埋弧焊中焊剂对焊缝金属成分调控的研究进展
收稿日期: 2021-04-08
修回日期: 2021-06-10
网络出版日期: 2021-06-18
基金资助
国家自然科学基金项目(U20A20277);中央高校基本科研业务费项目(N2025025);兴辽英才基金项目(XLYC1807024);辽宁省工业重大专项项目(2019JH1/10100014);辽宁省区域创新发展联合基金项目(2020-YKLH-39);英国皇家工学院项目(TSPC1070);海洋装备用金属材料及其应用国家重点实验室开放基金项目(SKLMEA-K201903)
Fine-Tuning Weld Metal Compositions via Flux Optimization in Submerged Arc Welding: An Overview
Received date: 2021-04-08
Revised date: 2021-06-10
Online published: 2021-06-18
Supported by
National Natural Science Foundation of China(U20A20277);Fundamental Research Funds for the Central Universities(N2025025);Xingliao Talents Program(XLYC1807024);Liaoning Key Industrial Program(2019JH1/10100014);Regional Innovation Joint Fund of Liaoning Province(2020-YKLH-39);Royal Academy of Engineering(TSPC1070);Open Foundation of State Key Laboratory of Metal Material for Marine Equipment and Application(SKLMEA-K201903)
王聪 , 张进 . 埋弧焊中焊剂对焊缝金属成分调控的研究进展[J]. 金属学报, 2021 , 57(9) : 1126 -1140 . DOI: 10.11900/0412.1961.2021.00148
Flux is an indispensable consumable for submerged arc welding. Owing to the occurrence of complex chemical reactions between flux (slag), weld pool, and arc plasma, flux plays an essential role in determining the final composition of weld metal. To ensure a sound weldment, understanding how submerged arc welded metal compositions are fine-tuned by flux optimization is necessary. Herein, recent progress regarding the control mechanisms of fluxes on submerged arc welded metal compositions is studied. Particularly, the element transfer behaviors of major elements, including oxygen, silicon, manganese, titanium, and carbon, are documented from thermodynamic perspectives. Salient element transfer features incurred by the application of high heat input welding are interpreted. Moreover, the capabilities and limitations of prevailing compositional prediction models are evaluated. Finally, fundamental challenges to be explored further are discussed.
| 1 | Kou S. Welding Metallurgy [M]. 2nd Ed., Hoboken, New Jersey: John Wiley & Sons, Inc., 2003: 22 |
| 2 | Wu C X, Zhang J X, Zhu B K, et al. Development and application of high efficiency submerged arc welding technology [J]. Hot Work. Technol., 2009, 38(23): 173 |
| 2 | 武春学, 张俊旭, 朱丙坤等. 高效埋弧焊技术的发展及应用 [J]. 热加工工艺, 2009, 38(23): 173 |
| 3 | Zhang J, Leng J, Wang C. Tuning weld metal mechanical responses via welding flux optimization of TiO2 content: Application into EH36 shipbuilding steel [J]. Metall. Mater. Trans., 2019, 50B: 2083 |
| 4 | Qiu C L, Lan L Y, Zhao D W, et al. Microstructural evolution and toughness in the HAZ of submerged arc welded low welding crack susceptibility steel [J]. Acta Metall. Sin. (Engl. Lett.), 2013, 26: 49 |
| 5 | Xu K, Fang T, Zhao L F, et al. Effect of trace element on microstructure and fracture toughness of weld metal [J]. Acta Metall. Sin. (Engl. Lett.), 2020, 33: 425 |
| 6 | Olson D, Liu S, Frost R, et al. Nature and behavior of fluxes used for welding [M]. ASM Handbook, Materials Park, OH, 1993, 6: 55 |
| 7 | Natalie C A, Olson D L, Blander M. Physical and chemical behavior of welding fluxes [J]. Annu. Rev. Mater. Sci., 1986, 16: 389 |
| 8 | Cao J M, Tang B G, Wang S L, et al. A new fused flux for low hydrogen high toughness welds [J]. Trans. China Weld. Inst., 1989, 10(1): 1 |
| 8 | 曹进茂, 唐伯钢, 王世亮等. 熔炼型低氢高韧性焊剂的研究 [J]. 焊接学报, 1989, 10(1): 1 |
