直接包套轧制铸态Ti-46Al-8Nb合金的组织特征及热变形机制

  • 李天瑞 ,
  • 刘国怀 ,
  • 于少霞 ,
  • 王文娟 ,
  • 张风奕 ,
  • 彭全义 ,
  • 王昭东
展开
  • 1 东北大学轧制技术与连轧自动化国家重点实验室 沈阳 110819
    2 东北大学材料科学与工程学院 沈阳 110819
李天瑞,女,1992年生,博士生

收稿日期: 2019-11-08

  修回日期: 2020-02-25

  网络出版日期: 2020-05-07

基金资助

国家重点研发计划项目(2016YFB0301200);国家自然科学基金项目(51504060);国家自然科学基金项目(51301140);中央高校基本科研业务费项目(N160713001)

Microstructure Evolution and Deformation Mechanisms by Direct Hot-Pack Rolling for As-Cast Ti-46Al-8Nb Alloys

  • Tianrui LI ,
  • Guohuai LIU ,
  • Shaoxia YU ,
  • Wenjuan WANG ,
  • Fengyi ZHANG ,
  • Quanyi PENG ,
  • Zhaodong WANG
Expand
  • 1 State Key Laboratory of Rolling and Automation, Northeastern University, Shenyang 110819, China
    2 School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China

Received date: 2019-11-08

  Revised date: 2020-02-25

  Online published: 2020-05-07

Supported by

National Key Research and Development Program of China(2016YFB0301200);National Natural Science Foundation of China(51504060);National Natural Science Foundation of China(51301140);Fundamental Research Funds for the Central Universities(N160713001)

摘要

根据热模拟实验结果和动态材料模型建立了Ti-46Al-8Nb合金的热加工图,确定了合理的热加工工艺制度,并采用包套轧制方法制备了TiAl合金板材,考察了轧制高铌TiAl合金的组织演变规律及流变软化机制。结果表明,在低应变时加工图中只存在2个失稳区,当应变增加到0.4时,在1250 ℃、0.006 s-1附近位置也出现了失稳;在1200 ℃、1 s-1和1150~1200 ℃、0.01 s-1附近存在典型的动态再结晶区域。最终结合应变速率敏感系数的分析,选择在1150~1200 ℃、0.01~0.03 s-1,每道次变形量约为18%的条件下进行复合包套轧制,获得厚度约为0.85 mm、变形均匀无裂纹缺陷的板材,其热轧组织局域流变软化严重,存在明显的轧制变形带,但整体组织均匀性较好。Ti-46Al-8Nb合金在热轧过程中的流变软化以γ相的动态再结晶以及热-力作用下L(α/γ)层片组织的相变分解为主,其中再结晶过程主要是通过位错塞积诱导亚晶界形成进而完成小角度晶界向大角度晶界的转化,L(α/γ)→γ+α+B2/βαγ转变是片层团分解的主要途径。此外,大量普通机械孪晶以及孪晶片层的出现,也可以显著提高热轧TiAl合金的组织均匀性。

本文引用格式

李天瑞 , 刘国怀 , 于少霞 , 王文娟 , 张风奕 , 彭全义 , 王昭东 . 直接包套轧制铸态Ti-46Al-8Nb合金的组织特征及热变形机制[J]. 金属学报, 2020 , 56(8) : 1091 -1102 . DOI: 10.11900/0412.1961.2019.00379

Abstract

TiAl alloys are considered attractive structural materials because of their low density, excellent high-temperature strength, and oxidation resistance. However, their intrinsic characteristics, including low-temperature brittleness, poor workability, and narrow processing window, restrict their wide use in industrial applications. Various hot-work processes are conducted to enhance the inherent ductility of TiAl alloys, especially hot-pack rolling. In this work, the hot processing maps at different strains were developed based on isothermal compression tests and dynamic material model (DMM). The optimum hot-working parameters were selected and a crack free Ti-46Al-8Nb (atomic fraction, %) sheet was directly fabricated by hot pack rolling from ingot. Moreover, microstructure evolution and hot deformation behavior of the as-rolled alloys were investigated. The processing maps showed two typical dynamic recrystallization (DRX) domains which would facilitate the hot-work process, of which the temperature was at 1200 ℃, strain rates was 1 s-1 with a peak efficiency of power dissipation of 0.38 and temperature of 1150~1200 ℃, strain rate of 0.01 s-1 with a peak efficiency of power dissipation of 0.45. The instable-area temperature was 1100~1200 ℃ and strain rate was 0.06~1 s-1 at low strain, which was expanded to low strain rate with the increasing strain. As the strain increased to 0.4, the region with the temperature of 1250 ℃ and strain rate of 0.006 s-1 always became instable. The Ti-46Al-8Nb alloy sheet with thickness of 0.85 mm was produced within processing windows of 1150~1200 ℃, 0.01~0.03 s-1 with engineering strain 18% per pass. The produced sheet showed uniform microstructure as a whole, though the local flow softening and deformation bands were inevitable. Furthermore, the main softening mechanism of Ti-46Al-8Nb alloy was DRX which began with the pile-up of dislocations, the formation of sub-boundaries and mechanical twins. Then the substructures would rearrange to inducing the formation of DRXed grains with the cumulative reduction increasing. The phase transitions of Lamellae (α/γ)→γ+α+B2/β and αγ during hot-pack rolling combining with the growth of DRXed grains were simultaneously a main softening mechanism. The formations of plentiful mechanical twinning and twin lamellae also contributed to the uniformity of as-rolled microstructure.

