高强7050铝合金超低温大变形加工与组织、性能调控
作者简介 侯陇刚,男,1982年生,博士
收稿日期: 2017-02-15
网络出版日期: 2017-06-15
基金资助
国家自然科学基金项目No.51401016,中央高校基本科研业务费专项资金项目No;FRF-TP-12-137A,现代交通金属材料与加工技术北京实验室项目及新金属材料国家重点实验室基金项目No.2011Z-05
Cryogenic Processing High-Strength 7050 Aluminum Alloy and Controlling of the Microstructures and Mechanical Properties
Received date: 2017-02-15
Online published: 2017-06-15
Supported by
Supported by National Natural Science Foundation of China (No.51401016), Fundamental Research Funds for the Central Universities of China (No.FRF-TP-12-137A), Beijing Laboratory of Metallic Materials and Processing for Modern Transportation, and Funds from State Key Laboratory of Advanced Metals and Materials (No.2011Z-05)
通过低温冷却+轧制变形的方法研究了高强7050铝合金的低温塑性变形及其对合金组织性能的影响。结果表明,高强7050铝合金经液氮冷却预处理后可实现与温/热轧相比较高的轧制变形加工量,并产生大量亚结构和高密度位错,使合金显著强化,其中低温下的高变形能力主要与合金在低温下具有高的加工硬化能力密切相关,而强度提升主要来自于固溶强化和变形位错强化的贡献。虽然超低温变形能够明显加快淬火态高强7050铝合金的时效进程,但直接时效处理可使超低温变形态7050铝合金保有较高的强度和一定延伸率,其中析出和位错强化是其强化主因,而时效引起的回复和强化相析出共同促进延伸率的改善。淬火态高强7050铝合金在室温变形过程中,形变热引起基体中析出的溶质原子团簇(或GP区)和η′相与变形位错发生交互作用,导致大量剪切带(失稳区)形成,从而易引发轧板开裂或边裂,而超低温变形过程中溶质扩散受阻以致强化相析出被抑制,从而明显降低了剪切失稳区的发生,使合金能够获得均匀、稳定的塑性变形或良好的加工硬化,确保获得较高质量的超低温轧板。高强铝合金在低温下所表现出来的优异塑性变形和加工能力有望成为改善高强铝合金难变形加工的有效途径。
侯陇刚 , 刘明荔 , 王新东 , 庄林忠 , 张济山 . 高强7050铝合金超低温大变形加工与组织、性能调控[J]. 金属学报, 2017 , 53(9) : 1075 -1090 . DOI: 10.11900/0412.1961.2017.00047
The high strength or flow stress as well as low plastic deformability of 7000 series Al alloys makes it difficult to improve their microstructures and mechanical properties by cold processing, and many advanced alloying methods and processing technologies are continually developed for higher mechanical properties and acceptable elongation. In this work, the cryogenic deformation (rolling) was applied to process high-strength 7050 Al alloys, and its effects on the microstructures and mechanical properties were studied. The results showed that after the pre-cooling with liquid nitrogen, the quenched 7050 Al alloy can obtain much higher rolling reduction, similar to that under warm or hot rolling, and a great number of substructures and high-density dislocations were formed which greatly increased the strength. The higher cryogenic deformability would be mainly related with the higher work-hardening ability at low temperature, while the strength enhancement would be largely attributed to the solution strengthening and dislocation strengthening. The cryogenic deformation can obviously stimulate the ageing process of the quenched 7050 Al alloy, but the direct ageing of the cryogenic-rolling 7050 Al alloy can assure higher strength and acceptable elongation, which would be greatly attributed to the precipitation strengthening and dislocation strengthening, while the recovery and ageing-induced precipitates help improving the tensile elongation. During room-temperature rolling, the formation of GP zones and η′ phases caused by the heats transformed from the deformation as well as their interaction with dislocations leads to the appearance of amounts of shear bands (instability areas), which will easily cause the cracking or edge-cracking of the rolling sheets. However, the cryogenic rolling with distinctly impeding the solute diffusion can result in the suppression of precipitation of the strengthening phases so as to decrease the occurrence of the shear instability areas, and uniform and stable plastic deformation or good work-hardening as well as high-quality rolling sheets are obtained. The excellent plastic deformability of high-strength Al alloys at cryogenic temperatures could be suggested as an effective way to improve the processing of high-strength Al alloys.
