纳米结构金属材料的塑性变形制备技术*

  • 陶乃镕 ,
  • 卢柯
展开
  • 中国科学院金属研究所沈阳材料科学国家(联合)实验室, 沈阳 110016

收稿日期: 2013-12-10

  修回日期: 2013-12-10

  网络出版日期: 2014-02-20

基金资助

*国家重点基础研究发展计划项目2012CB932201和国家自然科学基金项目51171181和51371172资助

PREPARATION TECHNIQUES FOR NANO-STRUCTURED METALLIC MATERIALS VIA PLASTIC DEFORMATION

  • Nairong TAO ,
  • Ke LU
Expand
  • Shenyang National Laboratory for Materials Science, Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016
null

陶乃镕, 男, 1969 年生, 研究员

Received date: 2013-12-10

  Revised date: 2013-12-10

  Online published: 2014-02-20

Supported by

Supported by National Basic Research Program of China (No.2012CB932201) and National Natural Science Foundation of China (Nos.51171181 and 51371172)

摘要

本文总结了制备纳米结构金属材料的塑性变形技术, 包括大应变量变形技术(冷轧、累积叠轧、等通道挤压和高压扭转)、高应变速率变形技术(动态塑性变形)和高应变梯度变形技术(表面机械研磨和表面机械碾压), 分析了变形方式及变形参数对晶粒细化的影响规律, 展望了利用塑性变形技术制备纳米结构金属材料的发展趋势及挑战.

本文引用格式

陶乃镕 , 卢柯 . 纳米结构金属材料的塑性变形制备技术*[J]. 金属学报, 2014 , 50(2) : 141 -147 . DOI: 10.3724/SP.J.1037.2013.00803

Abstract

This work summarized the deformation techniques of preparing the nanostructured metallic materials, including large-strain deformation techniques (clod rolling, accumulative cold-bonding, equal channel angular pressing, high pressure torsion), high-strain-rate deformation technique (dynamic plastic deformation), and high-strain-gradient deformation techniques (surface mechanical attrition treatment and surface mechanical grinding treatment). The effects of deformation modes and deformation parameters on grain refinement are analyzed. Future trends and challenges of the deformation techniques for preparing nanostructured metallic materials are discussed.

