综述

Ti2AlNb基合金微观组织调制及热成形研究进展

  • 沈军 ,
  • 冯艾寒
展开
  • 1) 同济大学材料科学与工程学院, 上海 200092
    2) 哈尔滨工业大学材料科学与工程学院, 哈尔滨 150001
沈军, 男, 1965年生, 教授

收稿日期: 2013-08-27

  网络出版日期: 2013-11-11

RECENT ADVANCES ON MICROSTRUCTURAL CONTROLLING AND HOT FORMING OF Ti2AlNb-BASED ALLOYS

  • SHEN Jun ,
  • FENG Aihan
Expand
  • 1) School of Materials Science and Engineering, Tongji University, Shanghai 200092
    2) School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001

Received date: 2013-08-27

  Online published: 2013-11-11

摘要

以有序O相为基的Ti2AlNb基金属间化合物(简称Ti2AlNb基合金),以其较高的强度和塑性, 优良的抗蠕变性能以及较低的密度,逐渐发展成为一种极具潜力的航空应用材料.本文总结了Ti2AlNb基合金微观组织与力学性能方面的最新研究进展,重点对晶体结构、相变、微观组织及热成形等方面进行评述.

本文引用格式

沈军 , 冯艾寒 . Ti2AlNb基合金微观组织调制及热成形研究进展[J]. 金属学报, 2013 , 49(11) : 1286 -1294 . DOI: 10.3724/SP.J.1037.2013.00607

Abstract

Intermetallic alloys based on an ordered orthorhombic phase Ti2AlNb,hereafter referred to as the Ti2AlNb-based alloys, are continually developing as attractive materials for aerospace applications due to their desirable properties like a unique combination of strength and ductility, good creep resistance, and low densities. This review article is thus aimed at summarizing recent advances on the microstructural evolution and mechanical properties of the Ti2AlNb-based alloys. Particular attention is paid to their crystal structure, phase transformations, microstructure and hot forming processing.

