核用新型耐高温、抗辐照、耐液态金属腐蚀结构材料——SIMP钢的研究进展*

  • 杨柯 ,
  • 严伟 ,
  • 王志光 ,
  • 单以银 ,
  • 石全强 ,
  • 史显波 ,
  • 王威
展开
  • 1 中国科学院金属研究所, 沈阳 110016
    2 中国科学院近代物理研究所, 兰州 730000

收稿日期: 2016-07-20

  网络出版日期: 2016-08-29

基金资助

* 中国科学院战略先导专项项目XDA03010301和XDA03010302资助

DEVELOPMENT OF A NOVEL STRUCTURAL MATERIAL (SIMP STEEL) FOR NUCLEAR EQUIPMENT WITH BALANCED RESIS-TANCES TO HIGH TEMPERATURE, RADIATION AND LIQUID METAL CORROSION

  • Ke YANG ,
  • Wei YAN ,
  • Zhiguang WANG ,
  • Yiyin SHAN ,
  • Quanqiang SHI ,
  • Xianbo SHI ,
  • Wei WANG
Expand
  • 1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
    2 Institute of Modern Physics, Chinese Academy of Sciences, Lanzhou 730000, China

Received date: 2016-07-20

  Online published: 2016-08-29

Supported by

Supported by Strategic Priority Research Program of Chinese Academy of Sciences (Nos.XDA03010301 and XDA03010302)

摘要

加速器驱动次临界(accelerator driven subcritical system, ADS)系统由加速器、散裂靶、反应堆3部分组成, 被认为是安全处理核废料最具前景的技术方案. 其中, 散裂靶用结构材料需要同时具有耐高温、抗辐照、抗液态金属腐蚀等性能. 针对这一挑战研发了新型核用(9%~12%)Cr马氏体耐热钢——SIMP钢. 通过制衡(9%~12%)Cr马氏体耐热钢中C, Cr, Si等元素含量对耐高温、抗辐照、抗液态金属腐蚀性能的影响, 获得了SIMP钢优化的化学成分, 极好地平衡了SIMP钢耐高温、抗辐照、抗液态金属腐蚀3方面性能. 对1 t和5 t SIMP钢各项性能进行测试, 结果表明, SIMP钢是ADS系统中散裂靶的首选结构材料.

本文引用格式

杨柯 , 严伟 , 王志光 , 单以银 , 石全强 , 史显波 , 王威 . 核用新型耐高温、抗辐照、耐液态金属腐蚀结构材料——SIMP钢的研究进展*[J]. 金属学报, 2016 , 52(10) : 1207 -1221 . DOI: 10.11900/0412.1961.2016.00320

Abstract

Accelerator driven subcritical (ADS) system has been recognized to be the most promising technology for safely treating the nuclear wastes by now. In China, ADS system has achieved great progress in both fundamental research and engineering practice. This system is composed of three parts, which are accelerator, spallation target and reactor. The biggest challenge exists in the structural material for the spallation target is to possess not only good heat-resistance and radiation resistance but also a resistance to liquid metal corrosion. A novel martensitic heat-resistant steel, SIMP steel, has been developed against this challenge. By negotiating the effects of the contents of those important elements such as C, Cr and Si in the (9%~12%)Cr martensitic heat-resistant steel on heat resistance, radiation resistance, and liquid metal corrosion resistance, an optimized chemical composition was obtained for SIMP steel and a good balance was reached among these three properties. The test results conducted on 1 t and 5 t grade SIMP steels showed that this novel steel is much potential as a candidate structural material for the spallation target in ADS system.

