基于飞秒激光时域热反射法的微尺度Cu-Sn金属间化合物热导率研究
收稿日期: 2021-05-19
修回日期: 2021-11-30
网络出版日期: 2022-04-26
基金资助
国家自然科学基金项目(51971231);国家自然科学基金项目(52105327);国家自然科学基金项目(51720105007);国家重大科学仪器开发专项项目(2013YQ120355);中央高校基本科研业务费专项资金项目(FRF-BD-20-09A)
Investigations on the Thermal Conductivity of Micro-Scale Cu-Sn Intermetallic Compounds Using Femtosecond Laser Time-Domain Thermoreflectance System
Received date: 2021-05-19
Revised date: 2021-11-30
Online published: 2022-04-26
Supported by
National Natural Science Foundation of China(51971231);National Natural Science Foundation of China(52105327);National Natural Science Foundation of China(51720105007);National Key Scientific Instrument and Equipment Development Projects of China(2013YQ120355);Fundamental Research Funds for the Central Universities(FRF-BD-20-09A)
利用双波长飞秒激光时域热反射系统对微尺度Cu-Sn金属间化合物的热输运性能开展研究。利用回流与时效工艺制备Cu-Sn扩散偶,界面处生成均匀连续的Cu6Sn5和Cu3Sn金属间化合物,材料厚度均在微米量级且Cu6Sn5的(001)晶面具有明显的择优取向特征。由于实验参数对待测参量的敏感度会影响拟合精度,重点分析了铝传感层厚度与加热光调制频率对金属间化合物热导率测量敏感度的影响,以选定具体的实验参数。经测试,Cu6Sn5和Cu3Sn的热导率分别为47.4和87.6 W/(m·K),均略高于已有研究报道,分析认为主要是由于样品制备技术不同而导致的材料微观结构差异所致。讨论了加热光斑尺寸、铝传感层厚度及材料比热容的不确定性对热导率测量误差的影响,得到Cu6Sn5热导率误差为-6.8%~4.6%,Cu3Sn热导率误差为-7.1%~4.4%。本工作表明飞秒激光时域热反射技术在电子封装微尺度金属间化合物热输运特性研究方面具备适用性,所得实测数据对于电子封装热设计及可靠性评价有重要参考意义。
周丽君 , 位松 , 郭敬东 , 孙方远 , 王新伟 , 唐大伟 . 基于飞秒激光时域热反射法的微尺度Cu-Sn金属间化合物热导率研究[J]. 金属学报, 2022 , 58(12) : 1645 -1654 . DOI: 10.11900/0412.1961.2021.00216
An accurate temperature analysis of electronic packaging requires an understanding of the thermal-transport parameters of the material. However, studies on the thermal conductivity of intermetallic compounds (IMCs) in micro-interconnect solder joints are scarce, particularly common IMCs forming in Cu-Sn systems, which seriously affect the precise prediction of the temperature field and thermal stress for electronic packaging structures. This work proposes a novel method to quantitatively measure the thermophysical parameters of Cu-Sn IMCs based on the dual-wavelength femtosecond laser time-domain thermoreflectance (TDTR) system. Cu-Sn diffusion couple samples were prepared using a reflow and aging process. Two layers of Cu6Sn5 and Cu3Sn IMCs formed at the interface with micron thickness, and the (001) crystal plane of Cu6Sn5 was the preferred orientation. The sensitivity of the experimental parameters to the measurement parameters affects the fitting accuracy. Therefore, before testing, the effects of the aluminum transducer thickness and pump laser modulation frequency on the phase signal sensitivity in the thermal conductivity measurements of Cu6Sn5 and Cu3Sn were analyzed to help select the specific experimental parameters. After testing, the thermal conductivities of Cu6Sn5 and Cu3Sn were 47.4 and 87.6 W/(m·K), respectively, which are slightly higher than the previous results because of the microstructure discrepancy caused by different material preparation techniques. Finally, the influence of the pump laser diameter, aluminum transducer thickness, and material specific heat on the measurement error of thermal conductivity for Cu6Sn5 and Cu3Sn was examined. The test errors of the Cu6Sn5 and Cu3Sn thermal conductivity were -6.8%~4.6% and -7.1%~4.4%, respectively. Overall, the TDTR technology can evaluate the thermal-transport characteristics of micron-scale intermetallic compounds in electronic packaging and guide the thermal design and reliability evaluations of electronic components.
