组织与结构

一类介于晶体与准晶体之间的有序结构

  • 秦高梧 ,
  • 谢红波 ,
  • 潘虎成 ,
  • 任玉平
展开
  • 东北大学材料科学与工程学院材料各向异性与织构教育部重点实验室 沈阳 110819

作者简介 秦高梧,男,1970年生,教授,博士

收稿日期: 2018-07-30

  网络出版日期: 2018-08-31

基金资助

国家重点研发计划项目No.2016YFB0701202及国家自然科学基金项目Nos.51371046、51525101、51501032和U1610253

A New Class of Ordered Structure Between Crystals and Quasicrystals

  • Gaowu QIN ,
  • Hongbo XIE ,
  • Hucheng PAN ,
  • Yuping REN
Expand
  • Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education), School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China

Received date: 2018-07-30

  Online published: 2018-08-31

Supported by

Supported by National Key Research and Development Program of China (No.2016YFB0701202) and National Natural Science Foundation of China (Nos.51371046, 51525101, 51501032 and U1610253)

摘要

本文简要介绍了固态物质结构研究的发展历程,并着重介绍了作者课题组最近在凝聚态结构物质上的新发现。(1) 与传统的Laves结构不同,等温时效析出的(Mg, In)2Ca “Laves相”包含2种晶胞单元,这2种单胞沿6个特定的方向排列,构成5种拼砌图案,这5种拼砌模型随机键合在一起,形成一个在(0001)L基面长程范围内不具有6次旋转对称的“C14”型Laves相。(2) Mg-Zn二元合金等温时效析出的纳米棒状相是由2种最小结构单元,即72°菱形结构单元(MgZn2)和72°等边六边形结构单元(MgZn),沿5个方向自组装而成的一个包含C14、C15等短程有序的Laves晶体相和二维5次旋转对称结构的纳米畴结构。(Mg, In)2Ca Laves相和Mg-Zn 5次纳米畴结构沿法线方向具有周期性的原子排列,然而在法平面上不具有任何平移周期性,是一类既不属于晶体相也不同于任何已发现的准晶体或准晶近似相的二维有序结构。

本文引用格式

秦高梧 , 谢红波 , 潘虎成 , 任玉平 . 一类介于晶体与准晶体之间的有序结构[J]. 金属学报, 2018 , 54(11) : 1490 -1502 . DOI: 10.11900/0412.1961.2018.00357

Abstract

This paper briefly reviews the development and research history of strutures of the solid matters, and highlight two new strcutures of precipitates in Mg alloys found by our group recently. (1) The isothermally aged (Mg, In)2Ca "Laves phase" contains two separate unit cells promoting the formation of five tiling patterns. The bonding of these patterns leads to the generation of the present phase but without any six-fold rotational symmetry in a long-range on the (0001)L basal plane, constrainted by the Penrose geometrical rule, completely different from the known Laves phases. (2) The MgZn five-fold nanodomain structure is self-assembled by two separate unit cells (72° rhombus structure: MgZn2, and 72° equilateral hexagon structure: MgZn) under the Penrose geomotrical constraints, containing 2D five-fold symmetry locally and short-range ordered C14 and C15 Laves structures. These two special structures without any translational symmetry on the normal plane while periodical arrangement along the normal direction, are a new class of intermediate structures between crystals and quasicrystals. And thus, they does not belong to any crystals or 2D ordered structures in quasicrystals or quasicrystal approximants.

