连续SiC纤维增强钛基复合材料研究进展*
ADVANCES IN SiC FIBER REINFORCED TITANIUM MATRIX COMPOSITES
Received date: 2016-08-01
Online published: 2016-08-29
Supported by
王玉敏 , 张国兴 , 张旭 , 杨青 , 杨丽娜 , 杨锐 . 连续SiC纤维增强钛基复合材料研究进展*[J]. 金属学报, 2016 , 52(10) : 1153 -1170 . DOI: 10.11900/0412.1961.2016.00347
SiC fibers can be used to reinforce a range of titanium base materials including alloys of the (α+β) type, metastable β type and near α type, as well intermetallic based γ-TiAl and orthorhombic Ti2AlNb. Along the fiber directions the obtained composites possess exceptional strength and stiffness, creating a large room and great flexibility for the design of higher performance components to be used in both aero engine and aircraft. The composites can be used by itself such as in sheet and bar form, or as a reinforcing module embedded in titanium alloy components, e.g., as a ring at the rim of a compressor disk. In this paper, recent progress in the development and application of SiC fiber reinforced titanium matrix composites was reviewed, emphasizing the work conducted at the Institute of Metal Research, Chinese Academy of Sciences. Five aspects of research were covered, the first is fiber manufacture and batch production, in which the influence of the chemical vapor deposition parameters on the quality of the W-core SiC fiber was discussed, and the relationship between the tungsten-SiC interface reaction and the high temperature stability of the fiber was described. The second part covers the composite interface, in which a detailed discussion was given to both the chemical and physical compatibility, followed by the design of different reaction layers between the SiC fiber and different titanium based matrixs. The mechanical property section presents tensile data of a range of composites developed in the authors' group and compares to literature reports where available, together with a comprehensive discussion of failure due to fatigue and creep. The fourth part deals with nondestructive testing, presenting new results of inspection on real size composite components using a combination of several techniques including X-ray, industrial CT and ultrasonic scanning. The limitations of each method were shown and the technical challenges were identified. The last part describes the development of structural parts and their verification testing. Titanium matrix composite sheets with [0/90] laminate prepared by both the foil-fiber-foil and matrix coated fiber methods were highlighted, followed by a description of the development of full size bladed ring and excess revolution testing. Future directions of research on SiC fiber reinforced titanium matrix composites were also discussed.
| [1] | Yang R, Shi N L, Wang Y M, Lei J F, Zhang G X, Fu Y C, Li Y H, Zhang D Z.Titanium Ind Prog, 2005; 22(5): 32 |
| [1] | (杨锐, 石南林, 王玉敏, 雷家峰, 张国兴, 符跃春, 李艳华, 张德志. 钛工业进展, 2005; 22(5): 32) |
| [2] | Guo Z X, Derby B.Prog Mater Sci, 1995; 39: 411 |
| [3] | Leyens C, Kocian F, Hausmann J, Kaysser W A.Aerosp Sci Technol, 2003; 7: 201 |
