复杂场景下的焊接智能制造中的信息感知与控制方法
收稿日期: 2021-12-03
修回日期: 2022-03-01
网络出版日期: 2022-04-18
基金资助
国家自然科学基金项目(52175351)
Key Information Perception and Control Strategy of Intellignet Welding Under Complex Scene
Received date: 2021-12-03
Revised date: 2022-03-01
Online published: 2022-04-18
Supported by
National Natural Science Foundation of China(52175351)
陈华斌 , 陈善本 . 复杂场景下的焊接智能制造中的信息感知与控制方法[J]. 金属学报, 2022 , 58(4) : 541 -550 . DOI: 10.11900/0412.1961.2021.00528
The robotic arc welding equipment and automated welding system can not fulfill the requirements in self-sensing, intelligent decision-making,and robust process-controlling in the complex welding environment. Artificial intelligence techniques were used to simulate observation actions, knowledge,and behavior of experienced welders, to realize functions,such as multi-mode information perception, knowledge judgment, and intelligent control during the welding process. Essential techniques in intelligent robotic welding as well as intelligent modeling and its coordinate control strategies of flexible welding manufacturing system were also proposed. These formed the technique,structure,and theoretical framework of intelligent welding manufacturing technique and system. They also provided a scientific method and technical realization to solve problems in intelligent manufacturing techniques and systems of other complex materials forming processes.
| 1 | Zhou J, Zhou Y H, Wang B C, et al. Human-cyber-physical systems (HCPSs) in the context of new-generation intelligent manufacturing [J]. Engineering, 2019, 5: 624 |
| 2 | Wang B C, Hu S J, Sun L, et al. Intelligent welding system technologies: State-of-the-art review and perspectives [J]. J. Manuf. Syst., 2020, 56: 373 |
| 3 | Zhang G J, Li Y Z. Towards intelligent welding in the context of industry 4.0 [J]. Aeronaut. Manuf. Technol., 2016, (11): 28 |
| 3 | 张广军, 李永哲. 工业4.0语义下智能焊接技术发展综述 [J]. 航空制造技术, 2016, (11): 28 |
| 4 | David S A, Chen J, Gibson B T, et al. Intelligent weld manufacturing: Role of integrated computational welding engineering [A]. Transactions on Intelligent Welding Manufacturing [M]. Singapore: Springer, 2018: 3 |
| 5 | Ogbemhe J, Mpofu K. Towards achieving a fully intelligent robotic arc welding: A review [J]. Ind. Robot: Int. J., 2015, 42: 475 |
| 6 | Jin Z S, Li H C, Jia G Q, et al. Dynamic nonlinear modeling of 3D weld pool surface in GTAW [J]. Robot. Comput. Integr. Manuf., 2016, 39: 1 |
| 7 | Severson K, Chaiwatanodom P, Braatz R D. Perspectives on process monitoring of industrial systems [J]. Ann. Rev. Cont., 2016, 42: 190 |
| 8 | Yin S, Ding S X, Xie X C, et al. A review on basic data-driven approaches for industrial process monitoring [J]. IEEE Trans. Ind. Electron., 2014, 61: 6418 |
| 9 | Wang Q Y, Jiao W H, Zhang Y M. Deep learning-empowered digital twin for visualized weld joint growth monitoring and penetration control [J]. J. Manuf. Sys., 2020, 57: 429 |
| 10 | Park H, Trautmann M, Tanaka K, et al. Mixing of multiple metal vapours into an arc plasma in gas tungsten arc welding of stainless steel [J]. J. Phys., 2017, 50D: 43LT03 |