参考文献

[1] Segal V M, Reznikov V I, Drobyshevkij A E, Kopylov V I. Russ Metall, 1981; 1: 99
[2] Segal V M, Reznikov V I, Pavlik D A, Malyshev V F. Processes of Plastic Transformation of Metals. Minsk: Navuka Teknika, 1984: 295
[3] Valiev R Z, Annales de Chimie. Science des Materiaux, 1996; 21: 369
[4] Smirnova N A, Levit V I, Pilyugin V I, Kuznetsov R I, Davydova L S, Sazonnova V A. Fiz Met Metalloved, 1986; 61: 1170
[5] Zhilyaev A P, Nurislamova G V, Kim B K, Baro M D, Szpunar J A, Langdon T G. Acta Mater, 2003; 51: 753
[6] Zhilyaev A P, Langdon T G. Prog Mater Sci, 2008; 53: 893
[7] Saito Y, Tsuji N, Utsunomiya H, Sakai T, Hong R G. Scr Mater, 1998; 39: 1221
[8] Hosseini S A, Manesh H D. Mater Des, 2009; 30: 2911
[9] Tsuji N, Saito Y, Lee S H, Minamino Y. 2nd Int Conf on Nanomaterials by Severe Plastic Deformation (SPD): Fundamentals Processing Applications, Vienna, Austria: Wiley-V C H Verlag Gmbh, 2003: 338
[10] Lu K, Lu J. J Mater Sci Technol, 1999; 15: 193
[11] Tao N R, Sui M L, Lu J, Lu K. Nanostruct Mater, 1999; 11: 433
[12] Tao N R, Wang Z B, Tong W P, Sui M L, Lu J, Lu K. Acta Mater, 2002; 50: 4603
[13] Tong W P, Tao N R, Wang Z B, Lu J, Lu K. Science, 2003; 31: 299
[14] Lu K, Lu J. Mater Sci Eng, 2004; 375: 38
[15] Li W L, Tao N R, Lu K. Scr Mater, 2008; 59: 546
[16] Fang T H, Li W L, Tao N R, Lu K. Science, 2011; 331: 1587
[17] Zhao W S, Tao N R, Guo J Y, Lu Q H, Lu K. Scr Mater, 2005; 53: 745
[18] Tao N R, Lu K. J Mater Sci Technol, 2007; 23: 771
[19] Li Y S, Tao N R, Lu K. Acta Mater, 2008; 56: 230
[20] Bay B, Hansen N. Mater Sci Eng, 1989; A113: 385
[21] Ananthan V S, Leffers T, Hughes D A. Scr Metall Mater, 1991; 25: 137
[22] Hansen N. Mater Sci Technol, 1990; 6: 1039
[23] Li B L, Godfrey A, Meng Q C, Liu Q. Acta Mater, 2004; 52: 1069
[24] Liu Q, Huang X, Lloyd D J, Hansen N. Acta Mater, 2002; 50: 3789
[25] Wang Y M, Chen M W, Sheng H W, Ma E. J Mater Res, 2002; 17: 3004
[26] Valiev R Z, Krasilnikov N A, Tsenev N K. 5th Int Symp on Plasticity of Metals and Alloys, Prague, Czechoslovakia: Elsevier Science Sa Lausanne, 1990: 35
[27] Valiev R Z, Korznikov A V, Mulyukov R R. Symp on Nanophase Materials, at the Emrs 1992 Fall Meeting of the European-Materials-Research-Soc, Strasbourg, France: Elsevier Science Sa Lausanne, 1992: 141
[28] Valiev R Z, Langdon T G. Prog Mater Sci, 2006; 51: 881
[29] Valiev R Z, Islamgaliev R K, Alexandrov I V. Prog Mater Sci, 2000; 45: 103
[30] Bridgman P W. J Appl Phys, 1943; 15: 273
[31] Jiang H G, Zhu Y T, Butt D P, Alexandrov I V, Lowe T C. Mater Sci Eng, 2000; A290: 128
[32] Sakai G, Horita Z, Langdon T G. Mater Sci Eng, 2005; A393: 344
[33] Zhang Y, Tao N R, Lu K. Acta Mater, 2011; 58: 6048
[34] Hong C S, Tao N R, Huang X, Lu K. Acta Mater, 2010; 58: 3103
[35] Xiao G H, Tao N R, Lu K. Scr Mater, 2011; 65: 119
[36] Lu K, Yan F K, Wang H T, Tao N R. Scr Mater, 2012; 66: 878
[37] Yan F K, Liu G Z, Tao N R, Lu K. Acta Mater, 2012; 60: 1059
[38] Wang H T, Tao N R, Lu K. Acta Mater, 2012; 60: 4027
[39] Huang F, Tao N R, Lu K. J Mater Sci Technol, 2011; 27: 1
[40] Luo Z P, Zhang H W, Hansen N, Lu K. Acta Mater, 2012; 60: 1322
[41] Zhu K Y, Vassel A, Brisset F, Lu K, Lu J. Acta Mater, 2004; 52: 4101
[42] Wang K, Tao N R, Liu G, Lu J, Lu K. Acta Mater, 2006; 54: 5281
[43] Sun H Q, Shi Y N, Zhang M X, Lu K. Acta Mater, 2007; 55: 975
[44] Zhang H W, Hei Z K, liu G, Lu J, Lu K. Acta Mater, 2003; 51: 1871
[45] Wu X, Tao N, Hong Y, Lu J, Lu K. Acta Mater, 2002; 50: 2075
[46] Tao N R, Wu X L, Sui M L, Lu J, Lu K. J Mater Res, 2004; 19: 1623
[47] Liu X C, Zhang H W, Lu K. Science, 2013; 342: 337
[48] Zener C, Hollomon J H. J Appl Phys, 1944; 15: 22
[49] Li Y S, Zhang Y, Tao N R, Lu K. Acta Mater, 2009; 57: 761
[50] Ashby M F. Philos Mag, 1970; 21: 399
文章导航

/

〈 〉