论文

基于热溶质对流及晶粒运动的柱状晶-非球状等轴晶混合三相模型*

  • 李军 ,
  • 葛鸿浩 ,
  • GE Honghao ,
  • WU Menghuai ,
  • 李建国
展开
  • 1 上海交通大学材料科学与工程学院, 上海 200240
    2 Simulation and Modeling of Metallurgical Processes, University of Leoben, A-8700, Austria
    3 Christian-Doppler Lab for Advanced Process Simulation of Solidification and Melting, University of Leoben, A-8700, Austria

收稿日期: 2015-12-07

  网络出版日期: 2016-06-22

基金资助

* 克里斯汀-多普勒(先进凝固和融化模拟实验室)项目, 国家自然科学基金项目51404152, 国家重点基础研究发展计划项目2011CB012900, 上海市浦江人才支持计划项目14PJ1404800和上海市国际合作项目14140711000资助

A COLUMNAR & NON-GLOBULAR EQUIAXED MIXED THREE-PHASE MODEL BASED ON THERMOSOLUTAL CONVECTION AND GRAIN MOVEMENT

  • Jun LI ,
  • Honghao GE ,
  • Menghuai WU ,
  • Andreas LUDWIG ,
  • Jianguo LI
Expand
  • 1 School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China
    2 Simulation and Modeling of Metallurgical Processes, University of Leoben, A-8700, Austria
    3 Christian-Doppler Lab for Advanced Process Simulation of Solidification and Melting, University of Leoben, A-8700, Austria

Received date: 2015-12-07

  Online published: 2016-06-22

Supported by

Support by Christian-Doppler Lab for Advanced Process Simulation of Solidification and Melting (Austria), National Natural Science Foundation of China (No.51404152), National Basic Research Program of China (No.2011CB012900), Shanghai Pujiang Program (No.14PJ1404800) and Shanghai International Cooperation Project (No.14140711-000)

摘要

基于Eulerian-Eulerian方法, 阐述了简化枝晶状等轴晶、柱状晶以及金属液三相完全混合的凝固模型. 模型考虑了等轴晶的移动及柱状晶对等轴晶的捕获, 跟踪了柱状晶尖端的位置并考虑了等轴晶和柱状晶的相互竞争生长, 因此该模型具备了预测柱状晶向等轴晶转变(CET)的能力; 为了在不过量增加计算量的前提下提高模型的精度, 模型对等轴晶采取了简单的枝晶化处理, 即采用简化方法描述等轴晶包络线内固相分数. 分别模拟了3.25和25 t钢锭的凝固过程, 成功预测了大型钢锭凝固过程所形成的底部锥形负偏析、“类-A型”偏析以及CET等现象. 分析认为长细形状铸锭中出现的顶部负偏析区, 是由于凝固后期所形成的局部小钢锭及等轴晶在其内部的沉积聚集而成.

本文引用格式

李军 , 葛鸿浩 , GE Honghao , WU Menghuai , 李建国 . 基于热溶质对流及晶粒运动的柱状晶-非球状等轴晶混合三相模型*[J]. 金属学报, 2016 , 52(9) : 1096 -1104 . DOI: 10.11900/0412.1961.2015.00627

Abstract

The prediction of the macrosegregation in large ingot is a challenging issue due to the size of the ingots and the variety of the phenomena to be accounted for, such as thermal-solutal convection of the liquid, equiaxed grain motion, evolution of grain morphology by suitably considering a coupled grain growth model in the macroscopic solidification model, the columnar-to-equiaxed transition (CET), and shrinkage, etc.. Each of these phenomena is very important to the solidification pattern, while it is impossible for one model to consider all the phenomena together until now due to the computation power limited. Thus, the model capability and computational cost should be counterpoised for the simulation of large ingot. In this work, a mixed three-phase (simplified dendritic-equiaxed, columnar and liquid) solidification model is described based on Eulerian-Eulerian approach and volume average method. The model considers the thermosolutal buoyancy flow, the movement of equiaxed crystal, and the capture of the equiaxed crystals by growing columnar tree trunks. The mechanical interaction and impingement between columnar and equiaxed crystals are considered which give the capability to predict CET. In order to enhance the model capability without increasing the computational cost significantly, a simplified method is proposed to consider the dendritic of equiaxed crystal. This model is employed to simulate the formation process of macrosegregation for two different steel ingots (3.25 and 25 t). The general macrosegregation pattern predicted by this model includes the cone of negative segregation in the bottom of ingot, quasi-A-segregation in the columnar zone, and positive segregation in the top region, which are quite similar to the classic knowledge. The CET zones are also predicted. Although there is still some quantitative discrepancy, the macrosegregation distribution predicted by this model is quite similar to the experimental measurements. The non-globular equiaxed three-phase mixed model results are compared with the globular-equiaxed mixed three-phase model ones, which indicated that for large ingots the equiaxed dendritic structure plays an important role in liquid flow and it affects final characteristic of macrosegregation. It is predicted successfully that a negative segregation zone would be formed in the upper region due to the formation of a local mini-ingot and the subsequent sedimentation and piling up of equiaxed grains within the mini-ingot.

