Mn和In添加对SmCo7结构稳定性及磁矩影响的第一性原理计算
收稿日期: 2020-09-30
修回日期: 2020-12-17
网络出版日期: 2021-01-19
基金资助
国家重点研发计划项目(2018YFB0703902、2016YFB0700501、2016YFB0700503)
First-Principle Calculation on the Effect of Mn and In on the Structural Stability and Magnetic Moment of SmCo7 Alloys
Received date: 2020-09-30
Revised date: 2020-12-17
Online published: 2021-01-19
Supported by
National Key Research and Development Program of China(2018YFB0703902、2016YFB0700501、2016YFB0700503)
基于构建适用于第一性原理计算、原子比例准确为Sm∶Co = 1∶7的晶体结构模型,依据实验研究中得到的物相共存结果,对Mn和In掺杂的Sm-Co体系模型进行了系列计算分析。利用热力学计算方法,定量化研究了Mn和In在Sm-Co体系中优先占位特点及掺杂元素占位概率随温度的变化规律。通过Sm-Co合金掺杂体系的能量和电子结构计算,研究了Mn和In单掺杂SmCo7体系的结构稳定性。基于计算结果揭示了Mn和In对掺杂合金体系中原子间相互作用的影响,阐明了提升体系结构稳定性的微观机制,并提出了Mn添加可增加SmCo7合金的总磁矩,揭示了掺杂元素对SmCo7合金饱和磁化强度的影响规律。
关键词: Sm-Co基永磁合金; 第一性原理计算; 元素掺杂; 结构稳定性; 磁矩
毛斐 , 吕皓 , 唐法威 , 郭凯 , 刘东 , 宋晓艳 . Mn和In添加对SmCo7结构稳定性及磁矩影响的第一性原理计算[J]. 金属学报, 2021 , 57(7) : 948 -958 . DOI: 10.11900/0412.1961.2020.00397
Among the rare-earth permanent magnetic materials, Sm-Co-based alloys exhibit superior magnetic properties at high temperatures. However, their high-temperature applications are limited by their relatively low saturation magnetization and structural stability. The stability and magnetic properties of these alloys can be enhanced by adding proper alloying elements. In the search for new permanent high-performance magnets, researchers have systematically investigated the structures and magnetic properties of variously doped Sm-Co phases. The present research investigates the structural stability and magnetic properties of Sm-Co based alloys using a crystal structure model of SmCo7 with an accurate atomic ratio (Sm∶Co = 1∶7). To explain the coexisting multiphase phenomenon observed in experiments, Mn- and In-doped Sm-Co alloys were modeled by first-principles calculations. Systematic calculations were conducted on these models, and were combined with thermodynamics calculations to determine the preferred occupation sites of the doping elements and their change rule with temperature. Based on the calculated energy and electronic structures, the structural stabilities of the alloys were studied. The Mn and In dopants influenced the interactions among the Co atoms in the studied alloys. A microscopic mechanism of stability improvement in the SmCo7-based alloys was then proposed. The magnetic-moment calculation showed that the Mn additive enhanced the total magnetic moment of the SmCo7 alloys. This finding explains the effects of doping elements on the saturation magnetization of the SmCo7 alloys.
| 1 | Gutfleisch O, Willard M A, Brück E, et al. Magnetic materials and devices for the 21st century: Stronger, lighter, and more energy efficient [J]. Adv. Mater., 2011, 23: 821 |
| 2 | Liu J F, Chui T, Dimitrov D, et al. Abnormal temperature dependence of intrinsic coercivity in Sm(Co, Fe, Cu, Zr)z powder materials [J]. Appl. Phys. Lett., 1998, 73: 3007 |
| 3 | Seyring M, Song X Y, Zhang Z X, et al. Concurrent ordering and phase transformation in SmCo7 nanograins [J]. Nanoscale, 2015, 7: 12126 |
| 4 | Buschow K H J. New developments in hard magnetic materials [J]. Rep. Progr. Phys., 1991, 54: 1123 |
| 5 | Zhang Z X, Song X Y, Li D P, et al. Phase stability and phase transformation of nanocrystalline SmCo7 alloy and their effects on the magnetic performance [J]. Rare. Met. Mater. Eng., 2013, 42: 565 |
| 5 | 张哲旭, 宋晓艳, 李定朋等. 纳米晶SmCo7合金的相稳定性、相变行为及其对磁性能的影响 [J]. 稀有金属材料与工程, 2013, 42: 565 |
| 6 | Hirosawa S, Nishino M, Miyashita S. Perspectives for high-performance permanent magnets: Applications, coercivity, and new materials [J]. Adv. Nat. Sci: Nanosci. Nanotechnol., 2017, 8: 013002 |
| 7 | Sun J B, Bu S J, Ding H W, et al. The effects of CNTs and/or Si additions on the structure and magnetic properties of SmCo7-based alloys [J]. J. Alloys Compd., 2013, 563: 91 |
| 8 | Al-Omari A I, Yeshurun Y, Zhou J, et al. Magnetic and structural properties of SmCo7-xCuxalloys [J]. J. Appl. Phys., 2000, 87: 6710 |
| 9 | Zhou J, Al-Omari A I, Liu J P, et al. Structure and magnetic properties of SmCo7-xTixwith TbCu7-type structure [J]. J. Appl. Phys., 2000, 87: 5299 |
| 10 | Hsieh C C, Huang S T, Guo J S, et al. Effect of a carbon additive on the TbCu7-type melt-spun Sm(Co, M)7 (M = Ti, Zr, Hf, V and Ge) ribbons [J]. J. Korean Phys. Soc., 2013, 63: 401 |