参考文献

[1] Wang W H.The nature and properties of amorphous matter[J]. Prog. Phys., 2013, 33(5): 177(汪卫华. 非晶态物质的本质和特性 [J]. 物理学进展, 2013, 33(5): 177)
[2] Bindi L, Steinhardt P J, Yao N, et al.Natural quasicrystals[J]. Science, 2009, 324: 1306
[3] Shechtman D, Blech I, Gratias D, et al.Metallic phase with long-range orientational order and no translational symmetry[J]. Phys. Rev. Lett., 1984, 53: 1951
[4] Zhang Z, Ye H Q, Kuo K H.A new icosahedral phase with m35 symmetry[J]. Philos. Mag., 1985, 52A: L49
[5] Ohashi W, Spaepen F.Stable Ga-Mg-Zn quasi-periodic crystals with pentagonal dodecahedral solidification morphology[J]. Nature, 1987, 330: 555
[6] Abe E, Tsai A P.Quasicrystal-crystal transformation in Zn-Mg-rare-earth alloys[J]. Phys. Rev. Lett., 1999, 83: 753
[7] Guo J Q, Abe E, Tsai A P.Stable icosahedral quasicrystals in binary Cd-Ca and Cd-Yb systems[J]. Phys. Rev., 2000, 62B: R14605
[8] Tian Y, Huang H, Yuan G Y, et al.Nanoscale icosahedral quasicrystal phase precipitation mechanism during annealing for Mg-Zn-Gd-based alloys[J]. Mater. Lett., 2014, 130: 236
[9] Wang N, Chen H, Kuo K H.Two-dimensional quasicrystal with eightfold rotational symmetry[J]. Phys. Rev. Lett., 1987, 59: 1010
[10] Cao W, Ye H Q, Kuo K H.A new octagonal quasicrystal and related crystalline phases in rapidly solidified Mn4Si[J]. Phys. Status Solidi, 1988, 107A: 511
[11] Ma X L, Kuo K H.Decagonal quasicrystal and related crystalline phases in slowly solidified Al-Co alloys[J]. Metall. Trans., 1992, 23A: 1121
[12] Naumovi? D, Aebi P, Schlapbach L, et al.Formation of a stable decagonal quasicrystalline Al-Pd-Mn surface layer[J]. Phys. Rev. Lett., 2001, 87: 195506
[13] Abe E, Tsai A P.Structure of a metastable Al3Ni decagonal quasicrystal: Comparison with a highly perfect Al72Ni20Co8[J]. J. Alloys Compd., 2002, 342: 96
[14] Li H, Ma H K, Hou L G, et al.Shield-like tile and its application to the decagonal quasicrystal-related structures in Al-Cr-Fe-Si alloys[J]. J. Alloys Compd., 2017, 701: 494
[15] Ishimasa T, Nissen H U, Fukano Y.New ordered state between crystalline and amorphous in Ni-Cr particles[J]. Phys. Rev. Lett., 1985, 55: 511
[16] Conrad M, Krumeich F, Harbrecht B.A dodecagonal quasicrystalline chalcogenide[J]. Angew. Chem. Int. Ed., 1998, 37: 1383
[17] Ye X C, Chen J, Irrgang M E, et al.Quasicrystalline nanocrystal superlattice with partial matching rules[J]. Nat. Mater., 2017, 16: 214
[18] Kuo K H.Quasiperiodic Crystals [M]. Hangzhou: Zhejiang Science & Technology Press, 2004: 130(郭可信. 准晶研究 [M]. 杭州: 浙江科学技术出版社, 2004: 130)
[19] Kuo K H.Crystallographic features of quasicrystals[J]. Prog. Chem., 1994, 6: 266(郭可信. 准晶的晶体学特征 [J]. 化学进展, 1994, 6: 266)
[20] Abe E, Yamamoto A.Structure of an approximant crystal in Ni-rich Al71Ni22Co7[J]. Philos. Mag., 2011, 91: 2617
[21] Ye H Q, Wang D N, Kuo K H. Fivefold symmetry in real and reciprocal spaces[J]. Ultramicroscopy, 1985, 16: 273
[22] Ye H Q.Periodic and aperiodic arrangements of icosahedral columns in pentagonal Frank-Kasper phases and analogs [J]. Mater. Sci. Forum, 1987, 22-24: 103
[23] Zhou D S, Ye H Q, Li D X, et al.Microdomain structure displaying apparent decagonal symmetry[J]. Phys. Rev. Lett., 1988, 60: 2180
[24] Xie H B, Pan H C, Ren Y P, et al.New structured laves phase in the Mg-In-Ca system with nontranslational symmetry and two unit cells[J]. Phys. Rev. Lett., 2018, 120: 085701
