国内航空发动机涡轮盘用铸锻难变形高温合金热加工研究现状与展望
收稿日期: 2021-04-12
修回日期: 2021-07-07
网络出版日期: 2021-07-09
基金资助
国家重点研发计划项目(2019YFA0705300、2017YFA0700703);国家科技重大专项项目(2019-VI-0006-0120);辽宁省博士启动基金项目(2020-BS-007);中国科学院金属研究所创新基金项目(2021-PY09)
Present Research Situation and Prospect of Hot Working of Cast & Wrought Superalloys for Aero-Engine Turbine Disk in China
Received date: 2021-04-12
Revised date: 2021-07-07
Online published: 2021-07-09
Supported by
National Key Research and Development Program of China(2019YFA0705300、2017YFA-0700703);National Science and Technology Magjor Project of China(2019-VI-0006-0120);Doctoral Foundation of Liaoning Province(2020-BS-007);IMR Innovation Fund(2021-PY09)
张瑞 , 刘鹏 , 崔传勇 , 曲敬龙 , 张北江 , 杜金辉 , 周亦胄 , 孙晓峰 . 国内航空发动机涡轮盘用铸锻难变形高温合金热加工研究现状与展望[J]. 金属学报, 2021 , 57(10) : 1215 -1228 . DOI: 10.11900/0412.1961.2021.00153
In recent years, the demand for high-performance aero-engines has become crucial in China, and the service environment of turbine disk alloy becomes increasingly severe. A series of high resistant cast & wrought superalloys for turbine disks, such as GH4065, GH4720Li, GH4068, and GH4151, with working temperatures > 700°C, have been studied, produced, and applied widely. The current studies on cast & wrought alloys for turbine disks in China were summarized under the categories of homogenization treatment, cogging, disk forging, and microstructure and property regulation to promote the development of these superalloys and improve their comprehensive properties. The difficulties encountered during the research and preparation of these hard-to-deform superalloys and explored the alloys' potential development trend were outlined. The review would improve the production stability of the disk superalloys and promote their development.
| 1 | Logunov A V, Zavodov S A, Danilov D V. The challenges in development of nickel-based heat-resistant superalloys for gas turbine disks and creation of a new superalloy with increased operational characteristics [J]. Mater. Today: Proc., 2019, 11: 459 |
| 2 | Gu Y F, Fukuda T, Cui C Y, et al. Comparison of mechanical properties of TMW alloys, new generation of cast-and-wrought superalloys for disk applications [J]. Metall. Mater. Trans., 2009, 40A: 3047 |
| 3 | Li F L, Fu R, Yin F J, et al. Impact of γ′ (Ni3 (Al, Ti)) phase on dynamic recrystallization of a Ni-based disk superalloy during isothermal compression [J]. J. Alloys Compd., 2017, 693: 1076 |
| 4 | Reed R C. The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2008: 217 |
| 5 | Zhao G P, Huang S, Zhang B J, et al. Microstructure control and mechanical properties of the newest nickel-based wrought superalloy GH4065A [J]. J. Iron Steel Res., 2015, 27(2): 37 |
| 5 | 赵光普, 黄 烁, 张北江等. 新一代镍基变形高温合金GH4065A的组织控制与力学性能 [J]. 钢铁研究学报, 2015, 27(2): 37 |
| 6 | Qu J L, Bi Z N, Du J H, et al. Research on process optimization of isothermal forging for superalloy GH4720Li disc [A]. Proceedings of the 12th China Superalloy Annual Meeting [C]. Beijing: the Chinese Society for Metals, 2011: 263 |
| 6 | 曲敬龙, 毕中南, 杜金辉等. GH4720Li合金盘锻件的等温锻造工艺优化研究 [A]. 第十二届中国高温合金年会论文集 [C]. 北京: 中国金属学会, 2011: 263 |
| 7 | Cui C Y, Jin T, Sun X F. A nickel-cobalt base superalloy with good microstructure stability and easy processing ability [P]. Chin Pat, 201010505227.3, 2012 |
