高强韧Ti-Ni基块体金属玻璃复合材料高温变形行为

  • 赵燕春 ,
  • 孙浩 ,
  • 李春玲 ,
  • 蒋建龙 ,
  • 毛瑞鹏 ,
  • 寇生中 ,
  • 李春燕
展开
  • 1 兰州理工大学省部共建有色金属先进加工与再利用国家重点实验室 兰州 730050
    2 兰州理工大学机电工程学院 兰州 730050

作者简介 赵燕春,女,1984年生,副教授,博士

收稿日期: 2018-06-11

  网络出版日期: 2018-07-23

基金资助

国家自然科学基金项目No.51661017以及甘肃省杰出青年基金项目No.17JR5RA108

High Temperature Deformation Behavior of High Strength and Toughness Ti-Ni Base Bulk Metallic Glass Composites

  • Yanchun ZHAO ,
  • Hao SUN ,
  • Chunling LI ,
  • Jianlong JIANG ,
  • Ruipeng MAO ,
  • Shengzhong KOU ,
  • Chunyan LI
Expand
  • 1 State Key Laboratory of Advanced Processing and Recycling of Nonferrous Metals, Lanzhou University of Technology, Lanzhou 730050, China
    2 College of Mechano-Electronic Engineering, Lanzhou University of Technology, Lanzhou 730050, China

Received date: 2018-06-11

  Online published: 2018-07-23

Supported by

Supported by National Natural Science Foundation of China (No.516601017) and Outstanding Youth Funds of Gansu Province (No.17JR5RA108)

摘要

采用水冷Cu坩埚悬浮熔炼-Cu模吸铸法制备了 Ti-Ni基块体金属玻璃复合材料(BMGCs)试棒,研究了合金的微观组织、热力学行为以及室温和高温力学性能。结果表明,该铸态合金组织由非晶基体和过冷奥氏体及热致马氏体组成,且晶体相尺寸由表及里增大。在室温压应力加载时,合金表现出优异的综合力学性能,其屈服强度为1286 MPa,断裂强度为2256 MPa,且塑性应变为12.2%。在过冷液相区压应力加载时,合金在高的变形温度和低应变速率下,表现出近Newtonian流变特征,其最佳变形温度为T>480 ℃且与过冷液相区(SLR)的交集部分。温度为560 ℃、应变速率为5×10-4 s-1时,合金应力敏感指数m和能量耗散率ψ分别为0.81和0.895。

本文引用格式

赵燕春 , 孙浩 , 李春玲 , 蒋建龙 , 毛瑞鹏 , 寇生中 , 李春燕 . 高强韧Ti-Ni基块体金属玻璃复合材料高温变形行为[J]. 金属学报, 2018 , 54(12) : 1818 -1824 . DOI: 10.11900/0412.1961.2018.00256

Abstract

Room-temperature brittleness and strain-softening during deformation of bulk metallic glasses, and limited processability of shape memory alloys have been stumbling blocks for their advanced functional structural applications. To solve the key scientific problems, a new shape memory bulk metallic glass based composite, through the approach using transformation-induced plasticity (TRIP) effect of shape memory alloys to enhance both ductility and work-hardening capability of metallic glasses, and superplasticity of bulk metallic glass in supercooled liquid region to realize near net forming, was developed in this work. And the Ti-Ni base bulk metallic glass composites (BMGCs) rods were prepared by the levitation suspend melting-water cooled Cu mold process. Microstructure, thermal behavior, mechanical properties and high temperature deformation behavior of the alloy were investigated. The results show that the as-cast alloy microstructure consists of amorphous matrix, undercooled austenite and thermally-induced martensite. Besides, the size of the crystal phase precipitated on the amorphous matrix increases from the surface to the inside. The alloy exhibits excellent comprehensive mechanical properties at room temperature. The yield strength, fracture strength and the plastic strain of alloy are up to 1286 MPa, 2256 MPa and 12.2%, respectively. Under compressive loading in the supercooled liquid region, the composite exhibits approximate Newtonian behavior at lower strain rate in higher deformation temperature, and the optimum deformation temperature is T>480 ℃ and the intersection part with supercooled liquid region (SLR). When the temperature is 560 ℃ and the strain rate is 5×10-4 s-1, the stress sensitivity index m and the energy dissipation rate ψ are 0.81 and 0.895, respectively. Furthermore, the volume of activation is quantified to characterize the rheological behavior.

