镍基高温合金疲劳裂纹急速扩展敏感温度及成因
收稿日期: 2023-04-04
修回日期: 2023-06-02
网络出版日期: 2023-07-05
基金资助
国家自然科学基金项目(92160201)
Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy
Received date: 2023-04-04
Revised date: 2023-06-02
Online published: 2023-07-05
Supported by
National Natural Science Foundation of China(92160201)
对3种粉末高温合金FG4096、FGH4097和FGH4098,2种变形高温合金GH4720Li和GH4738等典型镍基高温合金,在550~800℃的宽温度范围内开展疲劳裂纹扩展实验,明确了合金在服役温度范围内的高温段存在疲劳裂纹急速扩展的敏感温度。综合考虑合金的高温组织演变和力学性能衰减对疲劳行为的影响,发现2者并非高温疲劳裂纹急剧扩展敏感温度存在的主因。不同温度下疲劳断口和裂纹扩展路径的对比以及氧化损伤分量的计算表明,高温下晶界氧化损伤是疲劳裂纹急剧扩展敏感温度存在的主要原因。采用分子动力学计算分析了不同温度下O对Ni和NiCr体系晶界强度的影响规律。通过实验和理论计算阐述了镍基高温合金疲劳裂纹扩展的高温敏感性现象和本质原因。
江河 , 佴启亮 , 徐超 , 赵晓 , 姚志浩 , 董建新 . 镍基高温合金疲劳裂纹急速扩展敏感温度及成因[J]. 金属学报, 2023 , 59(9) : 1190 -1200 . DOI: 10.11900/0412.1961.2023.00151
Superalloys are widely used in aerospace industry owing to the excellent mechanical properties and microstructure stability at high temperatures. However, the recent developments in the aerospace industry have piled higher demands on superalloys, especially for damage tolerance at high temperatures. The fatigue crack growth rate (FCGR) is an important parameter that describes damage tolerance. Although several domestic studies on FCGR in superalloys have been reported, systematic understanding is still lacking and urgently required. Hence, this study investigated the phenomenon of sensitive temperature for rapid fatigue crack propagation in several nickel-based superalloys and reasons for its emergence by adopting a systematic program of experiments and simulations. The fatigue crack propagation behavior of FGH4096, FGH4097, and FGH4098 powder-metallurgy nickel-based superalloys, and GH4720Li and GH4738 wrought nickel-based superalloys were systematically investigated in a wide temperature range of 550-800oC using a fatigue crack propagation test. The fatigue crack propagation paths and crack microstructures after the fatigue crack propagation tests were observed. The results clearly demonstrated that the relationship between fatigue life and temperature is nonlinear. A sensitive temperature for rapid fatigue crack propagation for all investigated nickel-based superalloys was also observed, where the fatigue crack propagation rate markedly increased and fatigue life dramatically shortened. Microstructure evolution and mechanical property degradation at high temperatures were not found to be the major reasons behind the occurrence of sensitive temperature of rapid fatigue crack propagation. However, a comparison of fracture morphologies and fatigue crack propagation paths at different temperatures combined with the analysis of oxidation damage components revealed the high-temperature oxidation damage of grain boundary as the major reason for the occurrence of sensitive temperature. The contributions of fatigue damage and oxidation damage at different temperatures were compared using the classical linear superposition damage component model. The results showed that the contribution of oxidation damage increased markedly with increasing temperature. As a result, the fatigue life decreased dramatically at high temperatures and the fatigue propagation rates increased rapidly. Furthermore, the effect of O on the grain boundary strength in the Ni and NiCr system at different temperatures was investigated by molecular dynamics simulations. The grain boundary separation work decreased with increasing temperature and after which the value decreased dramaticalloy. It was concluded that the accumulation of O on the grain boundary resulted in a decrease in the grain boundary separation work and weakened the grain boundary.
| 1 | Zhang R, Liu P, Cui C Y, et al. Present research situation and prospect of hot working of cast & wrought superalloys for aero-engine turbine disk in China [J]. Acta Metall. Sin., 2021, 57: 1215 |
| 张 瑞, 刘 鹏, 崔传勇 等. 国内航空发动机涡轮盘用铸锻难变形高温合金热加工研究现状与展望 [J]. 金属学报, 2021, 57: 1215 | |
| 2 | Zou J W, Wang W X. Development and application of P/M superalloy [J]. J. Aeronautical Mater., 2006, 26(3): 244 |
| 邹金文, 汪武祥. 粉末高温合金研究进展与应用 [J]. 航空材料学报, 2006, 26(3): 244 | |
| 3 | Gao S Y, Ge S X, Yang X H, et al. Effect of temperature on the creep behavior and mechanism of GH4169 alloy [J]. Chin. J. Eng., 2023, 45: 301 |
| 高圣勇, 葛树欣, 杨选宏 等. 温度对GH4169合金蠕变行为及机制的影响 [J]. 工程科学学报, 2023, 45: 301 | |
| 4 | Peng Z C, Liu P Y, Wang X Q, et al. Creep behavior of FGH96 superalloy at different service conditions [J]. Acta Metall. Sin., 2022, 58: 673 |