参考文献

[1] Banerjee D, Gogia A K, Nandi T K, Joshi V A. Acta Metall, 1988; 36: 871

[2] Banerjee D. Prog Mater Sci, 1997; 42: 135
[3] Boehlert C J. Mater Sci Eng, 1999; A267: 82
[4] Boehlert C J, Miracle D B. Metall Mater Trans, 1999; 30A: 2349
[5] Boehlert C J. Metall Mater Trans, 2001; 32A: 1977
[6] Dey S R, Suwas S, Fundenberger J J, Ray R K. Intermetallics, 2009; 17: 622
[7] Zhang J W, Li S Q, Liang X B, Cheng Y J. Chin J Nonferrous Met, 2010; 20(spec 1): 336
(张建伟, 李世琼, 梁晓波, 程云君. 中国有色金属学报, 2010; 20(专辑1): 336)
[8] Chen Z. Master Thesis, Harbin Institute of Technology, 2013
(陈 卓. 哈尔滨工业大学硕士学位论文, 2013)
[9] Shagiev M R, Galeyev R M, Valiakhmetov O R, Safiullin R V. Adv Mater Res, 2009; 59: 105
[10] Peng J H, Mao Y, Li S Q, Sun X F. Mater Sci Eng, 2001; A299: 75
[11] Ma X, Zeng W D, Xu B, Sun Y, Xue C, Han Y F. Intermetallics, 2012; 20: 1
[12] Germann L, Banerjee D, Guedou J Y, Strudel J L. Intermetallics, 2005; 13: 920
[13] Tang F, Nakazawa S, Hagiwara M. Mater Sci Eng, 2002; A329-331: 492
[14] Feng A H, Li B B, Shen J. J Mater Metall, 2011; 10: 30
(冯艾寒, 李渤渤, 沈 军. 材料与冶金学报, 2011; 10: 30)
[15] Yang S J, Nam S W, Hagiwara M. Intermetallics, 2004; 12: 261
[16] Boehlert C J. Mater Sci Eng, 2000; A279: 118
[17] Zhu H L, Li Z Q, Shang B S, Mao W F, Wang C X, Li S Q, Zhang J W. J Mater Sci Technol, 2001; 17: 119
[18] Wu Y T, Yang C T, Koo C H. Mater Chem Phys, 2002; 73: 212
[19] Guo H P, Zeng Y S, Li Z Q. Aeronaut Manuf Technol, 2009; (10): 64
(郭和平, 曾元松, 李志强. 航空制造技术, 2009; (10): 64)
[20] Li Z Q, Guo H P. Aeronaut Manuf Technol, 2010; (8): 32
(李志强, 郭和平. 航空制造技术, 2010; (8): 32)
[21] Sergueeva A V, Stolyarov V V, Valiev R Z, Mukherjee A K. Mater Sci Eng, 2002; A323: 318
[22] Valiev R Z, Islamgaliev R K, Alexandrov I V. Prog Mater Sci, 2000; 45: 103
[23] Sauvage X, Wilde G, Divinski S V, Horita Z, Valiev R Z. Mater Sci Eng, 2012; A540: 1
[24] Valiev R Z, Zehetbauer M J, Estrin Y, H$\ddot{\rm o$ppel H W, Ivanisenko Y, Hahn H,Wilde G, Roven H J, Sauvage X, Langdon T G. Adv Eng Mater, 2007; 9: 527
[25] Valiev R Z, Gertsman V Y, Kaibyshev O A. Phys Status Solidi, 1986; 97A: 11
[26] Salishchev G A, Galeyev R M, Malysheva S P, Myshlyaev M M. Nanostruct Mater, 1999; 11: 407
[27] Gleiter H. Prog Mater Sci, 1989; 33: 223
[28] Bendersky L A. Scr Metall Mater, 1993; 29: 1645
[29] Ren X, Hagiwara M. Acta Mater, 2001; 49: 3971
[30] Peng J H, Li S Q, Mao Y, Sun F. Mater Lett, 2002; 53: 57
[31] Sadi F A, Servant C. Mater Sci Eng, 2003; A346: 19
[32] Boehlert C J, Majumdar B S, Seetharaman V, Miracle D B. Metall Mater Trans, 1999; 30A: 2305
[33] Muraleedharan K, Gogia A K, Nandy T K, Banerjee D, Lele S. Metall Trans, 1992; 23A: 401
[34] Muraleedharan K, Nandy T K, Banerjee D, Lele S. Metall Trans, 1992; 23A: 417
[35] Li D Q, Boehlert C J. Metall Mater Trans, 2005; 36A: 2569
[36] Leyens C, Peters M. Titanium and Titanium Alloys--Fundamentals and Applications.Weinheim: Wiley-VCH GmbH {\& Co. KGaA, 2003: 1
[37] Ravi C, Vajeeston P, Mathijaya S, Asokamani R. Phys Rev, 1999; 60B: 15683
[38] Balasubramanian S, Anand L. Acta Mater, 2002; 50: 133
[39] Lin P, Feng A H, Yuan S J, Li G P, Shen J. Mater Sci Eng, 2013; A563: 16
[40] Froes F H, Suryanarayana C, Eliezer D. J Mater Sci, 1992; 27: 5113
[41] Banerjee D, Nandy T K, Gogia A K. Scr Metall, 1987; 21: 597
[42] Bendersky L A, Boettinger W J. Acta Metall Mater, 1994; 42: 2337
[43] Singh A K, Sarma B N, Lele S. Philos Mag, 2004; 84: 2865
[44] Muraleedharan K, Nandy T K, Banerjee D, Lele S. Intermetallics, 1995; 3: 187
[45] Sarosi P M, Hriljac J A, Jones I P. Philos Mag, 2003; 83: 4031
[46] Wu B. PhD Dissertation, General Research Institute for Non-ferrous Metals in Beijing, 2002
(吴 波. 北京有色金属研究总院博士学位论文, 2002)
[47] Wu Y, Zhen L, Yang D Z, Mao J F. Mater Lett, 1997; 32: 319
[48] Kazantseva N V, Demakov S L, Popov A A. Phys Met Metallograph, 2007; 103: 388
[49] Wen Y H, Wang Y, Bendersky L A, Chen L Q. Acta Mater, 2000; 48: 4125
[50] Bendersky L A, Boettinger W J, Roytburd A. Acta Metall Mater, 1991; 39: 1959
[51] Kazantseva N V, Demakov S L, Popov A A. Phys Met Metallograph, 2007; 103: 378
[52] Mozer B, Bendersky L A, Boettinger W J. Scr Metall Mater, 1990; 24: 2363
[53] Cui X Y, Yang J L, Li Q X, Xia S D, Wang C Y. J Phys: Condens Matter, 1999; 11: 6179