| 9 | Bang K S, Park C, Jung H C, et al. Effects of flux composition on the element transfer and mechanical properties of weld metal in submerged arc welding [J]. Met. Mater. Int., 2009, 15: 471 |
| 10 | Belton G R, Moore T J, Tankins E S. Slag-metal reactions in submerged arc welding [J]. Weld. J., 1963, 42: 289 |
| 11 | Fox A, Eakes M, Franke G. The effect of small changes in flux basicity on the acicular ferrite content and mechanical properties of submerged arc weld metal of navy HY-100 steel [J]. Weld. J., 1996, 75: 330S |
| 12 | North T, Bell H, Nowicki A, et al. Slag/metal interaction, O and toughness in submerged arc welding [J]. Weld. J., 1978, 57: 63 |
| 13 | Tuliani S, Boniszewski T, Eaton N. Notch toughness of commercial submerged arc weld metal [J]. Weld. Met. Fabr., 1969, 37: 327 |
| 14 | Chen B L, Zhou Y H. Improvement of toughness and strength of high strength steel submerged arc weld metal [J]. Trans. China Weld. Inst., 1987, 8(7): 153 |
| 14 | 陈伯蠡, 周运鸿. 高强钢埋弧焊焊缝的强韧化研究 [J]. 焊接学报, 1987, 8(7): 153 |
| 15 | Li X D, Shang C J, Han C C, et al. Influence of necklace-type M-A constituent on impact toughness and fracture mechanism in the heat affected zone of X100 pipeline steel [J]. Acta Metall. Sin., 2016, 52: 1025 |
| 15 | 李学达, 尚成嘉, 韩昌柴等. X100管线钢焊接热影响区中链状M-A组元对冲击韧性和断裂机制的影响 [J]. 金属学报, 2016, 52: 1025 |
| 16 | Zhang M, Jia F, Cheng K K, et al. Influence of quenching and tempering on microstructure and properties of welded joints of G520 martensitic steel [J]. Acta Metall. Sin., 2019, 55: 1379 |
| 16 | 张 敏, 贾 芳, 程康康等. 调质处理对G520钢焊接接头组织及性能的影响 [J]. 金属学报, 2019, 55: 1379 |
| 17 | Tian Z L, Xu L H, Peng Y, et al. Formation mechanism of the precipitate-free zone in high strength aluminum alloy welds [J]. Acta Metall. Sin., 2008, 44: 91 |
| 17 | 田志凌, 许良红, 彭 云等. 高强铝合金焊接接头无析出物区的形成机理 [J]. 金属学报, 2008, 44: 91 |
| 18 | Tabuchi M, Kondo M, Watanabe T, et al. Improvement of type IV cracking resistance of 9Cr heat resisting steel weldment by boron addition [J]. Acta Metall. Sin. (Engl. Lett.), 2009, 17: 331 |
| 19 | Guo M H, Shao D C, Dong Z G, et al. Welding between high manganese steel and high carbon steel [J]. Acta Metall. Sin. (Engl. Lett.), 2009, 13: 112 |
| 20 | Li X Q. Chemical reaction at slag/metal interface during quasi-steady welding based on non-equilibrium thermodynamics [D]. Tianjin: Tianjin University, 2007 |
| 20 | 李晓泉. 基于非平衡热力学的准稳态焊接钢-渣界面化学冶金行为 [D]. 天津: 天津大学, 2007 |
| 21 | Olson D L, Dixon R, Liby A L. Welding: Theory and Practice [M]. Amsterdam: Elsevier, 1990: 117 |
| 22 | Olson D, Edwards G, Liu S, et al. Non-equilibrium behaviour of weld metal in flux-related processes [J]. Weld. World, 1993, 31: 142 |
| 23 | Erokhin A A, translated by Zhao Y N. Theory of Fusion Welding [M]. Beijing: China Machine Press, 1981: 171 |
| 23 | Erokhin A A著, 赵裕民译. 熔焊原理 [M]. 北京: 机械工业出版社, 1981: 171 |
| 24 | Zhang J, Coetsee T, Basu S, et al. Impact of gas formation on the transfer of Ti and O from TiO2-bearing basic-fluoride fluxes to submerged arc welded metals: A thermodynamic approach [J]. Calphad, 2020, 71: 102195 |
| 25 | Chai C S, Eagar T W. Slag-metal equilibrium during submerged arc welding [J]. Metall. Trans., 1981, 12B: 539 |
| 26 | Chai C S. Slag-metal reactions during flux shielded arc welding [D]. Cambridge: Massachusetts Institute of Technology, 1980 |
