Fe-Co-Ni系组合合金热等静压高通量制备方法初探
收稿日期: 2021-02-07
修回日期: 2021-04-03
网络出版日期: 2021-04-30
基金资助
国家重点研发计划项目(2017YFB0701900)
First Exploration of Hot Isostatic Pressing High-Throughput Synthesis on Fe-Co-Ni Combinatorial Alloy
Received date: 2021-02-07
Revised date: 2021-04-03
Online published: 2021-04-30
Supported by
National Key Research and Development Program of China(2017YFB0701900)
提出基于热等静压工艺的高通量制备新方法,即采用纯Ni和Ti作为蜂巢结构骨架材料,内含不同组元合金粉末的成分梯度设计新思路,成功一次性制备出含有19种不同化学成分的Fe-Co-Ni组合块体合金。高通量成分与组织结构分析表明:蜂巢骨架内各区域成分均匀,含量符合设计要求;混粉均扩散形成合金相;块体合金内部致密度良好,无宏观缺陷。通过对高通量制备Fe-Co-Ni组合试样硬度的分析,探讨了合金化作用机理及其对力学行为的影响规律。铁基和镍基材料均是以固溶强化和第二相强化为主,钴基材料以双相固溶强化为主。对于铁基材料,Ni的强化效果优于Co;对于镍基材料,Fe的强化效果优于Co;对于钴基材料,Ni的强化效果优于Fe。
赵雷 , 王辉 , 杨丽霞 , 陈学斌 , 郎润秋 , 贺林峰 , 陈东风 , 王海舟 . Fe-Co-Ni系组合合金热等静压高通量制备方法初探[J]. 金属学报, 2021 , 57(12) : 1627 -1636 . DOI: 10.11900/0412.1961.2021.00070
Material genome engineering (MGE) is an advanced research concept that integrates high-throughput computing, high-throughput experiment (synthesis and characterization), and a special database. The purpose of MGE is to adopt an efficient and economical method to accelerate the correlation between the composition, microstructure, and performance. However, low composition, small size, characterization difficulty, and high cost limit its application in the high-throughput synthesis of a bulk metal. A new high-throughput synthesis based on hot isostatic pressing (HIP), which uses a honeycomb structure sleeve made of pure Ni and Ti foils, was proposed. A combinatorial-bulk-alloy with 19 gradient components was HIPed by filling different mixtures of pure Fe, Co, and Ni powders into each cell of the honeycomb sleeve. The high-throughput characterization of the composition and microstructure showed that the composition of each cell was homogeneous and in accordance with the design, the mixed powders diffused to the alloy phases, and the bulk alloy had good density and without macroscopic defects. The mechanism of alloying and its effect on the mechanical behavior was discussed by investigating the microhardness of Fe-Co-Ni combinatorial alloy. Fe- and Ni-based alloys were solid solution and second phase strengthened, whereas Co-based alloy was two-phase solid solution strengthened. The strengthening effect of Ni was better than that of Co for Fe-based alloy. The strengthening effect of Fe was better than that of Co for Ni-based alloy. The strengthening effect of Ni was better than that of Fe for Co-based alloy.
