稀土元素La对AlMgSi合金性能和微结构的影响
收稿日期: 2022-06-16
修回日期: 2022-07-26
网络出版日期: 2022-08-29
基金资助
国家自然科学基金项目(52001119);国家自然科学基金项目(51831004);国家自然科学基金项目(52171006)
Impacts of Rare Earth Element La on Properties and Microstructure of AlMgSi Alloys
Received date: 2022-06-16
Revised date: 2022-07-26
Online published: 2022-08-29
Supported by
National Natural Science Foundation of China(52001119);National Natural Science Foundation of China(51831004);National Natural Science Foundation of China(52171006)
微合金化是改善铝合金性能及微观结构的有效方法。本工作采用硬度、导电率和拉伸性能测试,以及SEM和TEM等表征分析手段,研究了不同含量La的添加对Al-0.75Mg-0.75Si (质量分数,%)合金性能和微观结构的影响。结果表明,随着La添加量的提高,(1) 合金的塑性和导电率逐渐提高,这是由于La诱导形成的AlSiLa第二相的含量及其溶质原子Si消耗量逐渐增多;(2) 合金的强度先上升后下降,强度的上升主要归因于AlSiLa相的强化作用及晶粒细化作用逐渐增大,强度的下降主要归因于固溶强化作用的减小;(3) 合金人工时效过程中析出相的类型逐渐发生改变:加La合金峰值时效态除形成β″相外,还会析出多晶β″相,而过时效态会析出β″/U2、β′/U2和β′/U2/β″复合相。
郑雄 , 赖玉香 , 向雪梅 , 陈江华 . 稀土元素La对AlMgSi合金性能和微结构的影响[J]. 金属学报, 2024 , 60(1) : 107 -116 . DOI: 10.11900/0412.1961.2022.00298
The 6xxx series aluminum alloys Al-Mg-Si(-Cu) are widely used in the automotive industry owing to their high strength-to-weight ratio, good formability, and corrosion resistance. Micro-alloying is an effective technique for enhancing the properties and microstructure of Al alloys. The effects of varying La additions on the microstructure and properties of Al-0.75Mg-0.75Si (mass fraction, %) alloy have been investigated using hardness, electrical conductivity, and tensile tests, as well as SEM and TEM. As the La content increases, the following observations are made: (1) the ductility and electrical conductivity of the alloy gradually increase due to the increase in the fraction of the AlSiLa secondary phases induced by the La addition and the amount of Si solute atoms consumed by these phases; (2) the strength of the alloy first increases due to the increase in the secondary-phase strengthening contribution of the AlSiLa phases and the grain refinement contribution, and then decreases owing to the decrease in the solid-solution strengthening contribution; and (3) the types of precipitates formed during aging gradually change; besides the β″ phase, polycrystalline β″ precipitates are also precipitated in the peak-aged alloys with La addition, while β″/U2, β′/U2, and β′/U2/β″ composite precipitates are precipitated in the over-aging condition of the La-added alloys.