| 1 | Braun T, Becker K F, T?pper M, et al. Fan-out wafer and panel level packaging—A platform for 3D integration [A]. 5th IEEE Electron Devices Technology and Manufacturing Conference [C]. Chengdu: IEEE, 2021: 1 |
| 2 | Liu J H, Zhao H Y, Li Z L, et al. Microstructures and mechanical properties of Cu/Sn/Cu structure ultrasonic-tlp joint [J]. Acta Metall. Sin., 2017, 53: 227 |
| 2 | 刘积厚, 赵洪运, 李卓霖 等. Cu/Sn/Cu超声-TLP接头的显微组织与力学性能 [J]. 金属学报, 2017, 53: 227 |
| 3 | Lancaster A, Keswani M. Integrated circuit packaging review with an emphasis on 3D packaging [J]. Integration, 2018, 60: 204 |
| 4 | Lable R, Ruythooren W, Baert K, et al. Resistance to electromigration of purely intermetallic micro-bump interconnections for 3D-device stacking [A]. 2008 International Interconnect Technology Conference [C]. Burlingame: IEEE, 2008: 19 |
| 5 | Oprins H, Cherman V, Beyne E, et al. Thermal performance comparison of advanced 3D packaging concepts for logic and memory integration in mobile cooling conditions [A]. 17th IEEE Intersociety Conference on Thermal and Thermomechanical Phenomena in Electronic Systems [C]. San Diego: IEEE, 2018: 318 |
| 6 | Oprins H, Beyne E. Thermal analysis of a 3D flip-chip fan-out wafer level package (fcFOWLP) for high bandwidth 3D integration [A]. 18th IEEE Intersociety Conference on Thermal and Thermomechanical Phenomena in Electronic Systems [C]. Las Vegas: IEEE, 2019: 1234 |
| 7 | Goodson K E, Flik M I. Solid layer thermal-conductivity measurement techniques [J]. Appl. Mech. Rev., 1994, 47: 101 |
| 8 | Mcconnell A D, Goodson K E. Thermal conduction in silicon micro- and nanostructures [J]. Annu. Rev. Heat Transfer, 2005, 14: 129 |
| 9 | Nishi T, Shibata H, Waseda Y, et al. Thermal conductivities of molten iron, cobalt, and nickel by laser flash method [J]. Metall. Mater. Trans., 2003, 34A: 2801 |
| 10 | Kim J H, Feldman A, Novotny D. Application of the three omega thermal conductivity measurement method to a film on a substrate of finite thickness [J]. J. Appl. Phys., 1999, 86: 3959 |
| 11 | Al-Ajlan S A. Measurements of thermal properties of insulation materials by using transient plane source technique [J]. Appl. Therm. Eng., 2006, 26: 2184 |
| 12 | Bentz D P. Transient plane source measurements of the thermal properties of hydrating cement pastes [J]. Mater. Struct., 2007, 40: 1073 |
| 13 | Ho C Y, Bogaard R H, Gibson C C. Thermophysical and mechanical properties of structural composites and alloys [J]. High Temp.-High Press., 1998, 30: 277 |
| 14 | Frederikse H P R, Fields R J, Feldman A. Thermal and electrical properties of copper-tin and nickel-tin intermetallics [J]. J. Appl. Phys., 1992, 72: 2879 |
| 15 | Papadogiannis N A, Mousta?zis S D, Girardeau-Montaut J P. Electron relaxation phenomena on a copper surface via nonlinear ultrashort single-photon photoelectric emission [J]. J. Phys., 1997, 30D: 2389 |
| 16 | Qiu T Q, Tien C L. Heat transfer mechanisms during short-pulse laser heating of metals [J]. J. Heat Transfer, 1993, 115: 835 |
| 17 | Cahill D G, Goodson K, Majumdar A. Thermometry and thermal transport in micro/nanoscale solid-state devices and structures [J]. J. Heat Transfer, 2002, 124: 223 |
| 18 | Capinski W S, Maris H J, Ruf T, et al. Thermal-conductivity measurements of GaAs/AlAs superlattices using a picosecond optical pump-and-probe technique [J]. Phys. Rev., 1999, 59B: 8105 |
| 19 | Stoner R J, Maris H J. Kapitza conductance and heat flow between solids at temperatures from 50 to 300 K [J]. Phys. Rev., 1993, 48B: 16373 |
| 20 | Losego M D, Grady M E, Sottos N R, et al. Effects of chemical bonding on heat transport across interfaces [J]. Nat. Mater., 2012, 11: 502 |
| 21 | Sun F Y, Zhang T, Jobbins M M, et al. Molecular bridge enables anomalous enhancement in thermal transport across hard-soft material interfaces [J]. Adv. Mater., 2014, 26: 6093 |
| 22 | Park M S, Gibbons S L, Arróyave R. Phase-field simulations of intermetallic compound growth in Cu/Sn/Cu sandwich structure under transient liquid phase bonding conditions [J]. Acta Mater., 2012, 60: 6278 |
| 23 | Lee J B, Hwang H Y, Rhee M W. Reliability investigation of Cu/in TLP bonding [J]. J. Electron. Mater., 2015, 44: 435 |
| 24 | Li J F, Agyakwa P A, Johnson C M. Kinetics of Ag3Sn growth in Ag-Sn-Ag system during transient liquid phase soldering process [J]. Acta Mater., 2010, 58: 3429 |
| 25 | Zhang W, Ruythooren W. Study of the Au/In reaction for transient liquid-phase bonding and 3D chip stacking [J]. J. Electron. Mater., 2008, 37: 1095 |
| 26 | Yu C C, Su P C, Bai S J, et al. Nickel-tin solid-liquid inter-diffusion bonding [J]. Int. J. Precis. Eng. Man., 2014, 15: 143 |
| 27 | Sun F Y, Zhu J, Tang D W. Thermal conductivity measurement of liquids using femto-second laser pump-probe technique [J]. Chinese Sci. Bull., 2015, 60: 1320 |
| 27 | 孙方远, 祝捷, 唐大伟. 飞秒激光抽运探测方法测量液体热导率 [J]. 科学通报, 2015, 60: 1320 |
| 28 | Schmidt A J. Optical characterization of thermal transport from the nanoscale to the macroscale [D]. Cambridge: Massachusetts Institute of Technology, 2008 |
| 29 | Li D, Franke P, Fürtauer S, et al. The Cu-Sn phase diagram part II: New thermodynamic assessment [J]. Intermetallics, 2013, 34: 148 |
| 30 | Yang M. Interfacial reaction between tin-based solders and polycrystalline copper pad [D]. Harbin: Harbin Institute of Technology, 2012 |
| 30 | 杨明. 锡基钎料与多晶铜焊盘界面反应行为研究 [D]. 哈尔滨: 哈尔滨工业大学, 2012 |
| 31 | Gundrum B C, Cahill D G, Averback R S. Thermal conductance of metal-metal interfaces [J]. Phys. Rev., 2005, 72B: 245426 |
/
| 〈 |
|
〉 |