溶质Ti对Al-Ti-B中间合金细化Al影响的新认识:TiB2粒子的动力学行为及溶质Ti的影响
作者简介 张丽丽,女,1987年生,博士生
收稿日期: 2017-03-17
网络出版日期: 2017-05-15
基金资助
国家自然科学基金项目Nos.51501207和51471173、中国载人空间站项目No.TGJZ800-2-RW024以及辽宁省自然科学基金项目No.201501043
A New Understanding Toward Effect of Solute Ti on Grain Refinement of Aluminum by Al-Ti-B Master Alloy: Kinetic Behaviors of TiB2 Particles and Effect of Solute Ti
1 The authors contributed equally to this work.
Received date: 2017-03-17
Online published: 2017-05-15
Supported by
Supported by National Natural Science Foundation of China (Nos.51501207 and 51471173), China's Manned Space Station Project (No.TGJZ800-2-RW024) and Natural Science Foundation of Liaoning Province (No.201501043)
实验研究了Ti添加量对Al-Ti-B中间合金细化工业纯Al晶粒效果的影响,建立了Al熔体中TiB2粒子动力学行为模型,模拟分析了Al-Ti-B中间合金细化工业纯Al过程中TiB2粒子的溶解、粗化和快速长大行为及溶质Ti的影响。实验和模拟结果表明,Al-Ti-B中间合金细化工业纯Al过程中,TiB2粒子的动力学行为对中间合金细化能力的影响不可忽视,溶质Ti能有效抑制Al熔体中TiB2粒子的溶解、粗化和快速长大行为,影响Al-Ti-B中间合金的细化能力。
关键词: 晶粒细化 ; Al-Ti-B中间合金 ; TiB2 ; 动力学行为 ; 模拟
张丽丽 , 江鸿翔 , 赵九洲 , 李璐 , 孙倩 . 溶质Ti对Al-Ti-B中间合金细化Al影响的新认识:TiB2粒子的动力学行为及溶质Ti的影响[J]. 金属学报, 2017 , 53(9) : 1091 -1100 . DOI: 10.11900/0412.1961.2017.00084
Grain refinement may not only promote the formation of a fine quiaxed grain structure, which endows the Al alloy castings with good mechanical properties, but also cause a reduction in the casting defects, such as segregation and hot tearing, which has a dominating effect on the processability of Al alloys. It is, thus, essential for both the cast and wrought Al alloys. Although many techniques, e.g. mechanical vibration, electromagnetic stirring, ultrasound vibration, etc. may be used for the grain refinement nowadays, inoculation remains the most widely applied method in the industrial production due to its simplicity and high efficiency. For most Al alloys, Al-Ti-B master alloy is used as the grain refiner. Much work has been done to investigate the solidification behaviors of the Al alloys inoculated with Al-Ti-B master alloys since the 1970 s. Models were developed to describe the microstructure formation under the effect of inoculants. These researches clearly demonstrate that the grain refining efficiency or the heterogeneous nucleation rate is closely related to the concentration of solute Ti as well as the number density and size distribution of TiB2 particles in the melt. One shortcoming of the previous research work in this field is that the kinetic behaviors of TiB2 particles during the heating or cooling processes of the melt, i.e. dissolution/growth, coarsening and precipitation of TiB2 particles, are neglected. Generally the size distribution of TiB2 particles in the Al-Ti-B master alloy was used in the modeling and simulation of the solidification of Al alloys. In this work, solidification experiments were carried out to investigate the kinetic behaviors of TiB2 particles in the melt and the effect of solute Ti. A model was developed to describe the kinetic behaviors of TiB2 particles during the whole process from the beginning of the addition of TiB2 particles to the melt until the solidification of the melt. Calculations were carried out according to the experiments conditions. The results demonstrate that TiB2 particles may dissolve and coarsen during the holding temperature period, and grow during the cooling period of the melt. The kinetic behaviors of TiB2 particles have an obvious effect on the grain refining efficiency of the master alloys. The addition of solute Ti can significantly suppress the growth/dissolution, the Ostwald ripening of TiB2 particles and thus affects the grain refining efficiency of the master alloy.