| [4] | Carrere N, Feyel F, Kruch S.Aerosp Sci Technol, 2003; 7: 307 |
| [5] | Khan T, Kuentzmann P.Mater Sci Forum, 2007; 546: 1171 |
| [6] | Vassel A, Pautonnier F, Raffestin M.ONERA, 2003; 2003: 112 |
| [7] | Hyde T H, Punyong K, Becker A A.J Mater: Des Appl, 2015; 229: 51 |
| [8] | Shi N L, Wang Y M, Feng J W, Yang R.Proc 2002 Symp on Space Materials, Special Committee, China Space Science Society, Tianjin: CSSR, 2002: 108 |
| [8] | (石南林, 王玉敏, 冯纪伟, 杨锐. 中国空间科学学会空间材料专业委员会2002学术交流会论文集, 天津: 中国空间科学学会, 2002: 108) |
| [9] | Yang Y Q, Wen Q, Ma Z J, Lv X H, Chen Y.Rare Met Lett, 2004; 23(7): 22 |
| [9] | (杨延清, 文琼, 马志军, 吕祥鸿, 陈彦. 稀有金属快报, 2004; 23(7): 22) |
| [10] | Huang H, Wen M, Chen D M, Li Z X, Huang X.J Aerona Mater, 2011; 31(S1): 135 |
| [10] | (黄浩, 文懋, 陈大明, 李臻熙, 黄旭. 航空材料学报, 2011; 31(增刊1): 135) |
| [11] | Shi N L.Chin Pat, 90 1 06461.0, 1990 |
| [11] | (石南林. 中国专利, 90 1 06461.0, 1990) |
| [12] | Shatwell R A, Dyos K L, Prentice C, Ward Y, Young R J.J Microsc, 2001; 201: 179 |
| [13] | Cheng T T, Jones I P, Shatwell R A, Doorbar P.Mater Sci Eng, 1999; A260: 139 |
| [14] | Giannuzzi L A, Lewinsohn C A, Bakis C E, Tressler R E.J Mater Res, 1998; 13: 1853 |
| [15] | Wang Y M.PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2005 |
| [15] | (王玉敏. 中国科学院金属研究所博士学位论文, 沈阳, 2005) |
| [16] | Zhao C B.Master Thesis, University of Chinese Academy of Sciences, Beijing, 2015 |
| [16] | (赵传保. 中国科学院大学硕士学位论文, 北京, 2015) |
| [17] | Gambone M L, Gundel D B.Key Eng Mater, 1996; 127: 1251 |
| [18] | Martineau P, Pailler R, Lahaye M, Naslain R.J Mater Sci, 1984; 19: 2749 |
| [19] | Zhu Y.PhD Dissertation, Northwestern Polytechnical University, Xi'an, 2003 |
| [19] | (朱艳. 西北工业大学博士学位论文, 西安, 2003) |
| [20] | Bilba K, Manand J P, Cirpa Y L, Qenisset J M.Mater Sci Eng, 1991; A135: 141 |
| [21] | Naka M, Feng J C, Schuster J C.Metall Mater Trans, 1997; 28A: 1385 |
| [22] | Dybkov V I.J Mater Sci, 1986; 21: 3078 |
| [23] | Yang J M, Jeng S M.JOM, 1989; 41(11): 56 |
| [24] | Ashby M F.Acta Metall Mater, 1993; 41: 1313 |
| [25] | Ramamurty U, Dary F C, Zok F W.Acta Mater, 1996; 44: 3397 |
| [26] | Aghdam M M, Khojeh A.Compos Struct, 2003; 62: 285 |
| [27] | Douin J, Donnadieu P, Finel A, Dirras G F, Silvain J F.Composites, 2002; 33A: 1397 |
| [28] | Guo Z X, Surodola J F, Derby B, Ruiz C.Composites, 1994; 25: 563 |
| [29] | Mackey R A.Scr Metall Mater, 1990; 24: 167 |
| [30] | Johnson W S.Composites, 1993; 24: 187 |
| [31] | Upadhyaya D, Froes F H, Wood M J, Ward-Close C M. Titanium'95: Science and Technology. Birmingham, United Kingdom: Inst. of Materials, 1995: 2747 |
| [32] | Koss D A, Copley S M.Metall Trans, 1971; 2A: 1557 |
| [33] | Sun C T, Chen J L, Sha G T, Koop W E.J Compos Mater, 1990; 24: 1029 |
| [34] | Durodola J F, Derby B.Acta Metall Mater, 1994; 42: 1525 |
| [35] | Mikata Y, Taya M.J Compos Mater, 1985; 19: 554 |
| [36] | Warwick C M, Clyne T W.J Mater Sci, 1991; 26: 3817 |
| [37] | Vedula M, Pangborn R N, Queeney R A.Composites, 1988; 19: 55 |
