Sn对Al-Pb偏晶合金凝固过程及组织的影响*

  • 陈书 ,
  • 赵九洲
展开
  • 中国科学院金属研究所, 沈阳110016

收稿日期: 2013-06-25

  修回日期: 2013-06-25

  网络出版日期: 2014-05-20

基金资助

*国家自然科学基金项目51071159, 51271185和51031003资助

EFFECT OF Sn ON THE SOLIDIFICATION PROCESS AND MICROSTRUCTURE OF Al-Pb MONOTECTIC ALLOYS

  • Shu CHEN ,
  • Jiuzhou ZHAO
Expand
  • Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
null

陈书, 男, 1986 年生, 博士生

Received date: 2013-06-25

  Revised date: 2013-06-25

  Online published: 2014-05-20

Supported by

National Natural Science Foundation of China (Nos.51071159, 51271185 and 51031003)

摘要

研究了添加第三组元Sn对定向凝固Al-Pb合金组织的影响. 结果表明, 添加微量Sn能降低Al-Pb合金液-液相变时两液相间的界面能, 促进富Pb相液滴形核和弥散型Al-Pb合金凝固组织的获得; 随着Sn添加量的增加, 弥散相体积分数增大, 液-液相变温度区间和液-液-固三相温度区间之和增大, 初生弥散相粒子和偏晶反应弥散相粒子的尺寸均增大; 添加Sn促进Al-Pb合金中凝固界面枝晶化, 这一方面促进弥散相液滴/粒子沿凝固方向均匀分布, 另一方面, 促进弥散相液滴/粒子沿定向凝固合金晶界分布.

本文引用格式

陈书 , 赵九洲 . Sn对Al-Pb偏晶合金凝固过程及组织的影响*[J]. 金属学报, 2014 , 50(5) : 561 -566 . DOI: 10.3724/SP.J.1037.2013.00351

Abstract

When a homogeneous, single-phase liquid of monotectic alloy is cooled into the miscibility gap, the components are no longer miscible and two liquid phases develop. Generally, the liquid-liquid decomposition causes the formation of the microstructure with serious phase segregation. Many efforts have been made to use the demixing phenomenon for the production of well dispersed composite materials. It has been demonstrated that the rapid directional solidification technique is an effective method to prevent the formation of the phase segregated microstructure in immiscible alloys. Directional solidification experiments were carried out to study the influence of the addition of Sn on the solidification process of Al-Pb alloys. The experimental results show that the addition of a small amount of Sn causes a decrease in the interface energy between the matrix and the minority phase liquids and, thus, an increase in the nucleation rate of the minority phase droplets during the liquid-liquid phase transformation or a decrease in the average size of the minority phase particles. With the increase of the Sn content, both the volume fraction of the minority phase droplets and the temperature range of the liquid-liquid phase zone and the liquid-liquid-solid tertiary phase zone of the phase diagram increase. These are favorable for the coarsening of the minority phase droplets. The addition of Sn leads to the formation of a dendrite solid/liquid interface. This may promote the formation of a well dispersed microstructure and shows great effect on the distribution of the minority phase particles.

参考文献

[1] Wang C P, Liu X J, Ohnuma I, Kainuma R, Ishida K. Science, 2002; 297: 990
[2] Li H L, Zhao J Z. Acta Metall Sin, 2011; 47: 87
[2] (李海丽, 赵九洲. 金属学报, 2011; 47: 87)
[3] Rudrakshi G B, Srivastava V C, Pathak J P, Ojha S N. Mater Sci Eng, 2004; A383: 30
[4] Liu Y, Guo J J, Jia J, Su Y Q, Ding H S. Acta Metall Sin, 2001; 37: 917
[4] (刘 源, 郭景杰, 贾 均, 苏彦庆, 丁宏升. 金属学报, 2001; 37: 917)
[5] Zhao J Z, Ratke L. Scr Mater, 1998; 39: 181
[6] Wang N, Wei B B. Mater Sci Eng, 2003; A345: 145
[7] Zhao J Z, Ratke L. Z Metallkd, 1998; 89: 241
[8] Zhu M, Gao Y, Chung C Y, Che Z X, Lou K C, Li B L. Wear, 2000; 242: 47
[9] Zhao J Z. Acta Metall Sin, 2002; 38: 525
[9] (赵九洲. 金属学报, 2002; 38: 525)
[10] Prinz B, Romero A, Ratke L. J Mater Sci, 1995; 30: 4715
[11] Grugel R G. Metall Trans, 1991; 22B: 339
[12] Chan J W. Metall Trans, 1979; 10A: 119
[13] Zhao J Z, Ratke L, Jia J, Li Q C. J Mater Sci Technol, 2002; 18: 197
[14] Shi R P, Wang Y, Wang C P, Liu X J. Appl Phys Lett, 2011; 98: 204106
[15] Wang W L, Li Z Q, Wei B. Acta Mater, 2011; 59: 5482
[16] Schaffer P L, Mathiesen R H, Arnberg L. Acta Mater, 2009; 57: 2887
[17] Kaban I, K?hler M, Ratke L, Hoyer W, Mattern N, Eckert J, Greer A L. Acta Mater, 2011; 59: 6880
[18] Wu M H, Ludwig A, Ratke L. Metall Mater Trans, 2003; 34A: 3009
[19] Carlberg T, fredriksson H. Metall Trans, 1980; 11A: 1665
[20] Guo J J, Liu Y, Su Y Q, Ding H S, Zhao J Z, Xue X. Scr Mater, 2001; 45: 1197
[21] He J, Zhao J Z. Mater Sci Eng, 2005; A404: 85
[22] Nestler B, Wheeler A A, Garcke H. Comput Mater Sci, 2003; 26: 111
[23] He J. PhD Dissertation, Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2006
[23] (何 杰. 中国科学院金属研究所博士学位论文, 沈阳, 2006)
[24] Lukas H L,Fries S G,Sundman B. Computational Thermodynamics: The Calphad Method. Cambridge: Cambridge University Press, 2007: 101
[25] Shim J H, Lee H N, Ha H P, Cho Y W, Yoon E P. J Alloys Compd, 2001; 327: 270
[26] Dinsdale A T. Calphad, 1991; 15: 317
[27] Liu Y J, Liang D. J Alloys Compd, 2005; 403: 110
[28] Yu S K, Sommer F, Predel B. Z Metallkd, 1996; 87: 574
[29] Miettinen J. Metall Mater Trans, 2002; 33A: 1639
[30] Ohtani H, Okuda K, Ishida K. J Phase Equilib, 1995; 16: 416
文章导航

/

〈 〉