研究论文

四元Co-Ni-Cr-Al合金高温氧化模式及其转变机理

  • 吕云蕾 ,
  • 任延杰 ,
  • 冯抗抗 ,
  • 周梦妮 ,
  • 王文 ,
  • 陈荐 ,
  • 牛焱
展开
  • 1 长沙理工大学 能源与动力工程学院 长沙 410076
    2 浙江科技大学 机械与能源工程学院 杭州 310023
    3 中国科学院金属研究所 沈阳 110016
吕云蕾,女,1995年生,硕士生
任延杰,yjren@csust.edu.cn,主要从事动力设备的腐蚀与防护研究;
牛 焱,yniu@csust.edu.cn,主要从事金属的高温腐蚀与防护研究

收稿日期: 2022-04-27

  修回日期: 2022-08-16

  网络出版日期: 2022-11-17

基金资助

国家自然科学基金项目(52171066);国家自然科学基金项目(51771034);湖南省自然科学基金项目(2020JJ4610);湖南省研究生科研创新项目(CX20200871)

High Temperature Oxidation Mode and Transformation Mechanism of Quaternary Co-Ni-Cr-Al Alloys

  • LV Yunlei ,
  • REN Yanjie ,
  • FENG Kangkang ,
  • ZHOU Mengni ,
  • WANG Wen ,
  • CHEN Jian ,
  • NIU Yan
Expand
  • 1 College of Energy and Power Engineering, Changsha University of Science and Technology, Changsha 410076, China
    2 School of Mechanical and Energy Engineering, Zhejiang University of Science and Technology, Hangzhou 310023, China
    3 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
REN Yanjie, professor, Tel: 13657310308, E-mail: yjren@csust.edu.cn;

Received date: 2022-04-27

  Revised date: 2022-08-16

  Online published: 2022-11-17

Supported by

National Natural Science Foundation of China(52171066);National Natural Science Foundation of China(51771034);Natural Science Foundation of Hunan Province(2020JJ4610);Postgraduate Scientific Research Innovation Project of Hunan Province(CX20200871)

摘要

为深入探究Cr、Al元素对Co-Ni合金高温氧化行为的影响,本工作研究了四元Co-20Ni-8Cr-xAl (x = 3、5,质量分数,%)合金在纯氧中800、900、1000和1100℃下的氧化行为。氧化后,2种合金表面均生成了复杂的氧化膜。2种合金在800、900和1000℃下均有不连续Al2O3膜生成,1100℃下仅在Co-20Ni-8Cr-5Al表面生成Al2O3。温度从800℃升到900℃,合金的氧化速率均提高,而温度从1000℃升高到1100℃后,2种合金的氧化速率均下降。合金中Al含量由3%增加到5%,Co-Ni-Cr-Al合金的氧化速率随之下降,但5%的Al含量仍不足以令合金表面生成保护性的Al2O3膜。与Al含量相同的Co-Ni-Al三元合金相比,Cr和Al的同时存在有利于降低四元Co-Ni-Cr-Al合金的氧化速率。

本文引用格式

吕云蕾 , 任延杰 , 冯抗抗 , 周梦妮 , 王文 , 陈荐 , 牛焱 . 四元Co-Ni-Cr-Al合金高温氧化模式及其转变机理[J]. 金属学报, 2024 , 60(7) : 947 -956 . DOI: 10.11900/0412.1961.2022.00200