| [1] | Prangnell P B, Bowen J R, Berta M, et al. Stability of ultra-fine 'grain structures' produced by severe deformation [J]. Mater. Sci. Forum, 2004, 467-470: 1261 |
| [2] | Zhang H W, Huang X, Pippan R, et al.Thermal behavior of Ni (99.967% and 99.5% purity) deformed to an ultra-high strain by high pressure torsion[J]. Acta Mater., 2010, 58: 1698 |
| [3] | Chandler H D, Bee J V.Cyclic strain induced precipitation in a solution treated aluminium alloy[J]. Acta Metall., 1987, 35: 2503 |
| [4] | Sha G, Wang Y B, Liao X Z, et al.Influence of equal-channel angular pressing on precipitation in an Al-Zn-Mg-Cu alloy[J]. Acta Mater., 2009, 57: 3123 |
| [5] | Engler O, Tome C N, Huh M Y.A study of through-thickness texture gradients in rolled sheets[J]. Metall. Mater. Trans., 2000, 31A: 2299 |
| [6] | Boldetti C, Pinna C, Howard I C, et al.Measurement of deformation gradients in hot rolling of AA3004[J]. Exp. Mech., 2005, 45: 517 |
| [7] | Humphreys F J, Prangnell P B, Bowen J R, et al.Developing stable fine-grain microstructures by large strain deformation[J]. Phil. Trans. R. Soc., 1999, 357A: 1663 |
| [8] | Pippan R, Scheriau S, Taylor A, et al.Saturation of fragmentation during severe plastic deformation[J]. Annu. Rev. Mater. Res., 2010, 40: 319 |
| [9] | Furui M, Kawakami T, Saji S, et al.Stored energy and its release behavior during recovery and recrystallization processes for aluminum alloys rolled at cryogenic temperature[J]. J. Jpn. Inst. Light Met., 2002, 52(8): 339 |
| [10] | Roumina R, Sinclair C W.Deformation geometry and through-thickness strain gradients in asymmetric rolling[J]. Metall. Mater. Trans., 2008, 39A: 2495 |
| [11] | Li S Y, Sun F W, Li H.Observation and modeling of the through-thickness texture gradient in commercial-purity aluminum sheets processed by accumulative roll-bonding[J]. Acta Mater., 2010, 58: 1317 |
| [12] | Wigley D A.Mechanical Properties of Materials at Low Temperatures [M]. New York-London: Plenum Press, 1971: 16 |
| [13] | Khan A S, Meredith C S.Thermo-mechanical response of Al 6061 with and without equal channel angular pressing (ECAP)[J]. Int. J. Plast., 2010, 26: 189 |
| [14] | Schneider R, Heine B, Grant R J.Mechanical behaviour of commercial aluminium wrought alloys at low temperatures [A]. Light Metal Alloys Applications[C]. Rijeka: InTech, 2014: 61 |
| [15] | Puchi-Cabrera E S, Staia M H, Ochoa-Pérez E, et al. Flow stress and ductility of AA7075-T6 aluminum alloy at low deformation temperatures[J]. Mater. Sci. Eng., 2011, A528: 895 |
| [16] | Senkov O N, Bhat R B, Senkova S V.High strength aluminum alloys for cryogenic applications [A]. Metallic Materials with High Structural Efficiency. NATO Science Series II: Mathematics, Physics and Chemistry[C]. Netherlands: Springer, 2004: 151 |
| [17] | Kaufman J G.Properties of Aluminum Alloys: Tensile, Creep, and Fatigue Data at High and Low Temperatures[M]. Materials Park: ASM International, 1999: 1 |
| [18] | Park J H, Park K T, Lee Y S, et al.Comparison of compressive deformation of ultrafine-grained 5083 Al alloy at 77 and 298 K[J]. Metall. Mater. Trans., 2005, 36A: 1365 |
| [19] | Saimoto S, Lloyd D J.A new analysis of yielding and work hardening in AA1100 and AA5754 at low temperatures[J]. Acta Mater., 2012, 60: 6352 |
| [20] | Zhou F, Nutt S R, Bampton C C, et al.Nanostructure in an Al-Mg-Sc alloy processed by low-energy ball milling at cryogenic temperature[J]. Metall. Mater. Trans., 2003, 34A: 1985 |
| [21] | Yildiz Y, Nalbant M.A review of cryogenic cooling in machining processes[J]. Int. J. Mach. Tools Manufact., 2008, 48: 947 |