| 1 | Williams J C, Starke Jr E A. Progress in structural materials for aerospace systems [J]. Acta Mater., 2003, 51: 5775 |
| 2 | Pantelakis S G, Alexopoulos N D. Assessment of the ability of conventional and advanced wrought aluminum alloys for mechanical performance in light-weight applications [J]. Mater. Des., 2008, 29: 80 |
| 3 | Zandbergen H W, Andersen S J, Jansen J. Structure determination of Mg5Si6 particles in Al by dynamic electron diffraction studies [J]. Science, 1997, 277: 1221 |
| 4 | Murayama M, Hono K. Pre-precipitate clusters and precipitation processes in Al-Mg-Si alloys [J]. Acta Mater., 1999, 47: 1537 |
| 5 | Chen J H, Costan E, van Huis M A, et al. Atomic pillar-based nanoprecipitates strengthen AlMgSi alloys [J]. Science, 2006, 312: 416 |
| 6 | Vissers R, van Huis M A, Jansen J, et al. The crystal structure of the β' phase in Al-Mg-Si alloys [J]. Acta Mater., 2007, 55: 3815 |
| 7 | Chen H N, Lu J B, Kong Y, et al. Atomic scale investigation of the crystal structure and interfaces of the B' precipitate in Al-Mg-Si alloys [J]. Acta Mater., 2020, 185: 193 |
| 8 | Andersen S J, Marioara C D, Vissers R, et al. The structural relation between precipitates in Al-Mg-Si alloys, the Al-matrix and diamond silicon, with emphasis on the trigonal phase U1-MgAl2Si2 [J]. Mater. Sci. Eng., 2007, A444: 157 |
| 9 | Andersen S J, Marioara C D, Fr?seth A, et al. Crystal structure of the orthorhombic U2-Al4Mg4Si4 precipitate in the Al-Mg-Si alloy system and its relation to the β' and β" phases [J]. Mater. Sci. Eng., 2005, A390: 127 |
| 10 | Lai Y X, Jiang B C, Liu C H, et al. Low-alloy-correlated reversal of the precipitation sequence in Al-Mg-Si alloys [J]. J. Alloys Compd., 2017, 701: 94 |
| 11 | Lai Y X, Fan W, Yin M J, et al. Structures and formation mechanisms of dislocation-induced precipitates in relation to the age-hardening responses of Al-Mg-Si alloys [J]. J. Mater. Sci. Technol., 2020, 41: 127 |
| 12 | Hirth S M, Marshall G J, Court S A, et al. Effects of Si on the aging behaviour and formability of aluminium alloys based on AA6016 [J]. Mater. Sci. Eng., 2001, A319-321: 452 |
| 13 | Jin M, Li J, Shao G J. The effects of Cu addition on the microstructure and thermal stability of an Al-Mg-Si alloy [J]. J. Alloys Compd., 2007, 437: 146 |
| 14 | Xiao Q, Liu H Q, Yi D Q, et al. Effect of Cu content on precipitation and age-hardening behavior in Al-Mg-Si-xCu alloys [J]. J. Alloys Compd., 2017, 695: 1005 |
| 15 | Saito T, Wenner S, Osmundsen E, et al. The effect of Zn on precipitation in Al-Mg-Si alloys [J]. Philos. Mag., 2014, 94: 2410 |
| 16 | Saito T, Ehlers F J H, Lefebvre W, et al. HAADF-STEM and DFT investigations of the Zn-containing β" phase in Al-Mg-Si alloys [J]. Acta Mater., 2014, 78: 245 |
| 17 | Jiao N N, Lai Y X, Chen S L, et al. Atomic-scale roles of Zn element in age-hardened AlMgSiZn alloys [J]. J. Mater. Sci. Technol., 2021, 70: 105 |
| 18 | M?rtsell E A, Marioara C D, Andersen S J, et al. Effects of germanium, copper, and silver substitutions on hardness and microstructure in lean Al-Mg-Si alloys [J]. Metall. Mater. Trans., 2015, 46A: 4369 |
| 19 | M?rtsell E A, Andersen S J, Friis J, et al. Atomistic details of precipitates in lean Al-Mg-Si alloys with trace additions of Ag and Ge studied by HAADF-STEM and DFT [J]. Philos. Mag., 2017, 97: 851 |
| 20 | M?rtsell E A, Marioara C D, Andersen S J, et al. The effects and behaviour of Li and Cu alloying agents in lean Al-Mg-Si alloys [J]. J. Alloys Compd., 2017, 699: 235 |