| [38] | Vedula M, Pangborn R N, Queeney R A.Composites, 1988; 19: 133 |
| [39] | Haque S, Choy K L.Mater Sci Eng, 2000; A291: 97 |
| [40] | Zhang X.PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2013 |
| [40] | (张旭. 中国科学院金属研究所博士学位论文, 沈阳, 2013) |
| [41] | An J M.Master Thesis, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2013 |
| [41] | (安江敏. 中国科学院金属研究所硕士学位论文, 沈阳, 2013) |
| [42] | Kendig K L, Soboyejo W O, Miracle D B.Scr Mater, 1995; 32: 669 |
| [43] | Willemse P F, Mulder F M, Wei W, Rekveldt M T, Knight K S.Scr Mater, 2000; 42: 775 |
| [44] | Greerberg B A, Gornostirev Y N.Scr Metall, 1988; 22: 853 |
| [45] | Hanamura T, Uemori R, Tanina M.J Mater Res, 1988; 3: 656 |
| [46] | Pickard S M, Miracle D B, Majumdar B S, Kendig K L, Rothenflue L, Coker D.Acta Mater, 1995; 43: 3105 |
| [47] | Fang Q, Sidky P S, Hocking G M.Mater Sci Eng, 2000; A288: 293 |
| [48] | Ward Y, Young R J, Shatwell R A.Composites, 2002; 33A: 1409 |
| [49] | Xiao P, Wang Y M, Lei J F, Shi N L, Yang R.Rare Met Mater Eng, 2011; 40: 1540 |
| [49] | (肖鹏, 王玉敏, 雷家峰, 石南林, 杨锐. 稀有金属材料与工程, 2011; 40: 1540) |
| [50] | Rangaswamy P, Prime M B, Daymond M, Bourke M A M, Clausen B, Choo H, Jayaraman N.Mater Sci Eng, 1999; A259: 209 |
| [51] | Xiao P.PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2010 |
| [51] | (肖鹏. 中国科学院金属研究所博士学位论文, 沈阳, 2010) |
| [52] | Zhang X, Xiao P, Yang Q, Wang Y M, Lei J F, Yang R.Chin Pat, 201110101268.0, 2011 |
| [52] | (张旭, 肖鹏, 杨青, 王玉敏, 雷家峰, 杨锐.中国专利, 201110101268.0, 2011) |
| [53] | Upadhyaya D, Wood M, Ward-Close C M, Tsakiropoulos P, Froes F H.JOM, 1994; 46(11): 62 |
| [54] | Baik K H, Grant P S.Scr Mater, 2001; 44: 607 |
| [55] | Fu Y C, Shi N L, Zhang D Z, Yang R.Mater Sci Eng, 2006; A426: 278 |
| [56] | Li Y H, Shi N L, Zhang D Z, Yang R.J Mater Sci Technol, 2005; 21: 657 |
| [57] | Wang Y M, Fu Y C, Shi N L, Zhang D Z, Yang R.Acta Metall Sin, 2004; 40: 359 |
| [57] | (王玉敏, 符跃春, 石南林, 张德志, 杨锐. 金属学报, 2004; 40: 359) |
| [58] | Guo C Y, Zhang C B, He L L, Zhang G X, Lei J F.Acta Metall Sin, 2006; 42: 792 |
| [58] | (郭长友, 张彩碚, 贺连龙, 张国兴, 雷家峰. 金属学报, 2006; 42: 792) |
| [59] | Zhang G X, Kang Q, Li G P, Shi N L, Li D.Acta Metall Sin, 2003; 39: 329 |
| [59] | (张国兴, 康强, 李阁平, 石南林, 李东. 金属学报, 2003; 39: 329) |
| [60] | Choo H, Rangaswamy P, Bourke M A M.Scr Mater, 2000; 42: 175 |
| [61] | Dudek H J, Borath R, Leucht R, Kaysser W A.J Mater Sci, 1997; 3: 5355 |
| [62] | Das G.Metall Mater Trans, 1990; 21A: 1571 |
| [63] | Yang Y Q, Zhu Y, Ma Z J, Chen Y.Scr Mater, 2004; 51: 385 |
| [64] | Jeng S M, Yang J M, Yang C J.Mater Sci Eng, 1991; A138: 155 |
| [65] | Goo G K, Graves J A, Mecartney M L.Scr Metall Mater, 1992; 26: 1043 |
| [66] | Zhang X, Wang Y M, Lei J F, Yang R.Acta Metall Sin, 2012; 48: 1306 |
| [66] | (张旭, 王玉敏, 雷家峰, 杨锐. 金属学报, 2012; 48: 1306) |
| [67] | Zhang X, Yang Q, Wang Y M, Lei J F, Yang R.In: Zhou L, Chang H, Lu Y F, Xu D S eds., Proc 12th World Conference on Titanium, Beijing: Science Press, 2011: 1545 |
| [68] | Hall I W, Lirn J L, Rizza J.J Mater Sci Lett, 1991; 10: 263 |