参考文献

[1] Team of Strategic Priority Program on ADS Transmutation System of Advanced Fission Energy.Bull Chin Acad Sci, 2015; (4): 527
[1] (中国科学院"未来先进核裂变能—ADS嬗变系统"战略性先导科技专项研究团队. 中国科学院院刊, 2015; (4): 527)
[2] Yeliseyeva O, Tsisar V, Benamati G.Corros Sci, 2008; 50: 1672
[3] Martinelli L, Balbaud-Célérier F, Terlain A, Delpech S, Santarini G, Favergeon J, Moulin G, Tabarant M, Picard G.Corros Sci, 2008; 50: 2523
[4] Martinelli L, Balbaud-Célérier F, Terlain A, Bosonnet S, Picard G, Santarini G.Corros Sci, 2008; 50: 2537
[5] Martinelli L, Balbaud-Célérier F.Mater Corros, 2011; 62: 531
[6] Schroer C, Konys J.J Eng Gas Turbines Power, 2010; 132: 082
[7] Klueh R L, Harries D R.High-Chromium Ferritic and Martensitic Steels for Nuclear Applications. ASTM West Conshohocken, PA: American Society for Testing and Materials, 2001: 1
[8] Klueh R, Nelson A.J Nucl Mater, 2007; 371: 37
[9] Chen Y X, Yan W, Hu P, Shan Y Y, Yang K.Acta Metall Sin, 2011; 11: 1372
[9] (陈云翔, 严伟, 胡平, 单以银, 杨柯. 金属学报, 2011; 11: 1372)
[10] Hu P, Yan W, Sha W, Wang W, Shan Y Y, Yang K.J Mater Sci Technol, 2011; 27: 344
[11] Chen X Z, Shen Z, Chen X, Lei Y C, Huang Q Y.Fusion Eng Des, 2011; 86: 2943
[12] Huang Q Y, Li C J, Wu Q S, Liu S J, Gao S, Guo Z H, Yan Z L, Huang B, Yong S, Zhu Z Q, Chen Y P, Ling X X, Wu Y C.J Nucl Mater, 2011; 417: 85
[13] Peng L, Huang Q Y, Li C J, Liu S J. J Nucl Mater, 2009; 386-388: 312
[14] Huang Q, Li J G, Chen Y X. J Nucl Mater, 2004; 329-333: 268
[15] Huang L X, Hu X, Yang C G, Yan W, Xiao F R, Shan Y Y, Yang K.J Nucl Mater, 2013; 443: 479
[16] Hu X, Huang L X, Yan W, Wang W, Sha W, Shan Y Y, Yang K.Mater Sci Eng, 2014; A613: 404
[17] Hu X, Huang L X, Yan W, Wang W, Sha W, Shan Y Y, Yang K.Mater Sci Eng, 2013; A586: 253
[18] Hu X, Huang L X, Wang W G, Yang Z G, Sha W, Wang W, Yan W, Shan Y Y.Fusion Eng Des, 2013; 88: 3050
[19] Lindau R, M?slang A, Rieth M, Klimiankou M, Materna-Morris E, Alamo A, Tavassoli A A F, Cayron C, Lancha A M, Fernandez P, Baluc N, Sch?ublin R, Diegele E, Filacchioni G, Rensman J W, van der Schaaf B, Lucon E, Dietz W. Fusion Eng Des, 2005; 75-79: 989
[20] Lindau R, M?slang A, Schirra M. Fusion Eng Des, 2002; 61-62: 659
[21] Lucon E, Decréton M, van Walle E.Fusion Eng Des, 2003; 69: 373
[22] Lucon E, Vandermeulen W. J Nucl Mater, 2009; 386-388: 254
[23] Marmy P, Kruml T.J Nucl Mater, 2008; 377: 52
[24] Tong Z, Dai Y.J Nucl Mater, 2010; 398: 43
[25] Wang J, Lu S P, Dong W C, Li D Z, Rong L J.Mater Des, 2014; 64: 550
[26] Stubbins J F, Gelles D S. J Nucl Mater, 1996; 233-237: 331
[27] Lapena J, Garcia-Mazario M, Fernandez P, Lancha A M. J Nucl Mater, 2000; 283-287: 662
[28] Nishimura A, Nagasaka T, Inoue N, Muroga T, Namba C. J Nucl Mater, 2000; 283-287: 677
[29] Li H L, Nishimura A, Li Z X, Nagasaka T, Muroga T.Fusion Eng Des, 2006; 81: 241
[30] Li Y F, Nagasaka T, Muroga T, Huang Q Y, Wu Y C. J Nucl Mater, 2009; 386-388: 495
[31] Eliseeva O, Tsisar V, Fedirko V, Matychak Y S.Mater Sci, 2004; 40: 260
[32] Eliseeva O I, Tsisar V P.Mater Sci, 2007; 43: 230
