单晶DD3与细晶GH4169高温合金摩擦焊接界面表征*

展开

录用日期: 2015-05-26

  网络出版日期: 2015-08-27

基金资助

*国家自然科学基金资助项目51175430

CHARACTERISTICS OF THE FRICTION WELDING INTERFACE BETWEEN SINGLE CRYSTAL SUPERALLOY DD3 AND FINE GRAINED SUPERALLOY GH4169

  • Suigeng DU ,
  • Xifeng WANG ,
  • Man GAO
Expand
  • Key Laboratory of Ministry of Education for Contemporary Design and Integrated Manufacturing Technology, Northwestern Polytechnical University, Xi'an 710072

Accepted date: 2015-05-26

  Online published: 2015-08-27

Supported by

Supported by National Natural Science Foundation of China (No.51175430)

摘要

采用SEM, TEM及EDS对制造焊接式整体涡轮叶盘所用的单晶DD3与细晶GH4169高温合金摩擦焊接界面进行了研究. 结果表明, 焊合区存在一条以GH4169合金为主的摩擦变形带, 两侧单晶和细晶合金的热力影响区均形成了动态再结晶晶粒; 连接界面处于两侧合金的动态再结晶晶粒之间, 通过连接界面上的共有晶粒和共有晶界实现了两侧合金的连接; 成分过渡主要发生在连接界面处的共有晶粒内和共有晶界处. TEM分析位置的共有晶粒(C2)与相邻GH4169动态再结晶晶粒(C3)具有特殊的取向关系: [1ˉ14]C2 ∥ [1ˉ10]C3 和(220)C2 ∥ (220)C3; 在摩擦焊热循环及焊后热处理作用下, 共有晶粒、两侧动态再结晶晶粒都存在g' 相析出, g' 相呈细小的球形分布, 并与g基体共格, 但未发现有g" 相析出.

本文引用格式

杜随更,王喜锋,高漫 . 单晶DD3与细晶GH4169高温合金摩擦焊接界面表征*[J]. 金属学报, 2015 , 51(8) : 951 -956 . DOI: 10.11900/0412.1961.2014.00686

Abstract

Due to high demand of welded turbine blisk, a fine grain superalloy, GH4169, has been widely used to make the disk and a single crystal superalloy, DD3, has been used for blades. In this work, the joint micro-structure and the mechanism of friction welding between the GH4169 and DD3 have been investigated by using the SEM and TEM equipped with EDS. The research results show that there is a friction deformed band of the GH4169 in the weld zone. The heat and mechanical affected zones of the two alloys form dynamic recrystallization grains. The bonding interface is between their dynamic recrystallization grains. The two alloys bond with the common grains and the common grain boundaries. Their compositional change mainly occurs within the common grains and the common grain boundaries at bonding interface. The common grain (C2) at the viewpoint of TEM analysis and adjacent dynamic recrystallization grain (C3) of the GH4169 has a specific orientation relationship, [1ˉ14]C2 ∥ [1ˉ10]C3 , (220)C2 ∥ (220)C3. With the friction welding thermal cycles and post weld heat treatment, the g' phase precipitates with tiny spherical distribution at the common grain and the two sides of dynamic recrystallization grains, and coherent with g matrix. But no g" phase precipitates.

参考文献

[1] Pollock T M, Tin S. J Propul Power, 2006; 22: 361
[2] Huang C F. Aero Manuf Technol, 2006; (4): 94 (黄春峰. 航空制造技术, 2006; (4): 94)
[3] Yilmaz O, Gindy N, Gao J. Rob Comput-Integrated Manuf, 2010; 26: 190
[4] Mateo A. Revista Metalurgia, 2014; 50(3): e023
[5] Preuss M, Withers P J, Baxter G J. Mater Sci Eng, 2006; A437: 38
[6] Schnell A, Hoebel M, Samuleson J. Adv Mater Res, 2011; 278: 434
[7] Henderson M B, Arrell D, Larsson R, Heobel M, Marchant G. Sci Technol Weld Joining, 2004; 9: 13
[8] Damodaram R, Raman S G S, Rao K P. Mater Sci Eng, 2013; A560: 781
[9] Bhamji I, Preuss M, Threadgill P L, Addison A C. Mater Sci Technol, 2011; 27: 2
[10] Moosavy H N, Aboutalebi M, Seyedein S H. J Mater Process Technol, 2012; 212: 2210
[11] Chamanfar A, Jahazi M, Cormier J. Metall Mater Trans, 2015; 46A: 1
[12] Ojo O A. J Mater Sci, 2012; 47: 1598
[13] Liu J D, Jin T, Zhao N R, Wang Z H, Sun X F, Guan H R, Hu Z Q. Sci Technol Weld Joining, 2010; 15: 194
[14] Steuer S, Singer R F. Metall Mater Trans, 2014; 45A: 3545
[15] Liu J, Cao J, Lin X, Song X, Feng J. Mater Des, 2013; 49: 622
[16] Karadge M, Preuss M, Withers P J, Bray S. Mater Sci Eng, 2008; A491: 446
[17] Du S G, Fu L, Wang Z P. J Northwest Polytech Univ, 2003; 21: 136 (杜随更, 傅 莉, 王忠平. 西北工业大学学报, 2003; 21: 136)
[18] Du S G, Wang Q, Fu L. Trans Chin Weld Ins, 2002; 23(4): 27 (杜随更, 王 庆, 傅 莉. 焊接学报, 2002; 23(4): 27)
[19] Du S G, Wang X F, Wang J W, Jiang Z. Trans Chin Weld Ins, 2014; 35(6): 13 (杜随更, 王喜锋, 王晋伟, 姜 哲. 焊接学报, 2014; 35(6): 13)
[20] China Aeronautical Materials Handbook Editorial Committee. China Aeronautical Materials Handbook. Vol.2, Beijing: China Standard Press, 2002: 842 (中国航空材料手册编辑委员会. 中国航空材料手册. 第2卷, 北京: 中国标准出版社, 2002: 842)
[21] Xiong J C, Li J R, Zhao J Q, Liu S Z, Dong J X. Acta Metall Sin, 2009; 45: 1232 (熊继春, 李嘉荣, 赵金乾, 刘世忠, 董建新. 金属学报, 2009; 45: 1232)
[22] Wu C L, Xu Q Y, Xiong J C, Li Z L, Li J R, Liu B C. Acta Metall Sin, 2013; 49: 523 (吴春龙, 许庆彦, 熊继春, 李忠林, 李嘉荣, 柳百成. 金属学报, 2013; 49: 523)
[23] Chen X, Lin Y C, Wen D, Zhang J, He M. Mater Des, 2014; 57: 568
[24] Geddes B, Leon H, Huang X. Superalloys: Alloying and Performance. Materials Park, Ohio: ASM International, 2010: 10
[25] Xie X S, Dong J X, Fu S H, Zhang M C. Acta Metall Sin, 2010; 46: 1289 (谢锡善, 董建新, 付书红, 张麦仓. 金属学报, 2010; 46: 1289)
文章导航

/

〈 〉