热输入对Q500qE钢模拟CGHAZ微观组织和冲击韧性的影响
收稿日期: 2021-04-26
修回日期: 2021-06-16
网络出版日期: 2021-09-30
基金资助
国家自然科学基金项目(51671165)
Effect of Welding Heat Input on Microstructure and Impact Toughness of the Simulated CGHAZ in Q500qE Steel
Received date: 2021-04-26
Revised date: 2021-06-16
Online published: 2021-09-30
Supported by
National Natural Science Foundation of China(51671165)
采用Gleeble-3500热模拟试验机模拟了Q500qE钢在不同热输入(Ej = 15~30 kJ/cm)下的焊接热循环过程,结合OM、SEM以及EBSD等手段探讨了热输入对粗晶热影响区(CGHAZ)微观组织和冲击韧性的影响规律及其作用机理。结果表明,随着焊接热输入的降低,板条贝氏体(LB)增多,粒状贝氏体(GB)减少,相变温度Ar3降低,贝氏体块(packet)和贝氏体束(block)明显细化;CGHAZ的冲击功KV2 (-40℃)随着热输入的降低而提高,冲击断口均表现出明显的解理断裂特征,其解理面尺寸Df随着热输入的降低而减小;贝氏体packet是Q500qE钢中控制CGHAZ冲击韧性最有效的结构单元。
朱东明 , 何江里 , 史根豪 , 王青峰 . 热输入对Q500qE钢模拟CGHAZ微观组织和冲击韧性的影响[J]. 金属学报, 2022 , 58(12) : 1581 -1588 . DOI: 10.11900/0412.1961.2021.00175
As China's economy enters a stage of high-quality development, it is important to study high-performance bridge steels with high strength, high toughness, high efficiency, and easy welding. Presently, coarse-grained heat-affected zones (CGHAZs) of high-performance bridge steels are prone to coarse-grain embrittlement, which reduces its impact toughness. To improve their low-temperature toughness, the relationship between their microstructure and impact toughness has been extensively researched and discussed. However, the control connection and internal mechanism between the bainite microstructure and impact toughness have not been clarified. In this study, the simulated samples of CGHAZs in Q500qE steel with varying heat inputs, from 15 to 30 kJ/cm, were reproduced in Gleeble 3500 thermal simulation-testing machine. The effect of different heat inputs on the microstructure, impact toughness of CGHAZs, and their inherent mechanism was discussed and analyzed in-depth using OM, SEM, and EBSD. The results indicate that the microstructure of each simulated sample of CGHAZs in Q500qE steel was composed of lath-like bainite (LB) and granular-like bainite (GB). The LB increased, the GB reduced, phase-transition temperature (Ar3) declined, and the bainitic packet/block substructure refined as the welding heat input decreased. In addition, with the decreased heat inputs, the Charpy impact energy (KV2) at -40oC of CGHAZs is enhanced because of the refined microstructure. The impact fracture of all samples showed cleavage fracture characteristics, and the cleavage face size of the simulated samples of CGHAZs decreased due to the reduced heat inputs. Compared with prior austenite grain boundary and bainite block, the bainite packet is the most effective microstructural unit for controlling the impact toughness of CGHAZs in Q500qE steel, and its boundary effectively facilitates the prevention of further propagation of a secondary crack.
