活性Ti表面电沉积Ni-CeO2复合镀层及其强韧性机理分析
收稿日期: 2016-04-29
网络出版日期: 2016-11-02
基金资助
国家自然科学基金项目No.51605203, 江苏省自然科学基金项目No.BK20150467和江苏科技大学博士科研启动金项目No.1062921501
Analysis of Toughness and Strengthening Mechanisms forNi-CeO2 Nanocomposites Coated on the ActivatedSurface of Ti Substrate
Received date: 2016-04-29
Online published: 2016-11-02
Supported by
Supported by National Natural Science Foundation of China (No.51605203), Natural Science Foundation of Jiangsu Province (No.BK20150467) and Scientific Research Fund of Jiangsu University of Science and Technology (No.1062921501)
基于双脉冲电沉积技术在活性钛基(TA2)表面制备纳米晶Ni镀层。通过涂层附着力测试对比研究HF体系和DMF改良型活化液对TA2基体与表面镀层界面结合力的影响;借助TEM、FESEM和XRD等表征技术探讨添加纳米CeO2粒子前后对纳米电沉积层中Ni晶织构生长的影响;通过对纳米压痕及不同载荷下“十字交叉”型环形硬度压痕特征观察,分析复合CeO2粒子对Ni镀层表面强韧性的影响机制; 进一步探讨在高速干摩擦条件下复合CeO2粒子对Ni镀层抗磨损的作用。结果表明:在45+80 kHz交变频率超声振荡条件下,电解液中的活性CeO2粒子能有效吸附在优先生长Ni晶尖端,同时降低了Ni晶生长Gibbs自由能,并演变为Ni晶的催化形核中心来诱发异质形核; 纳米压痕测试表明:在500 g高载荷测试条件下,相对于纯Ni镀层试样的硬度压痕边缘的明显开裂和外拓迹象,Ni-CeO2复合镀层试样则表现为收敛性和连续完整的压痕边缘特征,显示出良好的强韧性。基于干摩擦过程中释放出大量的热,促使部分稀土CeO2相弥散或少量析出Ce溶质原子,具有对滑移的位错和晶界等缺陷产生钉扎拖拽作用,由此建立以Orowan位错绕过强化和位错塞积的机制模型;干摩擦过程促使部分富Ce磨损产物与NiO氧化膜机械混合来充当固体润滑剂,能起到良好的减摩作用,弥补了Ti表面耐磨性差等缺陷。
周小卫 , 欧阳春 , 乔岩欣 , 沈以赴 . 活性Ti表面电沉积Ni-CeO2复合镀层及其强韧性机理分析[J]. 金属学报, 2017 , 53(2) : 140 -152 . DOI: 10.11900/0412.1961.2016.00163
With industrial developments of aerospace vehicles, marine devices, biomedical and bones, pure Ti and its alloys have gained a great deal of attraction due to their superior properties. Despite having promising properties, limitations of lower hardness, inferior weldability, and poor brittle fracture have restricted their applications. So the objective of this work was to make surface electrodeposition of nanocrystalline Ni coatings on the surface of TA2 substrate using pulsed electrodeposition. Scratch tests was used to compare how effects of two typical HF and DMF activating solutions on modifying interfacial adhesion between TA2 substrate and surface coatings. In order to disclose crystal growth of Ni coating without and with CeO2 addition, a variety of characterizations such as FESEM, TEM and XRD were employed. A novel decussating-type microhardness with different loading forces attached with nanoindentation tests was conducted to make a comparative study of toughness and strengthening mechanisms between surface coatings and the un-coated TA2 substrate. Besides, wear behaviors of specimens was carried out using the ball-disc dry sliding tests. Results indicated that the addition of CeO2 nanoparticles into electroplating solution has effectively modified textural growth of Ni grains. This result was attributed to the presence of nano-sized CeO2 particles that adsorbed onto the preferred locations of crystal Ni growth, leading into an increasing catalytic site of nucleation to reduce Gibbs energy for grain refinement. According to observations of edges for hardness indentations, a smaller size with convergence feature for Ni-CeO2 coatings was indicative of effects of CeO2 nanoparticles or its precipiated Ce solute atoms on alloying-dispersion strengthening for completing defective grain boundaries. While for the case of a divergency state of indentations edges within obviously spalling cracks, it exhibited poor surface toughness for pure nickel. Furthermore, An analytic modeling validated here was based on the by-passing Orowan for dislocations pile-up mechanisms, in which this was contributed to the co-existence of Ce-rich worn products and NiO passive film to be expected as solid lubricants and make the self-lubricating effect, thereby improving wear resistance of Ti alloys where subjected to harsh conditions.
