氘、氚在RAFM钢中的扩散渗透研究

  • 范东军 ,
  • 陆光达 ,
  • 张桂凯 ,
  • 包锦春 ,
  • 杨飞龙 ,
  • 向鑫 ,
  • 陈长安
展开
  • 1 表面物理与化学重点实验室 绵阳 621908
    2 中国工程物理研究院 绵阳 621907

作者简介 范东军,男,1993年生,硕士生

收稿日期: 2017-09-05

  网络出版日期: 2018-01-15

基金资助

国家磁约束核聚变能发展研究专项项目No.2015GB109006和国家自然科学基金项目No.51471154

Deuterium and Tritium Permeation in the Reduced Activation Ferritic/Martensitic Steel

  • Dongjun FAN ,
  • Guangda LU ,
  • Guikai ZHANG ,
  • Jinchun BAO ,
  • Feilong YANG ,
  • Xin XIANG ,
  • Chang'an CHEN
Expand
  • 1 Science and Technology on Surface Physics and Chemistry Laboratory, Mianyang 621908, China
    2 China Academy of Engineering Physics, Mianyang 621907, China

Received date: 2017-09-05

  Online published: 2018-01-15

Supported by

Supported by National Magnetic Confinement Nuclear Fusion Program (No.2015GB109006) and National Natural Science Foundation of China (No.51471154)

摘要

采用气相渗透方法,对国产低活化铁素体/马氏体钢(RAFM钢)之一的中国低活化马氏体钢(CLAM钢)进行了氘(D)、氚(T)渗透实验,得出了573~873 K间,氘在CLAM钢中的渗透率ΦD=3.41×10-8exp(-39181/(RT)) (mol/(msPa0.5)),扩散系数DD=1.43×10-7exp(-22110/(RT)) (m2/s),溶解度常数SD=2.38×10-1exp(-17071/(RT)) (mol/(m3Pa0.5))。在573~823 K间,氚在CLAM钢中的渗透率为ΦT=2.50×10-8exp(-38493/(RT)) (mol/(msPa0.5)),并根据渗透的同位素效应比值,推导出氚在CLAM钢中的扩散系数DT=1.95×10-7exp(-22797/(RT)) (m2/s),溶解度常数ST=1.28×10-1exp(-15696/(RT)) (mol/(m3Pa0.5))。实验还发现,风冷降温使钢的氘渗透通量出现先升后降的异常现象,其产生的机制及其对工程应用的影响有待进一步研究。

关键词: 氘(D); 氚(T); RAFM钢; 气相渗透

本文引用格式

范东军 , 陆光达 , 张桂凯 , 包锦春 , 杨飞龙 , 向鑫 , 陈长安 . 氘、氚在RAFM钢中的扩散渗透研究[J]. 金属学报, 2018 , 54(4) : 519 -526 . DOI: 10.11900/0412.1961.2017.00373

Abstract

Reduced activation ferritic/martensitic (RAFM) steel is the preferred structural material for test blanket module in fusion reactor. The study of the diffusion transport character of deuterium and tritium in the steel is of great significance for fuel recycling, tritium diffusion control, recovery and safety to China Fusion Engineering Test Reactor (CFETR) item. Two kind of RAFM steels have been developed in China and one of them, China low activation martensitic (CLAM) steel, is chosen to investigate its diffusive transport parameters of deuterium and tritium in this work. By gas-driven permeation experiment between 573 K and 873 K, deuterium transport parameters are measured. The permeability is: ΦD=3.41×10-8exp(-39181/(RT)) (mol/(msPa0.5)), the diffusion coefficient is DD=1.43×10-7exp(-22110/(RT)) (m2/s), the solubility constant is SD=2.38×10-1exp(-17071/(RT)) (mol/(m3Pa0.5)). Between 573 K and 823 K, the permeability of tritium is ΦT=2.50×10-8exp(-38493/(RT)) (mol/(msPa0.5)). According to the isotopes effect rule, the diffusion coefficient and solubility constant of tritium is deduced respectively: DT=1.95×10-7 exp(-22797/(RT)) (m2/s) and ST=1.28×10-1exp(-15696/(RT)) (mol/(m3Pa0.5)). A strange behavior appears in experiments with deuterium: after forced air cooling to the steel, the permeation flux through it quickly rise first and then anomaly lower for hours. The mechanism arousing the phenomenon and effects on use in engineering needs further investigation.