| 27 | Christensen N, Chipman J. Slag-metal interaction in arc welding [J]. Weld. J., 1953, 15: 1 |
| 28 | Mitra U, Eagar T W. Slag-metal reactions during welding: Part II. Theory [J]. Metall. Trans., 1991, 22B: 73 |
| 29 | Mitra U, Eagar T W. Slag-metal reactions during welding: Part I. Evaluation and reassessment of existing theories [J]. Metall. Trans., 1991, 22B: 65 |
| 30 | Mitra U, Eagar T. Slag-metal reactions during welding: Part III. Verification of the theory [J]. Metall. Trans., 1991, 22B: 83 |
| 31 | Burck P A, Indacochea J E, Olson D L. Effects of welding flux additions on 4340 steel weld metal composition [J]. Weld. J., 1990, 3: 115s |
| 32 | Indacochea J E, Blander M, Christensen N, et al. Chemical reactions during submerged arc welding with FeO-MnO-SiO2 fluxes [J]. Metall. Trans., 1985, 16B: 237 |
| 33 | Mitra U, Sutton R D, Eagar T W. Comparison of theoretically predicted and experimentally determined submerged arc weld deposit compositions [J]. Metall. Trans., 1983, 14B: 510 |
| 34 | Eagar T W. Thermochemistry of joining [A]. Proc. Elliott Symp. Chem. Process Metall. [C]. Warrendale, PA: Iron and Steel Society,1991: 197 |
| 35 | Zhang J, Coetsee T, Wang C. Element transfer behaviors of fused CaF2-SiO2 fluxes subject to high heat input submerged arc welding [J]. Metall. Mater. Trans., 2020, 51B: 16 |
| 36 | Zhang J, Coetsee T, Dong H B, et al. Element transfer behaviors of fused CaF2-SiO2-MnO fluxes under high heat input submerged arc welding [J]. Metall. Mater. Trans., 2020, 51B: 885 |
| 37 | Zhang J, Coetsee T, Dong H B, et al. Elucidating the roles of SiO2 and MnO upon decarburization during submerged arc welding: A thermodynamic study into EH36 shipbuilding steel [J]. Metall. Mater. Trans., 2020, 51B: 1805 |
| 38 | Zhang J, Coetsee T, Dong H B, et al. Fine-tuned element transfer strategies for ternary CaF2-SiO2-CaO fluxes in submerged arc welding: An environmentally friendly approach [J]. Metall. Mater. Trans., 2020, 51B: 1350 |
| 39 | Zhang J, Coetsee T, Dong H B, et al. Element transfer behaviors of fused CaF2-TiO2 fluxes in EH36 shipbuilding steel during high heat input submerged arc welding [J]. Metall. Mater. Trans., 2020, 51B: 1953 |
| 40 | Bale C W, Bélisle E, Chartrand P, et al. Reprint of: FactSage thermochemical software and databases, 2010-2016 [J]. Calphad, 2016, 55: 1 |
| 41 | Bale C W, Chartrand P, Degterov S A, et al. Factsage thermochemical software and databases [J]. Calphad, 2002, 26: 189 |
| 42 | Zhang J, Wang C, Coetsee T. Assessment of weld metal compositional prediction models geared towards submerged arc welding: Case studies involving CaF2-SiO2-MnO and CaO-SiO2-MnO fluxes [J]. Metall. Mater. Trans., 2021, doi: 10.1007/s11663-021-02190-x. |
| 43 | Zhang J, Wang C, Coetsee T. Thermodynamic evaluation of element transfer behaviors for fused CaO-SiO2-MnO fluxes subjected to high heat input submerged arc welding [J]. Metall. Mater. Trans., 2021, doi: 10.1007/s11663-021-02221-7 |
| 44 | Jindal S, Chhibber R, Mehta N P. Prediction of element transfer due to flux and optimization of chemical composition and mechanical properties in high-strength low-alloy steel weld [J]. Proc. Inst. Mech. Eng., 2015, 229B: 785 |
| 45 | Kanjilal P, Pal T, Majumdar S. Prediction of element transfer in submerged arc welding [J]. Weld. J., 2007, 10: 40 |
| 46 | Mitra U, Eagar T W. Slag metal reactions during submerged arc welding of alloy steels [J]. Metall. Trans., 1984, 15A: 217 |
