不锈钢纤维增强镁基仿生复合材料制备与力学性能
收稿日期: 2022-05-31
修回日期: 2022-09-29
网络出版日期: 2022-10-12
基金资助
国家重点研发计划项目(2020YFA0710404);国家自然科学基金项目(52173269;51871216;52101160);中国科学院青年创新促进会项目(2019191)
Fabrication and Mechanical Properties of Bioinspired Mg-Based Composites Reinforced by Stainless Steel Fibers
Received date: 2022-05-31
Revised date: 2022-09-29
Online published: 2022-10-12
Supported by
National Key Research and Development Program of China(2020YFA0710404);National Natural Science Foundation of China(52173269;51871216;52101160);Youth Innovation Promotion Association of Chinese Academy of Sciences(2019191)
天然鱼鳞由于具有独特的组织结构而表现出优异的力学性能,可为金属材料的组织结构优化设计提供有益启示。本工作利用Mg熔体浸渗不锈钢纤维编织骨架的方法,制备了具有类似天然鱼鳞的正交层合板和双螺旋层合板结构的镁基仿生复合材料,并选用二维平面随机取向结构作为对比,表征了复合材料的相组成、微观结构以及在室温与200℃条件下的力学性能,揭示了其微观结构与力学性能之间的关系。结果表明,镁基复合材料中不锈钢纤维能够起到显著的强化作用,并且其力学性能与微观结构密切相关。与二维平面随机取向结构相比,类鱼鳞仿生结构表现出更高的拉伸强度和塑性,并且能够通过不锈钢纤维从Mg基体中拔出促进变形和消耗能量。特别是,类鱼鳞双螺旋层合板结构在室温条件下塑性更高,而在高温条件下强度更高,其不同取向的纤维之间能够协调变形,诱导裂纹发生偏转,并减弱变形和损伤的局域化程度。
谢丽文 , 张立龙 , 刘艳艳 , 张明阳 , 王绍钢 , 焦大 , 刘增乾 , 张哲峰 . 不锈钢纤维增强镁基仿生复合材料制备与力学性能[J]. 金属学报, 2024 , 60(6) : 760 -769 . DOI: 10.11900/0412.1961.2022.00269
Mg and Mg-based alloys are distinguished by their high specific strength-to-density ratios but demonstrate low strengths at ambient to elevated temperatures. Producing Mg-based composites offers an effective means of strengthening Mg. Nevertheless, the mechanical properties of Mg-based composites are primarily dependent on their architectures. Here, bioinspired Mg-based composites with fish-scale-like orthogonal plywood and double-twisted Bouligand-type (i.e., double-Bouligand) architectures were fabricated by the pressureless infiltration of an Mg melt into the woven contextures of stainless steel fibers. The phase constitution, microstructure, and tensile properties of the composites at room temperature and 200oC were compared with a composite where stainless steel fibers were randomly oriented in-plane. The relationships between the microstructure and mechanical properties were also explored. The results showed that the stainless steel fibers played a notable role in strengthening the composites and were pulled out from the Mg matrix to promote plastic deformation and energy consumption. The mechanical properties of the composites were closely associated with their microstructures, with fish-scale-like architectures displaying higher strengths and larger plasticity than the randomly oriented ones. In particular, the double-Bouligand architecture allowed coordinated deformation between the fibers of different orientations and promoted crack deflection along the fibers, thereby alleviating the localization of deformation and damage in the composite. Therefore, it bestowed larger plasticity at room temperature and higher tensile strength at high temperature. By exploiting new bioinspired architectures, this study provides guidance for optimizing the architectural design of Mg-based composites to improve their mechanical properties.