| [1] | Liu F C, Mao Y Q, Lin X, et al.Microstructure and high temperature oxidation resistance of Ti-Ni gradient coating on TA2 titanium alloy fabricated by laser cladding[J]. Opt. Laser Technol., 2016, 83: 140 |
| [2] | Xie L, Guo W H, Huo F J, et al.A new method for non-destructive stripping of coatings on titanium substrates[J]. Surf. Coat. Technol., 2016, 294: 1 |
| [3] | Liu X Y, Chu P K, Ding C X.Surface modification of titanium, titanium alloys, and related materials for biomedical applications[J]. Mater. Sci. Eng., 2004, R47: 49 |
| [4] | Wu S M.New technology and applications of electroplating on titanium alloys[J]. Aerosp. Shanghai, 1994, (3): 22 |
| [4] | (吴申敏. 钛合金电镀新工艺及其应用[J]. 上海航天, 1994, (3): 22) |
| [5] | Liu H T, Wang L P, Deng C C.Friction and wear characteristics of nickel plating coating on titanium alloy surface[J]. Mater. Mech. Eng., 2013, 37(2): 46 |
| [5] | (刘洪涛, 王路平, 邓长城. 钛合金表面镀镍层的摩擦磨损特性[J]. 机械工程材料, 2013, 37(2): 46) |
| [6] | Li M C, Tu Z M, Zhang J S, et al.Mechanism of direct metal plating on titanium[J]. Mater. Prot., 1991, 24(11): 12 |
| [6] | (李萌初, 屠振密, 张景双等. 钛上直接电镀机理的研究[J]. 材料保护, 1991, 24(11): 12) |
| [7] | Ohtsu N, Komiya S, Kodama K.Effect of electrolytes on anodic oxidation of titanium for fabricating titanium dioxide photocatalyst[J]. Thin Solid Films, 2013, 534: 70 |
| [8] | Wang Y M, Lei T Q, Jiang B L, et al.Growth, microstructure and mechanical properties of microarc oxidation coatings on titanium alloy in phosphate-containing solution[J]. Appl. Surf. Sci., 2004, 233: 258 |
| [9] | Lin Y H, Lei Y P, Fu H G, et al.Laser in situ synthesized titanium diboride and nitinol reinforce titanium matrix composite coatings[J]. Acta Metall. Sin., 2014, 50: 1513 |
| [9] | (林英华, 雷永平, 符寒光等. 激光原位制备硼化钛与镍钛合金增强钛基复合涂层[J]. 金属学报, 2014, 50: 1513) |
| [10] | Khor K A, Yip C S, Cheang P.Ti-6Al-4V/hydroxyapatite composite coatings prepared by thermal spray techniques[J]. J. Therm. Spray Technol., 1997, 6: 109 |
| [11] | Marin E, Offoiach R, Regis M, et al.Diffusive thermal treatments combined with PVD coatings for tribological protection of titanium alloys[J]. Mater. Des., 2016, 89: 314 |
| [12] | Li B, Shen Y F, Hu W Y, et al.Surface modification of Ti-6Al-4V alloy via friction-stir processing: Microstructure evolution and dry sliding wear performance[J]. Surf. Coat. Technol., 2014, 239: 160 |
| [13] | Chen C, Ding R D, Feng X M, et al.Fabrication of Ti-Cu-Al coatings with amorphous microstructure on Ti-6Al-4 V alloy substrate via high-energy mechanical alloying method[J]. Surf. Coat. Technol., 2013, 236: 485 |
| [14] | Li L L, He J, Yang X.Preparation of conversion coating on Ti-6Al-4V alloy in mixed solution of phytic acid and ammonium fluoride through chemical modification[J]. Appl. Surf. Sci., 2016, 371: 488 |
| [15] | Yuan H, Fu C Y.A potential-PH diagram for Ti-H2O system[J]. J. Sichuan Normal Univ.(Nat. Sci.), 1980, (2): 63 |
| [15] | (袁华, 付成玉. Ti-H2O体系电位-PH图[J]. 四川师范大学学报(自然科学版), 1980, (2): 63) |
| [16] | Kong L B, Zhang T S, Ma J, et al.Mullite phase formation in oxide mixtures in the presence of Y2O3, La2O3?and CeO2[J]. J. Alloys Compd., 2004, 372: 290 |
