高性能铜系层状金属材料设计: 纳米尺度下强化能力与韧化能力思考*

  • 张广平 ,
  • 朱晓飞
展开
  • 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016
null

张广平, 男, 1966年生, 研究员

收稿日期: 2013-12-13

  修回日期: 2013-12-13

  网络出版日期: 2014-02-20

基金资助

*国家重点基础研究发展计划项目2010CB631003及国家自然科学基金项目51001105, 51071158和51371180资助

DESIGN OF HIGH-PERFORMANCE Cu-BASED NANO-LAYERED MATERIALS: ON STRENGTHENING AND TOUGHENING ABILITIES AT THE NANOSCALES

  • Guangping ZHANG ,
  • Xiaofei ZHU
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016

Received date: 2013-12-13

  Revised date: 2013-12-13

  Online published: 2014-02-20

Supported by

Supported by National Basic Research Program of China (No.2010CB631003) and National Natural Science Foundation of China (Nos.51001105, 51071158 and 51371180)

摘要

对近年来国内外在纳米层状金属材料的强化能力及其尺度与界面效应、塑性形变行为及稳定性等基本规律的研究进展进行了系统的总结, 并对纳米层状材料的强化能力与韧化能力进行了深入的探讨. 最后, 对纳米层状金属材料的强化与韧化能力中的关键科学问题及未来研究进行了展望.

本文引用格式

张广平 , 朱晓飞 . 高性能铜系层状金属材料设计: 纳米尺度下强化能力与韧化能力思考*[J]. 金属学报, 2014 , 50(2) : 148 -155 . DOI: 10.3724/SP.J.1037.2013.00680

Abstract

In this paper, recent investigations on strengthening ability and effects of length scale and interface, plastic deformation behavior and stability of nanolayered metallic materials are reviewed systematically. The basic mechanisms on the abilities in strengthening and toughening for nanolayered metallic materials were discussed. Finally, several key issues on improving the strengthening and toughening abilities of the nanolayered materials and the potential investigations in the future are stressed.