[54] Altan B S. Severe Plastic Deformation: Toward Bulk Production of Nanostructured Materials.New York: Nova Publishers, 2006: 1

[55] Lu B, Yang R. Rare Met Mater Eng, 2008; 37(suppl 3): 61

(卢斌, 杨锐. 稀有金属材料与工程, 2008; 37(增刊 3): 61)
[56] Quast J P, Boehlert C J. Metall Mater Trans, 2007; 38A: 529
[57] Lu B, Yang R, Cui Y Y. Acta Metall Sin, 2002; 38(suppl): 55
(卢 斌, 杨 锐, 崔玉友. 金属学报, 2002; 38(增刊): 55)
[58] Mao Y, Hagiwara M, Emura S. Scr Mater, 2007; 57: 261
[59] Yang S J, Nam S W, Hagiwara M. J Alloys Compd, 2003; 350: 280
[60] Peng J H, Li S Q, Mao Y, Sun X F. Chin J Nonferrous Met, 2000; 10(suppl 1): 50
(彭继华, 李世琼, 毛 勇, 孙训芳. 中国有色金属学报, 2000; 10(增刊 1): 50)
[61] Mao Y, Li S Q, Zhang J W, Peng J H, Zou D X, Zhong Z Y. Intermetallics, 2000; 8: 659
[62] Mao Y, Li S X, Zhang J W, Peng J H, Zou D X, Zhong Z Y. Acta Metall Sin, 2000; 36: 135
(毛 勇, 李世琼, 张建伟, 彭继华, 邹敦叙, 仲增墉. 金属学报, 2000; 36: 135)
[63] Chen Y Y, Si Y F, Kong F T, Chen Z Y. Rare Met Mater Eng, 2006; 35: 655
(陈玉勇, 司玉峰, 孔凡涛, 陈子勇. 稀有金属材料与工程, 2006; 35: 655)
[64] Ke Y B, Duan H P, Sun Y R. Mater Sci Eng, 2010; A528: 220
[65] Tang F, Nakazawa S, Hagiwara M. Mater Sci Eng, 2001; A315: 147
[66] Valiev R Z, Estrin Y, Horita Z, Langdon T G, Zehetbauer M J, Zhu Y T.JOM, 2006; 58: 33
[67] Semenova I P, Polyakov A V, Raab G I, Lowe T C, Valiev R Z. J Mater Sci, 2012; 47: 7777
[68] Ko Y G, Jung W S, Shin D H, Lee C S. Scr Mater, 2003; 48: 197
[69] Ko Y G, Kim W G, Lee C S, Shin D H. Mater Sci Eng, 2005; A410-411: 156
[70] Ko Y G, Lee C S, Shin D H, Semiatin S L. Metall Mater Trans, 2006; 37A: 381
[71] Gallego J, Pinheiro T S, Valiev R Z, Polyakova V, Bolfarini C, Kiminami C S,Jorge A M, Botta W J. Mater Res-Ibero-Am J Mater, 2012; 15: 786
[72] Sergueeva A V, Stolyarov V V, Valiev R Z, Mukherjee A K. Scr Mater, 2000; 43: 819
[73] Mishra R S, Stolyarov V V, Echer C, Valiev R Z, Mukherjee A K. Mater Sci Eng, 2001; A298: 44
[74] Noda M, Hirohashi M, Funami K. Mater Trans, 2003; 44: 2288
[75] Salishchev G A, Galeyev R M, Valiakhmetov O R, Safiullin R V, Lutfullin R Y,Senkov O N, Froes F H, Kaibyshev O A. J Mater Process Technol, 2001; 116: 265
[76] Patankar S N, Escobedo J P, Field D P, Salishchev G, Galeyev R M,Valiakhmetov O R, Froes F H S. J Alloys Compd, 2002; 345: 221
[77] Tsuji N, Saito Y, Utsunomiya H, Tanigawa S. Scr Mater, 1999; 40: 795
[78] Li B B. Master Thesis, Harbin Institute of Technology, 2011