| 11 | Tanaka K, Shigeta M, Tanaka M, et al. Investigation of the bilayer region of metal vapor in a helium tungsten inert gas arc plasma on stainless steel by imaging spectroscopy [J]. J. Phys., 2019, 52D: 354003 |
| 12 | Wu S J, Gao H M, Zhang W, et al. Analytic weld pool model calibrated by measurements—Part 1: Principles [J]. Weld. J., 2017, 96: 193 |
| 13 | Wu S J, Gao H M, Zhang W, et al. Analytic weld pool model calibrated by measurements—Part 2: Verification and robustness [J]. Weld. J., 2017, 96: 250 |
| 14 | Chen C, Lv N, Chen S B. Welding penetration monitoring for pulsed GTAW using visual sensor based on AAM and random forests [J]. J. Manuf. Process, 2021, 63: 152 |
| 15 | Zhang Z F, Wen G R, Chen S B. Audible sound-based intelligent evaluation for aluminum alloy in robotic pulsed GTAW: Mechanism, feature selection, and defect detection [J]. IEEE Trans. Ind. Inform., 2017, 14: 2973 |
| 16 | Zhang W J, Zhang Y M. Modeling of human welder response to 3D weld pool surface: Part I—principles [J]. Weld. J., 2012, 91: 310S |
| 17 | Chen S B, Lv N. Research evolution on intelligentized technologies for arc welding process [J]. J. Manuf. Process, 2014, 16: 109 |
| 18 | Liu Y K, Zhang W J, Zhang Y M. Estimation of weld joint penetration under varying GTA pools [J]. Weld. J., 2013, 92: 313S |
| 19 | Zhang S Q, Hu S S, Wang Z J. Weld penetration sensing in pulsed gas tungsten arc welding based on arc voltage [J]. J. Mater. Process. Technol., 2016, 229: 520 |
| 20 | Huang J K, Yang M H, Chen J S, et al. The oscillation of stationary weld pool surface in the GTA welding [J]. J. Mater. Process. Technol., 2018, 256: 57 |
| 21 | Zhang K, Zhang Y M, Chen J S, et al. Observation and analysis of three-dimensional weld pool oscillation dynamic behaviors [J]. Weld. J., 2017, 96: 143S |
| 22 | Coniglio N, Mathieu A, Aubreton O, et al. Plasma effect on weld pool surface reconstruction by shape-from-polarization analysis [J]. Appl. Phys. Lett., 2014, 104: 131603 |
| 23 | Feng Z, Chen J, Chen Z. Monitoring weld pool surface and penetration using reversed electrode images [J]. Weld. J., 2017, 96: 367S |
| 24 | Chen Z Y, Chen J, Feng Z L. Welding penetration prediction with passive vision system [J]. J. Manuf. Process., 2018, 36: 224 |
| 25 | Tarn J, Huissoon J. Developing psycho-acoustic experiments in gas metal arc welding [A]. IEEE International Conference Mechatronics and Automation, 2005 [C]. Niagara Falls: IEEE, 2005: 1112 |
| 26 | Asif K, Zhang L, Derrible S, et al. Machine learning model to predict welding quality using air-coupled acoustic emission and weld inputs [J]. J. Intell. Manuf., 2022, 33: 881 |
| 27 | Wang J F, Chen B, Chen H B, et al. Analysis of arc sound characteristics for gas tungsten argon welding [J]. Sensor Rev., 2009, 29: 240 |
| 28 | Wang J F, Yu H D, Qian Y Z, et al. Feature extraction in welding penetration monitoring with arc sound signals [J]. Proc. Inst. Mech. Eng., 2011, 225B: 1683 |
| 29 | Lv N, Fang G, Xu Y L, et al. Real-time monitoring of welding path in pulse metal-inert gas robotic welding using a dual-microphone array [J]. Int. J. Adv. Manuf. Technol., 2017, 90: 2955 |
