双脉冲磁控溅射峰值靶电流密度对TiN薄膜结构与力学性能的影响

  • 时惠英 ,
  • 杨超 ,
  • 蒋百灵 ,
  • 黄蓓 ,
  • 王迪
展开
  • 西安理工大学材料科学与工程学院 西安 710048

作者简介 时惠英,女,1959年生,教授

收稿日期: 2017-09-25

  网络出版日期: 2018-04-09

基金资助

国家自然科学基金项目No.51571114

Influences of Target Peak Current Density on the Microstructure and Mechanical Properties of TiN Films Deposited by Dual Pulsed Power Magnetron Sputtering

  • Huiying SHI ,
  • Chao YANG ,
  • Bailing JIANG ,
  • Bei HUANG ,
  • Di WANG
Expand
  • School of Materials Science and Engineering, Xi'an University of Technology, Xi'an 710048, China

Received date: 2017-09-25

  Online published: 2018-04-09

Supported by

Supported by National Natural Science Foundation of China (No.51571114)

摘要

自主研发了双脉冲磁控溅射技术,提出在一个脉冲周期内电流呈阶梯式上升的双脉冲电场设计理念,通过对2个脉冲阶段持续时间和峰值靶电流密度的调配,既满足提高镀料粒子动能与离化率以制备高性能薄膜的工艺要求,又达到增加脉冲持续时间以提高薄膜沉积速率的效能目标。采用双脉冲磁控溅射技术,在后期脉冲阶段的不同峰值靶电流密度下制备4组TiN薄膜,研究了峰值靶电流密度对薄膜微观结构和力学性能的影响。结果表明,将峰值靶电流密度提高至0.87 A/cm2时,所制备的TiN薄膜呈现出颗粒细小且致密的组织,平均晶粒尺寸为17 nm。同时,薄膜的显微硬度和膜基结合力可分别达29.5 GPa和30.0 N。

本文引用格式

时惠英 , 杨超 , 蒋百灵 , 黄蓓 , 王迪 . 双脉冲磁控溅射峰值靶电流密度对TiN薄膜结构与力学性能的影响[J]. 金属学报, 2018 , 54(6) : 927 -934 . DOI: 10.11900/0412.1961.2017.00406

Abstract

The low kinetic energy and low ionization rate of deposited particle of traditional magnetron sputtering led to low density and poor adhesion of TiN film. The peak current density between cathodic target and anodic chamber was increased several times through the adoption of pulsed power supply mode with low duty cycle, which further enhanced kinetic energy and ionization rate of deposited particle. But the average deposition rate of thin film was significantly reduced. Therefore, a design concept of dual pulsed electric field mode was proposed, which allowed to adjust duration time and target peak current density of the dual pulses. It not only enhanced kinetic energy and ionization rate of deposited particle to satisfy the demand of fabrication of high performance film, but also increased the duration time of pulse to achieve high average deposition rate. In the manuscript, TiN films were deposited by dual pulsed power magnetron sputtering with different target peak current densities of the second pulse stage. The microstructure and mechanical properties of TiN films were characterized using XRD, SEM, nanoindentation and microscratch test. It was found that the TiN film deposited under target peak current density of 0.87 A/cm2 exhibited finely dense microstructure with average grain size of 17 nm. Additionally, the hardness and film-substrate adhesion of such film were as high as 29.5 GPa and 30.0 N, respectively.

