金属材料的凝固专刊

纵向静磁场对定向凝固GCr15轴承钢柱状晶向等轴晶转变的影响

  • 侯渊 ,
  • 任忠鸣 ,
  • 王江 ,
  • 张振强 ,
  • 李霞
展开
  • 上海大学省部共建高品质特殊钢冶金与制备国家重点实验室 上海 200072

作者简介 侯 渊,男,1985年生,博士生

收稿日期: 2017-12-25

  网络出版日期: 2018-03-05

基金资助

资助项目 国家自然科学基金项目Nos.U1560202、51604171、51690162,上海市科委项目No.17JC1400602及上海商用航空发动机联合创新项目Nos.AR910 和AR911

Effect of Longitudinal Static Magnetic Field on the Columnar to Equiaxed Transition in Directionally Solidified GCr15 Bearing Steel

  • Yuan HOU ,
  • Zhongming REN ,
  • Jiang WANG ,
  • Zhenqiang ZHANG ,
  • Xia LI
Expand
  • State Key Laboratory of Advanced Special Steel, Shanghai University, Shanghai 200072, China

Received date: 2017-12-25

  Online published: 2018-03-05

Supported by

Supported by National Natural Science Foundation of China (Nos.U1560202, 51604171 and 51690162), Shanghai Municipal Science and Technology Commission (No.17JC1400602) and United Innovation Program of Shanghai Commercial Aircraft Engine (Nos.AR910 and AR911)

摘要

进行了外加纵向静磁场下GCr15轴承钢的定向凝固实验,考察了纵向静磁场对试样凝固过程中柱状枝晶向等轴枝晶转变(columnar to equiaxed transition,CET)的影响。结果表明,在温度梯度(104 K/cm)和抽拉速率(20 μm/s)一定时,随着磁场强度的增加(0~5 T),试样棒边缘柱状枝晶的生长逐渐地遭到破坏,从而发生不同程度的CET;当磁场强度和温度梯度分别为4 T和104 K/cm时,在较低抽拉速率(5 μm/s)下,试样的凝固组织发生了完全CET;在试样发生完全CET后,其合金元素分布趋于均匀。结合数值模拟,可将这些现象归结为纵向静磁场与热电流相互作用产生的热电磁力对枝晶和熔体的作用所致。

本文引用格式

侯渊 , 任忠鸣 , 王江 , 张振强 , 李霞 . 纵向静磁场对定向凝固GCr15轴承钢柱状晶向等轴晶转变的影响[J]. 金属学报, 2018 , 54(5) : 801 -808 . DOI: 10.11900/0412.1961.2017.00557

Abstract

Columnar to equiaxed transition (CET) generating a fine-grain structure of GCr15 bearing steel with the homogeneity of the solute contents and the rather small amount of internal defects is often desired in solidification processes. In recent years much attention has been paid to the effect of static magnetic fields on the CET of Al base alloys, Pb-Sn alloys and Ni base superalloys. However, there are few papers to investigate the effect of static magnetic fields on the CET of GCr15 bearing steel. The present work investigates how longitudinal static magnetic fields affect the CET in directionally solidified GCr15 bearing steel. Experimental results show that columnar dendrites degenerate and transform into equiaxed dendrites at the edge of the sample as the longitudinal static magnetic field increases at pulling rate of 20 μm/s and temperature gradient of 104 K/cm. The dendritic morphology without the longitudinal static magnetic field is regular and columnar at pulling rate of 5 and 50 μm/s and temperature gradient of 104 K/cm. When the 4 T longitudinal static magnetic field is applied, the dendritic morphology is still regular and columnar at pulling rate of 50 μm/s and temperature gradient of 104 K/cm. However, the CET occurs at low pulling rate of 5 μm/s and temperature gradient of 104 K/cm. This phenomenon is simultaneously accompanied by more uniformly distributed alloying elements. The corresponding numerical simulations verify that the thermoelectric (TE) magnetic force is induced by the interaction between the longitudinal static magnetic field and TE current. Owing to TE magnetic force localized into the root of the dendrite, the dendritic fragments detach from the primary dendrites. Then the TE magnetic convection induced by TE magnetic force acting on the melt transports the fragments from the interdendritic spacing to the region ahead of columnar dendrites. It can be deduced from above phenomena that the TE magnetic force leads to the CET under the longitudinal static magnetic field.

