CONTROL OF STRING SHAPED NON-METALLIC INCLUSIONS OF CaO-Al2O3 SYSTEM IN X80 PIPELINE STEEL PLATES

  • WANG Xinhua ,
  • LI Xiugang ,
  • LI Qiang ,
  • HUANG Fuxiang ,
  • LI Haibo ,
  • YANG Jian
Expand
  • 1)School of Metallurgical and Ecological Engineering, University of Science and Technology Beijing, Beijing 100083
    2)Shougang Technical Research Institute, Beijing 100042

Received date: 2012-08-30

  Revised date: 2013-02-05

  Online published: 2013-05-11

摘要

采用转炉-钢包精炼炉-RH真空精炼-钙处理炼钢工艺生产的X80管线钢板中, 条串状B类夹杂物主要为低熔点CaO-Al2O3系,其成因主要为: (1) 炉外精炼和钙处理后, 钢液中存在许多微小CaO-Al2O3系液态夹杂物, 连铸过程聚集成较大尺寸夹杂物(10-20μm), 轧制过程中变形为大型条串状夹杂物. (2) 尺寸较大的夹杂物在钢液钙处理时, 外表层转变为高熔点CaO, CaS或CaO-CaS系, 但内部仍为低熔点的CaO-Al2O3系, 此类夹杂物在钢板轧制时, 内部仍能够变形, 最终延展为条串状夹杂物. 对X80管线钢板B类夹杂物的控制采用新的策略, 将控制重点由钢液钙处理后去除低熔点CaO-Al2O3系夹杂物, 改为在钙处理前强化去除钢液中夹杂物, 尤其是较大尺寸的夹杂物. 采取新控制策略后, 真空精炼后夹杂物数量大幅度降低, 钙处理效果显著提高, 钢板中检测到的夹杂物全部为高熔点CaO-CaS系夹杂,B类夹杂物评级由以往低于2.0级降低至0级.

本文引用格式

王新华 , 李秀刚 , 李强 , 黄福祥 , 李海波 , 杨建 . X80管线钢板中条串状CaO-Al2O3系非金属夹杂物的控制[J]. 金属学报, 2013 , 49(5) : 553 -561 . DOI: 10.3724/SP.J.1037.2012.00505

Abstract

The string shaped B type non-metallic inclusions in API (American Petroleum Institute) X80 pipeline steel plates, produced by the BOF-LF-RH-Ca treatment steelmaking route, were mainly of CaO-Al2O3 system with lower melting temperatures. The formation reasons are as follows: (1) there existed many small sized liquid inclusions of CaO-Al2O3 system in liquid steel after the secondary refining and Ca treatment. These small inclusions could aggregate to larger ones of 10- 20μm in continuous casting and be deformed into string shaped inclusions in steel plates during rolling. (2) for the larger sized and low melting temperature CaO-Al2O3 inclusions, in Ca treatment, their surface layers could be modified into high melting temperature CaO, CaS or CaO-CaS system, but the centers remained to be CaO-Al2O3 system. During rolling, these inclusions could also be elongated to string typed ones because of their soft CaO-Al2O3 centers. A new strategy for control of B type  inclusions in X80 pipeline steel plates was adopted. The key of the control was shifted from removing low melting temperature inclusions of CaO-Al2O3 system after Ca treatment to remove as much as possible inclusions especially large sized inclusions before the Ca treatment. With the new strategy, the amount of inclusions after RH refining was remarkably decreased and the efficiency of Ca treatment significantly improved. The non-metallic inclusions found in steel plates were all of high melting temperature CaO-CaS system and theseverity of B-type inclusions has been lowered from ≤2.0 to 0.

参考文献

[1] Gatellier D C.  Tetsu-to-Hagane, 1984; 6: 872


[2] Simpson I D, Trit Z S, Moore L G.  Ironmaking Steelmaking, 2003; 30: 158

[3] Carneiro R A, Ratnapuli R C, Lins V C.  Mater Sci Eng, 2003; A357: 104

[4] Tanizawa K, Okumura H.  Proc of the Sixth International Iron and Steel Congress, Nagoya: ISIJ, 1990: 611

[5] Lachmund H, Yongkun X, Klaus H.  Steel Res, 2001; 72: 452

[6] Takahashi D, Kamo M, Kurose Y, Nomura H.  Ironmaking Steelmaking, 2003; 30: 116

[7] Haida O, Emi T, Sanbongi K, Shiraishi T, Fujiwara A.  Tetsu-to-Hagane, 1978; 64: 1538

[8] Holappa L, Helle A S.  J Mater Proc Technol, 1995; 53: 177

[9] Choudhary S K, Ghosh A.  ISIJ Int, 2008; 48: 1552

[10] Numata M, Higuchi Y.  Tetsu-to-Hagane, 2011; 97: 259

[11] Higuchi Y, Numata M, FukagawaS, Shinme K.  ISIJ Int (suppl), 1996; 36: 151

[12] Ye G, Jonsson P, Lund T.  ISIJ Int (suppl), 1996; 36: 105

[13] Holappa L, Hamalainen M, Liukkonen M, Lind M.  Ironmaking Steelmaking, 2003; 30: 111

[14] Lis T.  Metallurgia, 2009; 48: 95

[15] Ito Y, Suda M, Kato Y, Nakato H, Sorimachi K.  ISIJ Int (suppl), 1996; 36: 148

[16] Park J, Kim D, Lee S.  Metall Mater Trans, 2005; 36B: 67

[17] Han Z, Liu L, Lind M, Holappa L.  Acta Metall Sin (Engl Lett), 2009; 19: 1

[18] Lind M, Hollappa L.  Metall Mater Trans, 2010; 41B: 359

[19] Taguchi K, Hideki O. ISIJ Int, 2005; 45: 1572

[20] Vasilij P, Blazenko K, John W.  Hastie Steel Res, 1991; 62: 289

[21] Ye G, Jonsson P, Lund T.  ISIJ Int, 1996; 36: S105

[22] Cho S W, Suito H.  ISIJ Int, 1994; 3: 265

[23] Ohta H, Suito H.  ISIJ Int, 1996; 36: 983

[24] Kushida T, Higuchi Y, Numura M.  Sumitomo Res, 1996; 58(9): 24

[25] Ito Y, Nara S, Kato Y, Suda M.  Tetsu-to-Hagane, 2007; 93: 355

[26] Zhang L.  J Iron Steel Res Inter, 2006; 13: 1

文章导航

/

〈 〉