耦合热力学相变路径预测Fe-C包晶合金宏观偏析
收稿日期: 2020-09-09
修回日期: 2020-11-02
网络出版日期: 2021-03-08
基金资助
国家自然科学基金项目(51574074);国家自然科学基金钢铁联合研究基金项目(U1460108);辽宁省教育厅基金项目(L20150183)
Prediction of Macrosegregation of Fe-C Peritectic Alloy Ingot Through Coupling with Thermodynamic Phase Transformation Path
Received date: 2020-09-09
Revised date: 2020-11-02
Online published: 2021-03-08
Supported by
National Natural Science Foundation of China(51574074);National Natural Science Foundation of China and Shanghai Baosteel(U1460108);Natural Science Foundation of Liaoning Province(L20150183)
针对Fe-0.1%C (质量分数)包晶合金冷却过程中多固相共存及界面分配系数实时变化的情况,由杠杆定律结合热力学平衡计算(LR-TEC)获得合金由液相冷却至室温的相变路径,制成相变路径数据表,由成分与热焓线性插值获得相应温度、相质量分数、相成分和相焓,以及凝固潜热释放量和比热容随多固相析出以及成分和温度的变化关系,与连续介质宏观传输模型相结合,预测了铸锭宏观偏析形成过程。模型采用经典的Sn-5%Pb合金凝固基准实验进行了验证。在随温度和溶质成分即时变化的分配系数及多固相的影响下,预测的Fe-0.1%C合金截面偏析变得更为严重。计算结束时,采用LR-TEC耦合宏观传输预测的最大负偏析在距铸锭左侧x = 16 mm、距底面y = 45 mm处,偏析率为-2.22%;而杠杆定律解析式(LR Analytical)预测的最大负偏析位于y = 55 mm左侧壁面处,偏析率为-1.78%。2者预测的最大正偏析都位于铸锭右侧贴壁区域,合金冷却过程中的相变路径采用LR-TEC比LR Analytical预测的偏析率大1.13%。凝固计算结束时区域内仍多固相共存,其中α、γ两固相,α、渗碳体(CEM)两固相及α、γ、CEM三固相分别共存于铸锭左侧x < 0.0342 m的低温区域,δ、γ两固相共存于区域右侧x > 0.0858 m的高温区域。
关键词: Fe-0.1%C合金; 宏观偏析; 热力学相变路径; 多固相; 线性插值
冯苗苗 , 张红伟 , 邵景霞 , 李铁 , 雷洪 , 王强 . 耦合热力学相变路径预测Fe-C包晶合金宏观偏析[J]. 金属学报, 2021 , 57(8) : 1057 -1072 . DOI: 10.11900/0412.1961.2020.00358
The phase transformation path is vital to enclosing the macroscopic transport equations for predicting alloy macrosegregation. However, the analytical approximations for micro-segregation, such as the lever rule (LR), are invalid because an actual alloy is a multi-component system with several coexisting solids. The LR only expresses the phase transformation between a single solid phase and a liquid phase and adopts a constant solute partition coefficient, which is insufficient for micro-segregation. In this study, a model combining the thermodynamic phase transformation path calculation with the macroscopic transport was adopted to predict the macrosegregation formation in an Fe-0.1%C (mass fraction) peritectic alloy, which considers the coexistence of multi-solids and the variance of the local partition coefficient at the solid/liquid and solid/solid phase interface with a solidification process. The phase transformation path from the liquid state cooling to room temperature within a certain range of the solute concentrations was obtained using the LR approximation combined with the thermodynamic equilibrium calculation (LR-TEC). By tabulating the phase transformation path and interpolating the local concentration and enthalpy, the corresponding temperature, phase fraction, phase concentration, and phase enthalpy required in the continuum macroscopic transport model were achieved. The latent heat released and the specific heat corresponding to the amounts of the two solid phases at the peritectic or eutectic phase transformation zone were updated along with their dependence on the local concentration and temperature. This method was validated through the benchmark macrosegregation test of the binary Sn-5%Pb alloy. Regarding the Fe-0.1%C alloy, the varied local partition coefficients and the other thermodynamic parameters with multi-solids precipitating during solidification resulted in a more severe macrosegregation profile in the ingot. At the end of the solidification calculation, the predicted minimum relative solute concentration for the Fe-0.1%C alloy was -2.22% at y = 45 mm from the bottom and x = 16 mm from the left wall of the ingot by LR-TEC. In contrast, it was -1.78% using the LR Analytical model near y = 55 mm at the left-side wall. The predicted maximum macrosegregation ratio at the right wall of the ingot by LR-TEC was 1.13% larger than that achieved using the LR Analytical model. Several solids, such as α and γ, α and cementite (CEM), or α, γ, and CEM at the left part (x < 0.0342 m), and δ and γ at the right (x > 0.0858 m), still coexisted in the region at the end of solidification calculation.
