金属材料的构型化复合与强韧化
收稿日期: 2022-07-27
修回日期: 2022-08-21
网络出版日期: 2022-09-19
基金资助
国家自然科学基金项目(52192592);国家自然科学基金项目(52192595);国家自然科学基金项目(52171143);国家自然科学基金项目(51871149)
Architecture Design Strategies and Strengthening-Toughening Mechanisms of Metal Matrix Composites
Received date: 2022-07-27
Revised date: 2022-08-21
Online published: 2022-09-19
Supported by
National Natural Science Foundation of China(52192592);National Natural Science Foundation of China(52192595);National Natural Science Foundation of China(52171143);National Natural Science Foundation of China(51871149)
范根莲 , 郭峙岐 , 谭占秋 , 李志强 . 金属材料的构型化复合与强韧化[J]. 金属学报, 2022 , 58(11) : 1416 -1426 . DOI: 10.11900/0412.1961.2022.00355
The mechanical properties of metal matrix composites depend on not only the content of the reinforcements but also the composite architecture (shape, size, and spatial distribution). This paper focuses on the heterogeneous architecture design of metal matrix composites, including the heterogeneous architecture design of reinforcements and the intrinsic heterogeneous design of the matrix. In addition, it summarizes the development process of scale refinement, size quantification, and structural parameter diversification of metal matrix composite architecture design. The future development direction of architectural composite and the strengthening and toughing design of metal matrix composites based on the energy dissipation theory is also proposed.
| 1 | Zhang D, Zhang G D, Li Z Q. The current state and trend of metal matrix composites [J]. Mater. China, 2010, 29(4): 1 |
| 1 | 张 荻, 张国定, 李志强. 金属基复合材料的现状与发展趋势 [J]. 中国材料进展, 2010, 29(4): 1 |
| 2 | Wu G H, Kuang Z Y. Opportunities and challenges for metal matrix composites in the context of equipment upgrading [J]. Strategic Study CAE, 2020, 22(2): 79 |
| 2 | 武高辉, 匡泽洋. 装备升级换代背景下金属基复合材料的发展机遇和挑战 [J]. 中国工程科学, 2020, 22(2): 79 |
| 3 | Ibrahim I A, Mohamed F A, Lavernia E J. Particulate reinforced metal matrix composites—A review [J]. J. Mater. Sci., 1991, 26: 1137 |
| 4 | Rawal S P. Metal-matrix composites for space applications [J]. JOM, 2001, 53(4): 14 |
| 5 | Miracle D B. Metal matrix composites—From science to technological significance [J]. Compos. Sci. Technol., 2005, 65: 2526 |
| 6 | Tjong S C. Recent progress in the development and properties of novel metal matrix nanocomposites reinforced with carbon nanotubes and graphene nanosheets [J]. Mater. Sci. Eng., 2013, R74: 281 |
| 7 | Huang L J, An Q, Geng L, et al. Multiscale architecture and superior high-temperature performance of discontinuously reinforced titanium matrix composites [J]. Adv. Mater., 2021, 33: 2000688 |
| 8 | Kumar P L, Lombardi A, Byczynski G, et al. Recent advances in aluminium matrix composites reinforced with graphene-based nanomaterial: A critical review [J]. Prog. Mater. Sci., 2022, 128: 100948 |
| 9 | Wu G H, Qiao J, Jiang L T. Research progress on principle of dimensional stability and stabilization design of Al and its composites [J]. Acta Metall. Sin., 2019, 55: 33 |
| 9 | 武高辉, 乔 菁, 姜龙涛. Al及其复合材料尺寸稳定性原理与稳定化设计研究进展 [J]. 金属学报, 2019, 55: 33 |
| 10 | Bakshi S R, Lahiri D, Agarwal A. Carbon nanotube reinforced metal matrix composites—A review [J]. Int. Mater. Rev., 2010, 55: 41 |