参考文献

[1] Jones R H, Heinisch H L, McCarthy K A. Low activation materials [J]. J. Nucl. Mater., 1999, 271-272: 518
[2] Kohno Y, Kohyama A, Hirose T, et al. Mechanical property changes of low activation ferritic/martensitic steels after neutron irradiation [J]. J. Nucl. Mater., 1999, 271-272: 145
[3] Ehrlich K, Bloom E E, Kondo T. International strategy for fusion materials development [J]. J. Nucl. Mater., 2000, 283-287: 79
[4] Van Der Schaaf B, Gelles D S, Jitsukawa S, et al. Progress and critical issues of reduced activation ferritic/martensitic steel development [J]. J. Nucl. Mater., 2000, 283-287: 52
[5] Ehrlich K. Materials research towards a fusion reactor [J]. Fusion Eng. Des., 2001, 56-57: 71
[6] Muroga T, Gasparotto M, Zinkle S J. Overview of materials research for fusion reactors [J]. Fusion Eng. Des., 2002, 61-62: 13
[7] Klueh R L, Gelles D S, Jitsukawa S, et al. Ferritic/martensitic steels—Overview of recent results [J]. J. Nucl. Mater., 2002, 307-311: 455
[8] Wang P H, Nobuta Y, Hino T, et al.Helium retention and desorption behaviour of reduced activation ferritic/martenstic steel[J]. Plasma Sci. Technol., 2009, 11: 225
[9] Dolinsky Y N, Zouev Y N, Lyasota I A, et al. Permeation of deuterium and tritium through the martensitic steel F82H [J]. J. Nucl. Mater., 2002, 307-311: 1484
[10] Aiello A, Ricapito I, Benamati G, et al.Hydrogen isotopes permeability in Eurofer 97 martensitic steel[J]. Fusion Sci. Technol., 2002, 41: 872
[11] Klueh R L, Alexander D J, Rieth M.The effect of tantalum on the mechanical properties of a 9Cr-2W-0.25V-0.07Ta-0.1C steel[J]. J. Nucl. Mater., 1999, 273: 146
[12] Huang Q Y, Li C J, Li Y F, et al.R&D status of China low activation martensitic steel [A]. CORPHY-2008[C]. Hefei: Chinese Nuclear Society, 2008: 41(黄群英, 李春京, 李艳芬等. 中国低活化马氏体钢CLAM研究进展 [A].第十二届反应堆数值计算与粒子输运学术会议暨2008年反应堆物理会议[C]. 合肥: 中国核学会, 2008: 41)
[13] Zhao F, Qiao J S, Huang Y N, et al.Effect of irradiation temperature on void swelling of China low activation martensitic steel (CLAM)[J]. Mater. Charact., 2008, 59: 344
[14] Liu S J, Huang Q Y, Peng L, et al.Microstructure and its influence on mechanical properties of CLAM steel[J]. Fusion Eng. Des., 2012, 87: 1628
[15] Wang P H, Fu H Y, Chen J M, et al.Thermal ageing effect on the microstructure and mechanical properties of RAFM steel CLF-1[J]. Prog. Rep. China Nucl. Sci. Technol., 2009, 1: 56(王平怀, 付海英, 谌继明等. 时效处理对低活性铁素体/马氏体钢CLF-1组织及性能的影响[J]. 中国核科学技术进展报告, 2009, 1: 56)
[16] Wang P H, Chen J M, Fu H Y, et al.Technical issues for the fabrication of a CN-HCCB-TBM based on RAFM Steel CLF-1[J]. Plasma Sci. Technol., 2013, 15: 133
[17] Wang B, Liu L B, Xiang X, et al.Diffusive transport parameters of deuterium through China reduced activation ferritic-martensitic steels[J]. J. Nucl. Mater., 2016, 470: 30
[18] Liu L B, Dou T J, Wang B, et al.Thermal desorption behavior of retained deuterium in Chinese RAFM steel[J]. Mater. Rev., 2016, 30(14): 10(刘凌博, 窦天军, 王博等. 中国RAFM钢中驻留氘的热脱附行为研究[J]. 材料导报, 2016, 30(14): 10)
[19] He W B, Chen C A, Wang J J, et al.Exploring of tritium and helium behaviors in RAFM steels[J]. Mater. Rev., 2015, 29(17): 101(何伟波, 陈长安, 王佳佳等. RAFM钢中氚氦行为的研究进展[J]. 材料导报, 2015, 29(17): 101)
