STUDY OF MARTENSITIC TRANSFORMATION AND STRAIN BEHAVIOR IN Ni50-xCoxMn39Sn11 (x=0, 2, 4, 6) HEUSLER ALLOYS

  • Zhe LI ,
  • Chen XU ,
  • Kun XU ,
  • Hao WANG ,
  • Yuanlei ZHANG ,
  • Chao JING
Expand
  • 1 Key Laboratory for Advanced Functional and Low Dimensional Materials of Yunnan Higher Education Institute, College of Physics and Electronic Engineering, Qujing Normal University, Qujing 655011
    2 Department of Physics, Shanghai University, Shanghai 200444

Accepted date: 2015-04-28

  Online published: 2015-06-16

Supported by

Supported by National Natural Science Foundation of China (Nos.11364035, 11404186 and 51371111), Applied Basic Research Programs of Yunnan Province (Nos.2013FZ110 and 2012FD051) and Innovative Research Team of Qujing Normal University (No.TD201301)

摘要

通过结构和磁性测量, 研究了Ni50-xCoxMn39Sn11 (x=0, 2, 4, 6) Heusler合金的晶体结构、相变和磁性. 结果表明, 随Co含量增加, 该系列合金的马氏体相变温度明显下降, 而Curie温度却呈现出上升的趋势, 并在室温下展现出不同的晶体结构. 同时, Co含量的增加导致样品在奥氏体相的磁性迅速增加, 而马氏体相的磁性却几乎保持不变, 显著地提高了2相之间的磁化强度差异(ΔM). 特别是当Co含量增加到x=4时, 2相之间的ΔM达到40 Am2/kg, 并表现出磁场驱动马氏体相变的特征. 此外, 还研究了Ni50-xCoxMn39Sn11 (x=0, 2, 4)样品在马氏体相变过程中的应变行为. 其中, x=4样品的相变应变量达到了0.17%, 通过3 T的磁场循环, 该样品在215~235 K的温度范围均显示出可回复磁感生应变. 这种可回复的应变行为可归因于样品中的部分马氏体相变可由等温磁场驱动.

本文引用格式

李哲,徐琛,徐坤,王豪,张元磊,敬超 . Ni50-xCoxMn39Sn11 (x=0, 2, 4, 6) Heusler合金的马氏体相变和应变行为研究*[J]. 金属学报, 2015 , 51(8) : 1010 -1016 . DOI: 10.11900/0412.1961.2015.00071

Abstract

The crystal structure, phase transformations and magnetic properties for Ni50-xCoxMn39Sn11 (x=0, 2, 4, 6) Heusler alloys have been systematically studied by means of structure and magnetism measurements. The results show that with increase of Co concentration, the martensitic transformation temperatures are obviously decreased, while the Curie temperatures of austenite are gradually increased, and they present different structures at room temperature. At the same time, with increasing Co content, the austenitic magnetism rapidly enhances, while the martensitic magnetism almost keeps unchanged. This leads to a significant improvement of difference magnetization (ΔM) between two phases. For Co content added to x=4, the value of ΔM between two phases achieves about 40 Am2/kg and exhibits magnetic field-induced martensitic transformation. Using strain measurement, the strain behavior related to martensitic transition in Ni50-xCoxMn39Sn11 (x=0, 2, 4) samples was studied. It is found that the phase transition strain reaches 0.17% in Ni46Co4Mn39Sn11 sample. Within the magnetic cycles of 3 T, this sample displays a reproducible magnetostrain in temperature range of 215~235 K. Such a reproducible strain could be ascribed to the fact that a partial martensitic transformation of this sample can be driven by isothermal magnetic field.