| 11 | Withers P J, Preuss M. Fatigue and damage in structural materials studied by X-ray tomography [J]. Annu. Rev. Mater. Res., 2012, 42: 81 |
| 12 | Fan G H, Geng L, Wu H, et al. Improving the tensile ductility of metal matrix composites by laminated structure: A coupled X-ray tomography and digital image correlation study [J]. Scr. Mater., 2017, 135: 63 |
| 13 | Bakshi S R, Agarwal A. An analysis of the factors affecting strengthening in carbon nanotube reinforced aluminum composites [J]. Carbon, 2011, 49: 533 |
| 14 | Barai P, Weng G J. A theory of plasticity for carbon nanotube reinforced composites [J]. Int. J. Plast., 2011, 27: 539 |
| 15 | Kwon H, Park D H, Silvain J F, et al. Investigation of carbon nanotube reinforced aluminum matrix composite materials [J]. Compos. Sci. Technol., 2010, 70: 546 |
| 16 | Chen B, Jia L, Li S F, et al. In situ synthesized Al4C3 nanorods with excellent strengthening effect in aluminum matrix composites [J]. Adv. Eng. Mater., 2014, 16: 972 |
| 17 | Ritchie R O. The conflicts between strength and toughness [J]. Nat. Mater., 2011, 10: 817 |
| 18 | Meyers M A, McKittrick J, Chen P Y. Structural biological materials: Critical mechanics-materials connections [J]. Science, 2013, 339: 773 |
| 19 | Barthelat F, Yin Z, Buehler M J. Structure and mechanics of interfaces in biological materials [J]. Nat. Rev. Mater., 2016, 1: 16007 |
| 20 | Libonati F, Buehler M J. Advanced structural materials by bioinspiration [J]. Adv. Eng. Mater., 2017, 19: 1600787 |
| 21 | Gao H L, Chen S M, Mao L B, et al. Mass production of bulk artificial nacre with excellent mechanical properties [J]. Nat. Commun., 2017, 8: 287 |
| 22 | Grishaber R B, Sergueeva A V, Mishra R S, et al. Laminated metal composites—High temperature deformation behavior [J]. Mater. Sci. Eng., 2005, A403: 17 |
| 23 | Liu B X, Huang L J, Geng L, et al. Fabrication and superior ductility of laminated Ti-TiBw/Ti composites by diffusion welding [J]. J. Alloys Compd., 2014, 602: 187 |
| 24 | Liu B X, Huang L J, Rong X D, et al. Bending behaviors and fracture characteristics of laminatedductile-tough composites under different modes [J]. Compos. Sci. Technol., 2016, 126: 94 |
| 25 | Liu B X, Huang L J, Kaveendran B, et al. Tensile and bending behaviors and characteristics of laminated Ti-(TiBw/Ti) composites with different interface status [J]. Composites, 2017, 108B: 377 |
| 26 | Huang C X, Wang Y F, Ma X L, et al. Interface affected zone for optimal strength and ductility in heterogeneous laminate [J]. Mater. Today, 2018, 21: 713 |
| 27 | Qin S Y, Zhang G D. Preparation of high fracture performance SiCp-6061A1/6061A1 composite [J]. Mater. Sci. Eng., 2000, A279: 231 |
| 28 | Liu C, Qin S Y, Zhang G D, et al. Micromechanical properties of high fracture performance SiCp-6061Al/6061Al composite [J]. Mater. Sci. Eng., 2002, A332: 203 |
| 29 | Chen L, Hou Z C, Liu Y F, et al. High strength and high ductility copper matrix composite reinforced by graded distribution of carbon nanotubes [J]. Composites, 2020, 138A: 106063 |
| 30 | Guo C, Guo S W, Cheng Y, et al. Bending mechanical properties and its evaluation of aluminium alloy matrix gradient composites reinforced with SiC particles [J]. Acta Mater. Compos. Sin., 2002, 19(6): 57 |