参考文献

[1] Ludwig A, Wu M, Kharicha A.Metall Mater Trans, 2015; 46A: 4856
[2] Pickering E J. ISIJ, 2013; 53: 935
[3] Du Q, Li D Z, Li Y Y.Acta Metall Sin, 2000; 36: 1197
[3] (杜强, 李殿中, 李依依. 金属学报, 2000; 36: 1197)
[4] Han Z Q, Liu B C.Acta Metall Sin, 2003; 39: 140
[4] (韩志强, 柳百成. 金属学报, 2003; 39: 140)
[5] Cao H F, Shen H F, Liu B C.Acta Metall Sin, 2005; 41: 917
[5] (曹海峰, 沈厚发, 柳百成. 金属学报, 2005; 41: 917)
[6] Wang T M, Yao S, Zhang X G, Jin J Z, Wu M, Ludwig A, Pustal B, Polaczek A.Acta Metall Sin, 2006; 42: 584
[6] (王同敏, 姚山, 张兴国, 金俊泽, Wu M, Ludwig A, Pustal B, Polaczek A. 金属学报, 2006; 42: 584)
[7] Flemings M C, Nereo G E.Trans Met Soc AIME, 1967; 239: 1449
[8] Dantzig J A, Rappaz M. Solidification. Switzerland, EPFL Press, 2009: 568
[9] Li X, Noeppel A, Saadi B, Budenkova O, Zaidat K, Ciobanas A, Ren Z, Fautrelle Y.Trans Indian Ins Met, 2009; 62: 465
[10] Li J, Wu M, Hao J, Ludwig A.Comp Mater Sci, 2012; 55: 407
[11] Li J, Wu M, Hao J, Ludwig A.Comp Mater Sci, 2012; 55: 419
[12] Mehrabian R, Keane M, Flemings M C.Metall Trans, 1970; 1: 1209
[13] Flemings M C.Scand J Metall, 1976; 5: 1
[14] Olsson A, West R, Fredriksson H.Scand J Metall, 1986; 15: 104
[15] Schneider M, Beckermann C.Metall Mater Trans, 1995; 26A: 2373
[16] Liu D R, Li D Z, Sang B G.J Mater Sci Technol, 2009; 25: 561
[17] Liu D R, Kang X H, Fu P, Li D Z.Kovove Mater, 2011; 49: 143
[18] Liu D R, Kang X H, Sang B G, Li D Z.Acta Metall Sin (Engl Lett), 2011; 24: 54
[19] Liu D R, Sang B G, Kang X H, Li D Z.Int J Cast Met Res, 2010; 23: 354
[20] Li W S, Shen H F, Liu B C.Steel Res Int, 2010; 81: 994
[21] Tu W T, Shen H F, Liu B C.ISIJ, 2014; 54: 351
[22] Combeau H, Zaloznik M, Hans S, Richy P.Metall Mater Trans, 2009; 40B: 289
[23] Ge H H, Li J, Han X J, Xia M X, Li J G.J Mater Process Technol. 2016; 227: 308
[24] Wu M, Ludwig A.Metall Mater Trans, 2006; 37A: 1613
[25] Wu M, Ludwig A.Metall Mater Trans, 2007; 38A: 1465
[26] Li J, Wu M, Ludwig A, Kharicha A.IOP Conference Series: Mater Sci Eng, 2012; 33: 012091
[27] Li J, Wu M, Ludwig A, Kharicha A.Int J Heat Mass Transfer, 2014; 72: 668
[28] Wu M, Fjeld A, Ludwig A.Comp Mater Sci, 2010; 50: 32
[29] Rappaz M. Int Mater Rev, 1989; 34: 93
[30] Wu M, K?n?zsy L, Ludwig A, Schützenh?fer W, Tanzer R.Steel Res Int, 2008; 79: 637
[31] Wu M, Li J, Ludwig A, Kharicha A.Comp Mater Sci, 2013; 79: 830
[32] Wu M, Ludwig A.Acta Mater, 2009; 57: 5621
[33] Ahmadein M, Wu M, Ludwig A.J Cryst Growth, 2015; 417: 65
[34] Li J, Wu M, Ludwig A, Kharicha A, Schumacher P. Mater Sci Forum, 2014; 790-791: 121
[35] Wang C Y, Ahuja S, Beckermann C, de Groh H C.Metall Mater Trans, 1995; 26B: 111
[36] Heterogeneity Sub-Committee of the British Iron and Steel Institute.J Iron Steel Inst London, 1926; 113: 39
[37] Wu M, Li J, Ludwig A, Kharicha A.Comp Mater Sci, 2014; 92: 267
文章导航

/