T. Origin of stray grain formation in single-crystal superalloy weld pools from heat transfer and fluid flow modeling [J]. Acta Mater., 2010, 58: 1441 |
| 28 | Rappaz M, David S A, Vitek J M, et al. Development of microstructures in Fe-15Ni-15Cr single crystal electron beam welds [J]. Metall. Trans., 1989, 20A: 1125 |
| 29 | Yang J J, Li F Z, Pan A Q, et al. Microstructure and grain growth direction of SRR99 single-crystal superalloy by selective laser melting [J]. J. Alloys Compd., 2019, 808: 151740 |
| 30 | Zhang P Y, Zhou X, Zhang W Q, et al. Effects of melt-pool geometry on the oriented to misoriented transition in directed energy deposition of a single-crystal superalloy [J]. Addit. Manuf., 2022, 60: 103253 |
| 31 | Shi R P, Khairallah S A, Roehling T T, et al. Microstructural control in metal laser powder bed fusion additive manufacturing using laser beam shaping strategy [J]. Acta Mater., 2020, 184: 284 |
| 32 | Wang G W, Liang J J, Zhou Y Z, et al. Variation of crystal orientation during epitaxial growth of dendrites by laser deposition [J]. J. Mater. Sci. Technol., 2018, 34: 732 |
| 33 | T?nhardt R, Amberg G. Phase-field simulation of dendritic growth in a shear flow [J]. J. Cryst. Growth, 1998, 194: 406 |
| 34 | Zhou Z P, Lei Q, Yan Z, et al. Effects of process parameters on microstructure and cracking susceptibility of a single crystal superalloy fabricated by directed energy deposition [J]. Mater. Des., 2021, 198: 109296 |
/
| 〈 |
|
〉 |