研究论文

粉末高温合金中SiO2夹杂物与基体的界面反应机理及对其变形行为的影响

  • 冯业飞 ,
  • 周晓明 ,
  • 邹金文 ,
  • 王超渊 ,
  • 田高峰 ,
  • 宋晓俊 ,
  • 曾维虎
展开
  • 中国航发北京航空材料研究院先进高温结构材料重点实验室 北京100095
冯业飞,男,1985年生,工程师,博士

收稿日期: 2019-04-08

  修回日期: 2019-06-10

  网络出版日期: 2019-08-15

Interface Reaction Mechanism Between SiO2 and Matrix and Its Effect on the Deformation Behavior of Inclusionsin Powder Metallurgy Superalloy

  • Yefei FENG ,
  • Xiaoming ZHOU ,
  • Jinwen ZOU ,
  • Chaoyuan WANG ,
  • Gaofeng TIAN ,
  • Xiaojun SONG ,
  • Weihu ZENG
Expand
  • Science and Technology on Advanced High Temperature Structural Materials Laboratory, AEEC Beijing Institute of Aeronautical Materials, Beijing 100095, China

Received date: 2019-04-08

  Revised date: 2019-06-10

  Online published: 2019-08-15

摘要

通过人工植入夹杂物的方法,采用SEM、EPMA、TEM、纳米压痕和微纳CT研究了FGH96粉末高温合金中30和60 μm SiO2夹杂物在粉末态、热等静压(HIP)和热挤压(HEX)过程中形貌、尺寸以及化学成分的演变规律,深入揭示了SiO2夹杂物与基体发生界面反应的机理,定量研究了夹杂物在粉末态、HIP态以及HEX态下尺寸的变化,表征了夹杂物在挤压棒材中的三维形貌。结果表明,在粉末态时,夹杂物呈长条状或板条状;在HIP过程中,夹杂物与基体发生了置换反应,形成了内部TiO2、外部Al2O3并弥散分布于γ基体的复合夹杂物,确定了形成氧化物的物相种类,揭示了界面反应机理,同时,30 μm SiO2周围未出现γ'相贫化区,60 μm SiO2周围形成了γ'相贫化区,合金基体较γ'相贫化区具有较高弹性模量和纳米硬度,γ'相贫化区为软化区,反应后30和60 μm SiO2夹杂物尺寸分别约为35和75 μm, 体积得到进一步增大;在挤压过程中,60 μm SiO2由于贫化区的存在表现出与30 μm SiO2不同的变形行为,并通过SEM观察统计的夹杂物尺寸与理论计算和微纳CT测试结果进行了对比验证。

本文引用格式

冯业飞 , 周晓明 , 邹金文 , 王超渊 , 田高峰 , 宋晓俊 , 曾维虎 . 粉末高温合金中SiO2夹杂物与基体的界面反应机理及对其变形行为的影响[J]. 金属学报, 2019 , 55(11) : 1437 -1447 . DOI: 10.11900/0412.1961.2019.00101

Abstract

Powder metallurgy (P/M) Ni-based superalloy has been the most important material for high-temperature structural application in turbine disc owing to its good tensile and creep properties. However, the inclusions in P/M superalloy have an important impact on the safety and reliability of superalloy. By means of implanting SiO2 inclusions artificially, the evolution rule of morphology, size and chemical composition of 30 and 60 μm inclusions in FGH96 superalloy during powder, hot isostatic pressing (HIP) and hot extrusion (HEX) processes was investigated by SEM, EPMA, TEM, nanoindentation and Micro-CT. The interfacial reaction mechanism between inclusions and matrix alloy was revealed deeply, the size change of inclusions during different stages was studied quantitatively, and the 3D morphology of inclusions was characterized. The results show that the inclusions in powder stage are long stripe or plate-like shape, the displacement reaction happened in the process of HIP, which produced the composite inclusions with TiO2 inside and Al2O3 outside dispersed uniformly in the γ matrix, and the phase types of oxides were confirmed, furthermore, the reaction mechanism was figured out. Meanwhile, the denuded zone of γ' phase appeared around the inclusions with the dimension of 60 μm, but not 30 μm. The alloy matrix had higher elastic modulus and hardness than the denuded zone of γ' phase, implying that the denuded zone was softened zone. After the reaction, the dimension of inclusions became larger, the average size of 30 and 60 μm inclusions were 35 and 75 μm, respectively. During the HEX, owing to existence of the denuded zone, 60 μm inclusions had different deformation behaviors with 30 μm inclusions, and the dimension of inclusions obtained from statistics by SEM was used to contrast and validate with the results from formula calculation and Micro-CT.