| 7 | 崔传勇, 金 涛, 孙晓峰. 一种组织稳定性好、易加工的镍钴基高温合金 [P]. 中国专利, 201010505227.3, 2012) |
| 8 | Lv S M, Chen J B, He X B, et al. Investigation on Sub-Solvus recrystallization mechanisms in an advanced γ-γ' nickel-based superalloy GH4151 [J]. Materials, 2020, 13: 4553 |
| 9 | Liu F F, Chen J Y, Dong J X, et al. The hot deformation behaviors of coarse, fine and mixed grain for Udimet 720Li superalloy [J]. Mater. Sci. Eng., 2016, A651: 102 |
| 10 | Ning Y Q, Zhang B Y. Hot forming of superalloy parts and structures [A]. Reference Module in Materials Science and Materials Engineering [C]. Amsterdam: Elsevier, 2020: 1 |
| 11 | Huang S, Zhang B J, Tian Q, et al. Isothermal and static oxidation behavior of superalloy GH4065A [J]. J. Iron Steel Res., 2016, 28(7): 55 |
| 11 | 黄 烁, 张北江, 田 强等. 高温合金GH4065A的恒温静态氧化行为 [J]. 钢铁研究学报, 2016, 28(7): 55 |
| 12 | Du J H, Qu J L, Deng Q, et al. As-cast microstructure and homogenization process of alloy GH720Li [J]. J. Iron Steel Res., 2005, 17(3): 60 |
| 12 | 杜金辉, 曲敬龙, 邓 群等. GH720Li合金的铸态组织和均匀化工艺 [J]. 钢铁研究学报, 2005, 17(3): 60 |
| 13 | Zhou Z J, Zhang R, Cui C Y, et al. Effects of homogenization treatment on the microsegregation of a Ni-Co based superalloy produced by directional solidification [J]. Acta Metall. Sin. (Engl. Lett.), 2021, 34: 943 |
| 14 | Bi Z N, Qu J L, Du J H, et al. Segregation behavior and investigation on homogenization for a new difficult-to-deform superalloy ЭК151 ingot [J]. J. Iron Steel Res., 2011, 23(suppl.2): 263 |
| 14 | 毕中南, 曲敬龙, 杜金辉等. 新型难变形高温合金ЭК151的偏析行为及均匀化工艺研究 [J]. 钢铁研究学报, 2011, 23(): 263 |
| 15 | Zhang B J, Huang S, Zhang W Y, et al. Recent development of nickel-based disc alloys and corresponding cast-wrought processing techniques [J]. Acta Metall. Sin., 2019, 55: 1095 |
| 15 | 张北江, 黄 烁, 张文云等. 变形高温合金盘材及其制备技术研究进展 [J]. 金属学报, 2019, 55: 1095 |
| 16 | Zhang B J, Zhao G P, Zhang W Y, et al. Investigation of high performance disc alloy GH4065 and associated advanced processing techniques [J]. Acta Metall. Sin., 2015, 51: 1227 |
| 16 | 张北江, 赵光普, 张文云等. 高性能涡轮盘材料GH4065及其先进制备技术研究 [J]. 金属学报, 2015, 51: 1227 |
| 17 | Zhang R, Tian C G, Cui C Y, et al. Portevin-Le Chatelier effect in a wrought Ni-Co based superalloy [J]. J. Alloys Compd., 2020, 818: 152863 |
| 18 | Cui C Y, Zhang R, Zhou Y Z, et al. Portevin-Le Chatelier effect in wrought Ni-based superalloys: Experiments and mechanisms [J]. J. Mater. Sci. Technol., 2020, 51: 16 |
| 19 | Wang Q Z, Shi L, Tang C. Metallurgy quality of GH4720Li alloy by VIM + PESR + VAR [J]. Baosteel Tech., 2020, (3): 62 |
| 19 | 王庆增, 石 磊, 唐 超. GH4720Li合金VIM+PESR+VAR三联工艺及冶金质量 [J]. 宝钢技术, 2020, (3): 62 |
| 20 | Du J H, Lv X D, Dong J X, et al. Research progress of wrought superalloys in China [J]. Acta Metall. Sin., 2019, 55: 1115 |
| 20 | 杜金辉, 吕旭东, 董建新等. 国内变形高温合金研制进展 [J]. 金属学报, 2019, 55: 1115 |
| 21 | Li F L, Fu R, Feng D, et al. Microstructure and segregation behavior of Rene88DT alloy prepared by ESR-CDS [J]. Rare Met. Mater. Eng., 2016, 45: 1437 |
| 22 | Zhuang X P, Tan Y, Zhao L H, et al. Microsegregation of a new Ni-Co-based superalloy prepared through electron beam smelting and its homogenization treatment [J]. J. Mater. Res. Technol., 2020, 9: 5422 |