(李渤渤. 哈尔滨工业大学硕士学位论文, 2011)
[79] Xu B. Master Thesis, Northwestern Polytechnical University, Xi'an, 2007
(徐 斌. 西北工业大学硕士学位论文, 西安, 2007)
[80] Feng A H, Shen J. Scr Mater, submitted
[81] Margolin H, Cohen P. Titanium'80: Science and Technology. Warrendale: TMS, 1980: 1155
[82] Prasad Y V R K, Seshacharyulu T. Mater Sci Eng, 1998; A243: 82
[83] Sagar P K, Banerjee D, Muraleedaran K, Prasad Y V R K. Metall Mater Trans, 1996; 27A: 2593
[84] Zhang Y, Liu J Y, Zhang J W. Chin J Nonferrous Met, 2008; 18: 30
(张艺, 刘俊友, 张建伟. 中国有色金属学报, 2008; 18: 30)
[85] Salishchev G A, Valiakhmetov O R, Galeyev R M. J Mater Sci, 1993; 28: 2898
[86] Imayev R M, Salishchev G A, Senkov O N, Imayev V M, Shagiev M R,Gabdullin N K, Kuznetsov A V, Froes F H. Mater Sci Eng, 2001; A300: 263
[87] Zherebtsov S V, Salishchev G A, Galeyev R M, Valiakhmetov O R, Mironov S Y,Semiatin S L. Scr Mater, 2004; 51: 1147
[88] Valiakhmetov O R, Galeyev R M, Ivan'ko V A, Imayev R M, Inozemtsev A A,Koksharov N L, Kruglov A A, Lutfullin R Y, Mulyukov R R, Nazarov A A,Safiullin R V, Kharin S A. Nanotechnol Russ, 2010; 5: 108
[89] Imayev V M, Salishchev G A, Shagiev M R, Kuznetsov A V, Imayev R M.Scr Mater, 1999; 40: 183
[90] Semiatin S L, Smith P R. Mater Sci Eng, 1995; A202: 26
[91] Wu Y T, Yang C T, Koo C H, Singh A K. Mater Chem Phys, 2003; 80: 339
[92] Emura S, Tsuzaki K, Tsuchiya K. Mater Sci Eng, 2010; A528: 355
[93] Shen J, Huang Y J, Feng A H, Li B B. Chin Pat, ZL201110135507.4, 2011
(沈军, 黄永江, 冯艾寒, 李渤渤. 中国专利, ZL20111013- 5507.4, 2011)
[94] Xie H. Bachelor Thesis, Harbin Institute of Technology, 2012
(解 辉. 哈尔滨工业大学学士学位论文, 2012)
[95] Kim J H, Park C G, Ha T K, Chang Y W. Mater Sci Eng, 1999; A269: 197
[96] Rosenberg Y, Mukherjee A K. Mater Sci Eng, 1995; A192-193: 788
[97] Jobart D, Blandin J J. Mater Sci Eng, 1996; A207: 170
[98] Fu H C, Huang J C, Wang T D, Bampton C C. Acta Mater, 1998; 46: 465
[99] Yang K L, Huang J C, Wang Y N. Acta Mater, 2003; 51: 2577
[100] Wang X, Lu B, Wang J H, Wang J, Wang H W, Chen Y H. Chin J Nonferrous Met, 2010; 20(S1): s289
(王新, 卢 斌, 王娟华, 王 俭, 王红武, 陈永辉. 中国有色金属学报, 2010; 20(专辑1): s289)
[101] Yang R, Hao Y L, Obbard E C, Dong L M, Lu B. Acta Metall Sin, 2010; 46: 1443
(杨 锐, 郝玉琳, Obbard E C, 董利民, 卢 斌. 金属学报, 2010; 46: 1443)
[102] Li S Y. Master Thesis, Harbin Institute of Technology, 2013
(李少雨. 哈尔滨工业大学硕士学位论文, 2013)
文章导航

/

〈 〉