研究论文

纳米晶化对锆基非晶合金动态压缩性能的影响

  • 金辰日 ,
  • 杨素媛 ,
  • 邓学元 ,
  • 王扬卫 ,
  • 程兴旺
展开
  • 1. 北京理工大学材料学院 北京 100081
    2. 北京理工大学冲击环境材料技术重点实验室 北京 100081
金辰日,男,1994年生,硕士生

收稿日期: 2019-06-25

  修回日期: 2019-09-01

  网络出版日期: 2019-09-18

基金资助

国家部委项目(No.2017-ZD-022)

Effect of Nano-Crystallization on Dynamic Compressive Property of Zr-Based Amorphous Alloy

  • JIN Chenri ,
  • YANG Suyuan ,
  • DENG Xueyuan ,
  • WANG Yangwei ,
  • CHENG Xingwang
Expand
  • 1. School of Materials Science and Engineering, Beijing Institute of Technology, Beijing 100081, China
    2. National Key Laboratory of Science and Technology on Materials under Shock and Impact, Beijing Institute of Technology, Beijing 100081, China

Received date: 2019-06-25

  Revised date: 2019-09-01

  Online published: 2019-09-18

Supported by

National Ministries Program of China(No.2017-ZD-022)

摘要

以铸态Zr-Cu-Ni-Al-Nb非晶合金为材料,通过控制退火保温时间获得部分纳米晶化非晶合金,并采用DSC、XRD、HRTEM、SEM、准静态及动态压缩等手段,研究了纳米晶化对非晶合金在不同应变率下的抗压强度以及断裂机制的影响。结果表明,随着退火保温时间的增加,锆基非晶合金内部纳米级晶化相的体积分数及尺寸均增加。退火态非晶合金的抗压强度随着保温时间增加先增大后减小;应变率变化也会影响其抗压强度,从1×10-3 s-1增加到1×103 s-1时强度降低,继续增加到3×103 s-1时强度有所升高。不同程度的纳米晶化对非晶合金的断裂特征产生影响,随着晶化程度的增大,压缩试样的断口形貌从脉状花样向类准解理特征再向河流状花样转变。

本文引用格式

金辰日 , 杨素媛 , 邓学元 , 王扬卫 , 程兴旺 . 纳米晶化对锆基非晶合金动态压缩性能的影响[J]. 金属学报, 2019 , 55(12) : 1561 -1568 . DOI: 10.11900/0412.1961.2019.00207

Abstract

Zr-based amorphous alloys are characterized by high glass forming ability, high thermal stability and excellent mechanical properties. The amorphous alloys in thermodynamic metastable state have the tendency to change to metastable state with lower energy or even crystal structure in equilibrium state under certain temperature or pressure conditions. At present, few researches have been conducted on the mechanical behavior of partially crystallized Zr-Cu-Ni-Al-Nb amorphous alloys, especially the fracture behavior under dynamic loading. In this work, as-cast Zr-Cu-Ni-Al-Nb amorphous alloy was annealed to accomplish different levels of nano-crystallization by controlling holding time. DSC, XRD, HRTEM, SEM, quasi-static and dynamic compression tests were utilized to research the effect of nano-crystallization on compressive strength and fracture mechanism of Zr-based amorphous alloy under different strain rates. The results indicated that the volume fraction and size of nanoscale crystalline phase inside Zr-based amorphous alloy increased with the increasing of annealing holding time. The compressive strength of annealed Zr-based amorphous alloy increased first and then decreased with the increase of holding time. The variation of strain rates also affected the compressive strength, which decreased when the strain rate increased from 1×10-3 s-1 to 1×103 s-1, and increased when the strain rate continually increased to 3×103 s-1. Different degrees of nano-crystallization had an impact on the fracture characteristics of Zr-based amorphous alloy. As the degree of crystallization increased, the fracture morphology of compression samples changed from vein-like patterns to quasi-cleavage features and then to river patterns.