参考文献

[1] Bhadeshia H K D H. Steels for bearings[J]. Prog. Mater. Sci., 2012, 57: 268
[2] Dong Z Q, Jiang B, Mei Z, et al.Effect of carbide distribution on the grain refinement in the steel for large-size bearing ring[J]. Steel Res. Int., 2016, 87: 745
[3] Qiu H, Wang L N, Hanamura T, et al.Physical interpretation of grain refinement-induced variation in fracture mode in ferritic steel[J]. ISIJ Int., 2013, 53: 382
[4] Walker P F F, Kerrigan A, Green M, et al. Modelling of micro-segregation in a 1C-1.5Cr type bearing steel[J]. Bear. Steel Technol., 2015, 10: 54
[5] Grong O, Kolbeinsen L, Van Der Eijk C, et al. Microstructure control of steels through dispersoid metallurgy using novel grain refining alloys[J]. ISIJ Int., 2014, 46: 824
[6] Kivi? M, Holappa L, Iung T.Addition of dispersoid titanium oxide inclusions in steel and their influence on grain refinement[J]. Metall. Mater. Trans., 2010, 41B: 1194
[7] Sasaki M, Ohsasa K, Kudoh M, et al.Refinement of austenite grain in carbon steel by addition of titanium and boron[J]. ISIJ Int., 2008, 48: 340
[8] Watanabe T, Shiroki M, Yanagisawa A, et al.Improvement of mechanical properties of ferritic stainless steel weld metal by ultrasonic vibration[J]. J. Mater. Process. Technol., 2010, 210: 1646
[9] Lu J Z, Luo K Y, Zhang Y K, et al.Grain refinement mechanism of multiple laser shock processing impacts on ANSI 304 stainless steel[J]. Acta Mater., 2010, 58: 5354
[10] Abbasi-Khazaei B, Ghaderi S.A novel process in semi-solid metal casting[J]. J. Mater. Sci. Technol., 2012, 28: 946
[11] Li Q S, Song C J, Li H B, et al.Effect of pulsed magnetic field on microstructure of 1Cr18Ni9Ti austenitic stainless steel[J]. Mater. Sci. Eng., 2007, A466: 101
[12] Spitzer K H, Dubke M, Schwerdtfeger K.Rotational electromagnetic stirring in continuous casting of round strands[J]. Metall. Mater. Trans., 1986, 17B: 119
[13] Galindo V, Grants I, Lantzsch R, et al.Numerical and experimental modeling of the melt flow in a traveling magnetic field for vertical gradient freeze crystal growth[J]. J. Cryst. Growth, 2007, 303: 258
[14] Hernández F C R, Sokolowski J H. Comparison among chemical and electromagnetic stirring and vibration melt treatments for Al-Si hypereutectic alloys[J]. J. Alloys Compd., 2006, 426: 205
[15] Nafisi S, Emadi D, Shehata M T, et al.Effects of electromagnetic stirring and superheat on the microstructural characteristics of Al-Si-Fe alloy[J]. Mater. Sci. Eng., 2006, A432: 71
[16] Lu D H, Jiang Y H, Guan G S, et al.Refinement of primary Si in hypereutectic Al-Si alloy by electromagnetic stirring[J]. J. Mater. Process. Technol., 2007, 189: 13
[17] Chen Z, Wen X L, Chen C L.Fluid flow and microstructure formation in a rotating magnetic field during the directional solidification process[J]. J. Alloys Compd., 2010, 491: 395
[18] Campanella T, Charbon C, Rappaz M.Grain refinement induced by electromagnetic stirring: A dendrite fragmentation criterion[J]. Metall. Mater. Trans., 2004, 35A: 3201
[19] Harada H, Toh T, Ishii T, et al.Effect of magnetic field conditions on the electromagnetic braking efficiency[J]. ISIJ Int., 2001, 41: 1236
[20] Shercliff J A.Thermoelectric magnetohydrodynamics in closed containers[J]. Phys. Fluid., 1979, 22: 635
[21] Li X, Gagnoud A, Ren Z M, et al.Investigation of thermoelectric magnetic convection and its effect on solidification structure during directional solidification under a low axial magnetic field[J]. Acta Mater., 2009, 57: 2180
