低偏析异质籽晶制备单晶高温合金的籽晶熔合区形成机制研究

  • 郭静 ,
  • 李金国 ,
  • 刘纪德 ,
  • 黄举 ,
  • 孟祥斌 ,
  • 孙晓峰
展开
  • 1 中国科学院大学 北京 100049
    2 中国科学院金属研究所 沈阳 110016
    3 东北大学材料科学与工程学院 沈阳 110819

作者简介 郭 静,男,1991年生,硕士

收稿日期: 2017-04-21

  网络出版日期: 2017-10-31

基金资助

资助项目 国家自然科学基金项目Nos.51331005和U1508213

Formation Mechanism of Fusion Zone in Growth of Single Crystal Superalloy with Low-Segregated Heterogeneous Seed

  • Jing GUO ,
  • Jinguo LI ,
  • Jide LIU ,
  • Ju HUANG ,
  • Xiangbin MENG ,
  • Xiaofeng SUN
Expand
  • 1 University of Chinese Academy of Science, Beijing 100049, China
    2 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    3 School of Materials Science and Engineering, Northeastern University, Shenyang 110819, China

Received date: 2017-04-21

  Online published: 2017-10-31

Supported by

Supported by National Natural Science Foundation of China (Nos.51331005 and U1508213)

摘要

采用低偏析异质籽晶法研究了定向凝固制备单晶高温合金时籽晶熔合区的形成机制,利用SEM和EPMA对籽晶熔合区的组织以及元素分布进行分析。结果表明,籽晶回熔平衡界面前沿存在一个无微观偏析的熔合区,该区域是凝固界面发生平面状-胞状失稳转变的过渡区。增加籽晶材料中W含量或提高定向凝固速率均会促进凝固界面的平面状-胞状失稳转变,且凝固速率的影响更显著。相比于传统籽晶法,低偏析异质籽晶熔合区内的平界面凝固能有效避免籽晶回熔界面的枝晶熔断和成分过冷导致的杂晶形核,从而提高单晶的引晶生长成功率。

本文引用格式

郭静 , 李金国 , 刘纪德 , 黄举 , 孟祥斌 , 孙晓峰 . 低偏析异质籽晶制备单晶高温合金的籽晶熔合区形成机制研究[J]. 金属学报, 2018 , 54(3) : 419 -427 . DOI: 10.11900/0412.1961.2017.00144

Abstract

Seeding technique is a promising method for growing single crystal superalloy blade. However, sometimes stray grains nucleate in the transformation process of single crystal structure from a seed, which always cause failure of single crystal growth. In order to obtain single crystal with high perfection structure, Ni-based single crystal superalloy was prepared with low-segregated seeds by high rate solidification (HRS) method in the dual heating zone furnace. The melt-back zones of seeds were investigated systematically, and the results showed that a fusion zone without microsegregation exists in front of the melt-back equilibrium interface of seeds, in which solidification interface transited from planar to cellular. Further experiments showed that increasing the W content of seeds or the solidification rate can both accelerate the whole non-steady transition process and make fusion zone shrink. Compared with the traditional seeding method, the low segregated heterogeneous seeding technique can increase the casting yield by avoiding the nucleation of stray grains in the fusion zone, which caused by the pinched-off secondary dendrites and constitutional undercooling.