| [17] | Boizumault-Moriceau P, Pennequin A, Grzybowska B, et al.Oxidative dehydrogenation of propane on Ni-Ce-O oxide: effect of the preparation method, effect of potassium addition and physical characterization[J]. Appl. Catal., 2003, 245A: 55 |
| [18] | Aruna S T, William Grip s V K, Rajam K S. Ni-based electrodeposited composite coating exhibiting improved microhardness, corrosion and wear resistance properties[J]. J. Alloys Compd., 2009, 468: 546 |
| [19] | Oliver W C, Pharr G M.An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments[J]. J. Mater. Res., 1992, 7: 1564 |
| [20] | Zhou X W, Shen Y F.A comparative study of pure nickel and the Ni-CeO2 nanocrystalline coatings: microstructural evolution, oxidation behavior, and thermodynamic stability[J]. J. Mater. Sci., 2014, 49: 3755 |
| [21] | Zhou X W, Shen Y F.Surface morphologies, tribological properties, and formation mechanism of the Ni-CeO2?nanocrystalline coatings on the modified surface of TA2 substrate[J]. Surf. Coat. Technol., 2014, 249: 6 |
| [22] | Zhou X W, Shen Y F, Gu D D.Microstructure and high temperature oxidation resistance of nanocrystalline Ni-CeO2 composite coatings deposited by double-pulsed electro deposition[J]. Acta Metall. Sin., 2012, 48: 957 |
| [22] | (周小卫, 沈以赴, 顾冬冬. 双脉冲电沉积纳米晶Ni-CeO2复合镀层的微观结构及其高温抗氧化性能[J]. 金属学报, 2012, 48: 957) |
| [23] | Zhou X W.Research on Nanocrystalline Ni coating reinforced with CeO2 nanoparticles on Ti-based surface by double pulse electrodeposition [D]. Nanjing: Nanjing University of Aeronautics and Astronautics, 2014 |
| [23] | (周小卫. 钛基金属表面双脉冲电沉积纳米CeO2增强镍基镀层的研究 [D]. 南京: 南京航空航天大学, 2014) |
| [24] | Aruna S T,William Grips V K, Rajam K S. Ni-based electrodeposited composite coating exhibiting improved microhardness, corrosion and wear resistance properties[J]. J. Alloys Compd., 2009, 468: 546 |
| [25] | Kacher J, Elizaga P, House S D, et al.Thermal stability of Ni/NiO multilayers[J]. Mater. Sci. Eng., 2013, A568: 49 |
| [26] | Moon D P.The reactive element effect on the growth rate of nickel oxide scales at high temperature[J]. Oxid. Met., 1989, 32: 47 |
| [27] | Tudela I, Zhang Y, Pal M, et al.Ultrasound-assisted electrodeposition of thin nickel-based composite coatings with lubricant particles[J]. Surf. Coat. Technol., 2015, 276: 89 |
| [28] | Xue Y J, Si D H, Liu H B, et al.Effects of electrodeposition methods on friction and wear properties of Ni-CeO2 nanocomposite coatings[J]. Chin. J. Nonferrous Met., 2011, 21: 2157 |
| [28] | (薛玉君, 司东宏, 刘红兵等. 电沉积方式对Ni-CeO2纳米复合镀层摩擦磨损性能的影响[J]. 中国有色金属学报, 2011, 21: 2157) |
| [29] | Xue Y J, Jia X Z, Zhou Y W, et al.Tribological performance of Ni-CeO2 composite coatings by electro deposition[J]. Surf. Coat. Technol., 2006, 200: 5677 |
| [30] | Zhang Z, Chen D L. Contribution of Orowan strengthening effect in particulate-reinforced metal matrix nanocomposites [J]. Mater. Sci. Eng., 2008,A483-484: 148 |
| [31] | Bober D B, Kumar M, Rupert T J.Nanocrystalline grain boundary engineering: Increasing Σ3 boundary fraction in pure Ni with thermomechanical treatments[J]. Acta Mater., 2015, 86: 43 |
| [32] | Aruna S T, Bindu C N, Ezhil Selvi V, et al.Synthesis and properties of electrodeposited Ni/ceria nanocomposite coatings[J]. Surf. Coat. Technol., 2006, 200: 6871 |
/
| 〈 |
|
〉 |