[22] Lehmann P, Moreau R, Camel D, et al.Modification of interdendritic convection in directional solidification by a uniform magnetic field[J]. Acta Mater., 1998, 46: 4067
[23] Dold P, Szofran F R, Benz K W.Thermoelectromagnetic convection in vertical Bridgman grown germanium-silicon[J]. J. Cryst. Growth, 2006, 291: 1
[24] Li X, Gagnoud A, Fautrelle Y, et al.Dendrite fragmentation and columnar-to-equiaxed transition during directional solidification at lower growth speed under a strong magnetic field[J]. Acta Mater., 2012, 60: 3321
[25] Li X, Ren Z M, Shen Y, et al.Effect of thermoelectric magnetic force on the array of dendrites during directional solidification of Al-Cu alloys in a high magnetic field[J]. Philos. Mag. Lett., 2012, 92: 675
[26] Li X, Fautrelle Y, Zaidat K, et al.Columnar-to-equiaxed transitions in Al-based alloys during directional solidification under a high magnetic field[J]. J. Cryst. Growth, 2010, 312: 267
[27] Yu J B, Du D F, Ren Z M, et al.Influence of an axial magnetic field on microstructures and alignment in directionally solidified Ni-based superalloy[J]. ISIJ Int., 2017, 57: 337
[28] Kato T, Jones H, Kirkwood D H.Segregation and eutectic formation in solidification of Fe-1C-1.5Cr steel[J]. Mater. Sci. Technol., 2003, 19: 1070
[29] Baltaretu F, Wang J, Letout S, et al.Thermoelectric effects on electrically conducting particles in liquid metal[J]. Magnetohydrodynamics, 2015, 51: 45
[30] Wang J, Fautrelle Y, Nguyen-Thi H, et al.Thermoelectric magnetohydrodynamic flows and their induced change of solid-liquid interface shape in static magnetic field-assisted directional solidification[J]. Metall. Mater. Trans., 2017, 47A: 1
[31] Kurz W, Fisher D J.Fundamentals of Solidification[M]. 3rd Ed., Switzerland: Trans Tech Publications. Ltd., 1992: 80
[32] Wang W L, Luo S, Zhu M Y.Dendritic growth of high carbon iron-based alloy under constrained melt flow[J]. Comput. Mater. Sci., 2014, 95: 136
[33] Taniguchi S, Brimacombe J K.Application of pinch force to the separation of inclusion particles from liquid steel[J]. ISIJ Int., 1994, 34: 722
[34] Enderby J E, Dupree B C.The thermoelectric power of liquid Fe, Co and Ni[J]. Philos. Mag., 1977, 35: 791
[35] Hellawell A, Liu S, Lu S Z.Dendrite fragmentation and the effects of fluid flow in castings[J]. JOM, 1997, 49(3): 18
[36] Zimmermann G, Pickmann C, Hamacher M, et al.Fragmentation-driven grain refinement in directional solidification of AlCu10wt-% alloy at low pulling speeds[J]. Acta Mater., 2017, 126: 236
[37] Flemings M C.Behavior of metal alloys in the semisolid state[J]. Metall. Trans., 1991, 22B: 269
[38] Hunt J D.Steady state columnar and equiaxed growth of dendrites and eutectic[J]. Mater. Sci. Eng., 1984, 65: 75
[39] Cai B, Wang J, Kao A, et al.4D synchrotron X-ray tomographic quantification of the transition from cellular to dendrite growth during directional solidification[J]. Acta Mater., 2016, 117: 160
[40] Ruvalcaba D, Mathiesen R H, Eskin D G, et al.In situ observations of dendritic fragmentation due to local solute-enrichment during directional solidification of an aluminum alloy[J]. Acta Mater., 2007, 55: 4287
[41] Ananiev S, Nikrityuk P, Eckert K.Dendrite fragmentation by catastrophic elastic remelting[J]. Acta Mater., 2009, 57: 657
[42] Luo S, Zhu M Y, Louhenkilpi S.Numerical simulation of solidification structure of high carbon steel in continuous casting using cellular automaton method[J]. ISIJ Int., 2012, 52: 823
文章导航

/