凹坑深度对铝合金表面在不同润滑介质中摩擦学性能的影响

  • 马明明 ,
  • 连峰 ,
  • 臧路苹 ,
  • 项秋宽 ,
  • 张会臣
展开
  • 大连海事大学交通运输装备与海洋工程学院 大连 116026

收稿日期: 2016-06-27

  网络出版日期: 2017-04-07

基金资助

国家自然科学基金项目Nos.51275064和50975036,中央高校基本科研业务费专项资金项目No.3132016354及辽宁省工业公关计划项目No.2012220006

Effect of Dimple Depth on Friction Properties of Aluminum Alloy Under Different Lubrication Conditions

  • Mingming MA ,
  • Feng LIAN ,
  • Luping ZANG ,
  • Qiukuan XIANG ,
  • Huichen ZHANG
Expand
  • College of Transportation Equipments and Ocean Engineering, Dalian Maritime University, Dalian 116026, China

Received date: 2016-06-27

  Online published: 2017-04-07

Supported by

Supported by National Natural Science Foundation of China (Nos.51275064 and 50975036), Fundamental Research Funds for the Central Universities (No.3132016354) and Industrial Research Program of Liaoning Province (No.2012220006)

摘要

采用激光刻蚀技术在5083船用铝合金表面分别构建出深度为15和30 μm的圆台形凹坑织构,利用涂覆SiO2和低表面能修饰改变表面润湿性,制备超疏水且疏油的双疏表面。采用HSR-2M高速往复摩擦试验机测试其在水、海水和油介质中的摩擦学性能。结果表明,凹坑深度为30 μm的表面的双疏性能强于凹坑深度15 μm的表面,摩擦学性能也更优。与单纯的织构表面相比,将织构和化学组分相结合的双疏表面可以更加显著地提高摩擦学性能。双疏表面在油介质中的摩擦系数和磨损量最小,在海水中的摩擦系数小于在水中,磨损量大于在水中。仿真计算结果表明,随着圆台形凹坑深度的增大,润滑膜承载力先增大后减小。当凹坑深度为75 μm时润滑膜承载力最大。研究结果表明,双疏表面可以显著提高铝合金在润滑介质中的摩擦学性能。

本文引用格式

马明明 , 连峰 , 臧路苹 , 项秋宽 , 张会臣 . 凹坑深度对铝合金表面在不同润滑介质中摩擦学性能的影响[J]. 金属学报, 2017 , 53(4) : 406 -414 . DOI: 10.11900/0412.1961.2016.00257

Abstract

Notable properties of aluminum alloy such as high strength-to-weight ratio, easy to be recycled and good welding properties lead to a wide range of applications in marine industry. However, in addition to many advantages, there are also a lot obvious shortcomings in tribological properties. Especially, the passive state film of aluminum alloy could be destroyed by the Cl- in seawater and harsh marine environment, which can erode into the defects and then aggravate the friction behavior, and limit the use of aluminum alloy in the field of marine engineering. In recent years, the super-hydrophobic surfaces are gaining a wide application prospects in the field of marine engineering due to their properties of drag reduction, anti-adhesion and anti-corrosion abilities. In order to improve the tribological properties of aluminum alloy, the amphiphobic aluminum alloy surface is constructed through building dimple of cone frustum texture with depths of 15 and 30 μm on the surface of 5083 warship aluminum alloy by laser processing and changing the surface wettability by coating the nano-SiO2 powders and low surface energy modification. And the tribological performance was examined by high speed reciprocating friction test machine (HSR-2M) in the water/seawater/oil lubrication respectively. The test results show that the surface with dimple depth of 30 μm has stronger amphiphobic performance and tribological performance than that of 15 μm. Compared with the simple texture surface, the amphiphobic surface with both texture and chemical composition can improve the tribological performance significantly. The friction coefficient and the wear loss of amphiphobic surface are minimal in oil. The friction coefficient of amphiphobic surface in seawater is smaller than that in water while the wear loss of the former is bigger. The simulation results showed that the carrying capacity of the lubricating film increases first and then decreases as the increment of the dimple depth. The carrying capacity of the lubricating film is the biggest when the depth of cone frustum was 75 μm. It can be concluded that the amphiphobic surface can significantly improve the tribological properties of aluminum alloy in different lubrications.

