Cu-Nb复合线材在形变与退火过程中显微结构演变的研究*

  • 邓丽萍 ,
  • 杨晓芳 ,
  • HAN Ke ,
  • 孙泽元 ,
  • 刘庆
展开
  • 1 重庆大学材料科学与工程学院, 重庆 400044
    2 National High Magnetic Field Laboratory, Tallahassee, Florida, USA, 32310
null

邓丽萍, 女, 1986年生, 博士生

收稿日期: 2013-09-30

  修回日期: 2013-09-30

  网络出版日期: 2014-02-20

基金资助

*国家自然科学基金项目51031002和51201188, 中丹纳米金属合作项目NSFC-DNRF 51261130091, 重庆市自然科学基金项目2010BB4074, 先进金属及材料国家重点实验室项目2010ZD-02及美国国家科学基金合作项目DMR-0084173资助

STUDY ON THE MICROSTRUCTURE EVOLUTION OF Cu-Nb COMPOSITE WIRES DURING DEFORMATION AND ANNEALING

  • Liping DENG ,
  • Xiaofang YANG ,
  • Ke HAN ,
  • Zeyuan SUN ,
  • Qing LIU
Expand
  • 1 School of Materials Science and Engineering, Chongqing University, Chongqing 400044
    2 National High Magnetic Field Laboratory, Tallahassee, Florida, USA, 32310

Received date: 2013-09-30

  Revised date: 2013-09-30

  Online published: 2014-02-20

Supported by

Supported by National Natural Science Foundation of China (Nos.51031002 and 51201188), Danish National Research Foundation and National Natural Science Foundation of China (No. NSFC-DNRF 51261130091), Natural Science Foundation Project of Chongqing Science and Technology Commission (No.2010BB4074), State Key Laboratory For Advanced Metals and Materials (No.2010ZD-02) and National Science Foundation of United States (No.DMR-0084173)

摘要

采用SEM和TEM, 对不同形变量及退火温度下的Cu-Nb微观复合线材的显微组织结构进行了分析, 并对形变和退火试样进行了硬度测试. 结果表明: 随着形变量增大, 材料界面密度及其增加速率逐渐增大. 当材料结构达到纳米尺寸时(应变=24.8), 界面密度及其增加速率显著增加, 使得硬度及其增加速率明显增大, 同时伴随有纳米Cu基体内部层错和旋转晶界的产生. 退火过程中Cu基体的显微组织变化表现出明显的多尺度效应, 其变化可分为3个阶段: 微米及亚微米Cu基体先发生回复再结晶, 而纳米Cu基体回复再结晶受到抑制; 纳米Cu基体回复再结晶; Nb丝球化及长大.

本文引用格式

邓丽萍 , 杨晓芳 , HAN Ke , 孙泽元 , 刘庆 . Cu-Nb复合线材在形变与退火过程中显微结构演变的研究*[J]. 金属学报, 2014 , 50(2) : 231 -237 . DOI: 10.3724/SP.J.1037.2013.00622

Abstract

Microstructure of as-deformed and annealed Cu-Nb composite wires were investigated by SEM and TEM. Hardness of the as-deformed and annealed samples were measured. The results showed that both the interface density and the rate of interface-increasing increased with increasing strain. When the microstructure reached nano-scale (strain=24.8), the interface density showed a sharp increase which induced a rapid increase in hardness, accompanied by formation of stacking faults and rotation grain boundaries in Cu. During the annealing, the size effect impacted the evolution of microstructure of the multi-scale Cu matrix. The evolution can be classified in to three stages with respect to annealing temperatures: recovery and recrystallization of large Cu, while that of the nano Cu were restrained; recovery and recrystallization of nano Cu; spheroidization and coarsening of Nb.