[25] Xie H B, Pan H C, Ren Y P, et al.Self-assembly of two unit cells into a nanodomain structure containing five-fold symmetry[J]. J. Phys. Chem. Lett., 2018, 9: 4373
[26] Vainshtein B.K. Fundamentals of Crystals: Symmetry, and Methods of Structural Crystallography[M]. 1994: 1
[27] Cui Y H.Development of crystal symmetry theory in last three hundred years[J]. Explor. Nat., 1984,(4): 92(崔云昊. 晶体对称理论三百年 [J]. 大自然探索, 1984, (4): 92)
[28] Chen J Z.Discovery and development of crystallography and quasicrystallography[J]. J. China Univ. Geosci., 1993, 18(S1): 1(陈敬中. 晶体学、准晶体学的发生和发展 [J]. 中国地质大学学报, 1993, 18(S1): 1)
[29] Kroto H W, Heath J R, Obrien S C, et al.C60: Buckminsterfullerene[J]. Nature, 1985, 318: 162
[30] Bednorz J G, Mullerk A.Possible high Tc superconductivity in the Ba-La-Cu-O system[J]. Z. Phys.-Condensed Matter, 1986, 64B: 189
[31] Takakura H, Gomez C P, Yamamoto A, et al.Atomic structure of the binary icosahedral Yb-Cd quasicrystal[J]. Nat. Mater., 2007, 6: 58
[32] Abe E.Electron microscopy of quasicrystals-where are the atoms?[J]. Chem. Soc. Rev., 2012, 41: 6787
[33] Flicker F.One-dimensional quasicrystals from incommensurate charge order[J]. Phys. Rev. Lett., 2015, 115: 236401
[34] He Z B, Wei D X, Shen X, et al.Approximants of Al-Cr-Fe-Si decagonal quasicrystals described by single structural block[J]. J. Alloys Compd., 2015, 647: 797
[35] Sinha A K.Topologically close-packed structures of transition metal alloys[J]. Prog. Mater. Sci., 1972, 15: 81
[36] Liu C T, Zhu J H, Brady M P, et al.Physical metallurgy and mechanical properties of transition-metal Laves phase alloys[J]. Intermetallics, 2000, 8: 1119
[37] Kirkland E J, Loane R F, Silcox J.Simulation of annular dark field stem images using a modified multislice method[J]. Ultramicroscopy, 1987, 23: 77
[38] Muller D A.Structure and bonding at the atomic scale by scanning transmission electron microscopy[J]. Nat. Mater., 2009, 8: 263
[39] Nie J F.Precipitation and hardening in magnesium alloys[J]. Metall. Mater. Trans., 2012, 43A: 3891
[40] Sturkey L, Clark J B.Mechanism of age-hardening in magnesium zinc alloys[J]. J. Inst. Met., 1959, 88: 177
[41] Gallot J, Guinier A, Lal K, et al.Etude aus rayons X des phenomenes de precipitation dans un alliage magnesium-zinc a 6% de zinc[J]. C.R. Hebd. Seances Acad. Sci., 1964, 258: 2818
[42] Gallot J, Graf R.Nouvelles observations aux rayon X et au microscope electronique sur la phase transitoire apparaissant dans l'alliage magnesium-zinc a 6% de zinc[J]. C.R. Hebd. Seances Acad. Sci., 1965, 261: 728
[43] Chun J S, Bryne J G.Precipitate strengthening mechanisms in magnesium zinc alloy single crystals[J]. J. Mater. Sci., 1969, 4: 861
[44] Wei L Y, Dunlop G L, Westengen H.Precipitation hardening of Mg-Zn and Mg-Zn-RE alloys[J]. Metall. Mater. Trans., 1995, 26A: 1705
[45] Rokhlin L L. Oreshkina A A.Research into the structure of a metastable phase formed during the breakdown of a supersaturated solution in magnesium-zinc alloys[J]. Fiz. Met. Metalloved., 1988, 66: 559
[46] Gao X, Nie J F.Characterization of strengthening precipitate phases in a Mg-Zn alloy[J]. Scr. Mater., 2007, 56: 645
[47] Rosalie J M, Somekawa H, Singh A, et al.Structural relationships among MgZn2 and Mg4Zn7 phases and transition structures in Mg-Zn-Y alloys[J]. Philos. Mag., 2010, 90: 3355
[48] Langelier B, Korinek A, Donnadieu P, et al.Improving precipitation hardening behavior of Mg-Zn based alloys with Ce-Ca microalloying additions[J]. Mater. Charact., 2016, 120: 18
文章导航

/