Abstract

The addition of Ni to cobalt-based alloys can form the γ′ phase, which can significantly improve their mechanical properties and high-temperature oxidation resistance. The oxidation behavior of quaternary Co-20Ni-8Cr-xAl (x = 3 or 5, mass fraction, %) alloys was investigated in 1.013 × 105 Pa O2 at 800, 900, 1000, and 1100oC. Also, the effects of Al and/or Cr contents and temperature on the oxidation properties of the alloys were explored by analyzing the oxidation kinetics of the alloys and the cross-sectional morphology characteristics of the scales, revealing the oxidation mechanism of these alloys. After oxidation, both the alloys formed complex scales with irregular thickness and composition. Alumina scales were generated for each alloy at 800, 900, and 1000oC and only for Co-20Ni-8Cr-5Al at 1100oC. The increase in temperature from 800oC to 900oC has a negative effect on the oxidation resistance, resulting in greatly accelerated oxidation rates. Conversely, that from 1000oC to 1100oC has a positive effect on the oxidation of the two alloys, causing a decrease in the oxidation rate. The oxidation rate of the Co-Ni-Cr-Al alloy decreases when the Al content in the alloy is increased from 3% to 5%, but 5% is still not sufficient to form continuous alumina scales. The simultaneous presence of Cr and Al is beneficial to reducing the oxidation rate of the quaternary Co-Ni-Cr-Al alloys compared with the ternary Co-Ni-Al alloy with the same Al content.