| 1 | Pan F S, Jiang B. Development and application of plastic processing technologies of magnesium alloys [J]. Acta Metall. Sin., 2021, 57: 1362 |
| 潘复生, 蒋 斌. 镁合金塑性加工技术发展及应用 [J]. 金属学报, 2021, 57: 1362 | |
| 2 | Mordike B L, Ebert T. Magnesium: Properties-applications-Potential [J]. Mater. Sci. Eng., 2001, A302: 37 |
| 3 | Pollock T M. Weight loss with magnesium alloys [J]. Science, 2010, 328: 986 |
| 4 | Tian Y, Wu P P, Xiao L, et al. Technological advances in fabrication of magnesium matrix composites [J]. Mater. Rev., 2016, 30(19): 32 |
| 田 莹, 吴萍萍, 肖 旅 等. 镁基复合材料的制备技术进展 [J]. 材料导报, 2016, 30(19): 32 | |
| 5 | Li D J, Zeng X Q, Dong J, et al. Microstructure evolution of Mg-10Gd-3Y-1.2Zn-0.4Zr alloy during heat-treatment at 773 K [J]. J. Alloys Compd., 2009, 468: 164 |
| 6 | Luo A, Pekguleryuz M O. Cast magnesium alloys for elevated temperature applications [J]. J. Mater. Sci., 1994, 29: 5259 |
| 7 | Gu R C, Zhang J, Zhang M Y, et al. Fabrication of Mg-based composites reinforced by SiC whisker scaffolds with three-dimensional interpenetrating-phase architecture and their mechanical properties [J]. Acta Metall. Sin., 2022, 58: 857 |
| 谷瑞成, 张 健, 张明阳 等. 三维互穿结构SiC晶须骨架增强镁基复合材料制备及其力学性能 [J]. 金属学报, 2022, 58: 857 | |
| 8 | Ferkel H, Mordike B L. Magnesium strengthened by SiC nanoparticles [J]. Mater. Sci. Eng., 2001, A298: 193 |
| 9 | Wang X J, Xu D K, Wu R Z, et al. What is going on in magnesium alloys? [J]. J. Mater. Sci. Technol., 2018, 34: 245 |
| 10 | Wang S G, Xu J. Strengthening and toughening of Mg-based bulk metallic glass via in-situ formed B2-type AgMg phase [J]. J. Non-Cryst. Solids, 2013, 379: 40 |
| 11 | Pan H C, Qin G W, Xu M, et al. Enhancing mechanical properties of Mg-Sn alloys by combining addition of Ca and Zn [J]. Mater. Des., 2015, 83: 736 |
| 12 | Habibi M K, Joshi S P, Gupta M. Hierarchical magnesium nano-composites for enhanced mechanical response [J]. Acta Mater., 2010, 58: 6104 |
| 13 | Habibnejad-Korayem M, Mahmudi R, Poole W J. Enhanced properties of Mg-based nano-composites reinforced with Al2O3 nano-particles [J]. Mater. Sci. Eng., 2009, A519: 198 |
| 14 | Li D J, Wang Q D, Blandin J J, et al. High temperature compressive deformation behavior of an extruded Mg-8Gd-3Y-0.5Zr (wt. %) alloy [J]. Mater. Sci. Eng., 2009, A526: 150 |
| 15 | Wang L Q, Ren Y P, Sun S N, et al. Microstructure, mechanical properties and fracture behavior of as-extruded Zn-Mg binary alloys [J]. Acta Metall. Sin. (Engl. Lett.), 2017, 30: 931 |
| 16 | Luo A. Processing, microstructure, and mechanical behavior of cast magnesium metal matrix composites [J]. Metall. Mater. Trans., 1995, 26A: 2445 |
| 17 | Lloyd D J. Particle reinforced aluminium and magnesium matrix composites [J]. Int. Mater. Rev., 1994, 39: 1 |
| 18 | Mayer G. Rigid biological systems as models for synthetic composites [J]. Science, 2005, 310: 1144 |
| 19 | Munch E, Launey M E, Alsem D H, et al. Tough, bio-inspired hybrid materials [J]. Science, 2008, 322: 1516 |
| 20 | Tan G Q, Zhang J, Zheng L, et al. Nature-inspired nacre-like composites combining human tooth-matching elasticity and hardness with exceptional damage tolerance [J]. Adv. Mater., 2019, 31: 1904603 |
| 21 | Liu Z Q, Meyers M A, Zhang Z F, et al. Functional gradients and heterogeneities in biological materials: Design principles, functions, and bioinspired applications [J]. Prog. Mater. Sci., 2017, 88: 467 |
| 22 | Dastjerdi A K, Barthelat F. Teleost fish scales amongst the toughest collagenous materials [J]. J. Mech. Behav. Biomed. Mater., 2015, 52: 95 |
| 23 | Zimmermann E A, Gludovatz B, Schaible E, et al. Mechanical adaptability of the Bouligand-type structure in natural dermal armour [J]. Nat. Commun., 2013, 4: 2634 |