| 21 | Liu Y, Lai Y X, Chen Z Q, et al. Formation of β"-related composite precipitates in relation to enhanced thermal stability of Sc-alloyed Al-Mg-Si alloys [J]. J. Alloys Compd., 2021, 885: 160942 |
| 22 | Xiang X M, Lai Y X, Liu C H, et al. Sn-induced modification of the precipitation pathways upon high-temperature ageing in an Al-Mg-Si alloy [J]. Acta Metall. Sin., 2018, 54: 1273 |
| 向雪梅, 赖玉香, 刘春辉 等. 微合金化元素Sn对Al-Mg-Si合金高温时效强化相析出路径的改变 [J]. 金属学报, 2018, 54: 1273 | |
| 23 | Wen S P, Xing Z B, Huang H, et al. The effect of erbium on the microstructure and mechanical properties of Al-Mg-Mn-Zr alloy [J]. Mater. Sci. Eng., 2009, A516: 42 |
| 24 | Yao D M, Xia Y M, Qiu F, et al. Effects of La addition on the elevated temperature properties of the casting Al-Cu alloy [J]. Mater. Sci. Eng., 2011, A528: 1463 |
| 25 | Zheng Q J, Zhang L L, Jiang H X, et al. Effect mechanisms of micro-alloying element La on microstructure and mechanical properties of hypoeutectic Al-Si alloys [J]. J. Mater. Sci. Technol., 2020, 47: 142 |
| 26 | Zheng Q J, Wu J, Jiang H X, et al. Effect of micro-alloying element La on corrosion behavior of Al-Mg-Si alloys [J]. Corros. Sci., 2021, 179: 109113 |
| 27 | Chang C H, Lee S L, Hsu T Y, et al. Impact of Cu/Mg ratio on thermal stability of hot extrusion of Al-4.6 pct Cu-Mg-Ag alloys [J]. Metall. Mater. Trans., 2007, 38A: 2832 |
| 28 | Wang T M, Zhao Y F, Chen Z N, et al. The bimodal effect of La on the microstructures and mechanical properties of in-situ A356-TiB2 composites [J]. Mater. Des., 2015, 85: 724 |
| 29 | Jiang H X, Li S X, Zheng Q J, et al. Effect of minor lanthanum on the microstructures, tensile and electrical properties of Al-Fe alloys [J]. Mater. Des., 2020, 195: 108991 |
| 30 | Sankaran K K, O'neal J E, Sastry S M L. Effects of second-phase dispersoids on deformation behavior of Al-Li alloys [J]. Metall. Trans., 1983, 14A: 2174 |
| 31 | Liu G, Zhang G J, Ding X D, et al. The influences of multiscale-sized second-phase particles on ductility of aged aluminum alloys [J]. Metall. Mater. Trans., 2004, 35A: 1725 |
| 32 | Liu G, Zhang G J, Wang R H, et al. Heat treatment-modulated coupling effect of multi-scale second-phase particles on the ductile fracture of aged aluminum alloys [J]. Acta Mater., 2007, 55: 273 |
| 33 | Nellist P D, Pennycook S J. The principles and interpretation of annular dark-field Z-contrast imaging [J]. Adv. Imaging Electron Phys., 2000, 113: 147 |
| 34 | Yang W C, Wang M P, Zhang R R, et al. The diffraction patterns from β" precipitates in 12 orientations in Al-Mg-Si alloy [J]. Scr. Mater., 2010, 62: 705 |
| 35 | Sauvage X, Bobruk E V, Murashkin M Y, et al. Optimization of electrical conductivity and strength combination by structure design at the nanoscale in Al-Mg-Si alloys [J]. Acta Mater., 2015, 98: 355 |
| 36 | Pande C S, Cooper K P. Nanomechanics of Hall-Petch relationship in nanocrystalline materials [J]. Prog. Mater. Sci., 2009, 54: 689 |
| 37 | Zhou S H, Napolitano R E. Phase equilibria and thermodynamic limits for partitionless crystallization in the Al-La binary system [J]. Acta Mater., 2006, 54: 831 |
| 38 | Chang C S T, Banhart J. Low-temperature differential scanning calorimetry of an Al-Mg-Si alloy [J]. Metall. Mater. Trans., 2011, 42A: 1960 |
| 39 | Mahidhara R K. Effect of grain size on the superplastic behavior of a 7475 aluminum alloy [J]. J. Mater. Eng. Perform., 1995, 4: 674 |
| 40 | Hirata T, Oguri T, Hagino H, et al. Influence of friction stir welding parameters on grain size and formability in 5083 aluminum alloy [J]. Mater. Sci. Eng., 2007, A456: 344 |
/
| 〈 |
|
〉 |