| 47 | Wu X N, Feng Y H, Li Y, et al. Numerical simulation and orthogonal analysis on coupled arc with molten pool for keyholing plasma arc welding [J]. Acta Metall. Sin., 2015, 51: 1365 |
| 47 | 吴宣楠, 冯妍卉, 李 岩等. 穿孔等离子弧焊接弧与熔池的耦合模拟及正交分析 [J]. 金属学报, 2015, 51: 1365 |
| 48 | Wu C S, Zhang M X, Li K H, et al. Study on the process mechanism of high-speed arc welding DE-GMAW [J]. Acta Metall. Sin., 2007, 43: 663 |
| 48 | 武传松, 张明贤, 李克海等. DE-GMAW高速电弧焊工艺机理的研究 [J]. 金属学报, 2007, 43: 663 |
| 49 | Jian X X, Wu C S. Influence of Fe vapour on weld pool behavior of plasma arc welding [J]. Acta Metall. Sin., 2016, 52: 1467 |
| 49 | 菅晓霞, 武传松. Fe蒸气对等离子弧焊接熔池行为的影响 [J]. 金属学报, 2016, 52: 1467 |
| 50 | Eagar T W. Sources of weld metal oxygen contamination during submerged arc welding [J]. Weld. J., 1978, 57: 76 |
| 51 | Lau T, Weatherly G, Mclean A. The sources of oxygen and nitrogen contamination in submerged arc welding using CaO-Al2O3 based fluxes [J]. Weld. J., 1985, 64: 343 |
| 52 | Polar A, Indacochea J, Blander M. Electrochemically generated oxygen contamination in submerged arc welding [J]. Weld. J., 1990, 69: 69 |
| 53 | Li X Q, Liu P F, Wang G Y. Investigation on mechanism of oxygen gaining occurring in droplet reaction zone during SAW [J]. J. Aeronaut. Mater., 2006, 26(1): 63 |
| 53 | 李晓泉, 刘鹏飞, 王光耀. SAW焊接熔滴反应区增氧机制探讨 [J]. 航空材料学报, 2006, 26(1): 63 |
| 54 | Mitra U. Kinetics of slag metal reactions during submerged arc welding of steel [D]. Cambridge: Massachusetts Institute of Technology, 1984 |
| 55 | Li X Q, Yang X G, Fang C F. Thermodynamical analysis of active SiO2 in interfacial chemical reaction between slag and liquid metal based on thermal-dynamic coupling [J]. Trans. China Weld. Inst., 2005, 26(10): 43 |
| 55 | 李晓泉, 杨旭光, 方臣富. 活性SiO2在焊接熔渣-金属界面化学反应的热动力学分析 [J]. 焊接学报, 2005, 26(10): 43 |
| 56 | Davis M L, Bailey N. Evidence from inclusion chemistry of element transfer during submerged arc welding [J]. Weld. J., 1991, 70: 57 |
| 57 | Dowling J M, Corbett J M, Kerr H W. Inclusion phases and the nucleation of acicular ferrite in submerged arc welds in high strength low alloy steels [J]. Metall. Trans., 1986, 17A: 1611 |
| 58 | Babu S S, David S A. Inclusion formation and microstructure evolution in low alloy steel welds [J]. ISIJ Int., 2002, 42: 1344 |
| 59 | Rein R H. Proceedings, workshop on welding research opportunities held at office of naval research [R]. Arlington: Office of Naval Research, Arlington VA, 1974 |
| 60 | Chai C, Eagar T. Slag metal reactions in binary CaF2-metal oxide welding fluxes [J]. Weld. J., 1982, 61: 229 |
| 61 | Dallam C B, Liu S, Olson D L. Flux composition dependence of microstructure and toughness of submerged arc HSLA weldments [J]. Weld. J., 1985, 64: 140 |
| 62 | Cruz-Crespo A, Quintana Puchol R, Perdomo González L, et al. Effect of CaO from the slag system MnO-SiO2-CaO on the chemical composition of weld metal [J]. Weld. Int., 2010, 24: 518 |
| 63 | Polar A, Indacochea J, Blander M. Fundamentals of the chemical behavior of select welding fluxes [J]. Weld. J., 1991, 70: 15 |
| 64 | Lau T, Weatherly G C, Mclean A. Gas/metal/slag reactions in submerged arc welding using CaO-Al2O3 based fluxes [J]. Weld. J., 1986, 65: 31 |
| 65 | Block-Bolten A, Eagar T W. Metal vaporization from weld pools [J]. Metall. Trans., 1984, 15B: 461 |