| 30 | Wang J F. Study on recognition method of penetration states based on welding sound feature [D]. Shanghai: Shanghai Jiao Tong University, 2009 |
| 30 | 王继锋. 基于焊接声音信号特征的熔透状态识别方法研究 [D]. 上海: 上海交通大学, 2009 |
| 31 | Song S, Chen H B, Lin T, et al. Penetration state recognition based on the double-sound-sources characteristic of VPPAW and hidden Markov Model [J]. J. Mater. Process. Technol., 2016, 234: 33 |
| 32 | Wu D, Chen H B, Huang Y M, et al. Monitoring of weld joint penetration during variable polarity plasma arc welding based on the keyhole characteristics and PSO-ANFIS [J]. J. Mater. Process. Technol., 2017, 239: 113 |
| 33 | Yu H W. Research on dynamic process and defect features of aluminum alloy pulsed GTAW based on the welding arc spectral information [D]. Shanghai: Shanghai Jiao Tong University, 2013 |
| 33 | 余焕伟. 基于电弧光谱信息的铝合金脉冲GTAW焊接动态过程及缺陷特征研究 [D]. 上海: 上海交通大学, 2013 |
| 34 | Katayama S, Uchiumi S, Mizutani M, et al. Penetration and porosity prevention mechanism in YAG laser-MIG hybrid welding [J]. Weld. Int., 2007, 21: 25 |
| 35 | Tanaka M, Tashiro S, Tsujimura Y. Visualizations and predictions of welding arcs [J]. Trans JWRI, 2012, 41: 1 |
| 36 | Liu L M, Hao X F. Study of the effect of low-power pulse laser on arc plasma and magnesium alloy target in hybrid welding by spectral diagnosis technique [J]. J. Phys.. 2008, 41D: 205202 |
| 37 | Hao X F, Liu L M. Effect of laser pulse on arc plasma and magnesium target in low-power laser/arc hybrid welding [J]. IEEE Trans. Plasma Sci., 2009, 37: 2197 |
| 38 | Yu H W, Chen H B, Xu Y L, et al. Spectroscopic diagnostics of pulsed gas tungsten arc welding plasma and its effect on weld formation of aluminum-magnesium alloy [J]. Spectrosc. Lett., 2013, 46: 350 |
| 39 | Otaki S, Matsuida T, Nomura K, et al. In-situ measurement of weld quality during MAG welding using laser ultrasonic [J]. Weld. Int., 2019, 33: 450 |
| 40 | Feng Y H, Chen Z Y, Wang D L, et al. DeepWelding: A deep learning enhanced approach to GTAW using multisource sensing images [J]. IEEE Trans. Ind. Inform., 2019, 16: 465 |
| 41 | Wang Q Y, Jiao W H, Yu R, et al. Modeling of human welders' operations in virtual reality human-robot interaction [J]. IEEE Robot. Autom. Lett., 2019, 4: 2958 |
| 42 | Fan C J. Weld pool characters extraction visual sensing and intelligent control during varied gap aluminum alloy [D]. Shanghai: Shanghai Jiao Tong University, 2008 |
| 42 | 樊重建. 变间隙铝合金脉冲GTAW熔池视觉特征获取及其智能控制研究 [D].上海: 上海交通大学, 2008 |
| 43 | Jiang Z. Multi-source information representation and penetration prediction and control for robotic TIG welding of aluminum alloy [D]. Shanghai: Shanghai Jiao Tong University, 2020 |
| 43 | 蒋 铮. 铝合金机器人TIG焊多源信息表征及熔透预测控制 [D]. 上海: 上海交通大学, 2020 |
| 44 | Wu D, Huang Y M, Zhang P L, et al. Visual-acoustic penetration recognition in variable polarity plasma arc welding process using hybrid deep learning approach [J]. IEEE Access, 2020, 8: 120417 |
| 45 | Wu D, Chen J S, Liu H B, et al. Weld penetration in situ prediction from keyhole dynamic behavior under time-varying VPPAW pools via the OS-ELM model [J]. Int. J. Adv. Manuf. Technol., 2019, 104: 3929 |
| 46 | Wu D, Huang Y M, Chen H B, et al. VPPAW penetration monitoring based on fusion of visual and acoustic signals using t-SNE and DBN model [J]. Mater. Des., 2017, 123: 1 |