参考文献

[1] Han K, Chen J, Cui B, Davy C A, Kalu P N. Mater Res Soc, 2006; 977: 53
[2] Vidal V, Thilly L, Van Petegem S, Stuhr U, Lecouturier F, Renault P O, Van Swygenhoven H. Scr Mater, 2009; 60: 171
[3] Thilly L, Lecouturier F, von Stebut J. Acta Mater, 2002; 50: 5049
[4] Spitzig W A, Pelton A R, Laabs F C. Acta Metall, 1987; 35: 2427
[5] Liang M, Lu Y, Chen Z, Li C. IEEE T Appl Supercon, 2010; 20: 1619
[6] Spitzig W A, Downing H L, Laabs F C, Gibson E D, Verhoeven J D. Metall Trans, 1993; 24A: 7
[7] Chung J H, Song J S, Hong S I. J Mater Process Technol, 2001; 113: 604
[8] Bevk J, Harbison J P, Bell J. Appl Phys, 1978; 49: 6031
[9] Deng L, Yang X, Han K, Lu Y, Liang M, Liu Q. Mater Charact, 2013; 81: 124
[10] Leprince-Wang Y, Han K, Huang Y, Yu-zhang K. Mater Sci Eng, 2003; A351: 214
[11] Lu Y F, Liang M, Li C S, Feng J Q, Yu Z M, Xu X Y, Liu Q, Liu Z Y. Chin Nonferrous Met, 2012; 22: 1650
[11] (卢亚锋, 梁 明, 李成山, 冯建情, 于泽铭, 徐晓燕, 刘 庆, 柳忠元. 中国有色金属学报, 2012; 22: 1650)
[12] Wang N. PhD Dissertation, University of Toronto, 1997
[13] Thilly T, Veron M, Ludwig O, Lecouturier F. Mater Sci Eng, 2001; A309: 510
[14] Popova E N, Popov V V, Romanov E P, Hlebova N E, Shikov A K. Scr Mater, 2004; 51: 727
[15] Sandim H R Z, Sandim M J R, Bernardi H H, Lins J F C, Raabe D. Bernardi H HScr Mater, 2004; 51: 1099
[16] Thilly L, Lecouturier F, Coffe G, Peyrade J P, Askenazy S. Physica, 2001; 294-295B: 648
[17] Shikov A, Pantsyrnyi V, Vorobieva A, Khlebova N, Silaev A. Physica, 2001; 354C: 410
[18] Han K, Lawson A C, Wood J T, Embury J D, Von Dreele R B, Richardson J W. Philos Mag, 2004; 84: 2579
[19] Han K, Yu-zhang K, Kung H, Embury J D, Daniels B J, Clemens B M. Philos Mag, 2002; 82A: 1633
[20] Liao X Z, Zhao Y H, Srinivasan S G, Zhu Y T. Appl Phys Lett, 2004; 84: 592
[21] Van Swygenhoven H. Science, 2002; 296: 66
[22] Branicio P S, Zhang J Y, Srolovitz D J. Phys Rev, 2013; 88: 1
[23] He J, Liu J B, Meng L. Acta Metall Sin, 2007; 43: 643
[23] (贺 佳, 刘嘉斌, 孟 亮. 金属学报, 2007; 43: 643)
[24] Raabe D, Heringhaus F, Hangen U, Gottstein G. Z Metallkd, 1995; 86: 405
[25] Guo G Z. Pingyuan Univ, 2006; 23: 129
[25] (郭贵中. 平原大学学报, 2006; 23: 129)
[26] Carpenter J S, Vogel S C, LeDonne J E, Hammon D L, Beyerlein I J, Mara N A. Acta Mater, 2012; 60: 1576
[27] Lim S C V, Rollett A D. Mater Sci Eng, 2009; A520: 189
[28] Takata N, Yamada K, Ikeda K-I, Yoshida F, Nakashima H, Tsuji N. Mater Trans, 2007; 48: 2043
[29] Sandim M J R, Sandim H R Z, Bernardi H H, Shigue C Y, Virgens M G D, Ghivelder L, Awaji S, Watanabe K, Iwaki G. Supercond Sci Technol, 2005; 18: 35
文章导航

/

〈 〉