论文

DD407/FGH95合金热等静压扩散连接反应层元素互扩展规律: I.扩散连接模型的建

  • 姚瑶 ,
  • 叶建水 ,
  • 董建新 ,
  • 姚志浩 ,
  • 张麦仓 ,
  • 国为民
展开
  • 1)北京科技大学材料科学与工程学院, 北京100083
    2)钢铁研究总院, 北京 100081
姚瑶, 女, 1990年生, 硕士生

收稿日期: 2013-03-04

  修回日期: 2013-06-29

  网络出版日期: 2013-09-11

基金资助

国家重点基础研究发展计划资助项目2010CB631200

ELEMENTS DIFFUSION LAW OF DD407/FGH95 DIFFU-SION BONDING UNDER HOT ISOSTATIC PRESSING: I. Building Diffusion Bonding Model

  • YAO Yao ,
  • YE Jianshui ,
  • DONG Jianxin ,
  • YAO Zhihao ,
  • ZHANG Maicang ,
  • GUO Weimin
Expand
  • 1)School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
    2)Central Iron & Steel Research Institute, Beijing 100081

Received date: 2013-03-04

  Revised date: 2013-06-29

  Online published: 2013-09-11

摘要

建立了热等静压扩散连接的数学模型, 利用DICTRA软件与Thermal-Calc软件相结合的方法计算了不同温度、不同时间热等静压扩散连接界面反应层元素的互扩散规律与相分布情况,并根据计算结果给出了建议的扩散连接工艺范围, 为工艺参数的设计提供了理论依据.计算结果表明: 与时间相比, 温度对扩散连接界面的元素扩散影响更大.针对DD407/FGH95合金系, 扩散连接温度应选择在1120—1210℃的温度区间内.综合考虑扩散连接的元素互扩散区宽度及界面元素富集情况,1120℃时扩散连接的合理扩散时间为3—5 h,1170和1210℃时扩散连接的合理扩散时间为1—3 h.

本文引用格式

姚瑶 , 叶建水 , 董建新 , 姚志浩 , 张麦仓 , 国为民 . DD407/FGH95合金热等静压扩散连接反应层元素互扩展规律: I.扩散连接模型的建[J]. 金属学报, 2013 , 49(9) : 1041 -1050 . DOI: 10.3724/SP.J.1037.2013.00105

Abstract

Turbine platform and blade are two main parts of aero engines and gas turbines.Due to different requirements in practice, platforms are always fabricated by single crystal superalloys, which have high temperature strength and resistance to hot corrosion and oxidation. The platforms employed at relatively lower temperatures can be made of powder superalloys. Therefore there is a great demand for bonding single crystal superalloys to powder superalloys. Because of high content of γ′ forming elements, traditional fusion welding methods employed in bonding the two materials are high susceptibility to cracking. Hot isostatic pressure (HIP) bonding is a preferable technique now to join nickel base superalloys. However, using experimental methods to explore appropriate HIP bonding parameters is time consuming and costly. This work puts forward a calculated method to simulate diffusion process and phase distribution of diffusion couples obtained by HIP diffusion bonding. In this work, the numerical model of HIP diffusion bonding was built, and distribution of elements and phases of DD407/FGH95 diffusion couples under different HIP temperature and bonding time were calculated  with DICTRA and Thermal—Calc software. The simulated results indicated that the appropriate HIP temperature should be chosen between 1120℃ and 1210℃. γ′ in DD407 and FGH95 kept initial concentration under 1120℃ HIP bonding.γ′ in FGH95 began to entirely solute and γ′ in DD407 partly solute under 1170℃ HIP bonding, and under 1210℃ HIP bonding, γ′ in DD407 could solute completely near the interface and partly solute away from the interface. The simulated results also implied that appropriate time for 1120℃ HIP bonding is 3—5 h, 1—3 h for 1170 and 1210℃ HIP bonding.

参考文献

[1] Mao J, Wang W X, Yang W H.  Aviation Eng Maint, 1997; (2): 2

(毛健, 汪武祥, 杨万宏.航空制造工程, 1997; (2): 2)
[2] Klotz U E, Henderson M B, Wilcock I M, Davies S, Janschek P, Roth M, Casser P, Mccolvin G.  Mater Sci Technol, 2005; 21: 218
[3] Atkinson H V, Davies S.   Metall Mater Tans, 2000; 31A: 2981
[4] Borgenstam A, Engstrom A, Hoglund L, Agren J.  J Phase Equilib, 2000; 21: 269
[5] Larsson H, Hoglund L.   Comput Coupl Phase Diagrams Therm, 2009; 33: 495
[6] Anderson J O, Helander T, Hoglund L, Shi P F, Sundman B.  Calphad, 2002; 26: 273
[7] Tancret F.  Comput Mater Sci, 2007; 41: 13
[8] Ojo O A, Tancret F.  Comput Mater Sci, 2009; 45: 388
[9] He Y L, Li L, Huang S G, Vleugels J, Van der Bies O.   Rare Mater, 2007; 26: 492
[10] Engstrom A, Morral J E, Agren J.  Metall Mater Trans, 1994; 25A: 1127
[11] Jiang C, Jin Z P.  Trans Nonferrous Met Soc China, 2000; 10: 158
[12] Campbell C E, Zhao J C, Henry M F.  J Phase Equilib Diffus, 2004; 25: 6
[13] Larsson H, Enstrom A.  Acta Mater, 2006; 54: 2431
[14] Walter C, Hallstedt B, Warnken N.  Mater Sci Eng, 2005; A397: 385
[15] Dayananda M A.   Metall Trans, 1996; 27A: 2504
[16] Loh N L, Sia K Y.   J Mater Process Technol, 1992; 30: 45
[17] Jiao S Y, Dong J X, Zhang M C, Xie X S.  Mater Eng, 2009; (12): 10
(焦少阳, 董建新, 张麦仓, 谢锡善. 材料工程, 2009; (12): 10)
[18] Chen R Z.  Mater Eng, 1995; (8): 3
(陈荣章. 材料工程, 1995; (8): 3)
[19] Henrik S, Henrik L.  Acta Mater, 2004; 52: 4695
[20] Ashworth M A, Jacobs M H, Davies S.  Mater Des, 2000; 21: 351
[21] Orhan N, Aksoy M, Eroglu M.  Mater Sci Eng, 1999; A271: 458
[22] Peng X K, Heness G, Yeung W Y.  J Mater Sci, 1999; 34: 227
[23] Jia J, Tao Y, Zhang Y W.  J Iron Steel Res, 2011; 23: 510
(贾建, 陶宇, 张义文.钢铁研究学报, 2011; 23: 510)
[24] Yan L C, Yan P, Zhao J C.  Powder Metall Ind, 2012; 22: 21
(闫来成, 燕平, 赵京晨. 粉末冶金工程, 2012; 22: 21)
[25] Yan L C, Sun J H, Yan P, Zhao J C.   J Iron Steel Res, 2000; 12: 31

(阎来成, 孙家华, 燕平, 赵京晨. 钢铁研究学报, 2000; 12: 31)

文章导航

/

〈 〉