| 66 | Mills K. Slag Atlas [M]. 2nd Ed., Dusseldorf: Verlag Stahleisen GmbH, 1995: 186 |
| 67 | Sommerville I D, Kay D A R. Activity determinations in the CaF2-CaO-SiO2 system at 1450oC [J]. Metall. Trans., 1971, 2: 1727 |
| 68 | Kohno R, Takami T, Mori N, et al. New fluxes of improved weld metal toughness for HSLA steels [J]. Weld. J., 1982, 61: 373 |
| 69 | Liao F C, Liu S. The effect of deoxidation sequence of carbon manganese steel weld metal microstructures [J]. Weld. J., 1990, 71: 94 |
| 70 | Eriksson G, Pelton A D. Critical evaluation and optimization of the thermodynamic properties and phase diagrams of the MnO-TiO2, MgO-TiO2, FeO-TiO2, Ti2O3-TiO2, Na2O-TiO2, and K2O-TiO2 systems [J]. Metall. Trans., 1993, 24B: 795 |
| 71 | Cancarevic M, Zinkevich M, Aldinger F. Thermodynamic description of the Ti-O system using the associate model for the liquid phase [J]. Calphad, 2007, 31: 330 |
| 72 | Sengupta V, Havrylov D, Mendez P. Physical phenomena in the weld zone of submerged arc welding—A review [J]. Weld. J., 2019, 98: 283S |
| 73 | Singh B, Khan Z A, Siddiquee A N, et al. Effect of CaF2, FeMn and NiO additions on impact strength and hardness in submerged arc welding using developed agglomerated fluxes [J]. J. Alloys Compd., 2016, 667: 158 |
| 74 | Singh B, Khan Z A, Siddiquee A N, et al. Experimental study on effect of flux composition on element transfer during submerged arc welding [J]. Sādhanā, 2018, 43: 26 |
| 75 | Loder D, Michelic S K, Mayerhofer A, et al. On the capability of nonmetallic inclusions to act as nuclei for acicular ferrite in different steel grades [J]. Metall. Mater. Trans., 2017, 48B: 1992 |
| 76 | Evans G. The effect of carbon on the microstructure and properties of C-Mn all-weld metal deposits [J]. Weld. J., 1983, 62: 313 |
| 77 | Farrar R A, Harrison P L. Acicular ferrite in carbon-manganese weld metals: An overview [J]. J. Mater. Sci., 1987, 22: 3812 |
| 78 | Ferrante M, Farrar R A. The role of oxygen rich inclusions in determining the microstructure of weld metal deposits [J]. J. Mater. Sci., 1982, 17: 3293 |
| 79 | Ito J, Nakanishi M. Study on charpy impact properties of weld metal with submerged arc welding [J]. Sumit. Search, 1976, 15: 42 |
| 80 | Jindal S, Chhibber R, Mehta N P. Effect of flux constituents and basicity index on mechanical properties and microstructural evolution of submerged arc welded high strength low alloy steel [J]. Mater. Sci. Forum, 2013, 738-739: 242 |
| 81 | Evans G. Effect of manganese on the microstructure and properties of all-weld-metal deposits [J]. Weld. J., 1980, 59: 68 |
| 82 | Harrison P, Farrar R. Microstructural development and toughness of C-Mn and C-Mn-Ni weld metals. Part 1. Microstructural development [J]. Met. Constr., 1987, 34: 15 |
| 83 | Chai C S, Eagar T W. Prediction of weld-metal composition during flux-shielded welding [J]. J. Mater. Energy Syst., 1983, 5: 160 |
| 84 | Coetsee T. Phase chemistry of submerged arc welding (SAW) fluoride based slags [J]. J. Mater. Res. Technol., 2020, 9: 9766 |
| 85 | Devletian J, Chen J, Wood W, et al. Fundamental Aspects of Electroslag Welding of Titanium Alloys [M]. Materials Park, OH: ASM International, 1990, 6: 419 |
| 86 | Sikorski A K. Effects of the chemical composition of the gas shield on the properties of flux-cored wire welds [J]. Weld. Int., 1993, 7: 683 |
/
| 〈 |
|
〉 |