Al掺杂Mg/Mg2Sn合金界面的第一性原理计算
收稿日期: 2022-09-15
修回日期: 2022-12-16
网络出版日期: 2023-03-28
基金资助
国家自然科学基金项目(52074246);国家自然科学基金项目(22008224);国家自然科学基金项目(52275390);国家自然科学基金项目(52205429);国家自然科学基金项目(52201146);国防基础科研项目(JCKY20204-08B002);国防基础科研项目(WDZC2022-12);山西省重点研发计划项目(202102050-201011);中央引导地方计划项目(YDZJSX-2022A025);中央引导地方计划项目(YDZJSX2021A027)
First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface
Received date: 2022-09-15
Revised date: 2022-12-16
Online published: 2023-03-28
Supported by
National Natural Science Foundation of China(52074246);National Natural Science Foundation of China(22008224);National Natural Science Foundation of China(52275390);National Natural Science Foundation of China(52205429);National Natural Science Foundation of China(52201146);National Defense Basic Scientific Research Program of China(JCKY20204-08B002);National Defense Basic Scientific Research Program of China(WDZC2022-12);Key Research and Development Program of Shanxi Province(202102050-201011);Guiding Local Science and Technology Development Projects by the Central Government(YDZJSX-2022A025);Guiding Local Science and Technology Development Projects by the Central Government(YDZJSX2021A027)
为研究Mg-Sn合金中Al掺杂Mg基体与Mg2Sn相不同取向以及Al元素在界面处的分布位置,基于密度泛函理论计算了Al元素掺杂Mg/Mg2Sn不同指数面的界面黏附功、界面能以及界面掺杂能来寻找较稳定的掺杂位置。采用态密度和晶体轨道重叠布居分析了Al元素掺杂对Mg(0001)/Mg2Sn(022)界面电子特性的影响。结果表明,界面处添加Al元素后只有部分掺杂位置有益于加强Mg/Mg2Sn界面的稳定性。添加Al元素后,Mg(0001)/Mg2Sn(001)界面处Sn端黏附功均高于Mg端,而Mg(0001)/Mg2Sn(111)界面正好相反。Al掺杂后的Mg(0001)/Mg2Sn(022)界面能降低了0.07 eV/nm。添加Al元素后,Mg(0001)/Mg2Sn(022)界面位置Ⅳ比较容易掺杂,该位置处的电子结构分析表明掺杂Al元素后Al的s轨道和Sn的p轨道存在明显交互作用,在界面处Al—Sn键占主导地位。
王福容 , 张永梅 , 柏国宁 , 郭庆伟 , 赵宇宏 . Al掺杂Mg/Mg2Sn合金界面的第一性原理计算[J]. 金属学报, 2023 , 59(6) : 812 -820 . DOI: 10.11900/0412.1961.2022.00454
Mg-Sn alloy is a high temperature-creep resistant magnesium alloy that has potential applications in lightweight automobiles. The addition of Sn to Mg can reduce the overall cost of the alloy as Sn is cheaper than rare earth elements. Sn and Mg form Mg2Sn phase on the grain boundary, and this Mg2Sn phase has an excellent precipitation hardening effect. However, coarsened Mg2Sn phase can reduce the age hardening effect of the alloy. Previous experimental studies have showed that the addition of Al element can considerably improve the age hardening effect of Mg-Sn alloy as it segregated at the interface between the Mg matrix and Mg2Sn phase. However, there is a lack of research on the different orientations of Al-doped Mg matrix and Mg2Sn phase and the distribution position of Al element at the interface. Therefore, in this study, the interface adhesion energy, interface energy, and interface doping energy of Al-doped Mg/Mg2Sn with different index surfaces were calculated based on density functional theory to determine more stable doping positions. The effects of Al doping on the electronic structure of Mg(0001)/Mg2Sn(022) interface were analyzed using the density of states and crystal orbital Hamilton population. The results demonstrate that only a part of the Al-doping positions is beneficial in strengthening the stability of Mg/Mg2Sn interface. After the addition of Al, the adhesion energy of Sn termination at Mg(0001)/Mg2Sn(001) interface is higher than that of Mg termination, but the adhesion energy of Sn termination at Mg(0001)/Mg2Sn(111) interface is lower than that of Mg termination. In addition, the interface energy of Mg(0001)/Mg2Sn(022) interface doped with Al decreased by 0.07 eV/nm compared to that of Mg(0001)/Mg2Sn(022) interface. The addition of Al element to Mg(0001)/Mg2Sn(022) facilitates the doping of a special position, which shows an obvious interaction between the s orbital of Al and the p orbital of Sn after Al doping. Moreover, the Al—Sn bonding is found to be dominant at the interface.
