研究论文

基于二次枝晶间距变化特征的连铸方坯CET位置判断新方法

  • 郭东伟 ,
  • 郭坤辉 ,
  • 张福利 ,
  • 张飞 ,
  • 曹江海 ,
  • 侯自兵
展开
  • 1.重庆大学 材料科学与工程学院 重庆 400044
    2.重庆大学 钒钛冶金及新材料重庆市重点实验室 重庆 400044
郭东伟,男,1995年生,博士生

收稿日期: 2021-04-21

  修回日期: 2021-06-25

  网络出版日期: 2021-07-20

基金资助

国家自然科学基金委员会-中国宝武钢铁集团有限公司钢铁联合研究基金项目(U1860101)

A New Method for CET Position Determination of Continuous Casting Billet Based on the Variation Characteristics of Secondary Dendrite Arm Spacing

  • Dongwei GUO ,
  • Kunhui GUO ,
  • Fuli ZHANG ,
  • Fei ZHANG ,
  • Jianghai CAO ,
  • Zibing HOU
Expand
  • 1.College of Materials Science and Engineering, Chongqing University, Chongqing 400044, China
    2.Chongqing Key Laboratory of Vanadium-Titanium Metallurgy and New Materials, Chongqing University, Chongqing 400044, China
HOU Zibing, associate professor, Tel: 13628489073, E-mail: houzibing@cqu.edu.cn

Received date: 2021-04-21

  Revised date: 2021-06-25

  Online published: 2021-07-20

Supported by

United Funds between National Natural Science Foundation and Baowu Steel Group Corporation Limited of China(U1860101)

摘要

从碳钢连铸坯实际凝固组织入手对典型枝晶二次枝晶间距(secondary dendrite arm spacing,SDAS)进行测量分析,并发现了铸坯表面向中心凝固过程中的SDAS突增现象。结合铸坯横断面二维温度场数值模型分析可知,柱状晶向等轴晶转变(columnar to equiaxed transition,CET)的过程会影响铸坯内部的传热过程,这种影响最终以典型枝晶SDAS突增的形式体现出来。基于典型枝晶SDAS突增现象,确立了铸坯内部CET定量判定的新方法,即将典型枝晶SDAS最大增加率的起始位置确定为铸坯内部CET起始位置。计算所得CET位置与铸坯内部温度梯度变化拐点的最大相对误差仅为8.3%,且与生长速率变化区间相对应,同时也与实际凝固组织形貌转变位置吻合,证明了该方法的有效性。

本文引用格式

郭东伟 , 郭坤辉 , 张福利 , 张飞 , 曹江海 , 侯自兵 . 基于二次枝晶间距变化特征的连铸方坯CET位置判断新方法[J]. 金属学报, 2022 , 58(6) : 827 -836 . DOI: 10.11900/0412.1961.2021.00170

Abstract

High-end steel products play an essential role in economic development and infrastructure projects. Nowadays, continuous casting is an important production process of high-end steel products due to higher efficiency and lower energy consumption. However, the quality and properties of end products, such as steel billets, bloom, and bar, will be affected by internal segregation defects, which are closely related to solidification structure characteristics. In the research on the solidification structure characteristics of billets, the columnar to equiaxed transition (CET) determination is of great significance to determine equiaxed crystal zones and the quality control of continuous casting billets. In this work, the secondary dendrite arm spacing (SDAS) of typical dendrites was measured and analyzed using the actual solidification structure of continuous casting billets and the mutation of SDAS during the solidification process from the billet surface to the center was found. Combined with the two-dimensional temperature field numerical model of the billet cross section, it can be seen that the CET will affect the heat transfer process in the billet and this will be reflected as the mutation of SDAS in typical dendrites. This work proposed a new method for the quantitative determination of CET in the continuous casting billets based on this mutation, and the starting position of the maximum SDAS increase rate is determined as the starting position of the CET. The CET positions calculated using the new method correspond to changes in the thermal gradient and growth rate in the billet, and are consistent with the positions of the actual solidification structure morphology transformations, which prove the effectiveness of this method.

