Mn含量对Fe-Cu-Mn合金纳米富Cu析出相影响的相场法研究
收稿日期: 2018-11-07
修回日期: 2019-01-24
网络出版日期: 2019-03-04
基金资助
国家自然科学基金项目(U1610123);国家自然科学基金项目(51674226);国家自然科学基金项目(51574206);国家自然科学基金项目(51774254);国家自然科学基金项目(51701187);山西省科技重点项目(MC2016-06)
Effect of Mn Composition on the Nanometer Cu-Rich Phase of Fe-Cu-Mn Alloy by Phase Field Method
Received date: 2018-11-07
Revised date: 2019-01-24
Online published: 2019-03-04
Supported by
National Natural Science Foundation of China(U1610123);National Natural Science Foundation of China(51674226);National Natural Science Foundation of China(51574206);National Natural Science Foundation of China(51774254);National Natural Science Foundation of China(51701187);Science and Technology Major Project of Shanxi Province(MC2016-06)
采用相场法模拟了Fe-Cu-Mn合金在823 K时效时富Cu析出相的三维组织演化图像、体积分数、数量密度和平均颗粒半径随时效时间的变化等。相场模拟研究表明:相分离早期阶段通过失稳分解机制形成富Cu相;同时Mn原子也在富Cu相的中心发生偏聚,在富Cu相开始Ostwald粗化的过程中,Mn原子又从其核心处偏聚到富Cu相和基体的界面处,最终在富Cu相外部形成富Mn环。富Mn环的存在会抑制富Cu相的扩散长大和粗化;富Cu相在时效前期是球状的bcc结构,随着不断长大,转变为椭球形或棒状的fcc结构;提高Mn含量可以加快富Cu相的析出,有利于富Cu相的粗化。
赵宝军 , 赵宇宏 , 孙远洋 , 杨文奎 , 侯华 . Mn含量对Fe-Cu-Mn合金纳米富Cu析出相影响的相场法研究[J]. 金属学报, 2019 , 55(5) : 593 -600 . DOI: 10.11900/0412.1961.2018.00506
The precipitation of nanometer Cu-rich phase can be observed in Fe-Cu alloy systems during isothermal ageing. The existence of Cu-rich phase is one of the reasons for the embrittlement of reactor pressure vessel (RPV) steel. The phase-field method applies a set of field variables defined by functions of space and time to describe the temporal evolution of composition and structural parameter, characterizing microstructure evolution during phase transformation. This work uses phase-field model to simulate the three-dimensional morphology, the volume fraction, number density and average particle radius of Cu-rich phase in Fe-Cu-Mn alloy at 823 K. The chemical free energy is derived from the thermodynamic database of the calculated phase diagram (CALPHAD), so the microstructure evolution of precipitation changes are directly corresponded to phase diagram of the real alloy system. The simulation results show that nanometer Cu-rich phase are formed by the spinodal decomposition mechanism in the early stage of phase separation. Meanwhile, Mn atoms segregate to the center of the Cu-rich phase. During the process of Ostwald coarsening, Mn atoms migrate from core to the interface of Cu-rich phase, finally forming Mn-rich ring distributed in the exterior of Cu-rich phase. Its existence can decrease the rates of diffusion growth and coarsening of Cu-rich phase. The Cu-rich phase is bcc structure and disperses in the matrix with spherical shape in the early stage of ageing. As the Cu-rich phase continues to grow, it will transform into fcc structure with ellipsoid or rod shapes. Meanwhile, increasing Mn content of Fe-Cu-Mn alloy accelerates the precipitation of Cu-rich phase and facilitates the growth and coarsening of Cu-rich phase.