参考文献

[1] Yang R. Advances and challenges of TiAl base alloys [J]. Acta Metall. Sin., 2015, 51: 129
[1] (杨 锐. 钛铝金属间化合物的进展与挑战 [J]. 金属学报, 2015, 51: 129)
[2] Wu X H. Review of alloy and process development of TiAl alloys [J]. Intermetallics, 2006, 14: 1114
[3] Dimiduk D M. Gamma titanium aluminide alloys—An assessment within the competition of aerospace structural materials [J]. Mater. Sci. Eng., 1999, A263: 281
[4] Tetsui T, Shindo K, Kobayashi S, et al. A newly developed hot worked TiAl alloy for blades and structural components [J]. Scr. Mater., 2002, 47: 399
[5] Draper S L, Krause D, Lerch B, et al. Development and evaluation of TiAl sheet structures for hypersonic applications [J]. Mater. Sci. Eng., 2007, A464: 330
[6] Semiatin S L, Ohls M, Kerr W R. Temperature transients during hot pack rolling of high temperature alloys [J]. Scr. Metall., 1991, 25: 1851
[7] Schwaighofer E, Clemens H, Mayer S, et al. Microstructural design and mechanical properties of a cast and heat-treated intermetallic multi-phase γ-TiAl based alloy [J]. Intermetallics, 2014, 44: 128
[8] Kim J S, Lee Y H, Kim Y W, et al. High temperature deformation behavior of beta-gamma TiAl alloy [J]. Mater. Sci. Forum, 2007, 539-543: 1531
[9] Kong F T, Chen Y Y, Wang W, et al. Microstructures and mechanical properties of hot-pack rolled Ti-43Al-9V-Y alloy sheet [J]. Trans. Nonferrous Met. Soc. China, 2009, 19: 1126
[10] Liu Z C, Lin J P, Li S J, et al. Effects of Nb and Al on the microstructures and mechanical properties of high Nb containing TiAl base alloys [J]. Intermetallics, 2002, 10: 653
[11] Wang X, Lin J P, Zhang L Q, et al. Hot packed-rolling process of high-Nb TiAl alloy and its microstructure evolution [J]. Chin. J. Rare Met., 2010, 34: 658
[11] (王 兴, 林均品, 张来启等. 高铌TiAl基合金板材制备包套热轧工艺及组织控制 [J]. 稀有金属, 2010, 34: 658)
[12] Chen G L, Xu X J, Teng Z K, et al. Microsegregation in high Nb containing TiAl alloy ingots beyond laboratory scale [J]. Intermetallics, 2007, 15: 625
[13] Liu G H, Li X Z, Su Y Q, et al. Microstructure, microsegregation pattern and the formation of B2 phase in directionally solidified Ti-46Al-8Nb alloy [J]. J. Alloys Compd., 2012, 541: 275
[14] Li T R, Liu G H, Xu M, et al. Microstructures and high temperature tensile properties of Ti-43Al-4Nb-1.5Mo alloy in the canned forging and heat treatment process [J]. Acta Metall. Sin., 2017, 53: 1055
[14] (李天瑞, 刘国怀, 徐 莽等. Ti-43Al-4Nb-1.5Mo合金包套锻造与热处理过程的微观组织及高温拉伸性能 [J]. 金属学报, 2017, 53: 1055)
[15] Prasad Y V R K, Gegel H L, Doraivelu S M, et al. Modeling of dynamic material behavior in hot deformation: Forging of Ti-6242 [J]. Metall. Trans., 1984, 15A: 1883
[16] Zhou J, Zeng W D, Shu Y, et al. Study on globularization of lamellar a structure in TC17 titanium alloy during hot deformation using processing map [J]. Rare Met. Mater. Eng., 2006, 35: 265
[16] (周 军, 曾卫东, 舒 滢等. 应用热加工图研究TC17合金片状组织球化规律 [J]. 稀有金属材料与工程, 2006, 35: 265)
[17] Wang H, Tang H P, Liu Y, et al. Hot deformation behaviors and processing maps of as-cast TiAl based alloy [J]. Mater. Sci. Eng. Powder Metall., 2012, 17: 401
[17] (王 辉, 汤慧萍, 刘 咏等. 铸造TiAl基合金的热变形行为及加工图 [J]. 粉末冶金材料科学与工程, 2012, 17: 401)
[18] Niu H Z, Kong F T, Xiao S L, et al. Effect of pack rolling on microstructures and tensile properties of as-forged Ti-44Al-6V-3Nb-0.3Y alloy [J]. Intermetallics, 2012, 21: 97
[19] Wan Z P, Sun Y, Hu L X, et al. Experimental study and numerical simulation of dynamic recrystallization behavior of TiAl-based alloy [J]. Mater. Des., 2017, 122: 11
[20] Appel F, Wagner R. Microstructure and deformation of two-phase γ-titanium aluminides [J]. Mater. Sci. Eng., 1998, R22: 187
[21] Li T R, Liu G H, Xu M, et al. Flow stress prediction and hot deformation mechanisms in Ti-44Al-5Nb-(Mo, V, B) alloy [J]. Materials, 2018, 11: 2044
[22] Liu G H, Wang Z D, Fu T L, et al. Study on the microstructure, phase transition and hardness for the TiAl-Nb alloy design during directional solidification [J]. J. Alloys Compd., 2015, 650: 45
[23] Liu G H, Li T R, Fu T L, et al. Morphology and competitive growth during the development of the parallel lamellar structure by self-seeding in directionally solidified Ti-50Al-4Nb alloy [J]. J. Alloys Compd., 2016, 682: 601
[24] Tang B, Cheng L, Kou H C, et al. Hot forging design and microstructure evolution of a high Nb containing TiAl alloy [J]. Intermetallics, 2015, 58: 7
[25] Wang Q, Chen R R, Gong X, et al. Microstructure, mechanical properties, and crack propagation behavior in high-Nb TiAl alloys by directional solidification [J]. Metall. Mater. Trans., 2018, 49A: 4555
文章导航

/