参考文献

1 Lage M G, Da Costa e Silva A L V. Evaluating segregation in HSLA steels using computational thermodynamics [J]. J. Mater. Res. Technol., 2015, 4: 353
2 Long M J, Chen D F. Study on mitigating center macro-segregation during steel continuous casting process [J]. Steel Res. Int., 2011, 82: 847
3 Ayata K, Mori T, Fujimoto T, et al. Improvement of macrosegregation in continuously cast bloom and billet by electromagnetic stirring [J]. Trans. Iron Steel Inst. Jpn., 1984, 24: 931
4 Li P S, Lu J H, Qiu S T, et al. Control of equiaxed crystal ratio of high carbon steel billets by circular seam cooling nozzle [J]. J. Iron Steel Res. Int., 2011, 18: 24
5 Ludlow V, Normanton A, Anderson A, et al. Strategy to minimise central segregation in high carbon steel grades during billet casting [J]. Ironmak. Steelmak., 2005, 32: 68
6 Jiang D, Zhu M. Solidification structure and macrosegregation of billet continuous casting process with dual electromagnetic stirrings in mold and final stage of solidification: A numerical study [J]. Metall. Mater. Trans., 2016, 47B: 3446
7 Choudhary S K, Ganguly S. Morphology and segregation in continuously cast high carbon steel billets [J]. Trans. Iron Steel Inst. Jpn., 2007, 47: 1759
8 Hunt J D. Steady state columnar and equiaxed growth of dendrites and eutectic [J]. Mater. Sci. Eng., 1984, 65: 75
9 Shibata H, Itoyama S, Kishimoto Y, et al. Prediction of equiaxed crystal ratio in continuously cast steel slab by simplified columnar-to-equiaxed transition model [J]. ISIJ Int., 2006, 46: 921
10 Niu L, Qiu S T, Zhao J X, et al. Processing parameter optimization for continuous casting of 38CrMoAl round bloom based on a prediction model of the equiaxed crystal ratio [J]. Ironmak. Steelmak., 2019, 46: 835
11 Luo S, Zhu M Y, Louhenkilpi S. Numerical simulation of solidification structure of high carbon steel in continuous casting using cellular automaton method [J]. ISIJ Int., 2012, 52: 823
12 Hou Z B, Jiang F, Cheng G G. Solidification structure and compactness degree of central equiaxed grain zone in continuous casting billet using cellular automaton-finite element method [J]. ISIJ Int., 2012, 52: 1301
13 Biscuola V B, Martorano M A. Mechanical blocking mechanism for the columnar to equiaxed transition [J]. Metall. Mater. Trans., 2008, 39A: 2885
14 Zuo P F, Chen S Y, Wei M W, et al. Thermal behavior and grain evolution of 24CrNiMoY alloy steel prepared by pre-laid laser cladding technology [J]. Opt. Laser Technol., 2019, 119: 105613
15 Zhang K L, Li Y J, Yang Y S. Influence of the low voltage pulsed magnetic field on the columnar-to-equiaxed transition during directional solidification of superalloy K4169 [J]. J. Mater. Sci. Technol., 2020, 48: 9
16 Hou Z B, Guo Z A, Guo D W, et al. A new method for carbon content distribution based on grayscale image of casting blank macrostructure in carbon steel [J]. J. Iron Steel Res., 2019, 31: 620
16 侯自兵, 郭中傲, 郭东伟 等. 利用碳钢铸坯组织灰度图获取C含量分布的方法 [J]. 钢铁研究学报, 2019, 31: 620
17 Cao J H, Hou Z B, Guo Z, et al. An application of fractal theory to complex macrostructure: quantitatively characterization of segregation morphology [J]. ISIJ Int., 2020, 60: 1188
18 Wang W, Hou Z B, Chang Y, et al. Effect of superheat on quality of central equiaxed grain zone of continuously cast bearing steel billet based on two-dimensional segregation ratio [J]. J. Iron Steel Res. Int., 2018, 25: 9
19 Choudhary S K, Mazumdar D. Mathematical modelling of fluid flow, heat transfer and solidification phenomena in continuous casting of steel [J]. Steel Res. Int., 1995, 66: 199
20 Cai K K, Yang J C. Investigation of heat transfer in the spray cooling of continuous casting [J]. J. Univ. Sci. Technol. Beijing, 1989, 11: 509
21 Li B, Zhang Z H, Liu H S, et al. Characteristics and evolution of the spot segregations and banded defects in high strength corrosion resistant tube steel [J]. Acta Metall. Sin., 2019, 55: 762
21 李 博, 张忠铧, 刘华松 等. 高强耐蚀管钢点状偏析及带状缺陷的特征与演变 [J]. 金属学报, 2019, 55: 762
22 Ji Y, Tang H Y, Lan P, et al. Effect of dendritic morphology and central segregation of billet castings on the microstructure and mechanical property of hot‐rolled wire rods [J]. Steel Res. Int., 2017, 88: 1600426
23 Min Y, Liu C J, Wang D Y, et al. Prediction of equiaxed crystal ratio of continuous casting round billet of 37Mn5 steel [J]. J. Iron Steel Res., 2011, 23(10): 38
23 闵 义, 刘承军, 王德永 等. 37Mn5连铸圆坯中心等轴晶率预测 [J]. 钢铁研究学报, 2011, 23(10): 38
24 Esaka H, Wakabayashi T, Shinozuka K, et al. Origin of equiaxed grains and their motion in the liquid phase [J]. ISIJ Int., 2003, 43: 1415
25 Li J M, Jiang M F, Ning J X, et al. Effect of casting speed on dendrite arm spacing of Mn13 steel continuous casting slab [J]. J. Iron Steel Res. Int., 2020, 27: 665
26 Ziv I, Weinberg F. The columnar-to-equiaxed transition in Al 3 Pct Cu [J]. Metall. Trans., 1989, 20B: 731
27 Hu H Q. Metal Solidification Principle [M]. 2nd Ed., Beijing: Machine Industry Press, 2012: 84
27 胡汉起. 金属凝固原理 [M]. 第 2版, 北京: 机械工业出版社, 2012: 84
文章导航

/