井下含硫环空液中P110油管钢应力腐蚀开裂的电化学噪声特征
作者简介 余 军,男,1993年生,硕士生
收稿日期: 2018-01-20
网络出版日期: 2018-06-06
基金资助
国家自然科学基金项目No.51771079和国家油气重大专项项目No.2016ZX05016002-004
Electrochemical Noise of Stress Corrosion Cracking of P110 Tubing Steel in Sulphur-Containing Downhole Annular Fluid
Received date: 2018-01-20
Online published: 2018-06-06
Supported by
Supported by National Natural Science Foundation of China (No.51771079) and National Key Oil Program of China (No.2016ZX05016002-004)
采用慢应变速率拉伸(SSRT)实验,并结合电化学噪声(ECN)、SEM与EIS等方法,研究了P110低合金油管钢在模拟井下环空液中的应力腐蚀开裂(SCC)行为,并探讨了S2-浓度对裂纹萌生和扩展过程的影响。结果表明,在P110钢的弹性形变阶段,环空液中低浓度S2-的加入加速了P110钢拉伸试样表面钝化膜的破坏,导致ECN曲线上出现许多由亚稳态点蚀引起的短时电流噪声峰。S2-的加入还显著缩短了亚稳态点蚀向稳定点蚀转变的时间,促使拉伸试样表面出现较大尺寸的蚀坑,这些蚀坑在拉应力作用下可以转变为裂纹萌生源。相比亚稳态点蚀,裂纹生长产生的噪声峰平均寿命更长(约400 s),且噪声幅值(约40 μA)和积分电量(约4000 μC)也更大。P110钢的SCC以阳极溶解为主,且裂纹生长速率随S2-浓度的增加而增大,但裂纹生长是断续而非连续进行的。
余军 , 张德平 , 潘若生 , 董泽华 . 井下含硫环空液中P110油管钢应力腐蚀开裂的电化学噪声特征[J]. 金属学报, 2018 , 54(10) : 1399 -1407 . DOI: 10.11900/0412.1961.2018.00033
Stress corrosion cracking (SCC) is considered as the main risk of tubing steels during the exploitation of oil and gas fields, which could result in sudden and catastrophic failures of downhole tubing. Especially in annular downhole environment, P110 tubing steel is prone to sulfide stress corrosion cracking and hydrogen embrittlement (HE) where S2- could be originated from bio-reduction of SO42- inspired by sulfate-reducing bacteria (SRB). Currently, extensive work have been performed to investigate the influence factors on SCC and mechanism of tubing steels, but limited researches have been conducted on the SCC of P110 tubing steel in annular downhole environment, particularly, on the early detection of SCC. In this work, the SCC behavior of P110 low alloy steel in simulating sulphur-containing annular fluid (SAF) and the effect of S2- concentration on the initiation and propagation of crack were investigated by slow stress rate test (SSRT), non-destructive electrochemical noise (ECN), SEM and EIS techniques. The results showed that, during the elastic stress stage, the addition of S2- accelerated the breakdown of passivation film on the surface of P110 steel tensile specimen. There are many short duration current transients caused by metastable pits on ECN curves. The transformation time of metastable to stable pits is shortened significantly by the addition of S2-, which not only promotes the growth of pits but the initiation of cracks from the stable pits under the action of tensile stress. Compared with the ECN spikes from metastable pits, the spikes associated to the advance of cracks are featured by longer average duration (about 400 s), stronger amplitude (40 μA), and higher charge (about 4000 μC). As a result, the susceptibility of P110 steel to SCC increases with S2- concentration, and the propagation of SCC is dominated by anodic dissolution characteristic of discontinuous advance.
| [1] | Liu Z Y, Zhao T L, Liu R K, et al.Influence factors on stress corrosion cracking of P110 tubing steel under CO2 injection well annulus environment[J]. J. Cent. South Univ., 2016, 23: 757 |
| [2] | Wang P Y, Lv Z G, Zheng S Q, et al.Tensile and impact properties of X70 pipeline steel exposed to wet H2S environments[J]. Int. J. Hydrogen Energy, 2015, 40: 11514 |
| [3] | Roffey P, Davies E H.The generation of corrosion under insulation and stress corrosion cracking due to sulphide stress cracking in an austenitic stainless steel hydrocarbon gas pipeline[J]. Eng. Fail. Anal., 2014, 44: 148 |
| [4] | Bao M Y, Ren C Q, Lei M Y, et al.Electrochemical behavior of tensile stressed P110 steel in CO2 environment[J]. Corros. Sci., 2016, 112: 585 |
| [5] | Meriem-Benziane M, Bou-Sa?d B, Boudouani N.The effect of crude oil in the pipeline corrosion by the naphthenic acid and the sulfur: A numerical approach[J]. J. Pet. Sci. Eng., 2017, 158: 672 |
| [6] | Liu Z Y, Li H, Jia Z J, et al.Failure analysis of P110 steel tubing in low-temperature annular environment of CO2 flooding wells[J]. Eng. Fail. Anal., 2016, 60: 296 |
| [7] | Alexandrov V, Sushko M L, Schreiber D K, et al.Adsorption and diffusion of atomic oxygen and sulfur at pristine and doped Ni surfaces with implications for stress corrosion cracking[J]. Corros. Sci., 2016, 113: 26 |