| [1] | MillerM K, RussellK F. Embrittlement of RPV steels: An atom probe tomography perspective[J]. J. Nucl. Mater., 2010, 371: 145 |
| [2] | LuZ. Radiator-induced embrittlement and life evaluation of reactor pressure vessels[J].Acta Metall. Sin., 2011, 47: 777 |
| [2] | (吕 铮. 核反应堆压力容器的辐照脆化与延寿评估 [J]. 金属学报, 2011, 47: 777) |
| [3] | ZhangZ W, LiuC T, WangX L, et al. Effects of proton irradiation on nanocluster precipitation in ferritic steel containing fcc alloying additions[J]. Acta Mater., 2012, 60: 3034 |
| [4] | StymanP D, HydeJ M, WilfordK, et al. Precipitation in long term thermally aged high copper, high nickel model RPV steel welds[J]. Prog. Nucl. Energy, 2012, 57: 86 |
| [5] | LambrechtM, MeslinE, MalerbaL, et al. On the correlation between irradiation-induced microstructural features and the hardening of reactor pressure vessel steels[J]. J. Nucl. Mater., 2010, 406: 84 |
| [6] | RadiguetB, PareigeP, BarbuA. Irradiation induced clustering in low copper or copper free ferritic model alloys[J]. Nucl. Instrum. Methods Phys. Res., 2009, 267B: 1496 |
| [7] | LiB Y, ZhangL, LiC L, et al. Finding non-classical critical nuclei and minimum energy path of Cu precipitates in Fe-Cu alloys[J]. Modell. Simul. Mater. Sci. Eng., 2017, 25: 085006 |
| [8] | DeschampsA, MilitzerM, PooleW J. Precipitation kinetics and strengthening of a Fe-0.8wt%Cu alloy[J]. ISIJ Int., 2001, 41: 196 |
| [9] | LiuZ C, LiW X, WangY F, et al. Precipitation of Cu in Fe-1.12Cu alloys[J].Heat Treat. Met., 2005, 30(6): 40 |
| [9] | (刘宗昌, 李文学, 王玉峰等. Fe-1.12Cu合金中Cu的脱溶 [J]. 金属热处理, 2005, 30(6): 40) |
| [10] | XuG, ChuD F, CaiL L, et al. Investigation on the precipitation and structural evolution of Cu-rich nanophase in RPV model steel[J].Acta Metall. Sin., 2001, 47: 905 |
| [10] | (徐 刚, 楚大锋, 蔡琳玲等. RPV模拟钢中纳米富Cu相的析出和结构演化研究 [J]. 金属学报, 2011, 47: 905) |
| [11] | LiuF, ZhouB X, PengJ C, et al. Characterization of a complex crystal structure within Cu-rich precipitates in RPV model steel[J]. J.Mater. Eng., 2015, 43(7): 80 |
| [12] | LeeT H, KimY O, KimS J. Crystallographic model for bcc-to-9R martensitic transformation of Cu precipitates in ferritic steel[J]. Philos. Mag., 2007, 87: 209 |
| [13] | BlackstockJ J, AcklandG J. Phase transitions of copper precipitates in Fe-Cu alloys[J]. Philos. Mag., 2001, 81A: 2127 |
| [14] | MonzenR, IguchiM, JenkinsM L. Structural changes of 9R copper precipitates in an aged Fe-Cu alloy[J]. Philos. Mag. Lett., 2000, 80: 137 |
| [15] | WenY R, HirataA, ZhangZ W, et al. Microstructure characterization of Cu-rich nanoprecipitates in a Fe-2.5Cu-1.5Mn-4.0Ni-1.0Al multicomponent ferritic alloy[J]. Acta Mater., 2013, 61: 2133 |
| [16] | ShenQ, XiongX Y, LiT, et al. Effects of co-addition of Ni and Al on precipitation evolution and mechanical properties of Fe-Cu alloy[J]. Mater. Sci. Eng., 2018, A723: 279 |