| 1 | Su Y J, Fu H D, Bai Y, et al. Progress in materials genome engineering in China [J]. Acta Metall. Sin., 2020, 56: 1313 |
| 1 | 宿彦京, 付华栋, 白 洋等. 中国材料基因工程研究进展 [J]. 金属学报, 2020, 56: 1313 |
| 2 | Wang H Z, Xie J X. Editorial for special issue on materials genome engineering [J]. Engineering, 2020, 6: 585 |
| 3 | Li M X, Zhao S F, Lu Z, et al. High-temperature bulk metallic glasses developed by combinatorial methods [J]. Nature, 2019, 569: 99 |
| 4 | Zhao J C. A combinatorial approach for structural materials [J]. Adv. Eng. Mater., 2001, 3: 143 |
| 5 | Zhao J C, Zheng X, Cahill D G. High-throughput diffusion multiples [J]. Mater. Today, 2005, 8: 28 |
| 6 | Zhao J C. Combinatorial approaches as effective tools in the study of phase diagrams and composition-structure-property relationships [J]. Prog. Mater. Sci., 2006, 51: 557 |
| 7 | Kauffmann A, Stüber M, Leiste H, et al. Combinatorial exploration of the high entropy alloy system Co-Cr-Fe-Mn-Ni [J]. Surf. Coat. Technol., 2017, 325: 174 |
| 8 | Springer H, Raabe D. Rapid alloy prototyping: Compositional and thermo-mechanical high throughput bulk combinatorial design of structural materials based on the example of 30Mn-1.2C-xAl triplex steels [J]. Acta Mater., 2012, 60: 4950 |
| 9 | Springe, H, Belde M, Raabe D. Combinatorial design of transitory constitution steels: Coupling high strength with inherent formability and weldability through sequenced austenite stability [J]. Mater. Des., 2016, 90: 1100 |
| 10 | Borkar T, Gwalani B, Choudhuri D, et al. A combinatorial assessment of AlxCrCuFeNi2 (0 < x < 1.5) complex concentrated alloys: Microstructure, microhardness, and magnetic properties [J]. Acta Mater., 2016, 116: 63 |
| 11 | Nie J J, Wei L, Li D L, et al. High-throughput characterization of microstructure and corrosion behavior of additively manufactured SS316L-SS431 graded material [J]. Addit. Manuf., 2020, 35: 101295 |
| 12 | Chen H Y, Wang Y D, Nie Z H, et al. Unprecedented non-hysteretic superelasticity of [001]-oriented NiCoFeGa single crystals [J]. Nat. Mater., 2020, 19: 712 |
| 13 | Xing H, Zhao B B, Wang Y J, et al. Rapid construction of Fe-Co-Ni composition-phase map by combinatorial materials chip approach [J]. ACS Comb. Sci., 2018, 20: 127 |
| 14 | Priimets J, Ugaste ü. Relations between diffusion paths and interdiffusion coefficients in the ternary system Fe-Co-Ni [J]. Defect Diffus. Forum, 2012, 326-328: 209 |
| 15 | Shi Y S, Wei Q S, Xue P J, et al. Hot Isostatic Pressing Integral Forming Technology for Complex Metal Parts [M]. Wuhan: Huazhong University of Science and Technology Press, 2018: 7 |
| 15 | 史玉升, 魏青松, 薛鹏举等. 复杂金属零件热等静压整体成形技术 [M]. 武汉: 华中科技大学出版社, 2018: 7 |
| 16 | Qu X H, Zhang G Q, Zhang L. Applications of powder metallurgy technologies in aero-engines [J]. J. Aeronaut. Mater., 2014, 34: 1 |
| 16 | 曲选辉, 张国庆, 章 林. 粉末冶金技术在航空发动机中的应用 [J]. 航空材料学报, 2014, 34: 1 |
| 17 | He S L, Zhao Y S, Lu F, et al. Effects of hot isostatic pressure on microdefects and stress rupture life of second-generation nickel-based single crystal superalloy in as-cast and as-solid-solution states [J]. Acta Metall. Sin., 2020, 56: 1195 |
| 17 | 和思亮, 赵云松, 鲁 凡等. 热等静压对铸态及固溶态第二代镍基单晶高温合金显微缺陷及持久性能的影响 [J]. 金属学报, 2020, 56: 1195 |