参考文献

[1] Greer A L.Metallic glasses[J]. Science, 1995, 267: 1947
[2] L?ffler J F.Bulk metallic glasses[J]. Intermetallics, 2003, 11: 529
[3] Schuh C A, Hufnagel T C, Ramamurty U.Mechanical behavior of amorphous alloys[J]. Acta Mater., 2007, 55: 4067
[4] Wang W H.Bulk metallic glasses with functional physical properties[J]. Adv. Mater., 2009, 21: 4524
[5] Schroers J.Processing of bulk metallic glass[J]. Adv. Mater., 2010, 22: 1566
[6] Cao Q P, Liu J W, Yang K J, et al.Effect of pre-existing shear bands on the tensile mechanical properties of a bulk metallic glass[J]. Acta Mater., 2010, 56: 1276
[7] Liu Y H, Wang G, Wang R J, et al.Super plastic bulk metallic glasses at room temperature[J]. Science, 2007, 315: 1385
[8] Chen L Y, Fu Z D, Zhang G Q, et al.New class of plastic bulk metallic glass[J]. Phys. Rev. Lett., 2008, 100: 075501
[9] Hofmann D C, Suh J Y, Wiest A, et al.Designing metallic glass matrix composites with high toughness and tensile ductility[J]. Nature, 2008, 451: 1085
[10] Hofmann D C.Shape memory bulk metallic glass composites[J]. Science, 2010, 329: 1294
[11] Gargarella P, Pauly S, Song K K, et al.Ti-Cu-Ni shape memory bulk metallic glass composites[J]. Acta Mater., 2013, 61: 151
[12] Jiang M Q, Dai L H.On the origin of shear banding instability in metallic glasses[J]. J. Mech. Phys. Solids, 2009, 57: 1267
[13] Sun J F, Huang Y J, Shen J, et al.Superplastic formability of a Zr-Ti-Ni-Cu-Be bulk metallic glass[J]. J. Alloys Compd., 2006, 415: 198
[14] Liu M C, Du X H, Lin I C, et al.Superplastic-like deformation in metallic amorphous/crystalline nanolayered micropillars[J]. Intermetallics, 2012, 30: 30
[15] Yao K F, Ruan F, Yang Y Q, et al.Superductile bulk metallic glass[J]. Appl. Phys. Lett., 2006, 88: 122106
[16] Ferenc J, Erenc-S?dziak T, Kowalczyk M, et al.The supercooled liquid region span of Fe-based bulk metallic glasses[J]. J. Alloys Compd., 2010, 495: 327
[17] Wang Q, Wang D K, Fu T, et al.High temperature homogeneous plastic flow behavior of a Zr based bulk metallic glass matrix composite[J]. J. Alloys Compd., 2010, 495: 50
[18] Bae D H, Lim H K, Kim S H, et al.Mechanical behavior of a bulk Cu-Ti-Zr-Ni-Si-Sn metallic glass forming nano-crystal aggregate bands during deformation in the supercooled liquid region[J]. Acta Mater., 2002, 50: 1749
[19] Guo S F, Chan K C, Chen Q, et al.Tensile plastic deformation of a Zr-based bulk metallic glass composite in the supercooled liquid region[J]. Scr. Mater., 2009, 60: 369
[20] Wu Y, Ma D, Li Q K, et al.Transformation-induced plasticity in bulk metallic glass composites evidenced by in-situ neutron diffraction[J]. Acta Mater., 2017, 124: 478
[21] Wu Y, Bei H, Wang Y L, et al.Deformation-induced spatiotemporal fluctuation, evolution and localization of strain fields in a bulk metallic glass[J]. Int. J. Plast., 2015, 71: 136
