高速冲击载荷下预压缩AZ31镁合金的退孪生行为与动态力学性能
收稿日期: 2021-03-23
修回日期: 2021-04-07
网络出版日期: 2021-11-09
基金资助
辽宁省兴辽英才计划项目(XLYC1908006)
Detwinning Behaviors and Dynamic Mechanical Properties of Precompressed AZ31 Magnesium Alloy Subjected to High Strain Rates Impact
Received date: 2021-03-23
Revised date: 2021-04-07
Online published: 2021-11-09
Supported by
Liaoning Revitalization Talents Program(XLYC1908006)
为研究高应变速率冲击载荷下预压缩轧制态AZ31镁合金的退孪生行为与动态力学性能,将原始试样沿轧制方向(RD)进行真应变为4%的准静态预压缩,引入大量的{
陈扬 , 毛萍莉 , 刘正 , 王志 , 曹耕晟 . 高速冲击载荷下预压缩AZ31镁合金的退孪生行为与动态力学性能[J]. 金属学报, 2022 , 58(5) : 660 -672 . DOI: 10.11900/0412.1961.2021.00117
To investigate the detwinning behaviors and dynamic mechanical properties of a precompressed rolled AZ31 magnesium alloy sheet impacted under high strain rates, the as-received sheet was precompressed along the rolling direction (RD) to the true strain of 4% for inducing {
Key words: AZ31 magnesium alloy; precompression; high strain rate impact; detwinning
| 1 | Watanabe H, Ishikawa K. Effect of texture on high temperature deformation behavior at high strain rates in a Mg-3Al-1Zn alloy [J]. Mater. Sci. Eng., 2009, A523: 304 |
| 2 | Khosravani A, Fullwood D T, Adams B L, et al. Nucleation and propagation of { 10 1 ¯ 2 } twins in AZ31 magnesium alloy [J]. Acta Mater., 2015, 100: 202 |
| 3 | Shan Z W, Liu B Y. The mechanism of { 10 1 ¯ 2 } deformation twinning in magnesium [J]. Acta Metall. Sin., 2016, 52: 1267 |
| 3 | 单智伟, 刘博宇. Mg的{ 10 1 ¯ 2 }形变孪晶机制 [J]. 金属学报, 2016, 52: 1267 |
| 4 | Li X D, Mao P L, Liu Y Y, et al. Anisotropy and deformation mechanisms of as-extruded Mg-3Zn-1Y magnesium alloy under high strain rates [J]. Acta Metall. Sin., 2018, 54: 557 |
| 4 | 李旭东, 毛萍莉, 刘晏宇 等. 高应变速率下Mg-3Zn-1Y镁合金的各向异性及变形机制 [J]. 金属学报, 2018, 54: 557 |
| 5 | Luque A, Ghazisaeidi M, Curtin W A. A new mechanism for twin growth in Mg alloys [J]. Acta Mater., 2014, 81: 442 |
| 6 | Lou C, Zhang X Y, Ren Y. Twinning characteristic of AZ31 magnesium alloy during dynamic plastic deformation [J]. Chin. J. Nonferrous Met., 2015, 25: 2642 |
| 6 | 娄 超, 张喜燕, 任 毅. 动态塑性变形下AZ31镁合金的孪生特征 [J]. 中国有色金属学报, 2015, 25: 2642 |
| 7 | Wu W, Gao Y F, Li N, et al. Intragranular twinning, detwinning, and twinning-like lattice reorientation in magnesium alloys [J]. Acta Mater., 2016, 121: 15 |
| 8 | Huang H T, Godfrey A, Zheng J P, et al. Influence of local strain on twinning behavior during compression of AZ31 magnesium alloy [J]. Mater. Sci. Eng., 2015, A640: 330 |
| 9 | Wang B S, Deng L P, Chapuis A, et al. Study of twinning behavior of AZ31 Mg alloy during plane strain compression [J]. Acta Metall. Sin., 2015, 51: 1441 |
| 9 | 汪炳叔, 邓丽萍, Chapuis A 等. AZ31镁合金在平面应变压缩过程中的孪生行为研究 [J]. 金属学报, 2015, 51: 1441 |
| 10 | Yan Y Q, Luo J R, Zhang J S, et al. Study on the microstructural evolution and mechanical properties control of a strong textured AZ31 magnesium alloy sheet during cryorolling [J]. Acta Metall. Sin., 2017, 53: 107 |
| 10 | 闫亚琼, 罗晋如, 张济山 等. 强织构AZ31镁合金板材深低温轧制过程中微观组织演变及力学性能控制研究 [J]. 金属学报, 2017, 53: 107 |
| 11 | Hong S G, Park S H, Lee C S. Role of { 10 1 ¯ 2 } twinning characteristics in the deformation behavior of a polycrystalline magnesium alloy [J]. Acta Mater., 2010, 58: 5873 |
| 12 | Hou D W, Li Q Z, Wen H M. Study of reversible motion of { 10 1 ¯ 2 } tensile twin boundaries in a magnesium alloy during strain path changes [J]. Mater. Lett., 2018, 231: 84 |
| 13 | Lee J U, Song S W, Kim Y, et al. Effects of { 10 1 ¯ 2 } twins on dynamic torsional properties of extruded AZ31 magnesium alloy [J]. Met. Mater. Int., 2018, 24: 283 |
| 14 | Mokdad F, Chen D L, Li D Y. Twin-twin interactions and contraction twin formation in an extruded magnesium alloy subjected to an alteration of compressive direction [J]. J. Alloys Compd., 2018, 737: 549 |