| 23 | Fu R, Li F L, Yin F J, et al. Microstructure evolution and deformation mechanisms of the electroslag refined-continuous directionally solidified (ESR-CDS?) superalloy Rene88DT during isothermal compression [J]. Mater. Sci. Eng., 2015, A638: 152 |
| 24 | Wang Z X, Huang S, Zhang B J, et al. Study on freckle of a high-alloyed GH4065 nickel base wrought superalloy [J]. Acta Metall. Sin., 2019, 55: 417 |
| 24 | 王资兴, 黄 烁, 张北江等. 高合金化GH4065镍基变形高温合金点状偏析研究 [J]. 金属学报, 2019, 55: 417 |
| 25 | Bi Z N, Qu J L, Du J H, et al. Microstructure characteristics and thermodynamic calculation of equilibrium precipitated phases in a new difficult-to-deform superalloy ЭК151 [J]. Rare Met. Mater. Eng., 2013, 42: 919 |
| 25 | 毕中南, 曲敬龙, 杜金辉等. 新型难变形高温合金ЭК151的组织特征及平衡析出相热力学计算 [J]. 稀有金属材料与工程, 2013, 42: 919 |
| 26 | Li X X, Jia C L, Jiang Z H, et al. Investigation of solidification behavior in a new high alloy Ni-based superalloy [J]. JOM, 2020, 72: 4139 |
| 27 | Chang L T, Jin H, Sun W R. Solidification behavior of Ni-base superalloy Udimet 720Li [J]. J. Alloys Compd., 2015, 653: 266 |
| 28 | Li X X, Jia C L, Zhang Y, et al. Segregation and homogenization for a new nickel-based superalloy [J]. Vacuum, 2020, 177: 109379 |
| 29 | Semiatin S L, Kramb R C, Turner R E, et al. Analysis of the homogenization of a nickel-base superalloy [J]. Scr. Mater., 2004, 51: 491 |
| 30 | Zhu Y X. Shi Changxu's major contributions in the field of superalloy [J]. Sci. Technol. Rev., 2018, 36(19): 21 |
| 30 | 朱耀宵. 师昌绪在高温合金领域的重大贡献 [J]. 科技导报, 2018, 36(19): 21 |
| 31 | Qu J L, Du J H, Deng Q, et al. Effect of compound jacketing rolling process on microstructure of difficult-to-deform superalloy GH720Li [J]. Mater. Sci. Technol., 2008, 16: 121 |
| 31 | 曲敬龙, 杜金辉, 邓 群等. 复合包套轧制工艺对难变形高温合金GH720Li组织的影响 [J]. 材料科学与工艺, 2008, 16: 121 |
| 32 | Cao Y X, Application of the soft package technology on titanium alloy forging [J]. Aviat. Maint. Eng., 2015, (12): 92 |
| 32 | 曹颖玺. 钛合金锻造软包套工艺应用研究 [J]. 航空维修与工程, 2015, (12): 92 |
| 33 | Semiatin S L, Weaver D S, Kramb R C, et al. Deformation and recrystallization behavior during hot working of a coarse-grain, nickel-base superalloy ingot material [J]. Metall. Mater. Trans, 2004, 35A: 679 |
| 34 | Fan H Y, Jiang H, Dong J X, et al. An optimization method of upsetting process for homogenized, nickel-based superalloy Udimet 720Li ingot considering both cracking and recrystallization [J]. J. Mater. Process. Technol., 2019, 269: 52 |
| 35 | Chen X M, Lin Y C, Wen D X, et al. Dynamic recrystallization behavior of a typical nickel-based superalloy during hot deformation [J]. Mater. Des., 2014, 57: 568 |
| 36 | Kan Z. Study on microstructure evolvement and forging technology of great size bar for GH4720Li alloy [D]. Shenyang: Northeastern University, 2017 |
| 36 | 阚 志. GH4720Li合金微观组织演变及大尺寸棒坯锻造工艺研究 [D]. 沈阳: 东北大学, 2017 |
| 37 | Liu P, Zhang R, Yuan Y, et al. Hot deformation behavior and workability of a Ni-Co based superalloy [J]. J. Alloys Compd., 2020, 831: 154618 |
| 38 | Han G M, Li F, Sun B D. Multimodal distribution of γ′ phase and effect on hot deformation in a wrought nickel base superalloy [J]. Rare Met. Mater. Eng., 2019, 48: 2821 |