| 彭子超, 刘培元, 王旭青 等. 不同服役条件下FGH96合金的蠕变特征 [J]. 金属学报, 2022, 58: 673 | |
| 5 | Tian T, Hao Z B, Ge C C, et al. Effects of stress and temperature on creep behavior of a new third-generation powder metallurgy superalloy FGH100L [J]. Mater. Sci. Eng., 2020, A776: 139007 |
| 6 | Huang D W, Yan X J, Li P Y, et al. Modeling of temperature influence on the fatigue crack growth behavior of superalloys [J]. Int. J. Fatigue, 2018, 110: 22 |
| 7 | Nai Q L, Dong J X, Zhang M C, et al. Temperature sensitivity of fatigue crack growth rate for GH4720Li alloy [J]. Rare Met. Mater. Eng., 2017, 46: 2915 |
| 佴启亮, 董建新, 张麦仓 等. GH4720Li合金疲劳裂纹扩展速率的温度敏感性 [J]. 稀有金属材料与工程, 2017, 46: 2915 | |
| 8 | Liu F J. Investigation on high temperature oxidation of FGH95, FGH96 and FGH97 alloys [D]. Beijing: University of Science & Technology Beijing, 2007 |
| 刘丰军. FGH95、FGH96和FGH97合金的高温氧化行为研究 [D]. 北京: 北京科技大学, 2007 | |
| 9 | Krupp U, Kane W M, Liu X Y, et al. The effect of grain-boundary-engineering-type processing on oxygen-induced cracking of IN718 [J]. Mater. Sci. Eng., 2003, A349: 213 |
| 10 | Kruml T, Obrtlík K. Microstructure degradation in high temperature fatigue of TiAl alloy [J]. Int. J. Fatigue, 2014, 65: 28 |
| 11 | Osinkolu G A, Onofrio G, Marchionni M. Fatigue crack growth in polycrystalline IN 718 superalloy [J]. Mater. Sci. Eng., 2003, A356:425 |
| 12 | Chen X, Yang Z Q, Sokolov M A, et al. Effect of creep and oxidation on reduced fatigue life of Ni-based alloy 617 at 850oC [J]. J. Nucl. Mater., 2014, 444: 393 |
| 13 | Evangelou A, Soday K A, Lockyer S, et al. On the mechanism of oxidation-fatigue damage at intermediate temperatures in a single crystal Ni-based superalloy [J]. Mater. Sci. Eng., 2019, A742: 648 |
| 14 | Jiang R, Gao N, Reed P A S. Influence of orientation-dependent grain boundary oxidation on fatigue cracking behaviour in an advanced Ni-based superalloy [J]. J. Mater. Sci., 2015, 50: 4379 |
| 15 | Miller C F, Simmons G W, Wei R P. Evidence for internal oxidation during oxygen enhanced crack growth in P/M Ni-based superalloys [J]. Scr. Mater., 2003, 48: 103 |
| 16 | Tucker A M, Henderson M B, Wilkinson A J, et al. High temperature fatigue crack growth in powder processed nickel based superalloy U720Li [J]. Mater. Sci. Technol., 2002, 18: 349 |
| 17 | King J E. Fatigue crack propagation in nickel-base superalloys—Effects of microstructure, load ratio, and temperature [J]. Mater. Sci. Technol., 1987, 3: 750 |
| 18 | Jiang R, Everitt S, Lewandowski M, et al. Grain size effects in a Ni-based turbine disc alloy in the time and cycle dependent crack growth regimes [J]. Int. J. Fatigue, 2014, 62: 217 |
| 19 | Jiang R, Proprentner D, Callisti M, et al. Role of oxygen in enhanced fatigue cracking in a PM Ni-based superalloy: Stress assisted grain boundary oxidation or dynamic embrittlment? [J]. Corros. Sci., 2018, 139: 141 |
| 20 | Zhang M, Zhang Y X, Liu H, et al. Judgment criterion of the dominant factor of creep-fatigue crack growth in a nickel-based superalloy at elevated temperature [J]. Int. J. Fatigue, 2019, 118: 176 |
| 21 | Yang H Q, Bao R, Zhang J Z. An interaction crack growth model for creep-brittle superalloys with high temperature dwell time [J]. Eng. Fract. Mech., 2014, 124-125: 112 |
| 22 | Tong J, Dalby S, Byrne J, et al. Creep, fatigue and oxidation in crack growth in advanced nickel base superalloys [J]. Int. J. Fatigue, 2001, 23: 897 |
| 23 | Li H Y, Sun J F, Hardy M C, et al. Effects of microstructure on high temperature dwell fatigue crack growth in a coarse grain PM nickel based superalloy [J]. Acta Mater., 2015, 90: 355 |
| 24 | V?ianská M, ?ob M. The effect of segregated sp-impurities on grain-boundary and surface structure, magnetism and embrittlement in nickel [J]. Prog. Mater. Sci., 2011, 56: 817 |
| 25 | Xue H T, Luo Y Q, Tang F L, et al. Segregation behavior of alloying elements at Ni Σ5 [001](210) symmetrical tilt grain boundary in nickel-based superalloys and their stabilization and strengthening mechanisms for the grain boundary [J]. Mater. Chem. Phys., 2021, 258: 123977 |
| 26 | Liang C P, Wang W Q, Tang S, et al. Molecular dynamics simulation of symmetrical tilt grain boundary of body-centered cubic tungsten [J]. Chin. J. Nonferrous Met., 2021, 31: 1757 |
| 梁超平, 王文琦, 唐 赛 等. 钨对称倾斜晶界的分子动力学计算模拟 [J]. 中国有色金属学报, 2021, 31: 1757 | |
| 27 | Pham H H, Cagin T. Fundamental studies on stress-corrosion cracking in iron and underlying mechanisms [J]. Acta Mater., 2010, 58: 5142 |
/
| 〈 |
|
〉 |