参考文献

[1] Zhang L Q, Yang H S, Pang X L, et al.Microstructure, residual stress, and fracture of sputtered TiN films[J]. Surf. Coat. Technol., 2013, 224: 120
[2] He C L, Zhang J L, Wang J M, et al.Effect of structural defects on corrosion initiation of TiN nanocrystalline films[J]. Appl. Surf. Sci., 2013, 276: 667
[3] Craciun D, Stefan N, Socol G, et al.Very hard TiN thin films grown by pulsed laser deposition[J]. Appl. Surf. Sci., 2012, 260: 2
[4] Kelly P J, Arnell R D.Magnetron sputtering: A review of recent developments and applications[J]. Vacuum, 2000, 56: 159
[5] Weis H, Müggenburg T, Grosse P, et al.Advanced characterization tools for thin films in low-E systems[J]. Thin Solid Films, 1999, 351: 184
[6] Siemroth P, Schülke T.Copper metallization in microelectronics using filtered vacuum arc deposition-principles and technological development [J]. Surf. Coat. Technol., 2000, 133-134: 106
[7] Se J H, Kang T S, Noh D Y.Epitaxial and island growth of Ag/Si (001) by RF magnetron sputtering[J]. J. Appl. Phys., 1997, 81: 6716
[8] Li X Y, Wu W W, Dong H S.Microstructural characterisation of carbon doped CrAlTiN nanoscale multilayer coatings[J]. Surf. Coat. Technol., 2011, 205: 3251
[9] Christou C, Barber Z H.Ionization of sputtered material in a planar magnetron discharge[J]. J. Vac. Sci. Technol., 2000, 18A: 2897
[10] Ricard A, Nouvellon C, Konstantinidis S, et al.Density and temperature in an inductively amplified magnetron discharge for titanium deposition[J]. J. Vac. Sci. Technol., 2002, 20A: 1488
[11] Konstantinidis S, Ricard A, Ganciu M, et al.Measurement of ionic and neutral densities in amplified magnetron discharges by pulsed absorption spectroscopy[J]. J. Appl. Phys., 2004, 95: 2900
[12] Yang C, Jiang B L, Liu Z, et al.Nanocrystalline titanium films deposited via thermal-emission-enhanced magnetron sputtering[J]. Thin Solid Films, 2015, 597: 117
[13] Lin J L, Moore J J, Sproul W D, et al.The structure and properties of chromium nitride coatings deposited using dc, pulsed dc and modulated pulse power magnetron sputtering[J]. Surf. Coat. Technol., 2010, 204: 2230
[14] Arnell R D, Kelly P J, Bradley J W. Recent developments in pulsed magnetron sputtering [J]. Surf. Coat. Technol., 2004, 188-189: 158
[15] Kouznetsov V, Macák K, Schneider J M, et al.A novel pulsed magnetron sputter technique utilizing very high target power densities[J]. Surf. Coat. Technol., 1999, 122: 290
[16] Tian M B.Thin Film Technologies and Materials [M]. Beijing: Tsinghua University Press, 2006: 132(田民波. 薄膜技术与薄膜材料 [M]. 北京: 清华大学出版社, 2006: 132)
[17] Yang K.The research on TiN films deposited by magnetron sputtering [D]. Nanjing: Southeast University, 2006(杨凯. 反应磁控溅射法制备TiN薄膜的研究 [D]. 南京: 东南大学, 2006)
[18] Yeh T S, Wu J M, Hu L J.The properties of TiN thin films deposited by pulsed direct current magnetron sputtering[J]. Thin Solid Films, 2008, 516: 7294
[19] Cullity B D, Stock S R.Elements of X-Ray Diffraction[M]. 3rd Ed., London: Prentice-Hall Inc., 2001: 167
[20] Jenkins R, Snyder R.Introduction to X-Ray Powder Diffractometry[M]. New York: Wiley-Interscience, 1996: 89
[21] Fujimura N, Nishihara T, Goto S, et al.Control of preferred orientation for ZnOx films: Control of self-texture[J]. J. Cryst. Growth, 1993, 130: 269
[22] Gu M, Yang F Z, Huang L, et al.XRD study on highly preferred orientation Cu electrodeposit[J]. Electrochemistry, 2002, 8: 282(辜敏, 杨防祖, 黄令等. 高择优取向Cu电沉积层的XRD研究[J]. 电化学, 2002, 8: 282)
[23] Zhao Y H, Guo C Q, Yang W J, et al.TiN films deposition inside stainless-steel tubes using magnetic field-enhanced arc ion plating[J]. Vacuum, 2015, 112: 46
[24] Luo Q S, Yang S, Cooke K E.Hybrid HIPIMS and DC magnetron sputtering deposition of TiN coatings: Deposition rate, structure and tribological properties[J]. Surf. Coat. Technol., 2013, 236: 13
[25] Lin J L, Moore J J, Sproul W D, et al.Modulated pulse power sputtered chromium coatings[J]. Thin Solid Films, 2009, 518: 1566
[26] Nia N S, Savall C, Creus J, et al.On the implication of solute contents and grain boundaries on the Hall-Petch relationship of nanocrystalline Ni-W alloys[J]. Mater. Sci. Eng., 2016, A678: 204
[27] Kohlscheen J, Stock H R, Mayr P. Chemical bonding in magnetron sputtered TiNx coatings and its relation to diamond turnability [J]. Surf. Coat. Technol., 2001, 142-144: 992
[28] Stallard J, Poulat S, Teer D G.The study of the adhesion of a TiN coating on steel and titanium alloy substrates using a multi-mode scratch tester[J]. Tribol. Int., 2006, 39: 159
[29] Lin J L, Moore J J, Mishra B, et al.Effect of asynchronous pulsing parameters on the structure and properties of CrAlN films deposited by pulsed closed field unbalanced magnetron sputtering (P-CFUBMS)[J]. Surf. Coat. Technol., 2008, 202: 1418
[30] Laing K, Hampshire J, Teer D, et al.The effect of ion current density on the adhesion and structure of coatings deposited by magnetron sputter ion plating[J]. Surf. Coat. Technol., 1999, 112: 177
[31] Heinke W, Leylan A, Matthews A, et al.Evaluation of PVD nitride coatings, using impact, scratch and Rockwell-C adhesion test[J]. Thin Solid films, 1995, 270: 431
文章导航

/