参考文献

[1] ZouJ W, WangW X. Development and application of P/M superalloy [J]. J. Aero. Mater., 2006, 26(3): 244
[1] 邹金文, 汪武祥. 粉末高温合金研究进展与应用 [J]. 航空材料学报, 2006, 26(3): 244
[2] ChenH M, HuB F, ZhangY W, et al. Recent development in nickel-based powder superalloy used in aircraft turbines [J]. Mater. Rev., 2002, 16(11): 17
[2] 陈焕铭, 胡本芙, 张义文等. 飞机涡轮盘用镍基粉末高温合金研究进展 [J]. 材料导报, 2002, 16(11): 17
[3] WangW X, HeF, ZouJ W. The application and development of P/M superalloys [J]. Aviat. Eng. Main., 2002, (6): 26
[3] 汪武祥, 何 峰, 邹金文. 粉末高温合金的应用与发展 [J]. 航空工程与维修, 2002, (6): 26
[4] SunJ, ZouJ W, LiuP Y. Research and development of powder metallurgy superalloy [J]. Aviat. Eng. Main., 2001, (1): 28
[4] 孙 兼, 邹金文, 刘培英. 盘件用粉末高温合金的研究与发展 [J]. 航空工程与维修, 2001, (1): 28
[5] ShamblenC E, ChangD R. Effect of inclusions on LCF life of HIP plus heat treated powder metal René 95 [J]. Metall. Trans., 1985, 16B: 775
[6] PateS J, ElliottI C. Production of high-strength P/M disc alloys by "superclean" cast/wrought technology [A]. Superalloys 1992 [C]. Warrendale: Minerals, Metals & Materials Society, 1992: 13
[7] SimsC T, StoloffN S, HagelW C. Superalloys II: High-temperature Materials for Aerospace and Industrial Power [M]. New York: John Wiley & Sons Inc., 1987: 291
[8] HuronE S, RothP G. The influence of inclusions on low cycle fatigue life in a P/M nickel-base disk superalloy [A]. Superalloys 1996 [C]. Hopeland: Minerals, Metals & Materials Society, 1996: 359
[9] LaitinenA, H?nninenH. Effect of non-metallic inclusions on corrosion fatigue resistance of P/M duplex stainless steels [J]. Fatigue Fract. Eng. Mater. Struct., 1996, 19: 1045
[10] de BussacA. Prediction of the competition between surface and internal fatigue crack initiation in PM Alloys [J]. Fatigue Fract. Eng. Mater. Struct., 1994, 17: 1319
[11] AmbroiseM H, BretheauT, ZaouiA. Micromechanics and Inhomogeneity [M]. New York, NY: Springer, 1990: 41
[12] GabbT P, TelesmanJ, KantzosP T, et al. Initial assessment of the effects of nonmetallic inclusions on fatigue life of powder-metallurgy-processed udimet 720 [R]. Washington: National Aeronautics and Space Administration, 2002: 7
[13] ZhouX M, WangW X, YangH T, et al. Character of artificial non-metallic inclusions in HIPed FGH96 alloy [J]. J. Aeronaut. Mater., 2005, 25(4): 1
[13] 周晓明, 汪武祥, 杨洪涛等. HIP态FGH96合金中人工加入非金属夹杂物的特征 [J]. 航空材料学报, 2005, 25(4): 1
[14] ZhouX M, WangD L, WangY, et al. Deformation behavior of non-metallic inclusions in nickel-base P/M superalloy [J]. Fail. Anal. Prev., 2008, 3(3): 23
[14] 周晓明, 汪殿龙, 汪 煜等. 非金属夹杂物在镍基粉末高温合金中的变形行为 [J]. 失效分析与预防, 2008, 3(3): 23
[15] GuoW M, WuJ T, ZhangF G, et al. Characteristic of inclusions and its relationship with different forming processes in powder superalloy [J]. Mater. Rev., 2004, 18(11): 87
[15] 国为民, 吴剑涛, 张风戈等. 粉末高温合金中夹杂物特性及与不同成型工艺的关系 [J]. 材料导报, 2004, 18(11): 87
[16] ZhangM C, FangS, ChenY H, et al. Deformation behavior of non-metallic inclusions of FGH96 alloy in extrusion process [J]. Forg. Stamp. Technol., 2013, 38(6): 132
[16] 张敏聪, 方 爽, 陈由红等. FGH96合金挤压过程非金属夹杂物的变形行为 [J]. 锻压技术, 2013, 38(6): 132
[17] KantzosP T, BarrieR, BonacuseP, et al. The effects of forging strain on ceramic inclusions in a disk superalloy [A]. Advanced Materials and Processes for Gas Turbines [C]. Warrendale, PA: TMS, 2003: 245
[18] BonacuseP, TelesmanJ, KantzosP, et al. The effect of powder cleanliness on the fatigue behavior of powder metallurgy Ni-disk alloy Udimet 720 [A]. Proceedings of the 10th International Symposium on Superalloys: Technical Program & Calendar of Events [C]. Warrendale, PA: TMS, 2004: 409
[19] BonacuseP J, KantzosP, TelesmanJ, et al. Modeling ceramic inclusions in powder metallurgy alloys [A]. Proceedings of the 8th International Fatigue Congress [C]. West Midlands: Engineering Materials Advisory Services, Ltd., 2002: 1339
[20] McClungR C, EnrightM P, LiangW W. Integration of NASA-developed lifting for PM alloys into DARWIN [R]. Cleveland: NASA Glenn Research Center, 2011
[21] JablonskiD A. The effect of ceramic inclusions on the low cycle fatigue life of low carbon astroloy subjected to hot isostatic pressing [J]. Mater. Sci. Eng., 1981, 48: 189
[22] SimsC T, translated by ZhaoJ, ZhuS J, LiX G, et al. Superalloys [M]. Dalian: Dalian University of Technology Press, 1992: 124
[22] Sims C T著, 赵 杰, 朱世杰, 李晓刚等译. 高温合金 [M]. 大连: 大连理工大学出版社, 1992: 124
[23] LinJ Z, RuanX D, ChenB G, et al. Fluid Mechanics [M]. Beijing: Tsinghua University Press, 2005: 8
[23] 林建忠, 阮晓东, 陈邦国等. 流体力学 [M]. 北京: 清华大学出版社, 2005: 8
文章导航

/