| [17] | MillerM K, WirthB D, OdetteG R. Precipitation in neutron-irradiated Fe-Cu and Fe-Cu-Mn model alloys: A comparison of APT and SANS data[J]. Mater. Sci. Eng., 2003, A353: 133 |
| [18] | GladeS C, WirthB D, OdetteG R, et al. Positron annihilation spectroscopy and small-angle neutron scattering characterization of the effect of Mn on the nanostructural features formed in irradiated Fe-Cu-Mn alloys[J]. Philos. Mag., 2005, 85: 629 |
| [19] | WangX J. Mechanism research of nanaoscale composite precipitates in Fe-Cu-Ni-Al-Mn steel[D]. Shanghai: Shanghai University, 2016 |
| [19] | (王晓姣. Fe-Cu-Ni-Al-Mn钢中强化相复合析出机制的研究 [D]. 上海: 上海大学, 2016) |
| [20] | MaQ S, JinY C, ZhaoY H, et al. Microscopic phase-field simulation for the influence of interatomic potential on the precipitation process of Ni75Al14Mo11 alloy[J]. Acta Metall. Sin. (Engl. Lett.), 2016, 29: 975 |
| [21] | WangK, ZhaoY H, YangD R, et al. Microscopic phase-field simulation for formation of pre-precipitation for Ni75Al14 Mo11[J]. Rare Met. Mater. Eng., 2015, 44: 939 |
| [22] | ZhaoY H. Simulation for the Materials Microstructure Evolution in Phase Transformation Process[M]. Beijing: National Defend Industry Press, 2010: 12 |
| [22] | (赵宇宏. 材料相变过程微观组织模拟 [M]. 北京: 国防工业出版社, 2010: 12) |
| [23] | ZhaoY H, HouH. Simulation of dendritic crystal growth of pure Ni using the phase-field model[J]. Rev. Adv. Mater. Sci., 2013, 33: 246 |
| [24] | ZhaoY H. Atomic-Scale computer simulation for alloy during early precipitation process[D]. Xi'an: Northwestern Polytechnical University, 2003 |
| [24] | (赵宇宏. 合金早期沉淀过程的原子尺度计算机模拟 [D]. 西安: 西北工业大学, 2003) |
| [25] | CahnJ W. On Spinodal decomposition[J]. Acta Metall., 1961, 9: 795 |
| [26] | CahnJ W, HilliardJ E. Free energy of a nonuniform system. I. Iinterfacial free energy[J]. J. Chem. Phys., 1958, 28: 258 |
| [27] | CahnJ W, AllenS M. A microscopic theory for domain wall motion and its experimental verification in Fe-Al alloy domain growth kinetics[J]. J. Phys., 1977, 38: S51 |
| [28] | AllenS M, CahnJ W. A microscopic theory for antiphase boundary motion and its application to antiphase domain coarsening[J]. Acta Metall., 1979, 27: 1085 |
| [29] | KoyamaT, HashimotoK, OnoderaH. Phase-field simulation of phase transformation in Fe-Cu-Mn-Ni quaternary alloy[J]. J. Mater. Trans., 2006, 47: 2765 |
| [30] | KoyamaT, OnoderaH. Phase-field modeling of the microstructure evolutions in Fe-Cu base alloys[J]. Mater. Sci. Forum, 2007, 539-543: 2383 |
| [31] | BuergerM J. A handbook of lattice spacings and structures of metals and alloys[J]. Z. Kristallogr., 1961, 115: 319 |
| [32] | DinsdaleA T. SGTE data for pure elements[J]. Calphad, 1991, 15: 317 |
| [33] | WuX C. Precipitation kinetics in Ni-Al alloys using phase field simulation[D]. Nanjing: Nanjing University of Science & Technology, 2016 |
| [33] | (吴兴超. Ni-Al合金沉淀动力学的相场法研究 [D]. 南京: 南京理工大学, 2016) |
| [34] | MiettinenJ. Thermodynamic description of the Cu-Mn-Ni system at the Cu-Ni side[J]. Calphad, 2003, 27: 147 |
/
| 〈 |
|
〉 |