| [69] | Baumann S P, Brindley P K, Smith S D.Metall Trans, 1990; 21A: 1559 |
| [70] | Jones C, Kiely C J, Wang S S.J Mater Res, 1989; 4: 327 |
| [71] | Yang K, Guo Z X, Edmonds D V.Scr Metall Mater, 1992; 27: 1021 |
| [72] | Yang K, Guo Z X, Edmonds D V.Scr Metall Mater, 1992; 27: 1695 |
| [73] | Guo Z X, Li J H, Yang K, Derby B.Composites, 1994; 25: 881 |
| [74] | Zhou C H, Yang K, Lu Y X.Acta Metall Sin (Engl Lett), 1998; 11: 307 |
| [75] | Favre J P, Vassel A, Laclau C.Composites, 1994; 25: 482 |
| [76] | Kerans R J, Parthasarathy T A.J Am Ceram Soc, 1991; 74: 1585 |
| [77] | Dollar A, Steif P S, Wang Y C, Hui C Y.Int J Solids Struct, 1993; 30: 1313 |
| [78] | Petitcorps Y L, Pailler R, Naslain R.Compos Sci Technol, 1989; 35: 207 |
| [79] | Jeng S M, Yang J M, Yang C J.Mater Sci Eng, 1991; A138: 169 |
| [80] | Eldridge J I, Ebihara B T.J Mater Res, 1994; 9: 1035 |
| [81] | Bechel V T, Sottos N R.J Mater Sci, 1999; 34: 3471 |
| [82] | Yang C J, Jeng S M, Yang J M.Scr Metall Mater, 1990; 24: 469 |
| [83] | Jeng S M, Alassoeur J P, Yang C J.Mater Sci Eng, 1991; A148: 67 |
| [84] | Garc??a-Leiva M C, Oca?a I, Mart??n-Meizoso A, Mart??nez-Esnaola J M, Marqués V, Heredero F.Eng Fract Mecha, 2003; 70: 2137 |
| [85] | Yamazaki Y, Ikada A, Okazaki M.Key Eng Mater, 2004; 261: 1091 |
| [86] | Bettge D, Günther B, Wedell W, Portella P D, Hemptenmacher J, Peters P W M. Symposium Verbundwerkstoffe und Werkstoffverbunde, Wien, ?sterreich, 2003 |
| [87] | Bettge D, Gunther B, Wedell W, Portella P D, Hemptenmacher J, Peters P W M, Skrotzki B. Mater Sci Eng, 2007; A452-453: 536 |
| [88] | Robertson D D, Mall S.Proc Eleventh Int Conf on Composite Materials, Queensland, Australia, 1997: 365 |
| [89] | Calcaterra J R, Mall S, Coghlan S C.Metall Mater Trans, 1999; 30: 307 |
| [90] | Nguyen T H B, Jeng S M, Yang J M.Mater Sci Eng, 1994; A183: 1 |
| [91] | Ramamurty U.Compos Sci Technol, 2005; 65: 1815 |
| [92] | Fukushima A, Fujiwara C, Kagawa Y, Masuda C.Mater Sci Eng, 2000; A276: 243 |
| [93] | Peters P W M, Xia Z, Hemptenmacher J, Assler H.Composites, 2001; 32A: 561 |
| [94] | Hemptenmacher J, Assler H, Kumpfert J, Dudek H J.Sixth Annu Int Conf on Composites Engineering (ICCE/6), Orlando, Florida: International Conference on Composites Engineering, 1999: 313 |
| [95] | Gundel D B, Wawner F E.Composites, 1997; 57: 471 |
| [96] | Boyer R, Collings E W, Welsch G.Materials Properties Handbook: Titanium Alloys. ASM International, 1994: 1 |
| [97] | Suzuki T, Umehara H, Hayashi R.J Mater Res, 1993; 8: 2492 |
| [98] | Smith P R, Froes F H.J Met, 1984; 36: 19 |
| [99] | Ochial S, Osamura K.Metall Trans, 1990; 21A: 971 |
| [100] | Kagawa Y, Fujita T, Okura A.Acta Metall Mater, 1994; 42: 3019 |
| [101] | Curtin W A.J Am Ceram Soc, 1991; 74: 2837 |
| [102] | Curtin W A.Composites, 1993; 24: 98 |
| [103] | Zweben C.AIAA J, 1968; 6: 2325 |
| [104] | Zweben C, Rosen B W.J Mech Phys Solids, 1970; 18: 189 |
| [105] | Batdorf S B.J Reinf Plast Compos, 1982; 1: 153 |