Key words: Q500qE steel; CGHAZ; welding thermal simulation; impact toughness; bainite
| 1 | Editorial Department of China Journal of Highway. Review on China's bridge engineering research: 2021 [J]. China J. Highway Transp., 2021, 34(2): 1 |
| 1 | 《中国公路学报》编辑部. 中国桥梁工程学术研究综述·2021 [J]. 中国公路学报, 2021, 34(2): 1 |
| 2 | Fan Y. Study on controlling of mechanical and corrostion-resistance proeperties OFQ500EHPS steel for bridge [D]. Qinhuangdao: Yanshan University, 2017 |
| 2 | 范益. Q500EHPS桥梁钢力学性能和耐蚀性能的调控研究 [D]. 秦皇岛: 燕山大学, 2017 |
| 3 | Huang H Q, Che P, Pei X F, et al. Development status and prospects of welding technology for bridge steel structures in my country [J]. Weld Technol., 2019, 48(suppl.2) : 60 |
| 3 | 黄会强, 车平, 裴雪峰 等. 我国桥梁钢结构焊接技术发展现状及展望 [J]. 焊接技术, 2019, 48(): 60 |
| 4 | Hu X P, Wen D H, Li Z G. Development of high performance steel used for bridge [J]. Heat Process. Technol., 2008, 37(22): 91 |
| 4 | 胡晓萍, 温东辉, 李自刚. 高性能桥梁用钢的发展 [J]. 热加工工艺, 2008, 37(22): 91 |
| 5 | Yan Z G, Zhao X X, Xu X J. Study on applicability of Q500qE steel for Hutong Yangtze River Bridge [J]. China Railw. Sci., 2017, 38(3): 40 |
| 5 | 闫志刚, 赵欣欣, 徐向军. 沪通长江大桥Q500qE钢的适用性研究 [J]. 中国铁道科学, 2017, 38(3): 40 |
| 6 | Li Y G, Zhu X H, Liu Z G, et al. Experimental study of welding technique for Q500qE steel used to Tianshenggang Navigational Channel Bridge of Hutong Changjiang River Bridge [J]. World Bridge, 2018, 46(1): 61 |
| 6 | 李彦国, 朱新华, 刘志刚 等. 沪通长江大桥天生港专用航道桥Q500qE钢焊接工艺试验研究 [J]. 世界桥梁, 2018, 46(1): 61 |
| 7 | Gao J, Qu W S, Zhou K G. Research and development of high-performance weather-resistant wide and heavy steel plate Q50QqENH with rare earth for bridge [J]. Baogang Technol., 2020, 46(3): 39 |
| 7 | 高军, 屈文胜, 周可哥. 稀土高性能耐候桥梁宽厚钢板Q500qENH研发 [J]. 包钢科技, 2020, 46(3): 39 |
| 8 | Bei Y C, Xu X J. Study on weldability experimental for high performance Q500qE steel [J]. Met. Process. (Hot Work.), 2018, (12): 42 |
| 8 | 贝玉成, 徐向军. 高性能Q500qE钢焊接性试验研究 [J]. 金属加工(热加工), 2018, (12): 42 |
| 9 | Chen J X, Ren X L, He X, et al. Development of submerged arc welding wire for new high performances bridge steel Q500qE [J]. Weld. Technol., 2018, 47(3): 66 |
| 9 | 陈建雄, 任希乐, 何秀 等. 新型高性能桥梁钢Q500qE用埋弧焊丝的研制 [J]. 焊接技术, 2018, 47(3): 66 |
| 10 | Ma K, Zhao L P, He S Q, et al. The development of YSF105Q agglomerated flux for submerged welding of Q500qE high strength bridge steel [J]. Mach. Manuf. Dig. (Weld. Book), 2018, (2): 35 |
| 10 | 马昆, 赵利鹏, 何少卿 等. Q500qE高强度桥梁钢埋弧焊用YSF105Q烧结焊剂的研制 [J]. 机械制造文摘(焊接分册), 2018, (2): 35 |
| 11 | Shi Y W, Han Z X. Effect of weld thermal cycle on microstructure and fracture toughness of simulated heat-affected zone for a 800 MPa grade high strength low alloy steel [J]. J. Mater. Process. Technol., 2008, 207: 30 |
| 12 | Xu W W, Wang Q F, Pan T, et al. Effect of welding heat input on simulated HAZ microstructure and toughness of a V-N microalloyed steel [J]. J. Iron Steel Res. Int., 2007, 14(5 suppl.1) : 234 |
| 13 | Li X D, Shang C J, Han C C, et al. Influence of necklace-type M-A constituent on impact toughness and fracture mechanism in the heat affected zone of X100 pipeline steel [J]. Acta Metall. Sin., 2016, 52: 1025 |
| 13 | 李学达, 尚成嘉, 韩昌柴 等. X100管线钢焊接热影响区中链状M-A组元对冲击韧性和断裂机制的影响 [J]. 金属学报, 2016, 52: 1025 |
| 14 | Peng Y, Song L, Zhao L, et al. Research status of weldability of advanced steel [J]. Acta Metall. Sin., 2020, 56: 601 |
| 14 | 彭云, 宋亮, 赵琳 等. 先进钢铁材料焊接性研究进展 [J]. 金属学报, 2020, 56: 601 |