| [8] | Zhang L, Li X G, Du C W, et al.Corrosion and stress corrosion cracking behavior of X70 pipeline steel in a CO2-containing solution[J]. J. Mater. Eng. Perform., 2009, 18: 319 |
| [9] | Monnot M, Nogueira R P, Roche V, et al.Sulfide stress corrosion study of a super martensitic stainless steel in H2S sour environments: Metallic sulfides formation and hydrogen embrittlement[J]. Appl. Surf. Sci., 2017, 394: 132 |
| [10] | Qin M, Li J F, Chen S Y, et al.Experimental study on stress corrosion crack propagation rate of FV520B in carbon dioxide and hydrogen sulfide solution[J]. Results Phys., 2016, 6: 365 |
| [11] | Ziaei S M R, Kokabi A H, Nasr-Esfehani M. Sulfide stress corrosion cracking and hydrogen induced cracking of A216-WCC wellhead flow control valve body[J]. Case Stud. Eng. Fail. Anal., 2013, 1: 223 |
| [12] | Ding J H, Zhang L, Li D P, et al.Corrosion and stress corrosion cracking behavior of 316L austenitic stainless steel in high H2S-CO2-Cl- environment[J]. J. Mater. Sci., 2013, 48: 3708 |
| [13] | Yin Z F, Zhao W Z, Bai Z Q, et al.Corrosion behavior of SM 80SS tube steel in stimulant solution containing H2S and CO2[J]. Electrochim. Acta, 2008, 53: 3690 |
| [14] | Choi Y S, Nesic S, Ling S.Effect of H2S on the CO2 corrosion of carbon steel in acidic solutions[J]. Electrochim. Acta, 2011, 56: 1752 |
| [15] | Wang P Y, Wang J, Zheng S Q, et al.Effect of H2S/CO2 partial pressure ratio on the tensile properties of X80 pipeline steel[J]. Int. J. Hydrogen Energy, 2015, 40: 11925 |
| [16] | Wei L, Pang X L, Gao K W.Effect of small amount of H2S on the corrosion behavior of carbon steel in the dynamic supercritical CO2 environments[J]. Corros. Sci., 2016, 103: 132 |
| [17] | Liu Z Y, Wang X Z, Liu R K, et al.Electrochemical and sulfide stress corrosion cracking behaviors of tubing steels in a H2S/CO2 annular environment[J]. J. Mater. Eng. Perform., 2014, 23: 1279 |
| [18] | Fan Z, Hu X G, Liu J Y, et al.Stress corrosion cracking of L360NS pipeline steel in sulfur environment[J]. Petroleum, 2017, 3: 377 |
| [19] | Hao W K, Liu Z Y, Zhang X, et al.Effects of H2S with various concentration on stress corrosion cracking behavior of 35CrMo steel[J]. J. Chin. Soc. Corros. Prot., 2013, 33: 357(郝文魁, 刘智勇, 张新等. H2S浓度对35CrMo钢应力腐蚀开裂的影响[J]. 中国腐蚀与防护学报, 2013, 33: 357) |
| [20] | Zhou C S, Huang Q Y, Guo Q, et al.Sulphide stress cracking behaviour of the dissimilar metal welded joint of X60 pipeline steel and Inconel 625 alloy[J]. Corros. Sci., 2016, 110: 242 |
| [21] | Kong D J, Wu Y Z, Long D.Stress corrosion of X80 pipeline steel welded joints by slow strain test in NACE H2S solutions[J]. J. Iron Steel Res. Int., 2013, 20: 40 |
| [22] | Zhu L K, Yan Y, Qiao L J, et al.Stainless steel pitting and early-stage stress corrosion cracking under ultra-low elastic load[J]. Corros. Sci., 2013, 77: 360 |
| [23] | Breimesser M, Ritter S, Seifert H P, et al.Application of electrochemical noise to monitor stress corrosion cracking of stainless steel in tetrathionate solution under constant load[J]. Corros. Sci., 2012, 63: 129 |
| [24] | Acu?a-González N, García-Ochoa E, González-Sánchez J.Assessment of the dynamics of corrosion fatigue crack initiation applying recurrence plots to the analysis of electrochemical noise data[J]. Int. J. Fatigue, 2008, 30: 1211 |
| [25] | Dong Z H, Shi W, Guo X P.Initiation and repassivation of pitting corrosion of carbon steel in carbonated concrete pore solution[J]. Corros. Sci., 2011, 53: 1322 |
| [26] | Dong Z H, Guo X P, Zheng J X, et al.Investigation on inhibition of CrO42- and MoO42- ions on carbon steel pitting corrosion by electrochemical noise analysis[J]. J. Appl. Electrochem., 2002, 32: 395 |
| [27] | Dong Z H, Guo X P, Zheng J X.Review on electrochemical noise analysis methods[J]. Mater. Prot., 2001, 34(7): 20(董泽华, 郭兴蓬, 郑家燊. 电化学噪声的分析方法[J]. 材料保护, 2001, 34(7): 20) |
| [28] | Javidi M, Horeh S B.Investigating the mechanism of stress corrosion cracking in near-neutral and high pH environments for API 5L X52 steel[J]. Corros. Sci., 2014, 80: 213 |
| [29] | Wells D B, Stewart J, Davidson R, et al.The mechanism of intergranular stress corrosion cracking of sensitised austenitic stainless steel in dilute thiosulphate solution[J]. Corros. Sci., 1992, 33: 39 |
/
| 〈 |
|
〉 |