| [22] | Rao P N, Singh D, Jayaganthan R.Mechanical properties and microstructural evolution of Al 6061 alloy processed by multidirectional forging at liquid nitrogen temperature[J]. Mater. Des., 2014, 56: 97 |
| [23] | Lee Y B, Shin D H, Park K T, et al.Effect of annealing temperature on microstructures and mechanical properties of a 5083 Al alloy deformed at cryogenic temperature[J]. Scr. Mater., 2004, 51: 355 |
| [24] | Shanmugasundaram T, Murty B S, Sarma V S.Development of ultrafine grained high strength Al-Cu alloy by cryorolling[J]. Scr. Mater., 2006, 54: 2013 |
| [25] | Zhao Y H, Liao X Z, Cheng S, et al.Simultaneously increasing the ductility and strength of nanostructured alloys[J]. Adv. Mater., 2006, 18: 2280 |
| [26] | Panigrahi S K, Jayaganthan R.A study on the combined treatment of cryorolling, short-annealing, and aging for the development of ultrafine-grained Al 6063 alloy with enhanced strength and ductility[J]. Metall. Mater. Trans., 2010, 41A: 2675 |
| [27] | Tsujiuchi Y, Kita K, Watanabe C, et al.Enhancement in strength of a Cu-1.4 mass%Ni-0.25 mass%P-0.1 mass%Zr alloy by cryo-rolling and aging[J]. J. Jpn. Inst. Met., 2013, 77(2): 55 |
| [28] | Fritsch S, Hunger S, Scholze M, et al.Optimisation of thermo mechanical treatments using cryogenic rolling and aging of the high strength aluminium alloy AlZn5.5MgCu (AA7075)[J]. Materialwiss. Werkstofftech., 2011, 42: 573 |
| [29] | Weiss M, Taylor A S, Hodgson P D, et al.Strength and biaxial formability of cryo-rolled 2024 aluminium subject to concurrent recovery and precipitation[J]. Acta Mater., 2013, 61: 5278 |
| [30] | Lang Y J.Grain refinement of 7050 aluminum alloy and its mechanical behavior by hot deformation based on strain-induced precipitation [D]. Beijing: University of Science and Technology Beijing, 2012(郎玉婧. 基于应变诱导析出的热变形细化7050铝合金及其力学行为 [D]. 北京: 北京科技大学, 2012) |
| [31] | Hodowany J.On the conversion of plastic work into heat [D]. California: California Institute of Technology, 1997 |
| [32] | Kapoor R, Nemat-Nasser S.Determination of temperature rise during high strain rate deformation[J]. Mech. Mater., 1998, 27: 1 |
| [33] | Yu H L, Tieu A K, Lu C, et al.Mechanical properties of Al-Mg-Si alloy sheets produced using asymmetric cryorolling and ageing treatment[J]. Mater. Sci. Eng., 2013, A568: 212 |
| [34] | Di Russo E, Conserva M, Buratti M, et al.A new thermo-mechanical procedure for improving the ductility and toughness of Al-Zn-Mg-Cu alloys in the transverse directions[J]. Mater. Sci. Eng., 1974, 14: 23 |
| [35] | Engler O, Kong X W, Yang P.Influence of particle stimulated nucleation on the recrystallization textures in cold deformed Al-alloys Part I——Experimental observations[J]. Scr. Mater., 1997, 37: 1665 |
| [36] | De Siqueira R P, Sandim H R Z, Raabe D. Particle stimulated nucleation in coarse-grained ferritic stainless steel[J]. Metall. Mater. Trans., 2013, 44A: 469 |
| [37] | Buha J, Lumley R N, Crosky A G.Secondary ageing in an aluminium alloy 7050[J]. Mater. Sci. Eng., 2008, A492: 1 |
| [38] | Mukhopadhyay A K, Prasad K S.Formation of plate-shaped Guinier-Preston zones during natural aging of an Al-Zn-Mg-Cu-Zr alloy[J]. Phil. Mag. Lett., 2011, 91: 214 |
| [39] | Shu W X.Solidification characteristics and strengthening-toughening mechanisms of 7xxx Al alloys with tailored Mg and Cu elements [D]. Beijing: University of Science and Technology Beijing, 2016(舒文祥. Mg和Cu元素调控的7xxx系铝合金凝固特性及强韧化机理研究 [D]. 北京: 北京科技大学, 2016) |