参考文献

[1] Zhang X M, Deng Y L, Zhang Y.Development of high strength aluminum alloys and processing techniques for the materials[J]. Acta Metall. Sin., 2015, 51: 257
[1] (张新明, 邓运来, 张勇. 高强铝合金的发展及其材料的制备加工技术[J]. 金属学报, 2015, 51: 257)
[2] Kim S J, Jang S K, Han M S, et al.Mechanical and electrochemical characteristics in sea water of 5052-O aluminum alloy for ship[J]. Trans. Nonferrous Met. Soc. China, 2013, 23: 636
[3] Hu J, Tang Y G, Li S X.Vibration test and assessment for an ocean drilling rig derrick: Taking the ZJ50/3150DB drilling rig as an example[J]. Petrol. Exp. Dev., 2013, 40: 126
[4] Figueroa R, Abeu C M, Cristóbal M J, et al. Effect of nitrogen and molybdenum ion implantation in the tribological behavior of AA7075 aluminum alloy [J]. Wear, 2012, 276-277: 53
[5] Zou Y S, Zhou K, Wu Y F, et al.Structure, mechanical and tribological properties of diamond-like carbon films on aluminum alloy by arc ion plating[J]. Vacuum, 2012, 86: 1141
[6] Shi H Y, Long Y N, Jiang B L, et al.Effect of sublayer on the structures and tribological properties of GLC coating on Al-based alloy[J]. Acta Metall. Sin., 2012, 48: 983
[6] (时惠英, 龙艳妮, 蒋百灵等. 打底层对铝合金表面GLC镀层组织和摩擦学特性的影响[J]. 金属学报, 2012, 48: 983)
[7] Barati N, Meletis E I, Golestani Fard F, et al.Al2O3-ZrO2 nanostructured coatings using DC plasma electrolytic oxidation to improve tribological properties of Al substrates[J]. Appl. Surf. Sci., 2015, 356: 927
[8] Zhou H, Shan H Y, Tong X, et al.The adhesion of bionic non-smooth characteristics on sample surfaces against parts[J]. Mater. Sci. Eng., 2006, A417: 190
[9] Hu T C, Hu L T.The study of tribological properties of laser-textured surface of 2024 aluminium alloy under boundary lubrication[J]. Lubr. Sci., 2012, 24: 84
[10] Scaraggi M, Mezzapesa F P, Carbone G, et al.Friction properties of lubricated laser-microtextured-surfaces: An experimental study from boundary- to hydrodynamic-lubrication[J]. Tribol. Lett., 2013, 49: 117
[11] Liew K W, Kok C K, Ervina Efzan M N. Effect of EDM dimple geometry on friction reduction under boundary and mixed lubrication[J]. Tribol. Int., 2016, 101: 1
[12] Burton Z, Bhushan B.Surface characterization and adhesion and friction properties of hydrophobic leaf surfaces[J]. Ultramicroscopy, 2006, 106: 709
[13] Qin L G, Zhao W J, Hou H, et al.Achieving excellent anti-corrosion and tribological performance by tailoring the surface morphology and chemical composition of aluminum alloys[J]. RSC Adv., 2014, 4: 60307
[14] Wang H Y, Yan L, Gao D, et al.Tribological properties of superamphiphobic PPS/PTFE composite coating in the oilfield produced water[J]. Wear, 2014, 319: 62
[15] Shan L, Wang Y X, Li J L, et al.Tribological behaviours of PVD TiN and TiCN coatings in artificial seawater[J]. Surf. Coat. Technol., 2013, 226: 40
[16] Wenzel R N.Resistance of solid surfaces to wetting by water[J]. Ind. Eng. Chem., 1936, 28: 988
[17] Cassie A B D, Baxter S. Wettability of porous surfaces[J]. Trans. Faraday Soc., 1944, 40: 546
[18] Wen S Z.Study on lubrication theory-progress and thinking-over[J]. Tribology, 2007, 27: 497
[18] (温诗铸. 润滑理论研究的进展与思考[J]. 摩擦学学报, 2007, 27: 497)
[19] Yu H, Deng H, Huang W, et al.The effect of dimple shapes on friction of parallel surfaces[J]. Proc. Inst. Mech. Eng., 2010, 225: 693
[20] Uman A, Park C W.Optimizing the tribological performance of textured piston ring-liner contact for reduced frictional losses in SI engine: Warm operating conditions[J]. Tribol. Int., 2016, 99: 224
[21] Yoshimitsu T, Nakajima H, Nagaoka H.Synthesis of the CD ring system of paclitaxel by atom-transfer radical annulation reaction[J]. Tetrahedron Lett., 2002, 43: 8587
[22] Navier C L. Memoire sur les lois du mouvement des fluides [J]. Mém. Acad. Roy. Sci., 1823, 6: 389
[23] Kunert C, Harting J.Simulation of fluid flow in hydrophobic rough microchannels[J]. Int. J. Comput. Fluid Dyn., 2008, 22: 475
[24] Wang L, Yan C P, Wang Q D, et al.Study on the tribological properties of the amphiphobic textured metal surface[J]. J. Huazhong Univ. Sci. Technol.(Nat. Sci. Ed.), 2012, 40(Suppl. II): 21
[24] (王莉, 严诚平, 王权岱等. 金属微结构双疏表面的摩擦特性研究[J]. 华中科技大学学报(自然科学版), 2012, 40(Suppl.II): 21)
[25] Wang J H, Song M, Li J L, et al.The preparation and tribological properties of water-soluble nano-silica particales[J]. Tribology, 2011, 31: 118
[25] (王建华, 宋敏, 李金龙等. 水溶性纳米二氧化硅添加剂的制备及摩擦学性能研究[J]. 摩擦学学报, 2011, 31: 118)
[26] Liu N, Wang J Z, Chen B B, et al.Tribochemical aspects of silicon nitride ceramic sliding against stainless steel under the lubrication of seawater[J]. Tribol. Int., 2013, 61: 205
[27] Chen J, Yan F Y.Tribocorrosion behaviors of Ti-6Al-4V and Monel K500 alloys sliding against 316 stainless steel in artificial seawater[J]. Trans. Nonferrous Met. Soc. China, 2012, 22: 1356
[28] Osman M M.Corrosion inhibition of aluminium-brass in 3.5%NaCl solution and sea water[J]. Mater. Chem. Phys., 2001, 71: 12
[29] Ding H Y, Zhou G H, Hui D.Friction and wear performance of an aluminium alloy in artificial seawater[J]. Proc. Inst. Mech. Eng., 2011, 225: 43
[30] Liu T, Liu T, Chen S G, et al.Corrosion resistance improvement of aluminum in seawater by super-hydrophobic surfaces[J]. Chin. J. Inorg. Chem., 2008, 24: 1859
[30] (刘通, 刘涛, 陈守刚等. 超疏水表面改善铝基材料的抗海水腐蚀性能[J]. 无机化学学报, 2008, 24: 1859)
[31] Liu T, Chen S G, Cheng S, et al.Corrosion behavior of super-hydrophobic surface on copper in seawater[J]. Electrochim. Acta, 2007, 52: 8003
文章导航

/