Key words: Mg/Mg2Sn; Al; interface; first principle; doping
| 1 | Xin T Z, Zhao Y H, Mahjoub R, et al. Ultrahigh specific strength in a magnesium alloy strengthened by spinodal decomposition [J]. Sci. Adv., 2021, 7: eabf3039 |
| 2 | Xin T Z, Tang S, Ji F, et al. Phase transformations in an ultralight BCC Mg alloy during anisothermal ageing [J]. Acta Mater., 2022, 239: 118248 |
| 3 | Zhang W Z, Sun Z P, Zhang J Y, et al. A near row matching approach to prediction of multiple precipitation crystallography of compound precipitates and its application to a Mg/Mg2Sn system [J]. J. Mater. Sci., 2017, 52: 4253 |
| 4 | Jo S M, Kim S D, Kim T H, et al. Sequential precipitation behavior of Mg17Al12 and Mg2Sn in Mg-8Al-2Sn-1Zn alloys [J]. J. Alloys Compd., 2018, 749: 794 |
| 5 | Cheng W L, Park S S, You B S, et al. Microstructure and mechanical properties of binary Mg-Sn alloys subjected to indirect extrusion [J]. Mater. Sci. Eng., 2010, A527: 4650 |
| 6 | Jung I C, Kim Y K, Cho T H, et al. Suppression of discontinuous precipitation in AZ91 by addition of Sn [J]. Met. Mater. Int., 2014, 20: 99 |
| 7 | Huang S, Wang J F, Hou F, et al. Effect of Sn on the formation of the long period stacking ordered phase and mechanical properties of Mg-RE-Zn alloy [J]. Mater. Lett., 2014, 137: 143 |
| 8 | Zhou D W, Xu S H, Zhang F Q, et al. First-principle study on structural stability of Sn alloying MgZn2 phase and Mg2Sn phase [J]. Chin. J. Nonferrous Met., 2010, 20: 914 |
| 周惦武, 徐少华, 张福全 等. Sn合金化MgZn2相及Mg2Sn相结构稳定性的第一原理研究 [J]. 中国有色金属学报, 2010, 20: 914 | |
| 9 | Liu C Q, Chen H W, Wilson N C, et al. Zn segregation in interface between Mg17Al12 precipitate and Mg matrix in Mg-Al-Zn alloys [J]. Scr. Mater., 2019, 163: 91 |
| 10 | Elsayed F R, Sasaki T T, Mendis C L, et al. Compositional optimization of Mg-Sn-Al alloys for higher age hardening response [J]. Mater. Sci. Eng., 2013, A566: 22 |
| 11 | Sasaki T T, Oh-ishi K, Ohkubo T, et al. Enhanced age hardening response by the addition of Zn in Mg-Sn alloys [J]. Scr. Mater., 2006, 55: 251 |
| 12 | Mendis C L, Bettles C J, Gibson M A, et al. Refinement of precipitate distributions in an age-hardenable Mg-Sn alloy through microalloying [J]. Philos. Mag. Lett., 2006, 86: 443 |
| 13 | Pan H C, Qin G W, Xu M, et al. Enhancing mechanical properties of Mg-Sn alloys by combining addition of Ca and Zn [J]. Mater. Des., 2015, 83: 736 |
| 14 | Tian S K, Guo X F. Microstructure and mechanical properties of as-cast Mg-Sn-Al-Zn alloy [J]. Hot Work. Technol., 2014, 43(4): 64 |
| 田树科, 郭学锋. 铸态Mg-Sn-Al-Zn合金组织和力学性能 [J]. 热加工工艺, 2014, 43(4): 64 | |
| 15 | Kim S H, Park S H. Underlying mechanisms of drastic reduction in yield asymmetry of extruded Mg-Sn-Zn alloy by Al addition [J]. Mater. Sci. Eng., 2018, A733: 285 |
| 16 | Luo Y X, Chen Y, Ran L, et al. Effects of Zn/Al mass ratio on microstructure evolution and mechanical properties of Mg-Sn based alloys [J]. Mater. Sci. Eng., 2021, A815: 141307 |
| 17 | Xu X X. Microstructural characterization of aged Mg-Sn-Al alloy [D]. Chongqing: Chongqing University, 2019 |
| 徐孝新. 时效Mg-Sn-Al合金的微观结构研究 [D]. 重庆: 重庆大学, 2019 | |
| 18 | Bai G N, Tian J Z, Guo Q W, et al. First-principle study on Mg2 X (X = Si, Ge, Sn) intermetallics by Bi micro-alloying [J]. Crystals, 2021, 11: 142 |
| 19 | Wang S, Zhao Y H, Deng S J, et al. First-principle studies on the mechanical, thermodynamic and electronic properties of β″-Mg3Gdand β'-Mg7Gd alloys under pressure [J]. J. Phys. Chem. Solids, 2019, 125: 115 |