[33] Huntz A M, Bague V, Beauple G, Haut C, Severac C, Lecour P, Longaygue X, Ropital F.Appl Surf Sci, 2003; 207: 255
[34] Panait C G, Bendick W, Fuchsmann A, Gourgues-Lorenzon A F, Besson J.Int J Pressure Vessels Piping, 2010; 87: 326
[35] Aghajani A, Somsen C, Eggeler G.Acta Mater, 2009; 57: 5093
[36] Abd El-Azim M E, Ibrahim O H, El-Desoky O E.Mater Sci Eng, 2013; A560: 678
[37] Taneike M, Fujitsuna N, Abe F.Mater Sci Technol, 2004; 20: 1455
[38] Cerjak H, Hofer P, Schaffernak B.ISIJ Int, 1999; 39: 874
[39] Yong Q L.Secondary Phases in Steels. Beijing: Metallurgical Industry Press, 2006: 433
[39] (雍岐龙. 钢铁材料中的第二相. 北京: 冶金工业出版社, 2006: 433)
[40] Shi Q Q, Liu J, Wang W, Yan W, Shan Y Y, Yang K.Oxid Met, 2015; 83: 521
[41] Niu Y, Wang S, Gao F, Zhang Z G, Gesmundo F.Corros Sci, 2008; 50: 345
[42] Asteman H, Spiegel M.Corros Sci, 2008; 50: 1734
[43] Stott F H, Wei F I.Oxid Met, 1989; 31: 369
[44] Babu N, Balasubramaniam R, Ghosh A.Corros Sci, 2001; 43: 2239
[45] Abderrazik G B, Moulin G, Huntz A, Young E.Solid State Ionics, 1987; 22: 285
[46] Nychka J, Clarke D.Oxid Met, 2005; 63: 325
[47] Mougin J, Dupeux M, Antoni L, Galerie A.Mater Sci Eng, 2003; A359: 44
[48] Li M S.High Temperature Corrosion of Metal. Beijing: Metallurgical Industry Press, 2001: 1
[48] (李美栓. 金属的高温腐蚀. 北京: 冶金工业出版社, 2001: 1)
[49] Kaur I, Gust W.Fundamentals of Grain and Interphase Boundary Diffusion. Stuttgart: Ziegler Press, 1988: 1
[50] Tortorici P C, Dayananda M.Mater Sci Eng, 1998; A244: 207
[51] Pint B A, Wright I G. Mater Sci Forum, 2004; 461-464: 799
[52] Deacon R M, DuPont J, Kiely C, Marder A, Tortorelli P.Oxid Met, 2009; 72: 87
[53] Airiskallio E, Nurmi E, Heinonen M H, Vayrynen I J, Kokko K, Ropo M, Punkkinen M P J, Pitkanen H, Alatalo M, Kollar J, Johansson B, Vitos L.Corros Sci, 2010; 52: 3394
[54] Stott F H, Wei F I.Oxid Met, 1989; 31: 369
[55] Mikkelsen L, Linderoth S, Bilde-S?rensen J. Mater Sci Forum, 2004; 461-464: 117
[56] Pettersson R, Liu L, Sund J.Corros Eng Sci Technol, 2005; 40: 211
[57] Bamba G, Wouters Y, Galerie A, Charlot F, Dellali A.Acta Mater, 2006; 54: 3917
[58] Truman J E, Pirt K R.Corros Sci, 1976; 16: 103
[59] Ishitsuka T, Inoue Y, Ogawa H.Oxid Met, 2004; 61: 125
[60] Robertson J, Manning M I.Mater Sci Technol, 1989; 5: 741
[61] Wang S, Wu Y, Ni C S, Niu Y.Corros Sci, 2009; 51: 511
[62] Horita T, Kishimoto H, Yamaji K, Sakai N, Xiong Y, Brito M E, Yokokawa H.J Power Sources, 2006; 157: 681
[63] Horita T, Yamaji K, Yokokawa H, Toji A, Uehara T, Ogasawara K, Kameda H, Matsuzaki Y, Yamashita S.Int J Hydrogen Energy, 2008; 33: 6308
[64] Liu S, Tang D, Wu H B, Wang L D.J Mater Process Technol, 2013; 213: 1068
[65] Paúl A, Elmrabet S, Alves L C, da Silva M F, Soares J C, Odriozola J A.Nucl Instrum Methods Phys Res, 2001; 181B: 394
[66] Riffard F, Buscail H, Caudron E, Cueff R, Issartel C, Perrier S.Mater Charact, 2002; 49: 55
[67] Li B, Gleeson B.Oxid Met, 2006; 65: 101
[68] Trindade V B, Krupp U, Hanjari B Z, Yang S, Christ H J.Mater Res, 2005; 8: 371
[69] Steiner H.J Nucl Mater, 2009; 383: 267
[70] Eriko Y, Kevin G, Laure M.Corros Sci, 2011; 53: 3075