[20] Dolinski Y, Lyasota I, Shestakov A, et al. Heavy hydrogen isotopes penetration through austenitic and martensitic steels [J]. J. Nucl. Mater., 2000, 283-287: 854
[21] Zouev Y N, Podgornova I V, Sagaragze V V. Visualization of tritium distribution by autoradiography technique [J]. Fusion Eng. Des., 2000, 49-50: 971
[22] Otsuka T, Shimada M, Kolasinski R, et al.Application of tritium imaging plate technique to examine tritium behaviors on the surface and in the bulk of plasma-exposed materials[J]. J. Nucl. Mater., 2011, 415(suppl.1): S769
[23] Fedorov A V, Van Til S, Magielsen A J, et al.Tritium permeation in EUROFER in EXOTIC and LIBRETTO irradiation experiments[J]. Fusion Eng. Des., 2013, 88: 2918
[24] Jiang G Q, Luo D L, Lu G D, et al.Tritium and Industry Techniques of Tritium [M]. Beijing: National Defense Industry Press, 2007: 54(蒋国强, 罗德礼, 陆光达等. 氚和氚的工程技术 [M]. 北京: 国防工业出版社, 2007: 54)
[25] Pisarev A, Shestakov V, Kulsartov S, et al.Surface effects in diffusion measurements: Deuterium permeation through martensitic steel[J]. Phys. Scr., 2001, T94: 121
[26] Richardson O W.XXV. The solubility and diffusion in solution of dissociated gases[J]. Philos. Mag., 1904, 7: 266
[27] Nakamura H, Isobe K, Nakamichi M, et al.Evaluation of deuterium permeation reduction factor of various coatings deposited on ferritic/martensitic steels for development of tritium permeation barrier[J]. Fusion Eng. Des., 2010, 85: 1531
[28] Crank J.The Mathematics of Diffusion [M]. 2nd Ed., Oxford: Clarendon Press, 1975: 17
[29] Latanision R M, Kurkela M.Hydrogen permeability and diffusivity in nickel and Ni-base alloys[J]. Corrosion, 1983, 39: 174
[30] Sun X K, Xu J A, Li Y Y.Hydrogen permeation behavior in austenitic stainless-steels[J]. Mater Sci. Eng., 1989, A114: 179
[31] Wang P X, Song J S.Helium in Materials and the Permeation of Tritium [M]. Beijing: National Defense Industry Press, 2002: 81(王佩璇, 宋家树. 材料中的氦及氚渗透 [M]. 北京: 国防工业出版社, 2002: 81)
[32] Noh S J, Lee S K, Byeon W J, et al.Transport of hydrogen and deuterium in the reduced activation martensitic steel ARAA[J]. Fusion Eng. Des., 2014, 89: 2726
[33] Esteban G A, Pe?a A, Legarda F, et al.Hydrogen transport and trapping in ODS-EUROFER[J]. Fusion Eng. Des., 2007, 82: 2634
[34] Esteban G A, Perujo A, Douglas K, et al.Tritium diffusive transport parameters and trapping effects in the reduced activating martensitic steel OPTIFER-IVb[J]. J. Nucl. Mater., 2000, 281: 34
[35] Forcey K S, Ross D K, Simpson J C B, et al. Hydrogen transport and solubility in 316L and 1.4914 steels for fusion reactor applications[J]. J. Nucl. Mater., 1988, 160: 117
[36] Serra E, Benamati G.Hydrogen behaviour in aged low activation martensitic steel F82H for fusion reactor applications[J]. Mater. Sci. Technol., 1998, 14: 573
[37] Serra E, Perujo A, Benamati G.Influence of traps on the deuterium behaviour in the low activation martensitic steels F82H and Batman[J]. J. Nucl. Mater., 1997, 245: 108
[38] Zhang G K, Huang G Q, Hu M J, et al.Stability and clusterization of hydrogen-vacancy complexes in B2-FeAl: Insight from hydrogen embrittlement[J]. RSC Adv., 2017, 7: 11094
文章导航

/