| [106] | Batdorf S B, Ghaffarian R.J Reinf Plast Compos, 1982; 1: 165 |
| [107] | González C, Llorca J.Acta Mater, 2001; 49: 3505 |
| [108] | Wu X, Cooper C, Bowen P.Metall Mater Trans, 2001; 32A: 1851 |
| [109] | Naseem K, Yang Y Q, Luo X, Huang B, Feng G H.Mater Sci Eng, 2011; A528: 4507 |
| [110] | Peters P W M, Hemptenmacher J.Composites, 2002; 33A: 1373 |
| [111] | Gálvez F, González C, Poza P, LLorca J.Scr Mater, 2001; 44: 2667 |
| [112] | Weber C H, Chen X, Connell S J, Zok F W.Acta Metall Mater, 1994; 42: 3443 |
| [113] | Zhang X, Wang Y M, Yang Q, Lei J F, Yang R.Acta Metall Sin, 2015; 51: 1025 |
| [113] | (张旭, 王玉敏, 杨青, 雷家峰, 杨锐. 金属学报, 2015; 51: 1025) |
| [114] | Zhang X, Yang Q, Wang Y M, Lei J F, Yang R.Chin J Nonferrous Met, 2010; 20(spec 1): 203 |
| [114] | (张旭, 杨青, 王玉敏, 雷家峰, 杨锐. 中国有色金属学报, 2010; 20(专辑 1): 203) |
| [115] | Barney C, Beevers C J, Bowen P.Composites, 1993; 24: 229 |
| [116] | Rauchs G, Thomason P F, Withers P J.Comput Mater Sci, 2002; 25: 166 |
| [117] | Brett R L, Cotterill P J, Bowen P.Int J Fatigue, 1996; 18: 1 |
| [118] | Ibbotson A R, Beevers C J, Bowen P.In: Bailon J P, Dickson J eds., Int Fatigue Series-IFS, Vol. 1-3, Montreal, Canada: Engineering Materials Advisory Services LTD, 1993: 1079 |
| [119] | Cotterill P J, Bowen P.Composites, 1993; 24: 214 |
| [120] | Warrier S G, Maruyama B, Majumdar B S, Miracle D B.Mater Sci Eng, 1999; A259: 189 |
| [121] | Rauchs G, J Withers P.Int J Fatigue, 2002; 24: 1205 |
| [122] | Connell S J, Zok F W.Acta Mater, 1997; 45: 5203 |
| [123] | Hutson A, John R, Jira J.Scr Mater, 1999; 40: 529 |
| [124] | Ananth C R, Chandra N.Composites, 1996; 27A: 805 |
| [125] | Cotterill P J, Bowen P.Mater Sci Technol, 1996; 12: 523 |
| [126] | Jones C, Kiely C J, Wang S S.J Mater Res, 1990; 5: 1435 |
| [127] | Hung Y C, Withers P J.Acta Mater, 2012; 60: 958 |
| [128] | Covey S J, Lerch B A, Jayaraman N.Mater Sci Eng, 1995; A200: 68 |
| [129] | Xia Z H, Peters P W M, Dudek H J.Composites, 2000; 31A: 1031 |
| [130] | Thomas M P, Howard G, Pather R, Brown M R, Tranter P H.Int J Fatigue, 2001; 23: 851 |
| [131] | Peters P W M, Hemptenmacher J, Weber K, Assler H.J Comp Technol Res, 2002; 24: 246 |
| [132] | Jeng S M, Yang J M.Mater Sci Eng, 1993; A171: 65 |
| [133] | Schwenker S W, Eylon D.Metall Mater Trans, 1996; 27A: 4193 |
| [134] | Hemptenmacher J, Peters P W M, Weber K.Adv Eng Mater, 2004; 6: 129 |
| [135] | Carrere N, Martin E, Coutand B.Composites, 2003; 34A: 1065 |
| [136] | Gambone M L, Rosenberger A H.Acta Mater, 1999; 47: 1723 |
| [137] | Thomas M P.Mater Sci Eng, 2001; A303: 30 |
| [138] | Zhang X, Wang Y M, Cai G X, Zhang W, Yang R.Chin Pat, 201510247358.9, 2015 |
| [138] | (张旭, 王玉敏, 蔡桂喜, 张薇, 杨锐. 中国专利, 201510247358.9, 2015) |
| [139] | Zhang X, Xiao P, Yang Q, Wang Y M, Lei J F, Yang R.Chin Pat, 201110241083X, 2011 |
| [139] | (张旭, 肖鹏, 杨青, 王玉敏, 雷家峰, 杨锐. 中国专利, 201110241083X, 2011) |
| [140] | Wang Y M, Shi N L, Yang R.Chin Pat, 200510117833.7, 2005 |
| [140] | (王玉敏, 石南林, 杨锐. 中国专利, 200510117833.7, 2005) |
/
| 〈 |
|
〉 |