| 24 | Suksangpanya N, Yaraghi N A, Kisailus D, et al. Twisting cracks in Bouligand structures [J]. J. Mech. Behav. Biomed. Mater., 2017, 76: 38 |
| 25 | Ikoma T, Kobayashi H, Tanaka J, et al. Microstructure, mechanical, and biomimetic properties of fish scales from Pagrus major [J]. J. Struct. Biol., 2003, 142: 327 |
| 26 | Suksangpanya N, Yaraghi N A, Pipes R B, et al. Crack twisting and toughening strategies in Bouligand architectures [J]. Int. J. Solids Struct., 2018, 150: 83 |
| 27 | Quan H C, Yang W, Schaible E, et al. Novel defense mechanisms in the armor of the scales of the “living fossil” Coelacanth fish [J]. Adv. Funct. Mater., 2018, 28: 1804237 |
| 28 | Yin S, Yang W, Kwon J, et al. Hyperelastic phase-field fracture mechanics modeling of the toughening induced by Bouligand structures in natural materials [J]. J. Mech. Phys. Solids, 2019, 131: 204 |
| 29 | Yang F, Xie W H, Meng S H. Analysis and simulation of fracture behavior in naturally occurring Bouligand structures [J]. Acta Biomater., 2021, 135: 473 |
| 30 | Song Z Q, Ni Y, Cai S Q. Fracture modes and hybrid toughening mechanisms in oscillated/twisted plywood structure [J]. Acta Biomater., 2019, 91: 284 |
| 31 | Quan H C, Yang W, Lapeyriere M, et al. Structure and mechanical adaptability of a modern elasmoid fish scale from the common carp [J]. Matter, 2020, 3: 842 |
| 32 | Chen S M, Gao H L, Zhu Y B, et al. Biomimetic twisted plywood structural materials [J]. Natl. Sci. Rev., 2018, 5: 703 |
| 33 | Huang W, Restrepo D, Jung J Y, et al. Multiscale toughening mechanisms in biological materials and bioinspired designs [J]. Adv. Mater., 2019, 31: 1901561 |
| 34 | Grunenfelder L K, Suksangpanya N, Salinas C, et al. Bio-inspired impact-resistant composites [J]. Acta Biomater., 2014, 10: 3997 |
| 35 | Zhang Y, Tan G Q, Zhang M Y, et al. Bioinspired tungsten-copper composites with Bouligand-type architectures mimicking fish scales [J]. J. Mater. Sci. Technol., 2022, 96: 21 |
| 36 | Liu Y Y, Yu Q, Tan G Q, et al. Bioinspired fish-scale-like magnesium composites strengthened by contextures of continuous titanium fibers: Lessons from Nature [J]. J. Magnes. Alloy., 2023, 11: 869 |
| 37 | Zhang M Y, Zhao N, Yu Q, et al. On the damage tolerance of 3-D printed Mg-Ti interpenetrating-phase composites with bioinspired architectures [J]. Nat. Commun., 2022, 13: 3247 |
| 38 | Wang S G, Wang S C, Zhang L. Application of high resolution transmission X-ray tomography in material science [J]. Acta Metall. Sin., 2013, 49: 897 |
| 王绍钢, 王苏程, 张 磊. 高分辨透射X射线三维成像在材料科学中的应用 [J]. 金属学报, 2013, 49: 897 | |
| 39 | Hufenbach W, Ullrich H, Gude M, et al. Manufacture studies and impact behaviour of light metal matrix composites reinforced by steel wires [J]. Arch. Civ. Mech. Eng., 2012, 12: 265 |
| 40 | Li Q Y, Li J, He G. Compressive properties and damping capacities of magnesium reinforced with continuous steel wire [J]. Mater. Sci. Eng., 2017, A680: 92 |
| 41 | Wu S X, Wang S R, Wen D S, et al. Microstructure and mechanical properties of magnesium matrix composites interpenetrated by different reinforcement [J]. Appl. Sci., 2018, 8: 2012 |
| 42 | Bowman R R, Misra A K, Arnold S M. Processing and mechanical properties of Al2O3 fiber-reinforced NiAl composites [J]. Metall. Mater. Trans., 1995, 26A: 615 |
| 43 | Lin Z, Li V C. Crack bridging in fiber reinforced cementitious composites with slip-hardening interfaces [J]. J. Mech. Phys. Solids, 1997, 45: 763 |
| 44 | Liu Z Q, Zhang Y Y, Zhang M Y, et al. Adaptive structural reorientation: Developing extraordinary mechanical properties by constrained flexibility in natural materials [J]. Acta Biomater., 2019, 86: 96 |
| 45 | Hassan S F, Gupta M. Development of ductile magnesium composite materials using titanium as reinforcement [J]. J. Alloys Compd., 2002, 345: 246 |
/
| 〈 |
|
〉 |