[71] Schroer C, Skrypnik A, Wedemeyer O, Konys J.Corros Sci, 2012; 61: 63
[72] Schroer C, Wedemeyer O, Novotny J, Skrypnik A, Konys J.Corros Sci, 2014; 84: 113
[73] Cathcart J V, Manly W D.Corrosion, 1956; 12: 43
[74] Malkow T, Steiner H, Muscher H, Konys J.J Nucl Mater, 2004; 335: 199
[75] Marino A, Lim J, Keijers S, Van den Bosch J, Deconinck J.Nucl Eng Des, 2013; 265: 576
[76] Blacha L, Mizera J, Folega P.Metalurgija, 2014; 53: 51
[77] Koury D, Johnson A L, Welch J, Farley J W.J Nucl Mater, 2012; 429: 210
[78] Shankar Rao V, Lim J, Hwang I S, Singhal L K.Corros Sci, 2012; 63: 113
[79] Susmikanti M, Andiwijayakusuma D, Ghofir, Maulana A.In: Su'ud Z, Waris A eds., The 3rd Int Conf on Advances in Nuclear Science and Engineering, Melville: Amer Inst Physic, 2012: 185
[80] Hosemann P, Dickerson R, Dickerson P, Li N, Maloy S A.Corros Sci, 2013; 66: 196
[81] Lambrinou K, Koch V, Coen G, Van den Bosch J, Schroer C.J Nucl Mater, 2014; 450: 244
[82] Kondo M, Takahashi M, Miura K, Onizawa T.J Nucl Mater, 2006; 357: 97
[83] Brissonneau L, Beauchamp F, Morier O, Schroer C, Konys J, Kobzova A, Di Gabriele F, Courouau J L.J Nucl Mater, 2011; 415: 348
[84] Ganesan R, Gnanasekaran T, Srinivasa R S.J Nucl Mater, 2006; 349: 133
[85] Lim J, Manfredi G, Gavrilov S, Rosseel K, Aerts A, Van den Bosch J.Sens Actuators, 2014; 204B: 388
[86] Li N.J Nucl Mater, 2002; 300: 73
[87] Ilincev G, Karnik D, Paulovic M, Doubkova A.Nucl Eng Des, 2006; 236: 1909
[88] Viswanathan R, Sarver J, Tanzosh J M.J Mater Eng Perform, 2006; 15: 255
[89] Fry A, Osgerby S, Wright M.Comp Methods Appl Mech Eng, 2002; 85: 374
[90] Ren X, Sridharan K, Allen T R.Mater Corros, 2010; 61: 748
[91] Bischoff J, Motta A T, Comstock R J.J Nucl Mater, 2009; 392: 272
[92] Shi Q Q, Liu J, Luan H, Yang Z G, Wang W, Yan W, Shan Y Y, Yang K.J Nucl Mater, 2015; 457: 135
[93] Birks N, Meier G H, Pettit F S.Introduction to the High Temperature Oxidation of Metals. New York: Cambridge University Press: 2006: 1
[94] Martinelli L, Balbaud-Celerier F, Terlain A, Bosonnet S, Picard G, Santarini G.Corros Sci, 2008; 50: 2537
[95] Bischoff J, Motta A T.J Nucl Mater, 2012; 424: 261
[96] Liu J, Shi Q Q, Luan H, Yan W, Sha W, Wang W, Shan Y Y, Yang K.Mater Sci Eng, 2016; A670: 97
[97] Wang J, Gao X, Wang Z G, Wei K F, Yao C F, Cui M H, Sun J R, Li B S, Pang L L, Zhu Y B, Luo P, Chang H L, Zhang H P, Zhu H P, Wang D, Du Y Y, Xie E Q.Chin Phys Lett, 2015; 32(7): 076101
[98] Wang J, Gao X, Gao N, Wang Z G, Cui M H, Wei K F, Yao C F, Sun J R, Li B S, Zhu Y B, Pang L L, Li Y F, Wang D, Xie E Q.J Nucl Mater, 2015; 457: 182
[99] Zhu H P, Wang Z G, Gao X, Cui M H, Li B S, Sun J R, Yao C F, Wei K F, Shen T L, Pang L L.Nucl Instrum Meth, 2015; 344B: 5
[100] Zhu H P, Wang Z G, Cui M H, Li B S, Gao X, Sun J R, Yao C F, Wei K F, Shen T L, Pang L L, Zhu Y B, Li Y F, Wang J, Xie E Q.Appl Surf Sci, 2015; 326: 1
[101] Li Y F, Shen T L, Gao Xing, Yao C F, Wei K F, Sun J R, Li B S, Zhu Y B, Pang L L, Cui M H, Chang H L, Wang J, Zhu H P, Hu B T, Wang Z G.Chin Phys Lett, 2013; 30: 126101
文章导航

/