| 30 | 郭 成, 郭生武, 程 羽 等. SiC颗粒增强铝合金基梯度复合材料弯曲力学性能及其评价 [J]. 复合材料学报, 2002, 19(6): 57 |
| 31 | Wang W R, Xie H F, Xie L, et al. Fabrication of ceramics/high-entropy alloys gradient composites by combustion synthesis in ultra-high gravity field [J]. Mater. Lett., 2018, 233: 4 |
| 32 | Moon R J, Tilbrook M, Hoffman M, et al. Al-Al2O3 composites with interpenetrating network structures: Composite modulus estimation [J]. J. Am. Ceram. Soc., 2005, 88: 666 |
| 33 | Dong Z Q, Zhang L, Chen W X. Evaluation of Cu-Cr3C2 composite with interpenetrating network [J]. Mater. Sci. Eng., 2012, A552: 24 |
| 34 | Kaveendran B, Wang G S, Huang L J, et al. In situ (Al3Zr + Al2O3np)/2024Al metal matrix composite with novel reinforcement distributions fabricated by reaction hot pressing [J]. J. Alloys Compd., 2013, 581: 16 |
| 35 | Jiao Y, Huang L J, Duan T B, et al. Controllable two-scale network architecture and enhanced mechanical properties of (Ti5Si3 + TiBw)/Ti6Al4V composites [J]. Sci. Rep., 2016, 6: 32991 |
| 36 | De Castro V, Leguey T, Muñoz A, et al. Microstructure and tensile properties of Y2O3-dispersed titanium produced by arc melting [J]. Mater. Sci. Eng., 2006, A422: 189 |
| 37 | Yang Z F, Lu W J, Qin J N, et al. Microstructural characterization of Nd2O3 in in situ synthesized multiple-reinforced (TiB + TiC + Nd2O3)/Ti composites [J]. J. Alloys Compd., 2006, 425: 379 |
| 38 | Xiao L, Lu W J, Qin J N, et al. Creep behaviors and stress regions of hybrid reinforced high temperature titanium matrix composite [J]. Compos. Sci. Technol., 2009, 69: 1925 |
| 39 | Zhang X, Shi C S, Liu E Z, et al. Achieving high strength and high ductility in metal matrix composites reinforced with a discontinuous three-dimensional graphene-like network [J]. Nanoscale, 2017, 9: 11929 |
| 40 | Shen M J, Wang X J, Li C D, et al. Effect of bimodal size SiC particulates on microstructure and mechanical properties of AZ31B magnesium matrix composites [J]. Mater. Des., 2013, 52: 1011 |
| 41 | Chand S, Chandrasekhar P, Sarangi R K, et al. Influence of B4C particles on processing and strengthening mechanisms in aluminum metal matrix composites—A review [J]. Mater. Today: Proc., 2019, 18: 5356 |
| 42 | Khorshid M T, Jahromi S A J, Moshksar M M. Mechanical properties of tri-modal Al matrix composites reinforced by nano- and submicron-sized Al2O3 particulates developed by wet attrition milling and hot extrusion [J]. Mater. Des., 2010, 31: 3880 |
| 43 | Kai X Z, Li Z Q, Fan G L, et al. Strong and ductile particulate reinforced ultrafine-grained metallic composites fabricated by flake powder metallurgy [J]. Scr. Mater., 2013, 68: 555 |
| 44 | Xie K W, Nie J F, Ma X, et al. Increasing the ductility of heat-resistant AlNp/Al composites by submicron Al2O3 particles [J]. Mater. Charact., 2020, 170: 110672 |
| 45 | Carvalho O, Buciumeanu M, Madeira S, et al. Mechanisms governing the mechanical behavior of an AlSi-CNTs-SiCp hybrid composite [J]. Composites, 2016, 90B: 443 |
| 46 | Li S S, Su Y S, Zhu X H, et al. Enhanced mechanical behavior and fabrication of silicon carbide particles covered by in-situ carbon nanotube reinforced 6061 aluminum matrix composites [J]. Mater. Des., 2016, 107: 130 |