参考文献

[1] Luborsky F E. Amorphous Metallic Alloys [M]. London: Butterworth, 1983: 1
[2] Johnson W L. Bulk glass-forming metallic alloys: Science and technology [J]. MRS Bull., 1999, 24(10): 42
[3] Wang W H, Dong C, Shek C H. Bulk metallic glasses [J]. Mater. Sci. Eng., 2004, R44: 45
[4] Ashby M F, Greer A L. Metallic glasses as structural materials [J]. Scr. Mater., 2006, 54: 321
[5] Huang Y J, Chiu Y L, Shen J, et al. Mechanical performance of metallic glasses during nanoscratch tests [J]. Intermetallics, 2010, 18: 1056
[6] Peker A, Johnson W L. A highly processable metallic glass: Zr41.2Ti13.8Cu12.5Ni10Be22.5 [J]. Appl. Phys. Lett., 1993, 63: 2342
[7] Inoue A, Zhang T, Masumoto T. Zr-Al-Ni amorphous alloys with high glass transition temperature and significant supercooled liquid region [J]. Mater. Trans., 1990, 31: 177
[8] Inoue A, Zhang T, Nishiyama N, et al. Preparation of 16 mm diameter rod of amorphous Zr65Al7.5Ni10Cu17.5 alloy [J]. Mater. Trans., 1993, 34: 1234
[9] Jiang Q K, Wang X D, Nie X P, et al. Zr-(Cu, Ag)-Al bulk metallic glasses [J]. Acta Mater., 2008, 56: 1785
[10] Zhang Y, Zhao D Q, Pan M X, et al. Glass forming properties of Zr-based bulk metallic alloys [J]. J. Non-Cryst. Solids, 2003, 315: 206
[11] Lin X H, Johnson W L, Rhim W K. Effect of oxygen impurity on crystallization of an undercooled bulk glass forming Zr-Ti-Cu-Ni-Al alloy [J]. Mater. Trans., 1997, 38: 473
[12] Cao H B, Ma D, Hsieh K C, et al. Computational thermodynamics to identify Zr-Ti-Ni-Cu-Al alloys with high glass-forming ability [J]. Acta Mater., 2006, 54: 2975
[13] Deng S T, Zhang H F, Wang A M, et al. Improving glass forming ability of Zr50.5Cu36.5Ni4Al9 alloy by suppressing CuZr phase precipitation [J]. J. Alloys Compd., 2008, 460: 182
[14] Wu W F, Yao K F. The progress in research of nano-crystallization of amorphous alloys [J]. Rare Met. Mater. Eng., 2005, 34: 505
[14] (吴文飞, 姚可夫. 非晶合金纳米晶化的研究进展 [J]. 稀有金属材料与工程, 2005, 34: 505)
[15] Inoue A, Zhang T, Kim Y H. Synthesis of high strength bulk amorphous Zr-Al-Ni-Cu-Ag alloys with a nanoscale secondary phase [J]. Mater. Trans., 1997, 38: 749
[16] Bian Z, He G, Chen G L. Mechanical properties of Zr52.5Cu17.9-Ni14.6Al10Ti5 bulk amorphous alloys after annealing isothermally [J]. Acta Metall. Sin., 2000, 36: 693
[16] (边 赞, 何 国, 陈国良. Zr52.5Cu17.9Ni14.6Al10Ti5块体非晶退火后的力学性能 [J]. 金属学报, 2000, 36: 693)
[17] Zheng W. Dynamic mechanical behaviors of ZrCuNiAl bulk glass-forming alloy system [D]. Harbin: Harbin Institute of Technology, 2011
[17] (郑 伟. ZrCuNiAl系块体非晶合金的动态力学行为 [D]. 哈尔滨: 哈尔滨工业大学, 2011)
[18] Peng P, Zheng C X, Hu Y J, et al. Measurement and control of the crystallinity of amorphous alloy during crystallization by DSC [J]. J. Hunan Univ. (Nat. Sci.), 2003, 30(3): 40
[18] (彭 平, 郑采星, 胡艳军, 等. 非晶合金晶化过程中结晶度的DSC法测定与控制(I) [J]. 湖南大学学报(自然科学版), 2003, 30(3: 40)
[19] Wang G, Shen J, Qin Q H, et al. Investigation of deformation behavior of Zr-Ti-Ni-Cu-Be bulk metallic glass containing nanocrystals [J]. J. Mater. Sci., 2005, 40: 4561
[20] Fan C, Inoue A. Ductility of bulk nanocrystalline composites and metallic glasses at room temperature [J]. Appl. Phys. Lett., 2000, 77: 46
[21] Fan C, Li C F, Inoue A, et al. Deformation behavior of Zr-based bulk nanocrystalline amorphous alloys [J]. Phys. Rev., 2000, 61B: R3761
[22] Fan C, Louzguine D V, Li C F, et al. Nanocrystalline composites with high strength obtained in Zr-Ti-Ni-Cu-Al bulk amorphous alloys [J]. Appl. Phys. Lett., 1999, 75: 340
[23] Liu C T, Heatherly L, Horton J A, et al. Test environments and mechanical properties of Zr-base bulk amorphous alloys [J]. Metall. Mater. Trans., 1998, 29A: 1811
[24] Jiang W H, Liao H H, Liu F X, et al. Rate-dependent temperature increases in shear bands of a bulk-metallic glass [J]. Metall. Mater. Trans., 2008, 39A: 1822
[25] Liu J, Wang L, Cheng H W, et al. Fracture behavior of Zr-based bulk amorphous alloy under high-speed impact [J]. Trans. Beijing Inst. Technol., 2012, 32: 198
[25] (刘 俊, 王 鲁, 程焕武等. 高速冲击载荷下块体Zr基非晶合金断裂行为研究 [J]. 北京理工大学学报, 2012, 32: 198)
文章导航

/