综述

基于中子衍射和同步辐射X射线衍射的TWIP钢位错密度计算方法

  • 李亦庄 ,
  • 黄明欣
展开
  • 1.香港大学机械工程系 香港 999077
    2.香港大学深圳研究院 深圳 518057
李亦庄,男,1992年生,博士

收稿日期: 2020-01-13

  修回日期: 2020-03-09

  网络出版日期: 2020-03-16

基金资助

国家重点研发计划项目(2019YFA0209900);国家自然科学基金项目(U1764252);香港研究资助局项目(17255016);香港研究资助局项目(17210418);香港研究资助局项目(R7066-18)

A Method to Calculate the Dislocation Density of a TWIP Steel Based on Neutron Diffraction and Synchrotron X-Ray Diffraction

  • Yizhuang LI ,
  • Mingxin HUANG
Expand
  • 1.Department of Mechanical Engineering, The University of Hong Kong, Hong Kong 999077, China
    2.Shenzhen Institute of Research and Innovation, The University of Hong Kong, Shenzhen 518057, China

Received date: 2020-01-13

  Revised date: 2020-03-09

  Online published: 2020-03-16

Supported by

National Key Research and Development Program of China(2019YFA0209900);National Natural Science Foundation of China(U1764252);Research Grants Council of Hong Kong(17255016);Research Grants Council of Hong Kong(17210418);Research Grants Council of Hong Kong(R7066-18)

摘要

本文详细梳理并介绍了被广泛应用于高强钢及其它结构金属材料位错密度计算的修正Williamson-Hall法,并结合中子衍射和同步辐射X射线衍射实验结果,以一种孪生诱发塑性(TWIP)钢为例,计算其在变形后的位错密度演化。本文详细介绍如何正确使用该方法以及如何避免常见的一些错误,并介绍其背后的原理及假设。

本文引用格式

李亦庄 , 黄明欣 . 基于中子衍射和同步辐射X射线衍射的TWIP钢位错密度计算方法[J]. 金属学报, 2020 , 56(4) : 487 -493 . DOI: 10.11900/0412.1961.2020.00016

Abstract

The modified Williamson-Hall method, which has been widely used to calculate dislocation densities of high-strength steels and other structural alloys, is re-examined in this work, and is further applied to calculate the dislocation density of a deformed twinning-induced plasticity (TWIP) steel by using its neutron diffraction patterns and synchrotron X-ray diffraction patterns. This paper aims not only to promote the proper use of the method but also to shed light on its underlying pre-requisites and assumptions, and is thus expected to help avoid any errors during its usage.