Key words: grain refinement; Al-Ti-B master alloy; TiB2; kinetic behavior; simulation
| [1] | Quested T E.Understanding mechanisms of grain refinement of aluminium alloys by inoculation[J]. Mater. Sci. Technol., 2004, 20: 1357 |
| [2] | Wannasin J, Canyook R, Wisutmethangoon S, et al.Grain refinement behavior of an aluminum alloy by inoculation and dynamic nucleation[J]. Acta Mater., 2013, 61: 3897 |
| [3] | Wang H X, Zhang G P, Xu C X, et al.Effect of mechanical vibration on grain refinement and solidification shrinkage of aluminum[J]. Res. Stud. Foundry Equip., 2007, (1): 28(王红霞, 张国平, 许春香等. 机械振动对纯Al晶粒细化及凝固收缩的影响[J]. 铸造设备研究, 2007, (1): 28) |
| [4] | Yu J B.Influence of superposing electricity and magnetic field on the solidification structure of metals [D]. Shanghai: Shanghai University, 2009(余建波. 电、磁复合效应对金属凝固组织的影响 [D]. 上海: 上海大学, 2009) |
| [5] | Zhao Z X.The homogeneity of casting alloy process effected by ultrasonic[J]. Hot Working Technol., 1999, (5): 10(赵忠兴. 超声波对合金结晶过程的均匀化作用[J]. 热加工工艺, 1999, (5): 10) |
| [6] | Li J W, Tao Y Z.Effect of ultrasonic on structure of aluminum alloy ingots[J]. Foundry Technol., 2004, 25: 593(李军文, 桃野正. 超声波对铝合金铸锭组织的影响[J]. 铸造技术, 2004, 25: 593) |
| [7] | Han Y F, Shu D, Wang J, et al.Microstructure and grain refining performance of Al-5Ti-1B master alloy prepared under high-intensity ultrasound[J]. Mater. Sci. Eng., 2006, A430: 326 |
| [8] | Birol Y.Efficiency of binary and ternary alloys from Al-Ti-B system in grain refining aluminium foundry alloys[J]. Int. J. Cast Met. Res., 2013, 26: 283 |
| [9] | Easton M, StJohn D. Grain refinement of aluminum alloys: Part II. Confirmation of, and a mechanism for, the solute paradigm[J]. Metall. Mater. Trans., 1999, 30A: 1625 |
| [10] | Fan Z, Wang Y, Zhang Y, et al.Grain refining mechanism in the Al/Al-Ti-B system[J]. Acta Mater., 2015, 84: 292 |
| [11] | Qin T, Fan Z.Reconstruction of 2D Al3Ti on TiB2 in an aluminum melt[J]. Mater. Sci. Eng., 2011, 27: 012004 |
| [12] | Maxwell I, Hellawell A.A simple model for grain refinement during solidification[J]. Acta Metall., 1975, 23: 229 |
| [13] | Greer A L, Bunn A M, Tronche A, et al.Modelling of inoculation of metallic melts: Application to grain refinement of aluminium by Al-Ti-B[J]. Acta Mater., 2000, 48: 2823 |
| [14] | Quested T E, Greer A L.The effect of the size distribution of inoculant particles on as-cast grain size in aluminium alloys[J]. Acta Mater., 2004, 52: 3859 |
| [15] | Quested T E, Greer A L.Grain refinement of Al alloys: Mechanisms determining as-cast grain size in directional solidification[J]. Acta Mater., 2005, 53: 4643 |
| [16] | Easton M A, StJohn D H. A model of grain refinement incorporating alloy constitution and potency of heterogeneous nucleant particles[J]. Acta Mater., 2001, 49: 1867 |