[22] Huang Y J, Shen J, Sun Y, et al.High temperature deformation behaviors of Ti40Zr25Ni3Cu12Be20 bulk metallic glass[J]. J. Alloys Compd., 2010, 504(suppl.1): S82
[23] Chen G, Hao Y F, Chen X W, et al.Compressive behaviour of tungsten fibre reinforced Zr-based metallic glass at different strain rates and temperatures[J]. Int. J. Impact Eng., 2017, 106: 110
[24] Cheng S R, Wang C J, Ma M Z, et al.Mechanism for microstructural evolution induced by high temperature deformation in Zr-based bulk metallic glasses[J]. J. Alloys Compd., 2016, 676: 299
[25] Jiang M Q, Wilde G, Dai L H.Origin of stress overshoot in amorphous solids[J]. Mech. Mater., 2015, 81: 72
[26] Kim W J, Ma D S, Jeong H G.Superplastic flow in a Zr65Al10Ni10Cu15 metallic glass crystallized during deformation in a supercooled liquid region[J]. Scr. Mater., 2003, 49: 1067
[27] Nieh T G, Wadsworth J, Liu C T, et al.Plasticity and structural instability in a bulk metallic glass deformed in the supercooled liquid region[J]. Acta Mater., 2001, 49: 2887
[28] Yuan X Y, Chen L Q.Hot deformation at elevated temperature and recrystallization behavior of a high manganese austenitic TWIP steel[J]. Acta Metall. Sin., 2015, 51: 651(袁晓云, 陈礼清. 一种高锰奥氏体TWIP钢的高温热变形与再结晶行为[J]. 金属学报, 2015, 51: 651)
[29] Wang T, Wan Z P, Sun Y, et al.Dynamic softening behavior and microstructure evolution of nickel base superalloy[J]. Acta Metall. Sin., 2018, 54: 84(王涛, 万志鹏, 孙宇等. 镍基变形高温合金动态软化行为与组织演变规律研究[J]. 金属学报, 2018, 54: 84)
[30] Ghidelli M, Idrissi H, Gravier S, et al.Homogeneous flow and size dependent mechanical behavior in highly ductile Zr65Ni35 metallic glass films[J]. Acta Mater., 2017, 131: 246
[31] Liu Q, Xia C, Liu X D.The m-C-δ or m-k-δ relations of superplasticity of Zn-5%Al eutectic alloy[J]. Acta Metall. Sin., 1985, 21: 111(刘勤, 夏锄, 刘晓东. Zn-5%Al合金超塑性的m-C-δ (或m-k-δ)关系[J]. 金属学报, 1985, 21: 111)
[32] Yao Z F, Qiao J C, Pelletier J M, et al.High temperature deformation behaviors of the Zr63.36Cu14.52Ni10.12Al12 bulk metallic glass[J]. J. Mater. Sci., 2016, 51: 4079
[33] Zhang X Y, Yuan Z Z, Feng X L, et al.Homogeneous viscous flow behavior of a Cu-Zr based bulk metallic glass composites[J]. Mater. Sci. Eng., 2015, A620: 352
[34] Kawamura Y, Nakamura T, Inoue A.Superplasticity in Pd40Ni40P20 metallic glass[J]. Scr. Mater., 1998, 39: 301
[35] Spaepen F.A microscopic mechanism for steady state inhomogeneous flow in metallic glasses[J]. Acta Metall., 1977, 25: 407
[36] Cui J, Li J S, Wang J, et al.Deformation behavior of a Ti-based bulk metallic glass composite in the supercooled liquid region[J]. Mater. Des., 2015, 90: 595
[37] Hajlaoui K, Yavari A R, Lemoulec A, et al.Plasticity induced by nanoparticle dispersions in bulk metallic glasses[J]. J. Non-Cryst. Solids, 2007, 353: 327
[38] Inoue A, Fan C, Saida J, et al.High-strength Zr-based bulk amorphous alloys containing nanocrystalline and nanoquasicrystalline particles[J]. Sci. Technol. Adv. Mater., 2000, 1: 73