参考文献

[1] Ungár T. Microstructural parameters from X-ray diffraction peak broadening [J]. Scr. Mater., 2004, 51: 777
[2] Serquis A, Zhu Y T, Peterson E J, et al. Effect of lattice strain and defects on the superconductivity of MgB2 [J]. Appl. Phys. Lett., 2001, 79: 4399
[3] Budrovic Z, Van Swygenhoven H, Derlet P M, et al. Plastic deformation with reversible peak broadening in nanocrystalline nickel [J]. Science, 2004, 304: 273
[4] Wang Y M, Sansoz F, LaGrange T, et al. Defective twin boundaries in nanotwinned metals [J]. Nat. Mater., 2013, 12: 697
[5] Berry J, Provatas N, Rottler J, et al. Defect stability in phase-field crystal models: Stacking faults and partial dislocations [J]. Phys. Rev., 2012, 86B: 224112
[6] Williamson G K, Hall W H. X-ray line broadening from filed aluminium and wolfram [J]. Acta Metall., 1953, 1: 22
[7] Brandstetter S, Derlet P M, Van Petegem S, et al. Williamson-Hall anisotropy in nanocrystalline metals: X-ray diffraction experiments and atomistic simulations [J]. Acta Mater., 2008, 56: 165
[8] Bakshi S D, Sinha D, Chowdhury S G. Anisotropic broadening of XRD peaks of α′-Fe: Williamson-Hall and Warren-Averbach analysis using full width at half maximum (FWHM) and integral breadth (IB) [J]. Mater. Charact., 2018, 142: 144
[9] Ungár T. Dislocation densities, arrangements and character from X-ray diffraction experiments [J]. Mater. Sci. Eng., 2001, A309-310: 14
[10] He B B, Hu B, Yen H W, et al. High dislocation density-induced large ductility in deformed and partitioned steels [J]. Science, 2017, 357: 1029
[11] Zhou P, Liang Z Y, Liu R D, et al. Evolution of dislocations and twins in a strong and ductile nanotwinned steel [J]. Acta Mater., 2016, 111: 96
[12] Liang Z Y, Li Y Z, Huang M X. The respective hardening contributions of dislocations and twins to the flow stress of a twinning-induced plasticity steel [J]. Scr. Mater., 2016, 112: 28
[13] Gutierrez-Urrutia I, Del Valle J, Zaefferer S, et al. Study of internal stresses in a TWIP steel analyzing transient and permanent softening during reverse shear tests [J]. J. Mater. Sci., 2010, 45: 6604
[14] Ungár T, Borbély A. The effect of dislocation contrast on X-ray line broadening: A new approach to line profile analysis [J]. Appl. Phys. Lett., 1996, 69: 3173
[15] Révész A, Ungár T, Borbély A, et al. Dislocations and grain size in ball-milled iron powder [J]. Nanostruct. Mater., 1996, 7: 779
[16] Gubicza J, Ribárik G, Goren-Muginstein G, et al. The density and the character of dislocations in cubic and hexagonal polycrystals determined by X-ray diffraction [J]. Mater. Sci. Eng., 2001, A309-310: 60
[17] Woo W, Balogh L, Ungár T, et al. Grain structure and dislocation density measurements in a friction-stir welded aluminum alloy using X-ray peak profile analysis [J]. Mater. Sci. Eng., 2008, A498: 308
[18] Holzwarth U, Gibson N. The Scherrer equation versus the 'Debye-Scherrer equation' [J]. Nat. Nanotechnol., 2011, 6: 534
[19] Stokes A R, Wilson A J C. The diffraction of X rays by distorted crystal aggregates-I [J]. Proceed. Phys. Soc., 1944, 56: 174
[20] Akama D, Tsuchiyama T, Takaki S. Change in dislocation characteristics with cold working in ultralow-carbon martensitic steel [J]. ISIJ Int., 2016, 56: 1675
[21] Venkateswarlu K, Bose A C, Rameshbabu N. X-ray peak broadening studies of nanocrystalline hydroxyapatite by Williamson-Hall analysis [J]. Physica, 2010, 405B: 4256
[22] Zak A K, Majid W H A, Abrishami M E, et al. X-ray analysis of ZnO nanoparticles by Williamson-Hall and size-strain plot methods [J]. Solid State Sci., 2011, 13: 251
[23] Prabhu Y T, Rao K V, Kumar V S S, et al. X-ray analysis by Williamson-Hall and size-strain plot methods of ZnO nanoparticles with fuel variation [J]. World J. Nano Sci. Eng., 2014, 4: 21
[24] Williamson G K, Smallman R E. III. Dislocation densities in some annealed and cold-worked metals from measurements on the X-ray debye-scherrer spectrum [J]. Philos. Mag., 1956, 1A: 34
[25] Ungár T, Ott S, Sanders P G, et al. Dislocations, grain size and planar faults in nanostructured copper determined by high resolution X-ray diffraction and a new procedure of peak profile analysis [J]. Acta Mater., 1998, 46: 3693
[26] Ungár T, Dragomir I, áRévész, et al. The contrast factors of dislocations in cubic crystals: The dislocation model of strain anisotropy in practice [J]. J. Appl. Cryst., 1999, 32: 992
[27] Ungár T, Groma I, Wilkens M. Asymmetric X-ray line broadening of plastically deformed crystals. II. Evaluation procedure and application to [001]-Cu crystals [J]. J. Appl. Cryst., 1989, 22: 26
[28] Bouaziz O, Allain S, Scott C. Effect of grain and twin boundaries on the hardening mechanisms of twinning-induced plasticity steels [J]. Scr. Mater., 2008, 58: 484