参考文献

[1] Guo J T.The current situation of application and development of superalloys in the fields of energy industry[J]. Acta Metall. Sin., 2010, 46: 513(郭建亭. 高温合金在能源工业领域中的应用现状与发展 [J]. 金属学报, 2010, 46: 513)
[2] Guo J T.Materials Science and Engineering for Superalloys [M]. Beijing: Science Press, 2008: 4(郭建亭. 高温合金材料学(应用基础理论) [M]. 北京: 科学出版社, 2008: 4)
[3] Reed R C.The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2008: 1
[4] Chen W.Investigation of high strength superalloy used for investment casted combustor casing of high thrust-weight ratio aeroengine [D]. Nanjing: Nanjing University of Science and Technology, 2007(陈伟. 高推重比航空发动机整体精铸燃烧室机匣用高强度高温合金研究 [D]. 南京: 南京理工大学, 2007)
[5] Hu Z Q, Liu L R, Jin T, et al.Development of the Ni-base single crystal superalloys[J]. Aeroengine, 2005, 31(3): 1(胡壮麒, 刘丽荣, 金涛等. 镍基单晶高温合金的发展 [J]. 航空发动机, 2005, 31(3): 1)
[6] Meng X B, Lu Q, Zhang X L, et al.Mechanism of competitive growth during directional solidification of a nickel-base superalloy in a three-dimensional reference frame[J]. Acta Mater., 2012, 60: 3965
[7] Zhou Y Z, Volek A, Green N R.Mechanism of competitive grain growth in directional solidification of a nickel-base superalloy[J]. Acta Mater., 2008, 56: 2631
[8] Wang W, Lee P D, McLean M. A model of solidification microstructures in nickel-based superalloys: Predicting primary dendrite spacing selection[J]. Acta Mater., 2003, 51: 2971
[9] Ford D A, Hill A D.Single crystal seed alloy [P]. US Pat, 6740176, 2004
[10] Toloraiya V N, Orekhov N G, Kablov E N.Advanced method for single crystal casting of turbine blades for gas turbine engines and plants[J]. Met. Sci. Heat Treat., 2002, 44: 279
[11] Azhazha V M, Sverdlov V Y, Ladygin A N, et al.Self-organization processes in the cellular structure formation of Ni-W alloys[J]. J. Surf. Invest., 2008, 2: 156
[12] Azhazha V M, Ladygin A N, Sverdlov V J, et al.Morphological transition in the cellular structure of single crystals of nickel-tungsten alloys near the congruent melting point[J]. Crystallogr. Rep., 2005, 50(suppl.): S130
[13] Azhazha V M, Gorbenko V Y, Kovtun G P, et al.The growth of single crystals of Ni-W alloy under conditions of high temperature gradient[J]. Crystallogr. Rep., 2004, 49: 307
[14] Zhao N R, Li J G, Liu J L, et al.Solidification interface in growth of single crystal superalloys by seeding technique[J]. J. Mater. Eng., 2007,(11): 24(赵乃仁, 李金国, 刘金来等. 籽晶法生长高温合金单晶凝固界面研究 [J]. 材料工程, 2007, (11): 24)
[15] Zhou Y H, Hu Z Q, Jie W Q.Solidification Technology [M]. Beijing: China Machine Press, 1998: 6(周尧和, 胡壮麒, 介万奇. 凝固技术 [M]. 北京: 机械工业出版社, 1998: 6)
[16] Hu H Q.Fundamentals of Metal Solidification [M]. Beijing: China Machine Press, 1991: 75(胡汉起. 金属凝固原理 [M]. 北京: 机械工业出版社, 1991: 75)
[17] Stanford N, Djakovic A, Shollock B A, et al.Defect grains in the melt-back region of CMSX-4 single crystal seeds [A]. 10th International Symposium on Superalloys[C]. Warrendale, PA: TMS, 2004: 719
[18] Stanford N, Djakovic A, Shollock B A, et al.Seeding of single crystal superalloys-role of seed melt-back on casting defects[J]. Scr. Mater., 2004, 50: 159
[19] Zhao X B, Liu L, Zhang W G, et al.Analysis of competitive growth mechanism of stray grains of single crystal superalloys during directional solidification process[J]. Rare Met. Mater. Eng., 2011, 40: 9
[20] Yang X L, Ness D, Lee P D, et al. Simulation of stray grain formation during single crystal seed melt-back and initial withdrawal in the Ni-base superalloy CMSX4 [J]. Mater. Sci. Eng., 2005, A413-414: 571
[21] Mullins W W, Sekerka R F.Morphological stability of a particle growing by diffusion or heat flow[J]. J. Appl. Phys., 1963, 34: 323
[22] Mullins W W, Sekerka R F.Stability of a planar interface during solidification of a dilute binary alloy[J]. J. Appl. Phys., 1964, 35: 444
[23] Kurz W, Fisher D J.Fundamentals of Solidification[M]. Switzerland: Trans Tech Publications, 1986: 58
[24] Fu H Z, Wang Z J.Non-steady evolution of subhigh rate unidirectional solidification[J]. Chin. J. Mater. Res., 1996, 10: 253(傅恒志, 王祖锦. 亚快速单向凝固晶体生长的非稳态演化 [J]. 材料研究学报, 1996, 10: 253)
[25] Huang W D, Ding G L, Zhou Y H.Effects of non-steady state process on the interface pattern selection during unidirectional solidification[J]. Chin. J. Mater. Res., 1995, 9: 193(黄卫东, 丁国陆, 周尧和. 非稳态过程与凝固界面形态选择 [J]. 材料研究学报, 1995, 9: 193)
[26] D'souza N, Jennings P A, Yang X L, et al. Seeding of single-crystal superalloys—Role of constitutional undercooling and primary dendrite orientation on stray-grain nucleation and growth[J]. Metall. Mater. Trans., 2005, 36B: 657
[27] Gu J P, Beckermann C, Giamei A F.Motion and remelting of dendrite fragments during directional solidification of a nickel-base superalloy[J]. Metall. Mater. Trans., 1997, 28A: 1533
[28] Yang X L, Lee P D, D'Souza N. Stray grain formation in the seed region of single-crystal turbine blades[J]. JOM, 2005, 57(5): 40
[29] Zhou Y Z.Formation of stray grains during directional solidification of a nickel-based superalloy[J]. Scr. Mater., 2011, 65: 281
[30] Zhang X L.Fundamental research on production of single crystal superalloys by directional solidification [D]. Shenyang: Institute of Metal Research, Chinese Academy of Sciences, 2013(张小丽. 单晶高温合金定向凝固制备的基础研究 [D]. 沈阳: 中国科学院金属研究所, 2013)