参考文献

1 Young D J. High Temperature Oxidation and Corrosion of Metals [M]. 2nd Ed., Amsterdam: Elsevier, 2016: 1
2 Lai G Y. High-Temperature Corrosion and Materials Applications [M]. ASM International, 2007: 6
3 Yuan F H, Sun X F, Guan H R, et al. Cyclic oxidation behavior of a cobalt-base superalloy [J]. J. Chin. Soc. Corros. Prot., 2002, 22: 115
  袁福河, 孙晓峰, 管恒荣 等. 钴基高温合金的循环氧化行为研究 [J]. 中国腐蚀与防护学报, 2002, 22: 115
4 Hou P Y. Impurity effects on alumina scale growth [J]. J. Am. Ceram. Soc., 2003, 86: 660
5 Stott F H, Wood G C, Stringer J. The influence of alloying elements on the development and maintenance of protective scales [J]. Oxid. Met., 1995, 44: 113
6 Wallwork G R, Hed A Z. Mapping of the oxidation products in the ternary Co-Cr-Al system [J]. Oxid. Met., 1971, 3: 213
7 Wallwork G R, Hed A Z. Selection of an alloy composition in the ternary Co-Cr-Al system for oxidation resistance [J]. Oxid. Met., 1971, 3: 243
8 Wood G C, Stott F H. The influence of aluminum additions on the oxidation of Co-Cr alloys at 1000 and 1200oC [J]. Oxid. Met., 1971, 3: 365
9 Irving G N, Stringer J, Whittle D P. The oxidation behavior of Co-Cr-Al alloys at 1000oC [J]. Corrosion, 1977, 33: 56
10 Allam I M, Whittle D P, Stringer J. The oxidation behavior of CoCrAl systems containing active element additions [J]. Oxid. Met., 1978, 12: 35
11 Stott F H, Wood G C, Hobby M G. A comparison of the oxidation behavior of Fe-Cr-Al, Ni-Cr-Al, and Co-Cr-Al alloys [J]. Oxid. Met., 1971, 3: 103
12 Stott F H, Wood G C. The mechanism of oxidation of Ni-Cr-Al alloys at 1000oC-1200oC [J]. Corros. Sci., 1971, 11: 799
13 Giggins C S, Pettit F S. Oxidation of Ni-Cr-Al alloys between 1000℃ and 1200℃ [J]. J. Electrochem. Soc., 1971, 118: 1782
14 Kvernes I A, Kofstad P. The oxidation behavior of some Ni-Cr-Al alloys at high temperatures [J]. Mater. Trans., 1972, 3B: 1511
15 Nijdam T J, Jeurgens L P H, Sloof W G. Effect of partial oxygen pressure on the initial stages of high-temperature oxidation of γ-NiCrAl alloys [J]. Mater. High Temp., 2003, 20: 311
16 Nijdam T J, Jeurgens L P H, Sloof W G. Modelling the thermal oxidation of ternary alloys—Compositional changes in the alloy and the development of oxide phases [J]. Acta Mater., 2003, 51: 5295
17 Nijdam T J, Jeurgens L P H, Sloof W G. Promoting exclusive α-Al2O3 growth upon high-temperature oxidation of NiCrAl alloys: Experiment versus model predictions [J]. Acta Mater., 2005, 53: 1643
18 Nijdam T J, Van Der Pers N M, Sloof W G. Oxide phase development upon high temperature oxidation of γ-NiCrAl alloys [J]. Mater. Corros., 2006, 57: 269
19 Wang E P, Liu H F, Guo W, et al. Effect of pre-oxidation temperature on high-temperature cyclic oxidation resistance of Ni-15Cr-5Al-5Si alloy [J]. Mater. Mech. Eng., 2019, 43(2): 39
  王二鹏, 刘海飞, 郭 文 等. 预氧化温度对Ni-15Cr-5Al-5Si合金抗高温循环氧化性能的影响 [J]. 机械工程材料, 2019, 43(2): 39
20 Niu Y, Zhang X J, Wu Y, et al. The third-element effect in the oxidation of Ni-xCr-7Al (x=0, 5, 10, 15 at.%) alloys in 1 atm O2 at 900-1000oC [J]. Corros. Sci., 2006, 48: 4020
21 Zhang X J, Wang S Y, Gesmundo F, et al. The effect of Cr on the oxidation of Ni-10 at% Al in 1 atm O2 at 900-1000oC [J]. Oxid. Met., 2006, 65: 151
22 Wood G C. Fundamental factors determining the mode of scaling of heat-resistant alloys [J]. Werkst. Corros., 1971, 22: 491
23 Weiser M, Galetz M C, Chater R J, et al. Growth mechanisms of oxide scales on two-phase Co/Ni-base model alloys between 800oC and 900oC [J]. J. Electrochem. Soc., 2020, 167: 021504
24 Weiser M, Galetz M C, Zschau H E, et al. Influence of Co to Ni ratio in γ′-strengthened model alloys on oxidation resistance and the efficacy of the halogen effect at 900oC [J]. Corros. Sci., 2019, 156: 84
25 Gao B, Wang L, Liu Y, et al. High temperature oxidation behaviour of γ′-strengthened Co-based superalloys with different Ni addition [J]. Corros. Sci., 2019, 157: 109
26 Zenk C H, Neumeier S, Engl N M, et al. Intermediate Co/Ni-base model superalloys—Thermophysical properties, creep and oxidation [J]. Scr. Mater., 2016, 112: 83
27 Bastow B D, Whittle D P, Wood G C. Diffusion-controlled growth of solid solution scales on nickel-cobalt alloys [J]. Corros. Sci., 1976, 16: 57
28 Seraffon M, Simms N J, Sumner J, et al. The development of new bond coat compositions for thermal barrier coating systems operating under industrial gas turbine conditions [J]. Surf. Coat. Technol., 2011, 206: 1529
29 Seraffon M, Simms N J, Sumner J, et al. Oxidation behaviour of NiCrAl and NiCoCrAl bond coatings under industrial gas turbine conditions [J]. Oxid. Met., 2014, 81: 203
30 Ren Y J, Dai T, Guo X H, et al. Scaling behavior of four Co-20Ni-xCr-yAl (x = 8, 15 wt.%; y = 3, 5 wt.%) alloys exposed to 1 atm O2 at 1000oC and 1100oC [J]. Corros. Sci., 2021, 191: 109719
31 Ren Y J, Lv Y L, Dai T, et al. Oxidation behavior of ternary alloys Co-20Ni-3Al and Co-20Ni-5Al in 105 Pa O2 atmosphere at 800-1000oC [J]. J. Chin. Soc. Corros. Prot., 2022, 42: 995
  任延杰, 吕云蕾, 戴 汀 等. 三元Co-Ni-Al合金在800~1000℃纯氧中的氧化行为研究 [J]. 中国腐蚀与防护学报, 2022, 42: 995
文章导航

/