| 15 | Lan L Y, Qiu C L, Zhao D W, et al. Microstructural characteristics and toughness of the simulated coarse grained heat affected zone of high strength low carbon bainitic steel [J]. Mater. Sci. Eng., 2011, A529: 192 |
| 16 | Hu J, Du L X, Wang J J, et al. Effect of welding heat input on microstructures and toughness in simulated CGHAZ of V-N high strength steel [J]. Mater. Sci. Eng., 2013, A577: 161 |
| 17 | Cui J J, Zhu W T, Chen Z Y, et al. Effect of simulated cooling time on microstructure and toughness of CGHAZ in novel high-strength low-carbon construction steel [J]. Sci. Technol. Weld. Join., 2019, 25: 169 |
| 18 | Zhou P S, Wang B, Wang L, et al. Effect of welding heat input on grain boundary evolution and toughness properties in CGHAZ of X90 pipeline steel [J]. Mater. Sci. Eng., 2018, A722: 112 |
| 19 | Yang Y, Shang C J, Chen L, et al. Investigation on the crystallography of the transformation products of reverted austenite in intercritically reheated coarse grained heat affected zone [J]. Mater. Des., 2013, 43: 485 |
| 20 | Chen H D, Zhang S J, Liu D S. Phase transformation and joint properties of bridge steel plate Q500qE welding coarse grain zone [J]. Trans. Chin. Weld. Soc., 2017, 38(7): 123 |
| 20 | 陈焕德, 张淑娟, 刘东升. 桥梁钢板Q500qE焊接粗晶区相变及接头性能 [J]. 焊接学报, 2017, 38(7): 123 |
| 21 | Lambert-Perlade A, Gourgues A F, Pineau A. Austenite to bainite phase transformation in the heat-affected zone of a high strength low alloy steel [J]. Acta Mater., 2004, 52: 2337 |
| 22 | Morito S, Saito H, Ogawa T, et al. Effect of austenite grain size on the morphology and crystallography of lath martensite in low carbon steels [J]. Trans. Iron Steel Inst. Jpn., 2005, 45: 91 |
| 23 | Luo H W, Wang X H, Liu Z B, et al. Influence of refined hierarchical martensitic microstructures on yield strength and impact toughness of ultra-high strength stainless steel [J]. J. Mater. Sci. Technol., 2020, 51: 130 |
| 24 | Morito S, Tanaka H, Konishi R, et al. The morphology and crystallography of lath martensite in Fe-C alloys [J]. Acta Mater., 2003, 51: 1789 |
| 25 | Wang H B, Wang F L, Shi G H, et al. Effect of welding heat input on microstructure and impact toughness in CGHAZ of X100Q steel [J]. J. Iron Steel Res. Int., 2019, 26: 637 |
| 26 | Nohava J, Hau?ild P, Karl??K M, et al. Electron backscattering diffraction analysis of secondary cleavage cracks in a reactor pressure vessel steel [J]. Mater. Charact., 2002, 49: 211 |
| 27 | Yang Y, Shang C J, Nie W J, et al. Investigation on the microstructure and toughness of coarse grained heat affected zone in X-100 multi-phase pipeline steel with high Nb content [J]. Mater. Sci. Eng., 2012, A558: 692 |
| 28 | Zhang C Y, Wang Q F, Ren J X, et al. Effect of martensitic morphology on mechanical properties of an as-quenched and tempered 25CrMo48V steel [J]. Mater. Sci. Eng., 2012, A534: 339 |
| 29 | Daigne J, Guttmann M, Naylor J P. The influence of lath boundaries and carbide distribution on the yield strength of 0.4%C tempered martensitic steels [J]. Mater. Sci. Eng., 1982, 56: 1 |
| 30 | Terasaki H, Shintome Y, Takada A, et al. Visualization and analysis of variant grouping in continuously cooled low-carbon steel welds [J]. Metall. Mater. Trans., 2014, 45A: 3554 |
| 31 | Olasolo M, Uranga P, Rodriguez-Ibabe J M, et al. Effect of austenite microstructure and cooling rate on transformation characteristics in a low carbon Nb-V microalloyed steel [J]. Mater. Sci. Eng., 2011, A528: 2559 |
/
| 〈 |
|
〉 |