| 20 | Hou H, Pan Y, Bai G N, et al. High-throughput computing for hydrogen transport properties in ε-ZrH2 [J]. Adv. Compos. Hybrid Mater., 2022, 5: 1350 |
| 21 | Chen L Q, Zhao Y H. From classical thermodynamics to phase-field method [J]. Prog. Mater. Sci., 2022, 124: 100868 |
| 22 | Liu B, Gu M, Liu X L, et al. First-principles study of fluorine-doped zinc oxide [J]. Appl. Phys. Lett., 2010, 97: 122101 |
| 23 | Li R W, Chen Q C, Ouyang L, et al. Insight into the strengthening mechanism of α-Al2O3/γ-Fe ceramic-metal interface doped with Cr, Ni, Mg, and Ti [J]. Ceram. Int., 2021, 47: 22810 |
| 24 | Li R W, Chen Q C, Ji M X, et al. Exploring failure mode and enhancement mechanism of doped rare-earth elements iron-based/alumina-ceramic interface [J]. Ceram. Int., 2022, 48: 7827 |
| 25 | Wang X H, Zhang C L, Hu X P, et al. First principle study on alloying effect of Al and Zn doping on Mg-Li phase interface [J]. Rare Met. Mater. Eng., 2014, 43: 1661 |
| 王小宏, 张彩丽, 户秀萍 等. Al、Zn对Mg-Li相界合金化效应的第一性原理研究 [J]. 稀有金属材料与工程, 2014, 43: 1661 | |
| 26 | Liu P, Wang X Y, Chen D F, et al. Interface structure characterization and elements doping on interface bonding strength and tensile failure mechanism of NiCo coating/Cu matrix [J]. Results Phys., 2021, 30: 104883 |
| 27 | Zhang D L, Wang J, Kong Y, et al. First-principles investigation on stability and electronic structure of Sc-doped θ'/Al interface in Al-Cu alloys [J]. Trans. Nonferrous Met. Soc. China, 2021, 31: 3342 |
| 28 | Zhao Y H. Stability of phase boundary between L12-Ni3Al phases: A phase field study [J]. Intermetallics, 2022, 144: 107528 |
| 29 | Zhao Y H, Liu K X, Hou H, et al. Role of interfacial energy anisotropy in dendrite orientation in Al-Zn alloys: A phase field study [J]. Mater. Des., 2022, 216: 110555 |
| 30 | Tsuru T, Somekawa H, Chrzan D C. Interfacial segregation and fracture in Mg-based binary alloys: Experimental and first-principles perspective [J]. Acta Mater., 2018, 151: 78 |
| 31 | Jin Y R, Feng Z Z, Ye L Y, et al. Mg2Sn: A potential mid-temperature thermoelectric material [J]. RSC Adv., 2016, 6: 48728 |
| 32 | Kresse G, Furthmüller J. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set [J]. Phys. Rev., 1996, 54B: 11169 |
| 33 | Xiao J B, Yao J P. First-principle study on the influence of alloy elements on the stability of TiC/Mg interface [J]. Spec. Cast. Nonferrous Alloys, 2020, 40: 1152 |
| 肖江波, 尧军平. 合金元素对TiC/Mg界面稳定性影响的第一性原理研究 [J]. 特种铸造及有色合金, 2020, 40: 1152 | |
| 34 | Xie H N, Chen Y T, Zhang T B, et al. Adhesion, bonding and mechanical properties of Mo doped diamond/Al (Cu) interfaces: A first principles study [J]. Appl. Surf. Sci., 2020, 527: 146817 |
| 35 | Wang S, Zhang C, Li X, et al. First-principle investigation on the interfacial structure evolution of the δ'/θ'/δ' composite precipitates in Al-Cu-Li alloys [J]. J. Mater. Sci. Technol., 2020, 58: 205 |
| 36 | Wen Z Q, Zhao Y H, Hou H, et al. A first-principles study on interfacial properties of Ni(001)/Ni3Nb(001) [J]. Trans. Nonferrous Met. Soc. China, 2014, 24: 1500 |
| 37 | Wang C Q, Chen W G, Xie J P. Effects of transition element additions on the interfacial interaction and electronic structure of Al(111)/6H-SiC(0001) interface: A first-principles study [J]. Materials, 2021, 14: 630 |
| 38 | Deringer V L, Tchougréeff A L, Dronskowski R. Crystal orbital Hamilton population (COHP) analysis as projected from plane-wave basis sets [J]. J. Phys. Chem., 2011, 115A: 5461 |
/
| 〈 |
|
〉 |