| 47 | Qiu C H, Su Y S, Yang J Y, et al. Microstructural characteristics and mechanical behavior of SiC(CNT)/Al multiphase interfacial micro-zones via molecular dynamics simulations [J]. Composites, 2021, 220B: 108996 |
| 48 | Fan G L, Xu R, Tan Z Q, et al. Development of flake powder metallurgy in fabricating metal matrix composites: A review [J]. Acta Metall. Sin. (Engl. Lett.), 2014, 27: 806 |
| 49 | Xu R, Tan Z Q, Fan G L, et al. Microstructure-based modeling on structure-mechanical property relationships in carbon nanotube/aluminum composites [J]. Int. J. Plast., 2019, 120: 278 |
| 50 | Jiang L, Li Z Q, Fan G L, et al. A flake powder metallurgy approach to Al2O3/Al biomimetic nanolaminated composites with enhanced ductility [J]. Scr. Mater., 2011, 65: 412 |
| 51 | Jiang Y Y, Xu R, Tan Z Q, et al. Interface-induced strain hardening of graphene nanosheet/aluminum composites [J]. Carbon, 2019, 146: 17 |
| 52 | Zhang Z M, Fan G L, Tan Z Q, et al. Towards the strength-ductility synergy of Al2O3/Al composite through the design of roughened interface [J]. Composites, 2021, 224B: 109251 |
| 53 | Cao M, Xiong D B, Tan Z Q, et al. Aligning graphene in bulk copper: Nacre-inspired nanolaminated architecture coupled with in-situ processing for enhanced mechanical properties and high electrical conductivity [J]. Carbon, 2017, 117: 65 |
| 54 | Li Z, Guo Q, Li Z Q, et al. Enhanced mechanical properties of graphene (reduced graphene oxide)/aluminum composites with a bioinspired nanolaminated structure [J]. Nano Lett., 2015, 15: 8077 |
| 55 | Zhang Z M, Fan G L, Tan Z Q, et al. Bioinspired multiscale Al2O3-rGO/Al laminated composites with superior mechanical properties [J]. Composites, 2021, 217B: 108916 |
| 56 | Yang L, Gao Q, Liu H, et al. Fabrication and properties of dual-gradient nanostructured copper matrix composites reinforced by silicon carbide particles [J]. Powder Metall. Technol., 2016, 34: 428 |
| 56 | 杨 雷, 高 求, 刘 鸿 等. 碳化硅颗粒强化铜基双梯度纳米结构复合材料的制备及性能 [J]. 粉末冶金技术, 2016, 34: 428 |
| 57 | Ye J C, Han B Q, Lee Z, et al. A tri-modal aluminum based composite with super-high strength [J]. Scr. Mater., 2005, 53: 481 |
| 58 | Zhang Z H, Topping T, Li Y, et al. Mechanical behavior of ultrafine-grained Al composites reinforced with B4C nanoparticles [J]. Scr. Mater., 2011, 65: 652 |
| 59 | Zan Y N, Zhou Y T, Liu Z Y, et al. Enhancing strength and ductility synergy through heterogeneous structure design in nanoscale Al2O3 particulate reinforced Al composites [J]. Mater. Des., 2019, 166: 107629 |
| 60 | Fu X W, Yu Z Y, Tan Z Q, et al. Enhanced strain hardening by bimodal grain structure in carbon nanotube reinforced Al-Mg composites [J]. Mater. Sci. Eng., 2021, A803: 140726 |
| 61 | Ma K, Liu Z Y, Liu K, et al. Structure optimization for improving the strength and ductility of heterogeneous carbon nanotube/Al-Cu-Mg composites [J]. Carbon, 2021, 178: 190 |
| 62 | Liu Z Y, Ma K, Fan G H, et al. Enhancement of the strength-ductility relationship for carbon nanotube/Al-Cu-Mg nanocomposites by material parameter optimisation [J]. Carbon, 2020, 157: 602 |
| 63 | Fu X W, Tan Z Q, Min X R, et al. Trimodal grain structure enables high-strength CNT/Al-Cu-Mg composites higher ductility by powder assembly & alloying [J]. Mater. Res. Lett., 2021, 9: 50 |