| 15 | Chen H C, Liu T M, Hou D W, et al. Improving the mechanical properties of a hot-extruded AZ31 alloy by { 10 1 ¯ 2 } twinning lamella [J]. J. Alloys Compd., 2016, 680: 191 |
| 16 | Park S H, Hong S G, Lee J H, et al. Texture evolution of rolled Mg-3Al-1Zn alloy undergoing a { 10 1 ¯ 2 } twinning dominant strain path change [J]. J. Alloys Compd., 2015, 646: 573 |
| 17 | Long Z X, Liu T M, He J J, et al. The effects of pre-strain and subsequent annealing on the yielding behavior in a rolled magnesium alloy AZ31 [J]. J. Mater. Eng. Perform., 2015, 24: 16 |
| 18 | Song B, Xin R L, Sun L Y, et al. Enhancing the strength of rolled ZK60 alloys via the combined use of twinning deformation and aging treatment [J]. Mater. Sci. Eng., 2013, A582: 68 |
| 19 | Sun Q, Xia T, Tan L, et al. Influence of { 10 1 ¯ 2 } twin characteristics on detwinning in Mg-3Al-1Zn alloy [J]. Mater. Sci. Eng., 2018, A735: 243 |
| 20 | Sarker D, Friedman J, Chen D L. De-twinning and texture change in an extruded AM30 magnesium alloy during compression along normal direction [J]. J. Mater. Sci. Technol., 2015, 31: 264 |
| 21 | Huang H T, Godfrey A, Liu W, et al. Study on twinning behaviors during multi-directional compression for AZ31 magnesium alloy by EBSD [J]. J. Chin. Electron Microsc. Soc., 2011, 30: 294 |
| 21 | 黄洪涛, Godfrey A, 刘 伟 等. 多向压缩路径下AZ31镁合金孪生行为的EBSD研究 [J]. 电子显微学报, 2011, 30: 294 |
| 22 | Lou C, Zhang X Y, Wang R H, et al. Effects of untwinning and { 10 1 ¯ 2 } twin lamellar structure on the mechanical properties of Mg alloy [J]. Acta Metall. Sin., 2013, 49: 291 |
| 22 | 娄 超, 张喜燕, 汪润红 等. 退孪生行为以及{ 10 1 ¯ 2 }孪晶片层结构对镁合金力学性能的影响 [J]. 金属学报, 2013, 49: 291 |
| 23 | Proust G, Tomé C N, Jain A, et al. Modeling the effect of twinning and detwinning during strain-path changes of magnesium alloy AZ31 [J]. Int. J. Plast., 2009, 25: 861 |
| 24 | Wang R F, Mao P L, Liu Y Y, et al. Influence of pre-twinning on high strain rate compressive behavior of AZ31 Mg-alloys [J]. Mater. Sci. Eng., 2018, A742: 309 |
| 25 | Yu Q, Wang J, Jiang Y Y, et al. Twin-twin interactions in magnesium [J]. Acta Mater., 2014, 77: 28 |
| 26 | Guan D K, Rainforth W M, Gao J H, et al. Individual effect of recrystallisation nucleation sites on texture weakening in a magnesium alloy: Part 1—double twins [J]. Acta Mater., 2017, 135: 14 |
| 27 | Wang X X, Mao P L, Wang R F, et al. Role of { 10 1 ¯ 2 } twinning in the anisotropy and asymmetry of AZ31 magnesium alloy under high strain rate deformation [J]. Mater. Sci. Eng., 2020, A772: 138814 |
| 28 | Xiao J, Shu D W. Compressive behavior and constitutive analysis of AZ31B magnesium alloy over wide range of strain rates and temperatures [J]. Met. Mater. Int., 2015, 21: 823 |
| 29 | Zhang Y, Liu T M, Xu S, et al. Detwinning behavior of an extruded AZ31 magnesium alloy during uniaxial compression [J]. Trans. Mater. Heat Treat., 2013, 34(8): 26 |
| 29 | 张 愔, 刘天模, 徐 舜 等. 挤压态AZ31镁合金单向压缩过程中的退孪生行为 [J]. 材料热处理学报, 2013, 34(8): 26 |
| 30 | Guo L L, Chen Z C, Gao L. Effects of grain size, texture and twinning on mechanical properties and work-hardening behavior of AZ31 magnesium alloys [J]. Mater. Sci. Eng., 2011, A528: 8537 |
| 31 | Xi G Q, Chen Y, Chen S, et al. Study on twinning-detwinning behavior of magnesium alloy by Situ EBSD [J]. J. Chongqing Univ. Technol. (Nat. Sci.), 2020, 34(9): 147 |
| 31 | 席国强, 陈 艺, 陈 爽 等. 镁合金中孪生-退孪生行为的原位EBSD研究 [J]. 重庆理工大学学报(自然科学版), 2020, 34(9): 147 |
| 32 | Chen Y, Mao P L, Wang Z, et al. High strain rate deformation behaviors experimental study and numerical simulation of rolled AZ31 magnesium alloy loaded along different directions [J]. Chin. J. Nonferrous Met., 2020, 30: 997 |
| 32 | 陈 扬, 毛萍莉, 王志 等. 不同加载方向时轧制态AZ31镁合金高速变形行为的实验研究与数值模拟 [J]. 中国有色金属学报, 2020, 30: 997 |
/
| 〈 |
|
〉 |