强磁场作用时间对氧化法制备的Co掺杂ZnO薄膜微观结构和光学性能的影响

  • 李国建 ,
  • 王振 ,
  • 王强 ,
  • 王慧敏 ,
  • 杜娇娇 ,
  • 马永会 ,
  • 赫冀成
展开
  • 东北大学材料电磁过程研究教育部重点实验室, 沈阳 110819
null

李国建, 男, 1980年生, 副教授, 博士

修回日期: 2014-07-09

  网络出版日期: 2014-12-25

基金资助

* 国家自然科学基金项目51101034, 以及中央高校基本科研业务费项目N130509002, N120609001和N110809001资助

EFFECT OF OXIDATION TIME UNDER HIGH MAG- NETIC FIELD ON THE MICROSTRUCTURE AND OPTICAL PROPERTIES OF OXIDIZED Co-DOPED ZnO FILMS

  • Guojian LI ,
  • Zhen WANG ,
  • Qiang WANG ,
  • Huimin WANG ,
  • Jiaojiao DU ,
  • Yonghui MA ,
  • Jicheng HE
Expand
  • Key Laboratory of Electromagnetic Processing of Materials (Ministry of Education), Northeastern University, Shenyang 110819

Revised date: 2014-07-09

  Online published: 2014-12-25

Supported by

Supported by National Natural Science Foundation of China (No.51101034), Fundamental Research Funds for the Central Universities (Nos.N130509002, N120609001 and N110809001)

摘要

利用FESEM, XRD和紫外可见分光光度计研究了强磁场作用时间对真空蒸发氧化法制备的Co掺杂ZnO薄膜微观结构和光学性能的影响. 结果表明: 强磁场抑制了ZnO珊瑚枝状形貌的生长, 氧化60 min时, 无磁场下生长成球状颗粒, 而6 T磁场下则生长成片状组织. 强磁场作用时间的增加会使薄膜的择优生长从(101)变成(002); 影响磁性Co原子在ZnO中的分布; 薄膜的禁带宽度降低到2.95~3.13 eV的范围内. 另外, 无磁场时氧化时间的增加会降低薄膜的透光率, 而强磁场下氧化时间的增加会提高透光率. 这些研究结果为ZnO薄膜表面形貌、择优生长、磁性原子分布、透光率和禁带宽度等微观结构和光学性能的调控提供了一种新方法.

本文引用格式

李国建 , 王振 , 王强 , 王慧敏 , 杜娇娇 , 马永会 , 赫冀成 . 强磁场作用时间对氧化法制备的Co掺杂ZnO薄膜微观结构和光学性能的影响[J]. 金属学报, 2014 , 50(12) : 1538 -1542 . DOI: 10.11900/0412.1961.2014.00376

Abstract

The effects of the oxidation time under high magnetic field on the microstructure and optical properties of oxidized Co-doped Zn prepared by vacuum evaporation were studied by FESEM, XRD and ultraviolet visible spectrophotometer. The results show that the growth of coral dendritic structures of ZnO films is inhibited by high magnetic field. Spherical particles of ZnO film oxidized for 60 min without magnetic field transforms to leaf like morphologies with the application of a 6 T magnetic field. With increasing oxidation time under high magnetic field, the preferred orientation of (101) transforms to (002); distribution of magnetic Co atoms in ZnO is influenced; the band gap is decreased to the range of 2.95~3.13 eV. The transmittance is decreased by the spherical morphologies. However, it is increased by the application of high magnetic field. These results give a new method to tune the microstructure and optical properties of surface morphology, preferred orientation, magnetic atomic distribution, transmittance, and band gap.