| 39 | Li F, Fu R, Feng D, et al. Microstructure evolution during hot deformation of as cast ESR-CDSed superalloy Rene88DT [J]. Mater. Res. Innov., 2014, 18(suppl. 4): S4-421 |
| 40 | Ning Y Q, Wang T, Fu M W, et al. Competition between work-hardening effect and dynamic-softening behavior for processing as-cast GH4720Li superalloys with original dendrite microstructure during moderate-speed hot compression [J]. Mater. Sci. Eng., 2015, A642: 187 |
| 41 | Wang M J, Wang W R, Liu Z L, et al. Hot workability integrating processing and activation energy maps of Inconel 740 superalloy [J]. Mater. Today Commun., 2018, 14: 188 |
| 42 | Wan Z P, Hu L X, Sun Y, et al. Hot deformation behavior and processing workability of a Ni-based alloy [J]. J. Alloys Compd., 2018, 769: 367 |
| 43 | Liu P, Zhang R, Yuan Y, et al. Microstructural evolution of a Ni-Co based superalloy during hot compression at γ′ sub-/supersolvus temperatures [J]. J. Mater. Sci. Technol., 2020, 77: 66 |
| 44 | Katnagallu S, Vernier S, Charpagne M A, et al. Nucleation mechanism of hetero-epitaxial recrystallization in wrought nickel-based superalloys [J]. Scr. Mater., 2021, 191: 7 |
| 45 | Qu J L, Bi Z N, Du J H, et al. Hot deformation behavior of nickel-based superalloy GH4720Li [J]. J. Iron Steel Res. Int., 2011, 18: 59 |
| 46 | Zhou G, Han Y B, Qu J L, et al. A comparative study of various flow instability criteria in processing map of superalloy U720Li [J]. J Northeastern Univ (Nat Sci), 2012, 33: 702 |
| 46 | 周 舸, 韩寅奔, 曲敬龙等. U720Li镍基高温合金不同失稳判据的热加工图 [J]. 东北大学学报(自然科学版), 2012, 33: 702 |
| 47 | Shen J Y, Hu L X, Sun Y, et al. Hot deformation behaviors and three-dimensional processing map of a nickel-based superalloy with initial dendrite microstructure [J]. J. Alloys Compd., 2020, 822: 153735 |
| 48 | Xu L. Investigation on microstructures and mechanical properties of Ni-Co based wrought superalloys [D]. Beijing: University of Chinese Academy of Sciences, 2014 |
| 48 | 徐 玲. Ni-Co基变形高温合金组织性能研究 [D]. 北京: 中国科学院大学, 2014 |
| 49 | Xu L, Chu Z K, Cui C Y, et al. Creep mechanism of a Ni-Co base wrought superalloy [J]. Acta Metall. Sin., 2013, 49: 863 |
| 49 | 徐 玲, 储昭贶, 崔传勇等. 一种镍钴基变形高温合金蠕变变形机制的研究 [J]. 金属学报, 2013, 49: 863 |
| 50 | Gu Y F, Cui C Y, Yuan Y, et al. Research progress in a high performance cast & wrought superalloy for turbine disc applications [J]. Acta Metall. Sin., 2015, 51: 1191 |
| 50 | 谷月峰, 崔传勇, 袁 勇等. 一种高性能航空涡轮盘用铸锻合金的研究进展 [J]. 金属学报, 2015, 51: 1191 |
| 51 | Xu H, Zhang Z J, Zhang P, et al. The synchronous improvement of strength and plasticity (SISP) in new Ni-Co based disc superalloys by controling stacking fault energy [J]. Sci. Rep., 2017, 7: 8046 |
| 52 | Zhu C Z, Zhang R, Cui C Y, et al. Effect of Ta addition on the microstructure and tensile properties of a Ni-Co base superalloy [J]. Metall. Mater. Trans., 2021, 52A: 108 |
| 53 | Zhu C Z, Zhang R, Cui C Y, et al. Influence of Ta content on microstructure and creep behavior of a Ni-Co base disc superalloy [J]. Mater. Sci. Eng., 2021, A802: 140646 |
| 54 | Xu H, Zhang Z J, Zhang P, et al. Formation of nanograins in Ni-Co based superalloys compressed quasistatically at high temperature [J]. Scr. Mater., 2017, 136: 92 |
/
| 〈 |
|
〉 |