| 47 | Chen C, Xiao R Q, Chen H B, et al. Arc sound model for pulsed GTAW and recognition of different penetration states [J]. Int. J. Adv. Manuf. Technol., 2020, 108: 3175 |
| 48 | Chen C, Xiao R Q, Chen H B, et al. Prediction of welding quality characteristics during pulsed GTAW process of aluminum alloy by multisensory fusion and hybrid network model [J]. J. Manuf. Process., 2021, 68: 209 |
| 49 | Huang Y M, Li S S, Li J H, et al. Spectral diagnosis and defects prediction based on ELM during the GTAW of Al alloys [J]. Measurement, 2019, 136: 405 |
| 50 | Huang Y M, Zhao D J, Chen H B, et al. Porosity detection in pulsed GTA welding of 5A06 Al alloy through spectral analysis [J]. J. Mater. Process Technol., 2018, 259: 332 |
| 51 | Huang Y M, Wu D, Zhang Z F, et al. EMD-based pulsed TIG welding process porosity defect detection and defect diagnosis using GA-SVM [J]. J. Mater. Process. Technol., 2017, 239: 92 |
| 52 | Chen H B, Song Y L, Chen X Q, et al. In situ studies of full-field residual stress mapping of SS304 stainless steel welds using DIC [J]. Int. J. Adv. Manuf. Technol., 2020, 109: 45 |
| 53 | Song Y L. In situ studies of full field strain and residual stress of welding heat affect zone using digital image correlation [D]. Shanghai: Shanghai Jiao Tong University, 2019 |
| 53 | 宋育林. 数字图像相关法焊接热影响区高温应变原位测量及残余应力表征 [D]. 上海: 上海交通大学, 2019 |
| 54 | Zhang Z F, Chen H B, Xu Y L, et al. Multisensor-based real-time quality monitoring by means of feature extraction, selection and modeling for Al alloy in arc welding [J]. Mech. Syst. Signal Process., 2015, 60-61: 151 |
| 55 | Ma H B, Wei S C, Lin T, et al. Mixed logical dynamical model for back bead width prediction of pulsed GTAW process with misalignment [J]. J. Mater. Process. Technol., 2010, 210: 2036 |
| 56 | Wu D, Chen H B, Huang Y M, et al. Online monitoring and model-free adaptive control of weld penetration in VPPAW based on extreme learning machine [J]. IEEE Trans. Ind. Inform., 2019, 15: 2732 |
| 57 | Lv F L, Chen H B, Fan C J, et al. A novel control algorithm for weld pool control [J]. Ind. Robot, 2010, 37: 89 |
| 58 | Ye Z, Fang G, Chen S B, et al. Passive vision based seam tracking system for pulse-MAG welding [J]. Int. J. Adv. Manuf. Technol., 2013, 67: 1987 |
| 59 | Ye Z, Fang G, Chen S B, et al. A robust algorithm for weld seam extraction based on prior knowledge of weld seam [J]. Sensor Rev., 2013, 33: 125 |
| 60 | Hou Z, Xu Y L, Xiao R Q, et al. A teaching-free welding method based on laser visual sensing system in robotic GMAW [J]. Int. J. Adv. Manuf. Technol., 2020, 109: 1755 |
| 61 | Xiao R Q, Xu Y L, Hou Z, et al. An adaptive feature extraction algorithm for multiple typical seam tracking based on vision sensor in robotic arc welding [J]. Sens. Actuators, 2019, 297A: 111533 |
| 62 | Lin S Y, Yang X Q, Xu A J, et al. Recent advances in intelligentized robotic welding technologies and its application in launch vehicle tank [J]. Aerosp. Shanghai, 2021, 38(3): 8 |
| 62 | 林尚扬, 杨学勤, 徐爱杰 等. 机器人智能化焊接技术发展综述及其在运载火箭贮箱中的应用 [J]. 上海航天, 2021, 38(3): 8 |
/
| 〈 |
|
〉 |