| [17] | Easton M A, StJohn D H. An analysis of the relationship between grain size, solute content, and the potency and number density of nucleant particles[J]. Metall. Mater. Trans., 2005, 36A: 1911 |
| [18] | Easton M A, StJohn D H. Improved prediction of the grain size of aluminum alloys that includes the effect of cooling rate[J]. Mater. Sci. Eng., 2008, A486: 8 |
| [19] | Jones G P, Pearson J.Factors affecting the grain-refinement of aluminum using titanium and boron additives[J]. Metall. Trans., 1976, 7B: 223 |
| [20] | He J, Zhao J Z, Ratke L.Solidification microstructure and dynamics of metastable phase transformation in undercooled liquid Cu-Fe alloys[J]. Acta Mater., 2006, 54: 1749 |
| [21] | Zhao J Z, Li H L, Zhang X F, et al.Microstructure evolution during a liquid-liquid decomposition under the common action of the nucleation, growth and Ostwald ripening of droplets[J]. Int. J. Mater. Res., 2009, 100: 46 |
| [22] | Takaimchi I, Roderick I L, translated by Xian A P, Wang L W. The Physical Properties of Liquid Metals [M]. Beijing: Science Press, 2006: 73(Takaimchi I, Roderick I L著, 冼爱平, 王连文译. 液态金属的物理性能 [M]. 北京: 科学出版社, 2006: 73) |
| [23] | Sun X Y.Study on refinement mechanism of Al-Ti-B and Al-Ti-C master alloys in aluminum and its alloys [D]. Beijing: Tsinghua University, 2011(孙雪迎. Al-Ti-B、Al-Ti-C中间合金细化铝及铝合金机制研究 [D]. 北京: 清华大学, 2011) |
| [24] | Sigworth G K.The grain refining of aluminum and phase relationships in the Al-Ti-B system[J]. Metall. Trans., 1984, 15A: 277 |
| [25] | Zhao J Z, Gao L L, He J, et al.Liquid-liquid phase transformation kinetics of an atomized Al-Pb alloy drop[J]. Acta Metall. Sin., 2006, 42: 113(赵九洲, 高玲玲, 何杰等. Al-Pb合金雾化液滴的液-液相变动力学[J]. 金属学报, 2006, 42: 113) |
| [26] | Liu D M, Zhao J Z, Ye H Q.Modeling of the solidification of gas-atomized alloy droplets during spray forming[J]. Acta Metall. Sin., 2003, 39: 375(刘东明, 赵九洲, 叶恒强. 喷射成形中金属液滴凝固过程的计算机模拟[J]. 金属学报, 2003, 39: 375) |
| [27] | Teng X R.Surfactant Chemistry [M]. Beijing: Chemical Industry Press, 2009: 46(滕新荣. 表面物理化学 [M]. 北京: 化学工业出版社, 2009: 46) |
| [28] | Kaptay G.Partial surface tension of components of a solution[J]. Langmuir, 2015, 31: 5796 |
| [29] | Kaptay G.Modelling equilibrium grain boundary segregation, grain boundary energy and grain boundary segregation transition by the extended Butler equation[J]. J. Mater. Sci., 2016, 51: 1738 |
| [30] | Men H, Fan Z Y.An analytical model for solute segregation at liquid metal/solid substrate interface[J]. Metall. Mater. Trans., 2014, 45A: 5508 |
| [31] | Han Y F.Study on Al-5Ti-1B master alloy prepared under ultrasound and α-Al/diboride interface [D]. Shanghai: Shanghai Jiao Tong University, 2007(韩延峰. 超声制备Al-5Ti-1B中间合金及α-Al/异质核心界面研究 [D]. 上海: 上海交通大学, 2007) |
| [32] | Feuerbacher B, Hamacher H, Naumann R J.Materials Sciences in Space: A Contribution to the Scientific Basis of Space Processing[M]. Berlin: Springer-Verlag, 1986: 11 |
/
| 〈 |
|
〉 |