| 18 | Ma F K. Isostatic Pressing Technique [M]. Beijing: Metallurgical Industry Press, 1992: 14 |
| 18 | 马福康. 等静压技术 [M]. 北京: 冶金工业出版社, 1992: 14 |
| 19 | Xie R, Lü Z, Lu C Y, et al. Characterization of nanosized precipitates in 9Cr-ODS steels by SAXS and TEM [J]. Acta Metall. Sin., 2016, 52: 1053 |
| 19 | 谢 锐, 吕 铮, 卢晨阳等. 9Cr-ODS钢中纳米析出相的SAXS和TEM研究 [J]. 金属学报, 2016, 52: 1053 |
| 20 | Feng Y F, Zhou X M, Zou J W, et al. Interface reaction mechanism between SiO2 and matrix and its effect on the deformation behavior of inclusions in powder metallurgy superalloy [J]. Acta Metall. Sin., 2019, 55: 1437 |
| 20 | 冯业飞, 周晓明, 邹金文等. 粉末高温合金中SiO2夹杂物与基体的界面反应机理及对其变形行为的影响 [J]. 金属学报, 2019, 55: 1437 |
| 21 | Tian T, Hao Z B, Jia C L, et al. Microstructure and properties of a new third generation powder metallurgy superalloy FGH100L [J]. Acta Metall. Sin., 2019, 55: 1260 |
| 21 | 田 甜, 郝志博, 贾崇林等. 新型第三代粉末高温合金FGH100L的显微组织与力学性能 [J]. 金属学报, 2019, 55: 1260 |
| 22 | Liang J K, Hou X Y, Cui Y, et al. Effect of sintering temperature on microstructures and mechanical properties of Co-based wear-resistant alloy [J]. Powder Metall. Technol., 2017, 35: 188 |
| 22 | 梁锦奎, 侯星宇, 崔 宇等. 烧结温度对钴基耐磨合金微观组织和性能的影响 [J]. 粉末冶金技术, 2017, 35: 188 |
| 23 | Zheng B K, Che H Y. Analysis of wear resistance and corrosion resistance of hard materials prepared by hot isostatic pressing [J]. Powder Metall. Ind., 2018, 28(6): 56 |
| 23 | 郑秉堃, 车洪艳. 热等静压制备硬质材料的耐磨耐腐蚀性能分析 [J]. 粉末冶金工业, 2018, 28(6): 56 |
| 24 | Jones N G, Christofidou K A, Mignanelli P M, et al. Influence of elevated Co and Ti levels on polycrystalline powder processed Ni-base superalloy [J]. Mater. Sci. Technol., 2014, 30: 1853 |
| 25 | Wang X F, He W W, Zhu J L, et al. Microstructure and mechanical properties of Fe-Co-Ni based superalloy prepared by hot isostatic pressing [J]. Powder Metall. Technol., 2020, 38: 371 |
| 25 | 王新锋, 贺卫卫, 朱纪磊等. 热等静压铁钴镍基高温合金的显微组织和力学性能 [J]. 粉末冶金技术, 2020, 38: 371 |
| 26 | Sun C F, Dang X F, Li S W, et al. Sintering properties and microstructure of Fe-Ni-Co-based superalloy atomized powder [J]. Rare Met. Mater. Eng., 2016, 45: 3115 |
| 26 | 孙崇锋, 党晓凤, 李生文等. 铁镍钴基高温合金雾化粉末烧结特性及显微组织 [J]. 稀有金属材料与工程, 2016, 45: 3115 |
| 27 | Wang H Z, Jia Y H, Zhao L, et al. A method of high-throughput hot isostatic pressing micro-synthesis for the combinatorial materials and a sleeve mould [P]. Chin Pat, 201910014812.4, 2020 |
| 27 | 王海舟, 贾云海, 赵 雷等. 一种组合材料热等静压高通量微制造方法及其包套模具 [P]. 中国专利, 201910014812.4, 2020) |
| 28 | Yang L X, He L F, Huang D Qet al. Three-dimensional hydrogen distribution and quantitative determination of titanium alloys via neutron tomography [J]. Analyst, 2020,145: 4156 |
| 29 | Nikolay K, Robin W, Ingo M. Chapter 3 - Neutron Imaging, In Advanced Nanomaterials, Nanotechnologies and Nanomaterials for Diagnostic, Conservation and Restoration of Cultural Heritage [M]. Amsterdam: Elsevier, 2019: 49 |
| 30 | Лякишев Н П, translated by Guo Q Wet al. Handbook of Phase Diagrams for Metal Binary Systems [M]. Beijing: Chemical Industry Press, 2009: 408, 421, 597 |
| 30 | Лякишев Н П著, 郭青蔚等译. 金属二元系相图手册 [M]. 北京: 化学工业出版社, 2009: 408, 421, 597 |
| 31 | Jen S U, Chiang H P, Chung C M, et al. Magnetic properties of Co-Fe-Ni films [J]. J. Magn. Magn. Mater., 2001, 236: 312 |
/
| 〈 |
|
〉 |