| 64 | Fu X W, Tan Z Q, Ma Z Q, et al. Powder assembly & alloying to CNT/Al-Cu-Mg composites with trimodal grain structure and strength-ductility synergy [J]. Composites, 2021, 225B: 109271 |
| 65 | Luo X, Zhao K, He X, et al. Evading strength and ductility trade-off in an inverse nacre structured magnesium matrix nanocomposite [J]. Acta Mater., 2022, 228: 117730 |
| 66 | Gao H J, Ji B H, Jäger I L, et al. Materials become insensitive to flaws at nanoscale: Lessons from nature [J]. Proc. Natl. Acad. Sci. USA, 2003, 100: 5597 |
| 67 | Wang H Y, Li C, Li Z G, et al. Current research and future prospect on the preparation and architecture design of nanomaterials reinforced light metal matrix composites [J]. Acta Metall. Sin., 2019, 55: 683 |
| 67 | 王慧远, 李 超, 李志刚 等. 纳米增强体强化轻合金复合材料制备及构型设计研究进展与展望 [J]. 金属学报, 2019, 55: 683 |
| 68 | Zhao N Q, Liu X H, Pu B W. Progress on multi-dimensional carbon nanomaterials reinforced aluminum matrix composites: A review [J]. Acta Metall. Sin., 2019, 55: 1 |
| 68 | 赵乃勤, 刘兴海, 蒲博闻. 多维度碳纳米相增强铝基复合材料研究进展 [J]. 金属学报, 2019, 55: 1 |
| 69 | Liu G, Zhang G J, Jiang F, et al. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility [J]. Nat. Mater., 2013, 12: 344 |
| 70 | So K P, Kushima A, Park J G, et al. Intragranular dispersion of carbon nanotubes comprehensively improves aluminum alloys [J]. Adv. Sci., 2018, 5: 1800115 |
| 71 | Liu Q B, Fan G L, Tan Z Q, et al. Reinforcement with intragranular dispersion of carbon nanotubes in aluminum matrix composites [J]. Composites, 2021, 217B: 108915 |
| 72 | Liu Q B, Fan G L, Tan Z Q, et al. Effect of thermomechanical treatment and length-scales on spatial distribution of CNTs in Al matrix [J]. Carbon, 2022, 190: 384 |
| 73 | Zhang D L. Ultrafine grained metals and metal matrix nanocomposites fabricated by powder processing and thermomechanical powder consolidation [J]. Prog. Mater. Sci., 2021, 119: 100796 |
| 74 | Xiao B L, Huang Z Y, Ma K, et al. Research on hot deformation behaviors of discontinuously reinforced aluminum composites [J]. Acta Metall. Sin., 2019, 55: 59 |
| 74 | 肖伯律, 黄治冶, 马 凯 等. 非连续增强铝基复合材料的热变形行为研究进展 [J]. 金属学报, 2019, 55: 59 |
| 75 | Schwarze C, Kamachali R D, Steinbach I. Phase-field study of zener drag and pinning of cylindrical particles in polycrystalline materials [J]. Acta Mater., 2016, 106: 59 |
| 76 | Li Y, Lin Y J, Xiong Y H, et al. Extended twinning phenomena in Al-4%Mg alloys/B4C nanocomposite [J]. Scr. Mater., 2011, 64: 133 |
| 77 | Wang H, Geng H W, Zhou D S, et al. Multiple strengthening mechanisms in high strength ultrafine-grained Al-Mg alloys [J]. Mater. Sci. Eng., 2020, A771: 138613 |
| 78 | Hao S J, Cui L S, Jiang D Q, et al. A transforming metal nanocomposite with large elastic strain, low modulus, and high strength [J]. Science, 2013, 339: 1191 |
| 79 | Ni D R, Ma Z Y. Shape memory alloy-reinforced metal-matrix composites: A review [J]. Acta Metall. Sin. (Engl. Lett.), 2014, 27: 739 |
| 80 | Yang M X, Yan D S, Yuan F P, et al. Dynamically reinforced heterogeneous grain structure prolongs ductility in a medium-entropy alloy with gigapascal yield strength [J]. Proc. Natl. Acad. Sci. USA, 2018, 115: 7224 |
| 81 | Yang M X, Pan Y, Yuan F P, et al. Back stress strengthening and strain hardening in gradient structure [J]. Mater. Res. Lett., 2016, 4: 145 |