| [40] | Chandler H D, Bee J V.Cyclic strain induced precipitation in a solution treated aluminium alloy[J]. Acta Metall., 1987, 35: 2503 |
| [41] | Deschampsa A, Bréchet Y.Influence of predeformation and ageing of an Al-Zn-Mg alloy——II. Modeling of precipitation kinetics and yield stress[J]. Acta Mater., 1998, 47: 293 |
| [42] | Hoyt J J.On the coarsening of precipitates located on grain boundaries and dislocations[J]. Acta Metall. Mater., 1991, 39: 2091 |
| [43] | Berg L K, Gj?nnes J, Hansen V, et al.GP-zones in Al-Zn-Mg alloys and their role in artificial aging[J]. Acta Mater., 2001, 49: 3443 |
| [44] | Park J K, Ardell A J.Microstructures of the commercial 7075 Al Alloy in the T651 and T7 tempers[J]. Metall. Trans., 1983, 14A: 1957 |
| [45] | Deschamps A, Bréchet Y.Nature and distribution of quench-induced precipitation in an Al-Zn-Mg-Cu alloy[J]. Scr. Mater., 1998, 39: 1517 |
| [46] | Sha G, Cerezo A.Early-stage precipitation in Al-Zn-Mg-Cu alloy (7050)[J]. Acta Mater., 2004, 52: 4503 |
| [47] | Gubicza J, Schiller I, Chinh N Q, et al. The effect of severe plastic deformation on precipitation in supersaturated Al-Zn-Mg alloys [J]. Mater. Sci. Eng., 2007, A460-461: 77 |
| [48] | Ma K K, Hu T, Yang H, et al.Coupling of dislocations and precipitates: impact on the mechanical behavior of ultrafine grained Al-Zn-Mg alloys[J]. Acta Mater., 2016, 103: 153 |
| [49] | Hu T, Ma K, Topping T D, et al.Precipitation phenomena in an ultrafine-grained Al alloy[J]. Acta Mater., 2013, 61: 2163 |
| [50] | Peeters B, Seefeldt M, Teodosiu C, et al.Work-hardening/softening behaviour of b.c.c. polycrystals during changing strain paths: I. An integrated model based on substructure and texture evolution, and its prediction of the stress-strain behaviour of an IF steel during two-stage strain paths[J]. Acta Mater., 2001, 49: 1607 |
| [51] | Robinson J M.Serrated flow in aluminium base alloys[J]. Int. Mater. Rev., 1994, 39: 217 |
| [52] | Yilmaz A.The Portevin-Le Chatelier effect: A review of experimental findings[J]. Sci. Technol. Adv. Mater., 2011, 12: 063001 |
| [53] | Picu R C.A mechanism for the negative strain-rate sensitivity of dilute solid solutions[J]. Acta Mater., 2004, 52: 3447 |
| [54] | Jiang H F.On the plastic instabilities phenomenon (Portevin-Le Chatelier effect) in Al alloys: Experiments and theoretical investigations [D]. Hefei: University of Science and Technology of China, 2006(江慧丰. Al合金中塑性失稳现象(Portevin-Le Chatelier效应)的实验和机理研究 [D]. 合肥: 中国科学技术大学, 2006) |
| [55] | Sun L, Zhang Q C, Liu H W.Influence of precipitates on the serrated yielding in Al-Cu-Mg alloy and microscopic experiment investigation[J]. J. Exp. Mech., 2007, 22: 419(孙亮, 张青川, 刘颢文. 沉淀对Al-Cu-Mg 合金中锯齿形屈服现象影响及其微观实验研究 [J]. 实验力学, 2007, 22: 419) |
| [56] | Xu Y H, Huang D Q, Wang S L.A study on serrated flow of Al Zn Mg Cu by acoustic emission[J]. J. Wuhan Univ.(Nat. Sci. Ed.), 1983, (4): 50) |
| [57] | Lebyodkin M, Brechet Y, Estrin Y, et al.Statistical behaviour and strain localization patterns in the Portevin-Le Chatelier effect[J]. Acta Mater., 1996, 44: 4531 |
| [58] | Pink E.The effect of precipitates on characteristics of serrated flow in AlZn5Mg1[J]. Acta Metall., 1989, 37: 1773 |
| [59] | Thevenet D, Mliha-Touati M, Zeghloul A.The effect of precipitation on the Portevin-Le Chatelier effect in an Al-Zn-Mg-Cu alloy[J]. Mater. Sci. Eng., 1999, A266: 175 |
| [60] | Hu Q, Zhang Q C, Fu S H, et al.Influence of precipitation on the Portevin-Le Chatelier effect in Al-Mg alloys[J]. Theor. Appl. Mech. Lett., 2011, 1: 011007 |
/
| 〈 |
|
〉 |