论文

单晶高温合金螺旋选晶过程的数值模拟与实验研究一:引晶段

  • 张 航 许庆彦 孙长波 戚 翔 唐 宁 柳百成
展开
  • 1. 清华大学
    2. 清华大学机械工程系
    3.
    4. 沈阳黎明航空发动机(集团)有限责任公司

收稿日期: 2013-04-25

  修回日期: 2013-09-02

  网络出版日期: 2013-09-04

基金资助

国家重点基础研究发展计划(973);国家自然科学基金;国家科技重大专项;国家重大科技专项

THE SIMULATION AND EXPERIMENTAL STUDIES ON GRAIN SELECTION BEHAVIOR OF SINGLE CRYSTAL SUPERALLOYPARTⅠ. STARTER BLOCK OF GRAIN SELECTOR

Expand

Received date: 2013-04-25

  Revised date: 2013-09-02

  Online published: 2013-09-04

Supported by

;National Science and Technology Major Project

摘要

现代航空发动机及工业燃气轮机的快速发展对单晶叶片的性能提出了更高的要求。选晶器是单晶叶片铸件的重要部件,其关键的结构包括引晶段和螺旋段。本研究从实验及模拟角度对比研究了引晶段的晶粒密度和取向随晶粒生长高度(研究位置距试样底面的高度)的变化规律,并给出了引晶段参数的设计准则。采用EBSD晶体取向成像技术获得了引晶段截面的晶粒形貌和取向极图;采用CA-FD方法,针对单晶定向凝固过程进行数理建模与仿真,实现了凝固过程的三维宏观温度场与微观组织生长的模拟计算。从宏、微观角度解释了定向凝固过程的晶粒竞争演化行为,揭示了引晶段晶粒竞争生长的本质规律,为引晶段设计提供理论支持。

本文引用格式

张 航 许庆彦 孙长波 戚 翔 唐 宁 柳百成 . 单晶高温合金螺旋选晶过程的数值模拟与实验研究一:引晶段[J]. 金属学报, 0 , 0(0) : 0 -0 . DOI: 10.3724/SP.J.1037.2013.00213

Abstract

The rapid development of advanced aero-engine and industry gas turbine requires high performance of single crystal (SX) blade. Spiral selector is very important to produce SX blade, which includes starter block and spiral part. In this research, grain density changing and orientation deviating as the height of grain growth (the distance between section studied and the undersurface of the sample) increasing were studied by the experiment and simulation, and the designing rules for the starter block were given out. EBSD orientation mapping technology was used to get grains’ morphology and orientation. Mathematical and physical models were built for the directional solidification process. Adopting CA-FD method, the 3D macro temperature field of solidification process was calculated as well as grain growth. The properties of grains competitive growth and evolution process during directional solidification in starter block were analyzed based on macro and micro modeling results, and rules for grains competitive growth was explained, which provided theoretical supports for designing starter block.

文章导航

/

〈 〉