参考文献

[1] ?zgür ü, Alivov Y I, Liu C, Teke A, Reshchikov M A, Do?an S, Avrutin V, Cho S J, Morko? H. J Appl Phys, 2005; 98: 041301
[2] Look D C, Claflin B, Alivov Y I, Park S J. Phys Status Solidi, 2004; 201A: 2203
[3] Pan F, Song C, Liu X J, Yang Y C, Zeng F. Mater Sci Eng, 2008; R62: 1
[4] Hosono H. Thin Solid Films, 2007; 515: 6000
[5] Becheri A, Dürr M, Lo Nostro P, Baglioni P. J Nanopart Res, 2008; 10: 679
[6] Huang X H, Zhang C B, Tay C B, Venkatesan T, Chua S J. Appl Phys Lett, 2013; 102: 111106
[7] Behan A J, Mokhtari A, Blythe H J, Score D, Xu X H, Neal J R, Fox A M, Gehring G A. Phys Rev Lett, 2008; 100: 047206
[8] Li H L, Zhang Z, Lü Y B, Huang J Z, Liu R X. Acta Metall Sin, 2013; 29: 506
[8] (李泓霖, 张 仲, 吕英波, 黄金昭, 刘如喜. 金属学报, 2013; 29: 506)
[9] Aravind A, Hasna K, Jayaraj M K, Kumar M, Chandra R. Appl Phys, 2014; 115A: 843
[10] Li Q, Wang Y Y, Fan L L, Liu J D, Kong W, Ye B J. Scr Mater, 2013; 69: 694
[11] Ney A, Ney V, Kieschnick M, Wilhelm F, Ollefs K, Rogalev A. J Appl Phys, 2014; 115: 172603
[12] Li B B, Richard A, Chen Z F, Shen H L, Luo J. J Sol-Gel Sci Technol, 2014; 70: 19
[13] He R L, Tang B, Ton-That C, Phillips M, Tsuzuki T. J Nanopart Res, 2013; 15: 2030
[14] Rusu G G, Rambu A P, Buta V E, Dobromir M, Luca D, Rusu M. Mater Chem Phys, 2010; 123: 314
[15] Rambu A P, Sirbu D, Iftimie N, Rusu G I. Thin Solid Films, 2011; 520: 1303
[16] Condurache-Bota S, Tigau N, Rambu A P, Rusu G G, Rusu G I. Appl Surf Sci, 2011; 257: 10545
[17] Yildiz A, Kayhan B, Yurduguzel B, Rambu A P, Iacomi F, Simon S. J Mater Sci, 2011; 22: 1473
[18] Wang Q,He J C. Material Science Under High Magnetic Field. Beijing: Science Press, 2014: 1
[18] (王 强,赫冀成. 强磁场材料科学. 北京: 科学出版社, 2014: 1)
[19] Tahashi M, Sassa K, Hirabayashi I, Asai S. Mater Trans, 2000; 41: 985
[20] Ren S Y, Ren Z M, Ren W L, Cao G H. Acta Phys Sin, 2009; 58: 5567
[20] (任树洋, 任忠鸣, 任维丽, 操光辉. 物理学报, 2009; 58: 5567)
[21] Li G J, Du J J, Wang H M, Wang Q, Ma Y H, He J C. Mater Lett, 2014; 133: 53
[22] Wang Q, Cao Y Z, Li G J, Wang K, Du J J, He J C. Sci Adv Mater, 2013; 5: 447
[23] Cao Y Z, Wang Q, Li G J, Du J J, Wu C, He J C. J Magn Magn Mater, 2013; 332: 38
[24] Wang Q, Liu T, Gao A, Zhang C, Wang C J, He J C. Scr Mater, 2007; 56: 10587
[25] Rambu A P, Rusu G I. Superlattice Mirost, 2010; 47: 300
[26] Huang X H, Li G H, Cao B Q, Wang M, Hao C Y. J Phys Chem, 2009; 113C: 4381
[27] Rambu A P, Sirbu D, Dobromir M, Rusu G G. Solid State Sci, 2012; 14: 1543
[28] Huang X H, Tay C B, Zhan Z Y, Zhang C, Zheng L X, Venkatesan T, Chua S J. Cryst Eng Comm, 2011; 13: 447
[29] Huang X H, Zhang Z Y, Pramoda K P, Zhang C, Zheng L X, Chua S J. Cryst Eng Comm, 2012; 14: 5163
文章导航

/

〈 〉