参考文献

[1] Murray S J, Marioni M, Allen S M, O'Handley R C, Lograsso T A. Appl Phys Lett, 2000; 77: 886
[2] Sozinov A, Likhachev A A, Lanska N, Ullakko K. Appl Phys Lett, 2002; 80: 1746
[3] Weiss S, Scheerbaum N, Liu J, Klauss H, Schultz L, M?der E, H?bler R, Heinrich G, Gutfleisch O. Adv Eng Mater, 2012; 14: 20
[4] Li Z, Wang J M, Liu W C, Jiang C B. Acta Metall Sin, 2008; 44: 302 (李 灼, 王敬明, 刘伟超, 蒋成保. 金属学报, 2008; 44: 302)
[5] You S Q, Cui Y T, Wu L, Kong C Y, Ma Y, Yang X H, Pan F S. Acta Metall Sin, 2009; 45: 351 (游素琴, 崔玉婷, 武 亮, 孔春阳, 马 勇, 杨晓红, 潘复生. 金属学报, 2009; 45: 351)
[6] O'Handley R C. J Appl Phys, 1998; 83: 3263
[7] Sutou Y, Imano Y, Koeda N, Omori T, Kainuma R, Ishida K, Oikawa K. Appl Phys Lett, 2004; 85: 4358
[8] Koyama K, Watanabe K, Kanomata T, Kaimuma R, Oikawa K, Ishida K. Appl Phys Lett, 2006; 88: 132505
[9] Oikawa K, Ito W, Imano Y, Sutou Y, Kainuma R, Ishida K, Okamoto S, Kitakami O, Kanomata T. Appl Phys Lett, 2006; 88: 122507
[10] Kainuma R, Imano Y, Ito W, Sutou Y, Morito H, Okamoto S, Kitakami O, Oikawa K, Fujita A, Kanomota T, Ishida K. Nature, 2006; 439: 957
[11] Kainuma R, Imano Y, Ito W, Morito H, Sutou Y, Oikawa K, Fujita A, Ishida K, Okamoto S, Kitakami O. Appl Phys Lett, 2006; 88: 192513
[12] Krenke T, Duman E, Acet M, Wassermann E, Moya X, Ma?osa L, Planes A. Phys Rev, 2007; 75B: 104414
[13] Sharma V K, Chattopadhyay M K, Chouhan A, Roy S B. J Phys, 2009; 42D: 185005
[14] Pathaka A K, Dubenkoa I, Stadlerb S, Ali N. J Alloys Compd, 2011; 509: 1106
[15] Liu J, Aksoy S, Scheerbaum N, Acet M, Gutfleisch O. Appl Phys Lett, 2009; 95: 232515
[16] Li Z, Jing C, Zhang H L, Yu D H, Chen L, Kang B J, Cao S X, Zhang J C. J Appl Phys, 2010; 108: 113908
[17] Jing C, Wang X L, Liao P, Li Z, Yang Y J, Kang B J, Deng D M, Cao S X, Zhang J C, Zhu J. J Appl Phys, 2013; 114: 063907
[18] Planes A, Ma?osa L, Acet M. J Phys: Condens Matter, 2009; 21: 233201
[19] Ito W, Xu X, Umetsu R, Kanomata T, Ishida K, Kainuma R. Appl Phys Lett, 2010; 97: 242512
[20] Ma S C, Xuan H C, Zhang C L, Wang L Y, Cao Q Q, Wang D H, Du Y W. Appl Phys Lett, 2010; 97: 052506
[21] Cong D Y, Roth S, Schultz L. Acta Mater, 2012; 60: 5335
[22] Yu S Y, Wei J J, Kang S S, Chen J L, Wu G H. J Alloys Compd, 2014; 586: 328.
[23] Ye M, Kimura A, Miura Y, Shirai M, Cui Y T, Shimada K, Namatame H, Taniguchi M, Ueda S, Kobayashi K, Kainuma R, Shishido T, Fukushima K, Kanomata T. Phys Rev Lett, 2010; 104: 176401.
[24] Khan M, Jung J, Stoyko S S, Mar A, Quetz A, Samanta T, Dubenko I, Ali N, Stadler S, Chow K H. Appl Phys Lett, 2012; 100: 172403.
[25] Liu Z H, Yi B, Li G T, Ma X Q. Acta Phys Sin, 2012; 61: 108104 (柳祝红, 伊 比, 李歌天, 马星桥. 物理学报, 2012; 61: 108104)
[26] ?a?io?lu E, Sandratskii L M, Bruno P. Phys Rev, 2008; 77B: 064417
[27] Stager C V, Campbell C C M. Can J Phys, 1978; 56: 674
[28] Ma L, Zhang H W, Yu S Y, Zhu Z Y, Chen J L, Wu G H, Liu H Y, Qu J P, Li Y X. Appl Phys Lett, 2008; 92: 032509
[29] Yu S Y, Cao Z X, Ma L, Liu G D, Chen J L, Wu G H, Zhang B, Zhang X X. Appl Phys Lett, 2007; 91: 102507
[30] Yu S Y, Ma L, Liu G D, Liu Z H, Chen J L, Cao Z X, Wu G H, Zhang B, Zhang X X. Appl Phys Lett, 2007; 90: 242501
[31] Wang W H, Liu Z H, Chen J L, Zhang J, Wu G H, Zhan W S. Phys Rev, 2001; 65B: 012416
[32] Shamberger P J, Ohuchi F. Phys Rev, 2009; 79B: 144407
文章导航

/

〈 〉