一种基于黏弹性理论预测DP600钢板滞后回弹的新模型*

展开

网络出版日期: 2015-08-10

基金资助

* 国家自然科学基金资助项目51175044

A NOVEL MODEL BASED ON VISCOELASTIC THEO- RY TO PREDICT THE TIME-DEPENDENT SPRINGBACK FOR DP600 STEEL SHEET

  • Shuai SUN ,
  • Daxin E
Expand
  • School of Materials, Beijing Institute of Technology, Beijing 100081

Online published: 2015-08-10

Supported by

Supported by National Natural Science Foundation of China (No.51175044)

摘要

通过加载不同预应变和保压时间获得了DP600钢板的室温滞后回弹响应. 基于黏弹性理论, 采用309 MPa恒应力室温蠕变实验, 获得了预测滞后回弹过程的蠕变柔量函数. 基于DP600钢板室温弹性和塑性加载响应, 修正了线黏弹性本构方程的积分下限, 将柔量函数与修正的应力率函数进行卷积, 获得了影响滞后回弹过程的加载历史效应. 再将加载历史应变波形与卸载脉冲叠加, 获得不同预变形量的滞后回弹应变预测值. 结果表明, 滞后回弹初期应变率较高, 之后应变率逐渐降低; 随着预应变的增加, 滞后回弹应变的绝对值逐渐递增, 并且滞后回弹占总回弹比例逐渐增加; 滞后回弹预测方向与瞬时回弹方向相同, 与加载方向相反; 相同时间段内, 蠕变回弹应变比滞后回弹应变明显降低, 与滞后回弹实验相比, 蠕变恒应力与蠕变回弹应变的比值随预应变的变化规律呈现出良好的线性关系; 基于黏弹性理论的修正模型所得到的预测值接近实验测量值, 并能够较好地反映实验变化规律.

本文引用格式

孙帅,鄂大辛 . 一种基于黏弹性理论预测DP600钢板滞后回弹的新模型*[J]. 金属学报, 2015 , 51(11) : 1356 -1364 . DOI: 10.11900/0412.1961.2015.00176

Abstract

DP600 steel sheet with high strength has drawn much attention in the automotive industry, but the shape change following forming and unloading has not been known widely. The time-dependent springback of DP600 steel sheet was investigated under different pre-strains by uniaxial tension. According to the viscous behaviors under the elastic and plastic loading tests, the lower limit of integration in the constitutive equation of linear viscoelasticity was modified and the creep compliance was gained from the creep curve at a constant stress level of 309 MPa at room temperature. The predicted curve was acquired by using the superposition of the unloading impulse and the historical loading curve. The results reveal that the strain rates with high initial values gradually decreased following unloading at room temperature. As the pre-strain went up, both the absolute anelastic strain of time-dependent springback and the anelastic proportion of the total springback increased. Meanwhile, the direction of the time-dependent springback was same as that of the initial springback and opposite to the loading direction. In the same springback period, the ratio of the unloading stress to the creep springback strain tended to vary more linearly with the pre-strain than those obtained from immediate unloading. The simulated results using the revised model are in good agreement with the experimental data.

参考文献

[1] Wagoner R H, Lim H, Lee M G. Int J Plasticity, 2013; 45: 3
[2] Fei D Y, Hodgson P. Nucl Eng Des, 2006; 236: 1847
[3] Geng L M, Wagoner R H. Int J Mech Sci, 2002; 44: 123
[4] Li K P, Carden W P, Wagoner R H. Int J Mech Sci, 2002; 44: 103
[5] E D X, Liu Y F. Mater Des, 2010; 31: 3
[6] Cleveland R M, Ghosh A K. Int J Plasticity, 2002; 18: 769
[7] Correia J P M, Sim?es F, Gracio J J, Barlat F, Ahzi S. Mater Sci Eng, 2007; A456: 170
[8] Ryou H, Chung K. Compos Sci Technol, 2009; 69: 292
[9] Zener C. Elasticity and Anelasticity of Metals. Chicago: University of Chicago Press, 1948: 3
[10] Nowick A S,Berry B S. Anelastic Relaxation in Crystalline Solids. New York: Academic Press, 1972: 21
[11] Munitz A, Kaufman M J. J Mater Sci, 2013; 48: 5361
[12] Li B, McClelland Z, Horstemeyer S J, Aslam I, Wang P T, Horstemeyer M F. Mater Des, 2015; 66: 575
[13] Wang J F, Wagoner R H, Carden W D, Matlock D K, Barlat F. Int J Plasticity, 2004; 20: 12
[14] Lim H, Lee M G, Sung J H, Kim J H, Wagoner R H. Int J Plasticity, 2012; 29: 42
[15] Yang T Q,Luo W B,Xu P,Wei Y T,Gang Q G. Viscoelastic Theory and Application. Beijing: Science Press, 2004: 3 (杨挺青,罗文波,徐 平,危银涛,刚芹果. 黏弹性理论与应用. 北京: 科学出版社, 2004: 3)
[16] Zang S L, Lee M G, Kim J H. Int J Mech Sci, 2013; 77: 194
[17] Michael E, Kassner, Kamia S. J Mater Res Technol, 2014; 3: 280
[18] Nie D F, Zhao J, Zhang J S. Acta Metall Sin, 2011; 47: 179 (聂德福, 赵 杰, 张俊善. 金属学报, 2011; 47: 179)
[19] Shui L, Jin T, Tian S G, Hu Z Q. Acta Metall Sin, 2007; 43: 47 (水 丽, 金 涛, 田素贵, 胡壮麒. 金属学报, 2007; 43: 47)
[20] Nie D F, Zhao J. Acta Metall Sin, 2009; 45: 840 (聂德福, 赵 杰. 金属学报, 2009; 45: 840)
[21] Sorvari J, Malinen M. Int J Solids Struct, 2006; 44: 1291
[22] Sorvari J, Malinen M, Hamalainen J. Int J Non-Linear Mech, 2006; 41: 1050
[23] Findley W N, Lai J S, Onaran K. Creep and Relaxation of Nonlinear Viscoelastic Materials. New York: North-Holland Publishing Company, 1976: 50
[24] Park S W, Schapery R A. Int J Solids Struct, 1999; 36: 1653
[25] Schapery R A, Park S W. Int J Solids Struct, 1999; 36: 1677
[26] Sorvari J, Malinen M. Mech Time-Depend Mater, 2007; 11: 143
文章导航

/

〈 〉