| 82 | Wu X L, Zhu Y T. Heterogeneous materials: A new class of materials with unprecedented mechanical properties [J]. Mater. Res. Lett., 2017, 5: 527 |
| 83 | Zhu Y T, Wu X L. Perspective on hetero-deformation induced (HDI) hardening and back stress [J]. Mater. Res. Lett., 2019, 7: 393 |
| 84 | Shuai L F, Huang T L, Yu T B, et al. Segregation and precipitation stabilizing an ultrafine lamellar-structured Al-0.3%Cu alloy [J]. Acta Mater., 2021, 206: 116595 |
| 85 | Li X Y, Lu L, Li J G, et al. Mechanical properties and deformation mechanisms of gradient nanostructured metals and alloys [J]. Nat. Rev. Mater., 2020, 5: 706 |
| 86 | Shen M J, Wang X J, Zhang M F, et al. Significantly improved strength and ductility in bimodal-size grained microstructural magnesium matrix composites reinforced by bimodal sized SiCp over traditional magnesium matrix composites [J]. Compos. Sci. Technol., 2015, 118: 85 |
| 87 | Sun H, Saba F, Fan G L, et al. Micro/nano-reinforcements in bimodal-grained matrix: A heterostructure strategy for toughening particulate reinforced metal matrix composites [J]. Scr. Mater., 2022, 217: 114774 |
| 88 | Shi P J, Li R G, Li Y, et al. Hierarchical crack buffering triples ductility in eutectic herringbone high-entropy alloys [J]. Science, 2021, 373: 912 |
| 89 | Liu L, Yu Q, Wang Z, et al. Making ultrastrong steel tough by grain-boundary delamination [J]. Science, 2020, 368: 1347 |
| 90 | Wang D, Xiao B L, Ni D R, et al. Friction stir welding of discontinuously reinforced aluminum matrix composites: A review [J]. Acta Metall. Sin. (Engl. Lett.), 2014, 27: 816 |
| 91 | Avettand-Fènoël M N, Simar A. A review about friction stir welding of metal matrix composites [J]. Mater. Charact., 2016, 120: 1 |
| 92 | Dadkhah M, Mosallanejad M H, Iuliano L, et al. A comprehensive overview on the latest progress in the additive manufacturing of metal matrix composites: Potential, challenges, and feasible solutions [J]. Acta Metall. Sin. (Engl. Lett.), 2021, 34: 1173 |
| 93 | Tang S Y, Ummethala R, Suryanarayana C, et al. Additive manufacturing of aluminum-based metal matrix composites—A review [J]. Adv. Eng. Mater., 2021, 23: 2100053 |
| 94 | Zhang S, Van Dijk N, Van Der Zwaag S. A review of self-healing metals: Fundamentals, design principles and performance [J]. Acta Metall. Sin. (Engl. Lett.), 2020, 33: 1167 |
| 95 | Chen K X, Li L. Ordered structures with functional units as a paradigm of material design [J]. Adv. Mater., 2019, 31: 1901115 |
| 96 | Zhang X X, Zheng Z, Gao Y, et al. Progress in high throughput fabrication and characterization of metal matrix composites [J]. Acta Metall. Sin., 2019, 55: 109 |
| 96 | 张学习, 郑 忠, 高 莹 等. 金属基复合材料高通量制备及表征技术研究进展 [J]. 金属学报, 2019, 55: 109 |
| 97 | Roters F, Eisenlohr P, Hantcherli L, et al. Overview of constitutive laws, kinematics, homogenization and multiscale methods in crystal plasticity finite-element modeling: Theory, experiments, applications [J]. Acta Mater., 2010, 58: 1152 |
| 98 | Qiu C H, Su Y S, Yang J Y, et al. Structural modelling and mechanical behaviors of graphene/carbon nanotubes reinforced metal matrix composites via atomic-scale simulations: A review [J]. Composites, 2021, 4C: 100120 |
/
| 〈 |
|
〉 |