| 11 | Zaigham H, Khalid F A. Exchange coupling and magnetic behavior of SmCo5-xSnx alloys [J]. J. Mater. Sci. Technol., 2011, 27: 218 |
| 12 | Hsieh C C, Chang H W, Guo Z H, et al. Crystal structure and magnetic properties of melt spun SmCo7-xMx (M = Ta, Cr, and Mo; x = 0-0.6) ribbons [J]. J. Appl. Phys., 2010, 107: 09A738 |
| 13 | Hsieh C C, Shih C W, Liu Z, et al. Magnetic properties and crystal structure of melt spun Sm(Co, M)7 (M = Al and Si) ribbons [J]. J. Appl. Phys., 2012, 111: 07E306 |
| 14 | Hua G, Song X Y, Liu D, et al. Effects of Hf on phase structure and magnetic performance of nanocrystalline SmCo7-type alloy [J]. J. Mater. Sci., 2016, 51: 3390 |
| 15 | Qian J W, Guo Y Q. Effect on the structure stability of minor Al or Zn doping into SmCo7 [A]. DEStech Transactions on Materials Science and Engineering [C]. Sanya: DEStech Publications, 2017: 83 |
| 16 | Luo J, Liang J K, Guo Y Q, et al. Effects of the doping element on crystal structure and magnetic properties of Sm(Co, M)7, compounds (M = Si, Cu, Ti, Zr, and Hf) [J]. Intermetallics, 2005, 13: 710 |
| 17 | Chen Y Y, Hsieh C C, Lo S C, et al. The effect of doping element Zr on anisotropy and microstructure of SmCo7-xZrx [J]. J. Appl. Phys., 2011, 109: 07A748 |
| 18 | Sun J B, Bu S J, Yang W, et al. Structure and magnetic properties of SmCo7-xGax (0 ? x ? 1.2) alloys [J]. J. Alloys Compd., 2014, 583: 554 |
| 19 | Li Y Y, Jiang S, Chen Y. Atomistic simulation for disordered TbCu7-type compounds SmCo7 and Sm(Co,T)7 (T = Ti, Ga, Si, Cu, Hf, Zr) [J]. Solid State Sci., 2010, 12: 33 |
| 20 | Liu D, Guo K, Tang F W, et al. Selecting doping elements by data mining for advanced magnets [J]. Chem. Mater., 2019, 31: 10117 |
| 21 | Mao F. First-principles calculations on structure and magnetism properties of Sm-Co based alloys [D]. Beijing: Beijing University of Technology, 2020 |
| 21 | 毛 斐. Sm-Co合金体系相结构与磁学性能的第一性原理计算研究 [D]. 北京: 北京工业大学, 2020 |
| 22 | Zhang C W. Study on the electronic structure and magnetic properties of a new Sm-Co-based ternary permanent magnet alloy [D]. Jinan: Shandong University, 2006 |
| 22 | 张昌文. 新型Sm-Co基三元永磁合金的电子结构及磁性研究 [D]. 济南: 山东大学, 2006 |
| 23 | Zhang Z X. Preparation and characterizations on structures and properties of nanocrystalline metastable samarium-cobalt alloys [D]. Beijing: Beijing University of Technology, 2012 |
| 23 | 张哲旭. 纳米晶Sm-Co亚稳相合金的制备及结构性能研究 [D]. 北京: 北京工业大学, 2012 |
| 24 | Hua G. Effects of metallic element doping on phase stability and magnetic performance of metastable SmCo7-type alloys [D]. Beijing: Beijing University of Technology, 2016 |
| 24 | 华 刚. 添加金属元素对SmCo7亚稳相合金稳定性和磁性能的影响 [D]. 北京: 北京工业大学, 2016 |
| 25 | Kresse G, Furthmüller J. Efficient iterative schemes for ab initio total-energy calculations using a plane-wave basis set [J]. Phys. Rev., 1996, 54B: 11169 |
| 26 | Kresse G, Furthmüller J. Efficiency of ab-initio total energy calculations for metals and semiconductors using a plane-wave basis set [J]. Comput. Mater. Sci., 1996, 6: 15 |
| 27 | Perdew J P, Chevary J A, Vosko S H, et al. Atoms, molecules, solids, and surfaces: Applications of the generalized gradient approximation for exchange and correlation [J]. Phys. Rev., 1992, 46B: 6671 |
| 28 | Perdew J P, Burke K, Ernzerhof M. Generalized gradient approximation made simple [J]. Phys. Rev. Lett., 1996, 77: 3865 |
| 29 | Andreev A V, Zadvorkin S M. Thermal expansion and spontaneous magnetostriction of RCo5 intermetallic compounds [J]. Physica, 1991, 172B: 517 |
| 30 | Kohan A F, Ceder G, Morga D, et al. First-principles study of native point defects in ZnO [J]. Phys. Rev., 2000, 61B: 15019 |
| 31 | Condon E U. The principles of statistical mechanics [J]. J. Appl. Phys., 1939, 10: 691 |
| 32 | Dixit V, Nandadasa C N, Kim S G, et al. Site occupancy and magnetic properties of Al-substituted M-type strontium hexaferrite [J]. J. Appl. Phys., 2015, 117: 243904 |
| 33 | van de Walle A, Ceder G. The effect of lattice vibrations on substitutional alloy thermodynamics [J]. Rev. Mod. Phys., 2002, 74: 11 |
| 34 | Xu Z Y. Thermodynamics of Materials [M]. Beijing: Higher Education Press, 2009: 52 |
| 34 | 徐祖耀. 材料热力学 [M]. 北京: 高等教育出版社, 2009: 52 |
| 35 | Hua G, Song X Y, Tang F W, et al. Modeling and experimental studies of Hf-doped nanocrystalline SmCo7 alloys [J]. CrystEngComm., 2016, 18: 8080 |
/
| 〈 |
|
〉 |