参考文献

[1] Hall E O. Proc Phys Soc, 1951; 64B: 747
[2] Petch N J. J Iron Steel Inst, 1953; 174: 25
[3] Iwahashi Y, Wang J T, Horita Z, Nemoto M, Langdon T G. Scr Mater, 1996; 35: 143
[4] Valiev R Z, Estrin Y, Horita Z, Langdon T G, Zehetbauer M J, Zhu Y T. JOM, 2006; 58(4): 33
[5] Zhilyaev A P, Langdon T G. Prog Mater Sci, 2008; 53: 893
[6] Saito Y, Tsuji N, Utsunomiya H, Sakai T, Hong R G. Scr Mater, 1998; 39: 1221
[7] Hirth J P, Lothe J. Theory of Dislocations. 2nd Ed., New York: John Wiley & Sons, 1982: 788
[8] Meyers M A,Chawla K K. Mechanical Behavior of Materials. Cambridge: Cambridge University Press, 2009: 1
[9] Sevillano J G. In: Cahn R W, Haasen P, Kramer E, eds., Materials Science and Technology: A Comprehensive Treatment Plastic Deformation and Fracture of Materials. New York: VCH, 1993: 19
[10] Blum W. Trans Am Electrochem Soc, 1921; 40: 307
[11] Was G S, Foecke T. Thin Solid Films, 1996; 286: 1
[12] Clemens B M, Kung H, Barnett S A.MRS Bull, 1999; 24: 20
[13] Misra A, Hirth J P, Kung H. Philos Mag, 2002; 82A: 2935
[14] Zhang G P, Liu Y, Wang W, Tan J. Appl Phys Lett, 2006; 88: 013105
[15] Mara N A, Bhattacharyya D, Hoagland R G, Misra A. Scr Mater, 2008; 58: 874
[16] Misra A, Verdier M, Lu Y C, Kung H, Mitchell T E, Nastasi M, Embury J D. Scr Mater, 1998; 39: 555
[17] Wen S P, Zong R L, Zeng F, Gao Y, Pan F. Acta Mater, 2007; 55: 345
[18] Li Y P, Zhang G P, Wang W, Tan J, Zhu S J. Scr Mater, 2007; 57: 117
[19] McKeown J, Misra A, Kung H, Hoagland R G, Nastasi M. Scr Mater, 2002; 46: 593
[20] Zhang X, Misra A, Wang H, Shen T D, Nastasi M, Mitchell T E, Hirth J P, Hoagland R G, Embury J D. Acta Mater, 2004; 52: 995
[21] Yan J W, Zhang G P, Zhu X F, Liu H S, Yan C. Philos Mag, 2013; 93: 434
[22] Misra A, Hirth J P, Hoagland R G. Acta Mater, 2005; 53: 4817
[23] Armstrong R W. In: Martin J W, ed., Concise Encyclopedia of the Mechanical Properties of Materials. Oxford: Elsevier, 2007: 601
[24] Zhu Y T, Liao X Z, Wu X L. Prog Mater Sci, 2012; 57: 1
[25] Lehoczky S L. J Appl Phys, 1978; 49: 5479
[26] Zhang X, Misra A, Wang H, Shen T D, Swadener J G, Embury J D, Kung H, Hoagland R G, Nastasi A. J Mater Res, 2003; 18: 1600
[27] Huang H B, Spaepen F. Acta Mater, 2000; 48: 3261
[28] Lu L, Chen X, Huang X, Lu K. Science, 2009; 323: 607
[29] Hoagland R G, Kurtz R J, Henager C H. Scr Mater, 2004; 50: 775
[30] Anderson P M, Foecke T, Hazzledine P M. MRS Bull, 1999; 24: 27
[31] Li Y P, Zhang G P. Acta Mater, 2010; 58: 3877
[32] Koehler J S. Phys Rev, 1970; 2B: 547
[33] Hoagland R G, Mitchell T E, Hirth J P, Kung H. Philos Mag, 2002; 82A: 643
[34] Rao S I, Hazzledine P M. Philos Mag, 2000; 80A: 2011
[35] Zhu X F, Li Y P, Zhang G P, Tan J, Liu Y. Appl Phys Lett, 2008; 92: 161905
[36] Zhu X F, Zhang G P, Yan C, Zhu S J, Sun J.Philos Mag Lett, 2010; 90: 413
[37] Li Y P, Zhu X F, Tan J, Wu B, Zhang G P. Philos Mag Lett, 2009; 89: 66
[38] Li X Y, Wei Y J, Lu L, Lu K, Gao H J. Nature, 2010; 464: 877
[39] Tench D M, White J T. J Electrochem Soc, 1991; 138: 3757
[40] Mara N A, Misra A, Hoagland R G, Sergueeva A V, Tamayo T, Dickerson P, Mukherjee A K. Mater Sci Eng, 2008; A493: 274
[41] Lewis A C, Eberl C, Hemker K J, Weihs T P. J Mater Res, 2008; 23: 376
[42] Huang B, Ishihara K N, Shingu P H. J Mater Sci Lett, 2001; 20: 1669
[43] Wang Y M, Li J, Hamza A V, Barbee T W. Proc Nat Acad Sci, 2007; 104: 11155
[44] Zhang J Y, Zhang X, Liu G, Zhang G J, Sun J. Scr Mater, 2010; 63: 101
[45] Donohue A, Spaepen F, Hoagland R G, Misra A. Appl Phys Lett, 2007; 91: 241905
[46] Kavarana F H, Ravichandran K S, Sahay S S. Scr Mater, 2000; 42: 947
[47] Li Y P, Tan J, Zhang G P. Scr Mater, 2008; 59: 1226
[48] Li Y P, Zhu X F, Tan J, Wu B, Wang W, Zhang G P. J Mater Res, 2009; 24: 728
[49] Xie J Y, Huang P, Wang F, Li Y, Zhang L F, Xu K W. Integr Ferroelectr, 2013; 146: 168
[50] Wang D, Kups T, Schawohl J, Schaaf P.J Mater Sci, 2012; 23: 1077
[51] Wen S P, Zeng F, Pan F, Nie Z R. Mater Sci Eng, 2009; A526: 166
[52] Bhattacharyya D, Mara N A, Dickerson P, Hoagland R G, Misra A. J Mater Res, 2009; 24: 1291
[53] Knorr I, Cordero N M, Lilleodden E T, Volkert C A. Acta Mater, 2013; 61: 4984
[54] Li Y P, Zhu X F, Zhang G P, Tan J, Wang W, Wu B. Philos Mag, 2010; 90: 3049
[55] Wang F, Huang P, Xu M, Lu T J, Xu K W. Mater Sci Eng, 2011; A528: 7290
[56] Wen S P, Zong R L, Zeng F, Gao Y, Pan F. J Mater Res, 2007; 22: 3423
[57] Mara N A, Bhattacharyya D, Hirth J P, Dickerson P, Misra A. Appl Phys Lett, 2010; 97: 021909
[58] Liu M C, Lee C J, Lai Y H, Huang J C. Thin Solid Films, 2010; 518: 7295
[59] Zhang J Y, Lei S, Liu Y, Niu J J, Chen Y, Liu G, Zhang X, Sun J.Acta Mater, 2012; 60: 1610
[60] Kim Y, Lee J, Yeom M S, Shin J W, Kim H, Cui Y, Kysar J W, Hone J, Jung Y, Jeon S, Han S M. Nat Commun, 2013; 4: 2114
[61] Chen I W, Winn E J, Menon M.Mater Sci Eng, 2001; A317: 226
[62] Yan J W, Zhu X F, Yang B, Zhang G P. Phys Rev Lett, 2013; 110: 155502
[63] Lu K, Lu L, Suresh S. Science, 2009; 324: 349
[64] Fang T H, Li W L, Tao N R, Lu K. Science, 2011; 331: 1587
[65] Yan F K, Liu G Z, Tao N R, Lu K. Acta Mater, 2012; 60: 1059
[66] Zhang J Y, Zhang X, Wang R H, Lei S Y, Zhang P, Niu J J, Liu G, Zhang G J, Sun J.Acta Mater, 2011; 59: 7368
[67] Dayal P, Quadir M Z, Kong C, Savvides N, Hoffman M. Thin Solid Films, 2011; 519: 3213
[68] Liu M C, Du X H, Lin I C, Pei H J, Huang J C.Intermetallics, 2012; 30: 30
[69] Uchic M D, Dimiduk D M, Florando J N, Nix W D. Science, 2004; 305: 986
[70] Volkert C A, Minor A M.MRS Bull, 2007; 32: 389
[71] Zheng S J, Beyerlein I J, Wang J, Carpenter J S, Han W Z, Mara N A. Acta Mater, 2012; 60: 5858
[72] Wang J, Misra A, Hoagland R G, Hirth J P. Acta Mater, 2012; 60: 1503
[73] Zhang B, Tan H F, Yan J W, Zhang M D, Sun X D, Zhang G P. Nanoscale Res Lett, 2013; 8: 44
[74] Liu H S, Zhang B, Zhang G P.Scr Mater, 2011; 64: 13
[75] Liu H S, Zhang B, Zhang G P. Scr Mater, 2011; 65: 891
[76] Liu H S. PhD Dissertation. Institute of Metal Research, Chinese Academy of Sciences, Shenyang, 2012
[76] (刘华赛. 中国科学院金属研究所博士学位论文, 沈阳, 2012)