| 1 | Du Q, Li D Z, Li Y Y. Quantitative prediction of macrosegregation formation caused by natural convection during solidification of steel casting [J]. Acta Metall. Sin., 2000, 36: 1197 |
| 1 | 杜 强, 李殿中, 李依依. 铸钢件凝固过程中自然对流引起的宏观偏析模拟 [J]. 金属学报, 2000, 36: 1197 |
| 2 | Brody H D, Flemings M C. Solute redistribution in dendritic solidification [J]. Trans. TMS-AIME, 1966, 236: 615 |
| 3 | Clyne T W, Kurz W. Solute redistribution during solidification with rapid solid state diffusion [J]. Metall. Trans., 1981, 12A: 965 |
| 4 | Ohnaka I. Mathematical analysis of solute redistribution during solidification with diffusion in solid phase [J]. Trans. Iron Steel Inst. Japan, 1986, 26: 1045 |
| 5 | Ahmad N, Rappaz J, Desbiolles J L, et al. Numerical simulation of macrosegregation: A comparison between finite volume method and finite element method predictions and a confrontation with experiments [J]. Metall. Mater. Trans., 1998, 29A: 617 |
| 6 | Li T. Numerical simulation on macrosegregation formation during binary alloy solidification processes [D]. Shenyang: Northeastern University, 2013 |
| 6 | 李 铁. 二元合金凝固过程宏观偏析的数值预测 [D]. 沈阳: 东北大学, 2013 |
| 7 | Zalo?nik M, Kumar A, Combeau H. An operator splitting scheme for coupling macroscopic transport and grain growth in a two-phase multiscale solidification model: Part Ⅱ-Application of the model [J]. Comput. Mater. Sci., 2010, 48: 11 |
| 8 | Aboutalebi M R, Hasan M, Guthrie R I L. Coupled turbulent flow, heat, and solute transport in continuous casting processes [J]. Metall. Mater. Trans., 1995, 26B: 731 |
| 9 | Kraft T, Exner H E. Numerical simulation of solidification. 1. Microsegregation in binary alloys [J]. Z. Metallkd., 1996, 87: 598 |
| 10 | Gulliver G H. The quantitative effect of rapid cooling upon the constitution of binary alloys [J]. J. Inst. Met., 1913, 9: 120 |
| 11 | Scheil E. Uber die eutektische kristallisation on eutectic crystallization [J]. Z. Metallkd., 1942, 34: 70 |
| 12 | Kraft T, Rettenmayr M, Exner H E. An extended numerical procedure for predicting microstructure and microsegregation of multicomponent alloys [J]. Model. Simul. Mater. Sci. Eng., 1996, 4: 161 |
| 13 | Kobayashi S. A mathematical model for solute redistribution during dendritic solidification [J]. Trans. Iron Steel Inst. Japan, 1988, 28: 535 |
| 14 | Sundman B, Chen Q. Thermodynamic Calculation Interface TQ-Interface V7.0 [M]. Stockholm: Thermo-Calc Software AB, 2008: 1 |
| 15 | Zhu M F, Cao W, Chen S L, et al. Modeling of microstructure and microsegregation in solidification of multi-component alloys [J]. J. Phase Equilib. Diffus., 2007, 28: 130 |
| 16 | Dai T, Zhu M F, Chen S L, et al. Modeling of dendritic structure and microsegregation in Al-rich quaternary alloys [J]. Acta Metall. Sin., 2008, 44: 1175 |
| 16 | 戴 挺, 朱鸣芳, 陈双林等. 铝基四元合金枝晶组织及微观偏析的数值模拟 [J]. 金属学报, 2008, 44: 1175 |
| 17 | Wang T T. Numerical modeling and simulation software development of microporosity eveolution in aluminum alloy [D]. Nanjing: Southeast University, 2016 |
| 17 | 王韬涛. 铝合金显微气孔演化数值模拟及其软件开发 [D]. 南京: 东南大学, 2016 |
| 18 | Doré X, Combeau H, Rappaz M. Modelling of microsegregation in ternary alloys: Application to the solidification of Al-Mg-Si [J]. Acta Mater., 2000, 48: 3951 |
| 19 | Carozzani T, Gandin C A, Digonnet H, et al. Direct simulation of a solidification benchmark experiment [J]. Metall. Mater. Trans., 2013, 44A: 873 |
| 20 | Saad A, Gandin C A, Bellet M. Temperature-based energy solver coupled with tabulated thermodynamic properties—Application to the prediction of macrosegregation in multicomponent alloys [J]. Comput. Mater. Sci., 2015, 99: 221 |
| 21 | Carman P C. Flow of Gases Through Porous Media [M]. London: Butterworths Scientific Publications, 1956: 1 |
| 22 | Tu W T. Modelling and simulation of macrosegregation in large steel ingots by a multicomponent and multiphase model [D]. Beijing: Tsinghua University, 2016 |
| 22 | 涂武涛. 大型钢锭宏观偏析多元多相建模与仿真 [D]. 北京: 清华大学, 2016 |
| 23 | Bennon W D, Incropera F P. A continuum model for momentum, heat and species transport in binary solid-liquid phase change systems-I. Model formulation [J]. Int. J. Heat Mass Transf., 1987, 30: 2161 |
| 24 | Bennon W D, Incropera F P. A continuum model for momentum, heat and species transport in binary solid-liquid phase change systems-Ⅱ. Application to solidification in a rectangular cavity [J]. Int. J. Heat Mass Transf., 1987, 30: 2171 |
| 25 | Shi P. TCS Steels/Fe-Alloys Database V60 [M]. Stockholm: Thermo-Calc Software AB, 2008:1 |
| 26 | Hebditch D J, Hunt J D. Observations of ingot macrosegregation on model systems [J]. Metall. Trans., 1974, 5: 1557 |
/
| 〈 |
|
〉 |